Effect of alloying elements on liquid metal embrittlement of pure BCC Fe in contact with liquid lead-bismuth eutectic: Experiments and first principles calculation
Source abstract
Abstract
The effects of three alloying elements, i.e., Cr, Al, and Si, on liquid metal embrittlement (LME) of pure Fe (BCC) exposed to oxygen-poor liquid lead-bismuth eutectic (LBE) have been studied using tensile tests and first principles calculation. It is shown that all three elements induce an increase in strength while loss of ductility, and Si has the strongest effect. The LME enhancement sequence is Si>Al>Cr. First principles calculation reveals that the considerable decreases of surface energy and Young’s moduli as well as more directional and localized bonding due to the alloying elements intrinsically cause the LME susceptibility of BCC Fe.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Nuclear materials and radiation effects · Molten salt chemistry and electrochemical processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
2. OECD/NEA, Handbook on lead-bismuth eutectic alloy and lead properties, materials compatibility, thermal-hydraulics and technologies, 2015.
3. Investigation of liquid LBE embrittlement effects on irradiated ferritic/martensitic steels by slow-strain-rate tensile tests10.1016/j.jnucmat.2011.11.036 ↗
4. Effects of temperature and strain rate on the tensile behaviors of SIMP steel in static lead bismuth eutectic10.1016/j.jnucmat.2016.02.032 ↗
5. The role of oxide films in preventing liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic10.1016/j.jnucmat.2018.07.018 ↗
6. Liquid Metal Embrittlement. Mechanics - Microstructure - Corrosion Coupling. Concepts, Experiments
7. Liquid metal embrittlement susceptibility of T91 steel by lead-bismuth10.1016/j.scriptamat.2005.02.027 ↗
8. Initiation of LME Crack In ferritic martensitic steel in liquid lead-Bismuth10.1016/j.jnucmat.2018.09.033 ↗
9. S. Gavrilov, M. Lambrecht, G. Coen, E. Stergar, J. Van den Bosch, PIE of ASTIR: Report on the full set of results of tests on irradiated and non-irradiated specimens, in FP7–212175-GETMAT. 2014, SCK-CEN: Mol, Belgium.
10. Influence of LBE long term exposure and simultaneous fast neutron irradiation on the mechanical properties of T91 and 316L10.1016/j.jnucmat.2016.02.008 ↗
11. Corrosion behavior of steels in flowing lead-bismuth10.1016/S0022-3115(01)00521-9 ↗
12. Corrosion scales on various steels after exposure to liquid lead–bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗
13. Oxide scales formed on Fe–Cr–Al-based model alloys exposed to oxygen containing molten lead10.1016/j.jnucmat.2013.02.044 ↗
14. Influence of composition and microstructure on the corrosion behavior of different Fe-Cr-Al alloys in molten LBE10.1016/j.jnucmat.2011.11.049 ↗
15. Corrosion resistance and microstructural stability of austenitic Fe-Cr-Al-Ni model alloys exposed to oxygen-containing molten lead10.1016/j.jnucmat.2019.06.043 ↗
16. A comparative study on liquid metal embrittlement susceptibility of three FeCrAl ferritic alloys in contact with liquid lead-bismuth eutectic at 350°C10.1016/j.corsci.2021.109346 ↗
17. Liquid metal embrittlement of an Fe10Cr4Al ferritic alloy exposed to oxygen-depleted and -saturated lead-bismuth eutectic at 350°C10.1016/j.corsci.2019.108364 ↗
18. On the LME susceptibility of Si enriched steels10.1016/j.jnucmat.2012.05.017 ↗
19. Multiscale investigation of quasi-brittle fracture characteristics in a 9Cr-1Mo ferritic-martensitic steel embrittled by liquid lead-bismuth under low cycle fatigue10.1016/j.corsci.2015.10.003 ↗
20. Liquid metal embrittlement susceptibility of a high-entropy alloy exposed to oxygen-depleted liquid lead-bismuth eutectic at 250 and 350°C10.1016/j.jnucmat.2019.151859 ↗
21. Comparison of solid metal-metal oxide reference electrodes for potentiometric oxygen sensors in liquid lead-bismuth eutectic operating at low temperature ranges10.1016/j.snb.2015.03.004 ↗
22. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set10.1016/0927-0256(96)00008-0 ↗
23. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set10.1103/PhysRevB.54.11169 ↗
24. From ultrasoft pseudopotentials to the projector augmented-wave method10.1103/PhysRevB.59.1758 ↗
25. Atoms, molecules, solids, and surfaces: Applications of the generalized gradient approximation for exchange and correlation10.1103/PhysRevB.46.6671 ↗
26. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
27. Pathway to Understand Liquid Metal Embrittlement (LME) in Fe-Zn Couple: From Fundamentals toward Application10.1016/j.pmatsci.2021.100798 ↗
28. Atomic-scale investigation of liquid-metal-embrittlement crack-path: revealing mechanism and role of grain boundary chemistry10.1016/j.actamat.2020.116519 ↗
29. The materials science of thin films
30. Nye · 1985
31. Interfacial fracture toughness of transition metal nitrides10.1016/j.surfcoat.2008.05.040 ↗
32. First-principles study of fracture toughness enhancement in transition metal nitrides10.1016/j.surfcoat.2018.10.102 ↗
33. Interfacial stability and electronic properties of Ag/M (M= Ni, Cu, W, and Pd) and Cu/Cr interfaces10.1021/acs.jpcc.8b05920 ↗
34. Cohesion strength and fracture toughness of Mo-TiC interfaces10.1016/j.surfcoat.2019.125158 ↗
35. What is the Young’s Modulus of Silicon?10.1109/JMEMS.2009.2039697 ↗
36. First-principles calculations of mechanical properties of TiC and TiN10.1016/j.jallcom.2009.06.023 ↗
37. Effects of yttrium on mechanical and cohesion properties of zirconium diboride10.1016/j.vacuum.2021.110246 ↗
38. Mechanical properties and dislocation evolution of Cu–Fe interfaces from molecular dynamics simulation10.1016/j.matchemphys.2021.124270 ↗
39. Kittel · 1996 · Vol. 8
40. F.R. De Boer, Cohesion in metals. Transition metal alloys, 1988.
41. Elastic constants of iron from 4.2 to 300 K10.1103/PhysRev.122.1714 ↗
42. Influence of liquid lead and lead-bismuth eutectic on tensile, fatigue and creep properties of ferritic/martensitic and austenitic steels for transmutation systems10.1016/j.jnucmat.2011.04.047 ↗
43. Low cycle fatigue behavior of a modified 9Cr-1Mo ferritic-martensitic steel in lead-bismuth eutectic at 350°C - Effects of oxygen concentration in the liquid metal and strain rate10.1016/j.corsci.2015.02.022 ↗
44. Review of high-temperature wetting and complexion transitions with a critical assessment of their influence on liquid metal embrittlement and corrosion10.5006/1925 ↗
45. Liquid Pb-Bi embrittlement effects on the T91 steel after different heat treatments10.1016/j.jnucmat.2008.02.050 ↗