Abstract

Combining high-pressure heat treatment (HPHT) and artificial aging synergistically enhances the mechanical properties and corrosion resistance of high-Li-content Al-Cu-Li alloys. This study demonstrates that HPHT increases the solubility of Cu in the matrix, reducing intermetallic phase volume and promoting the precipitation of nanoprecipitates that strengthen the alloy. Additionally, it decreases micro-galvanic corrosion between intermetallic phases and the matrix, lowering the corrosion current density by three orders of magnitude compared to the T6-tempered sample, while also enhancing intergranular corrosion (IGC) resistance. Applying HPHT and artificial aging to high-Li-content Al-Cu-Li alloys effectively addresses the strength-corrosion trade-off.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Influence of the rolling direction on the microstructure, mechanical, anisotropy and gamma rays shielding properties of an Al-Cu-Li-Mg-X alloy10.1016/j.msea.2018.06.074 ↗
2. Effect of aging treatment on precipitation strengthening phase and mechanical properties of Al-Cu-Li Alloy10.1002/adem.202301079 ↗
3. Coarsening kinetics and strengthening mechanisms of core-shell nanoscale precipitates in Al-Li-Yb-Er-Sc-Zr alloy10.1016/j.jmst.2020.05.061 ↗
4. Recrystallization behavior and kinetic analysis of an Al-Cu-Li alloy during hot deformation and subsequent heat treatment10.1016/j.matchar.2024.113640 ↗
5. Lightweight single-phase Al-based complex concentrated alloy with high specific, nature communications10.1038/s41467-024-51387-6 ↗
6. Stress-corrosion cracking characterisation of the advanced aerospace Al-Li 2099-T86 alloy10.1016/j.msea.2016.07.013 ↗
7. Effect of crystal orientations and precipitates on corrosion behavior of Al-Cu-Li single crystals10.1016/S1003-6326(22)66065-5 ↗
8. Effect of age-forming on microstructure, mechanical and corrosion properties of a novel Al-Li alloy10.1016/j.jallcom.2015.03.212 ↗
9. The effect of pre-ageing temperature and retrogression heating rate on the strength and corrosion behaviour of AA715010.1016/j.corsci.2011.08.042 ↗
10. Effects of re-solution and re-aging treatment on mechanical property, corrosion resistance and electrochemical behavior of 2196 Al-Cu-Li alloy10.1016/j.matdes.2021.109662 ↗
11. Influence of aging treatment on corrosion behavior of extruded 2195 Al-Li alloy10.1016/S1003-6326(23)66432-5 ↗
12. Study of localized corrosion in AA2024 aluminium alloy using electron tomography10.1016/j.corsci.2012.02.001 ↗
13. Intermetallic phases in aluminum alloys and their roles in localized corrosion10.1149/2.0931811jes ↗
14. Local dissolution phenomena associated with S phase (Al2CuMg) particles in aluminum alloy 2024-T310.1149/1.1837874 ↗
15. Electrochemical characteristics of intermetallic phases in aluminum alloys10.1149/1.1869984 ↗
16. Cracks propagation mechanism of intergranular corrosion in Al-Cu-Li AA2195 alloys governed by constant relative humidity
17. Influence of thermomechanical treatment on the corrosion behaviour of 2A97 Al-Cu-Li alloy10.1016/j.corcom.2023.10.003 ↗
18. Insights on the Al-Cu-Fe-Mn intermetallic particles induced pitting corrosion of Al-Cu-Li alloy10.1016/j.corsci.2020.109040 ↗
19. Homogenization heat treatment of 2099 Al-Li alloy10.1007/s12598-013-0099-9 ↗
20. Effect of double-step homogenization treatments on the microstructure and mechanical properties of Al-Cu-Li-Zr alloy10.1016/j.msea.2020.139975 ↗
21. Microstructure evolution of the 1469 Al-Cu-Li-Sc alloy during homogenization10.1016/j.jallcom.2014.06.033 ↗
22. Influence of enhanced Li content on the as-cast eutectic phase features and the evolution during homogenization of Al-Cu-Li alloys10.1016/j.jmrt.2023.09.100 ↗
23. Unique strengthening mechanisms of ultrahigh pressure Mg alloys
24. Microstructure evolution and precipitation of Al-12Mg alloy solidified under high pressure10.1016/j.jallcom.2010.06.189 ↗
25. Effect of super-high pressure on microstructure and mechanical properties of Mg97Zn1Y2 alloys10.1016/j.jma.2016.09.001 ↗
26. Microstructural evolution and mechanical strengthening mechanism of the high pressure heat treatment (HPHT) on Al-Mg alloy10.1016/j.jallcom.2016.09.108 ↗
27. Achieving highest Young's modulus in Al-Li by tracing the size and bonding evolution of Li-rich precipitates10.1016/j.jmst.2022.10.052 ↗
28. Microstructure and mechanical properties of Al-Li alloy manufactured by additive friction stir deposition10.1016/j.msea.2023.145753 ↗
29. Enhancing the strength of Sc-containing Al-Cu-Li alloys by modifying the precipitation behavior through plastic deformation and heat treatment10.1016/j.matchar.2023.113558 ↗
30. In-situ growth of corrosion-resistant LDH/ZIF-8 hybrid film on the surface of MAO film based on LA93 alloy by the one-step method10.1016/j.apsusc.2024.160742 ↗
31. Multi-functional superhydrophobic coatings on Mg-Li alloys via SiO2 nano particles assembled surface modification10.1016/j.surfcoat.2024.131568 ↗
32. Construction of multilayer superhydrophobic film on Al alloy and corrosion resistance mechanism10.1016/j.matchemphys.2022.126313 ↗
33. Effects of aging treatment on the mechanical properties and corrosion resistance of an Al-Cu-Mg-Li alloy
34. On the corrosion of a high solute Al-Zn-Mg alloy produced by laser powder bed fusion10.1016/j.corsci.2021.109626 ↗
35. Effect of laser shock peening on corrosion behaviors of ultra-high strength Al-Zn-Mg-Cu alloys prepared by spray forming and ingot metallurgy10.1016/j.corsci.2022.110458 ↗
36. Quantifying intergranular corrosion susceptibility in AA2098-T351 weldments through friction stir welding10.1002/maco.202314245 ↗
37. Solid solubilities of manganese and titanium in aluminum at 0.1 MPa and 2.1 GPa10.1007/BF02670301 ↗
38. A novel atomic mobility model for alloys under pressure and its application in high pressure heat treatment Al-Si alloys by integrating CALPHAD and machine learning10.1016/j.jmst.2024.08.017 ↗
39. Achieving superior high-temperature mechanical properties in Al-Cu-Li-Sc-Zr alloy with nano-scale microstructure via laser additive manufacturing10.1080/21663831.2023.2285388 ↗
40. Microstructure and mechanical properties of cast Al-Li-Mg alloy: role of Cu10.1016/j.jmst.2023.12.076 ↗
41. Uncovering the kinetics of Li-rich clusters and monodisperse core-shell Al3(Zr, Sc) structures in Al-Li-Cu alloys10.1016/j.msea.2023.145393 ↗
42. The effect of thermo-mechanical treatment on the formation of T1 phase and δ′/θ′/δ′ composite precipitate in an Al-Cu-Li-Mg alloy10.1016/j.matchar.2021.111123 ↗
43. First-principle investigation on the interfacial structure evolution of the δ'/θ'/δ' composite precipitates in Al-Cu-Li alloys10.1016/j.jmst.2020.03.065 ↗
44. Addressing the strength-ductility trade-off in a cast Al-Li-Cu alloy-Synergistic effect of Sc-alloying and optimized artificial ageing scheme10.1016/j.jmst.2021.01.036 ↗
45. Effects of coarse Al2CuLi phase on the hot deformation behavior of Al-Li alloy10.1016/j.jallcom.2019.152469 ↗
46. Effect of heat treatment on the microstructure and mechanical properties of cryogenic rolling 2195 Al-Cu-Li alloy10.1016/j.msea.2021.141682 ↗
47. Microstructures and mechanical properties of Al-Li 2198-T8 alloys processed by two different severe plastic deformation methods: a comparative study10.1016/j.msea.2016.10.108 ↗
48. Tailoring precipitate distribution in 2024 aluminum alloy for improving strength and corrosion resistance10.1016/j.jmst.2023.12.055 ↗
49. Localized corrosion at nm-scale hardening precipitates in Al-Cu-Li alloys10.1016/j.actamat.2020.03.006 ↗
50. Time-varying electrochemically heterogeneous entities during the micro-galvanic corrosion associated with nanoscale precipitates in an Al-Cu-Li alloy10.1016/j.corsci.2022.110542 ↗
51. Intergranular corrosion of an Al-Cu-Li alloy: the influence from grain structure10.1016/j.corsci.2022.110845 ↗
52. The influence of grain structure on the corrosion behaviour of 2A97-T3 Al-Cu-Li alloy10.1016/j.corsci.2016.12.005 ↗
53. Role of constituent intermetallic phases and precipitates in initiation and propagation of intergranular corrosion of an Al-Li-Cu-Mg alloy10.1016/j.corsci.2022.110294 ↗