journal article·2023-07

In-situ measurement of hydrogen entry and hydrogen embrittlement of steel by atmospheric corrosion

Makoto Kawamori, Fumio Yuse

Corrosion Science· Volume 219
Publisher page

Abstract

Hydrogen entry and hydrogen embrittlement of high-strength steel in atmospheric corrosion environment was investigated using an in-situ hydrogen permeation technique and a strain gage method, respectively. The hydrogen concentration increased at the beginning of corrosion and when the corrosion reaction was accelerated, such as when a typhoon approached. The hydrogen embrittlement occurred when the surface hydrogen concentration exceeded the critical hydrogen concentration. It is directly demonstrated that hydrogen embrittlement crack initiation, arrest, and propagation are repeated accompanied with hydrogen entry and release due to environmental changes, leading to final fracture.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. A new model for hydrogen-assisted cracking (hydrogen “embrittlement”)10.1007/BF02642048 ↗
2. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
3. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
4. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
5. Effect of pre-strain on hydrogen embrittlement of high strength steels10.1016/j.msea.2014.07.085 ↗
6. Hydrogen related failure of steels –a new aspect10.1179/026708304225019687 ↗
7. Lattice defects dominating hydrogen-related failure of metals10.1016/j.actamat.2008.06.031 ↗
8. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: Overview10.1016/j.actamat.2018.12.013 ↗
9. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: Localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
10. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
11. Bolt steels used for steel structures10.2355/tetsutohagane1955.88.10_600 ↗
12. Evaluation of delayed fracture property of high strength bolt steels10.2355/isijinternational.52.307 ↗
13. Evaluation of hydrogen embrittlement for high strength steel sheets10.2355/tetsutohagane.95.887 ↗
14. Method for evaluating hydrogen embrittlement of high-strength steel sheets considering press formation and hydrogen existence state in steel10.2355/isijinternational.ISIJINT-2019-822 ↗
15. An evaluation method for hydrogen embrittlement of high strength steel sheets using U-bend specimens10.2355/tetsutohagane.TETSU-2019-036 ↗
16. Estimation of delayed fracture property of steels10.2355/tetsutohagane1955.79.2_227 ↗
17. Evaluation method of delayed fracture property of high strength steels10.2355/tetsutohagane1955.83.7_454 ↗
18. K. Yamakawa, Advances in Delayed Fracture Solution, Iron and Steel Institute of Japan, Tokyo, (1997), 79.
19. Hydrogen entry into steel by atmospheric corrosion10.2355/isijinternational.43.470 ↗
20. Hydrogen absorption into high strength bolts under atmospheric exposure and delayed fracture susceptibility evaluation10.2355/tetsutohagane1955.91.5_478 ↗
21. Effect of corrosion resistance and rust characterization for hydrogen absorption into steel under an atmospheric corrosion condition10.2355/isijinternational.ISIJINT-2015-309 ↗
22. Evaluation of delayed fracture of high strength steel sheets for cyclic corrosion test
23. Distribution of hydrogen occluded in bolts tightened beyond the yield strength and exposed at a seashore site10.2355/tetsutohagane1955.88.12_849 ↗
24. Evaluation of delayed fracture property of outdoor-exposed high strength AISI 4135 steels10.1016/j.corsci.2010.05.038 ↗
25. Steels for high strength bolts with high delayed fracture resistance
26. Super High Strength Bolt “SHTB®”
27. Hydrogen entry into steel during atmospheric corrosion process10.1016/j.corsci.2004.10.006 ↗
28. Evaluation of hydrogen entry into high strength steel under atmospheric corrosion10.1016/j.corsci.2009.11.046 ↗
29. Handbook of Outdoor Exposure Testing, Japan Weathering Test Center, Tokyo, (2007), 16.
30. Hydrogen uptake in high-strength steel corroded in actual use environment and in laboratory condition, and interpretation of diffusive hydrogen in thermal-desorption-spectroscopy-based gas chromatograph, Trans
31. Mechanism and suppression method of hydrogen entry into steel by blasting10.2355/isijinternational.ISIJINT-2022-065 ↗
32. Iwata · Koberunikusu · 2017 · 47 · 17
33. Evaluation of hydrogen absorption into steel in automobile moving environments10.1016/j.corsci.2015.05.049 ↗
34. Evaluation of corrosivity of atmosphere by ACM type corrosion sensor10.3323/jcorr1991.54.375 ↗
35. The mechanism of hydrogen evolution on iron in acid solutions by determination of permeation rates10.1149/1.2426195 ↗
36. A method for determination of the permeation rate of hydrogen through metal membranes10.1149/1.3087209 ↗
37. Electrochemical measurements for hydrogen entry and permeation of steel10.3323/jcorr.63.3 ↗
38. Quantities and distribution of strain-induced vacancies and dislocations enhanced by hydrogen in iron10.1016/j.actamat.2021.116663 ↗
39. Effect of typhoon on the atmospheric corrosion of carbon steel in Okinawa10.3323/jcorr.60.135 ↗
40. Corrosion behavior investigation of weathering steel by using electrical resistance technique10.3323/jcorr.67.292 ↗
41. Problems in measurement methods of hydrogen permeability through steel
42. Function of hydrogen in embrittlement of high-strength steels10.2355/isijinternational.41.590 ↗
43. Improved hydrogen embrittlement resistance of steel by shot peening and subsequent low-temperature annealing10.2355/isijinternational.ISIJINT-2020-463 ↗
44. Visualization of hydrogen in stress and strain fields using SIMS10.2355/isijinternational.ISIJINT-2020-191 ↗
45. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
46. Effects of local stress, strain, and hydrogen content on hydrogen-related fracture behavior in low-carbon martensitic steel10.1016/j.actamat.2021.116828 ↗