journal article·2024-04

Unraveling the effect of Al2O3-MnS complex inclusion on the pitting corrosion behavior of dual phase steel

Heng Chen, Guosheng Ma, Lin Lu, Yunhua Huang, Xiaogang Li

Corrosion Science· Volume 230
Publisher page

Abstract

Pitting corrosion behavior of dual phase steel triggered by Al 2O 3 -MnS complex inclusion in NaCl solution was investigated. Results indicated that neither micro-defects nor strain fields existed around the insulating Al 2O 3 -MnS inclusion, but an open circular pit was immediately initiated around the inclusion and grew in diameter approaching 200 μm in several minutes. The preferential dissolution of unstable MnS part created local acidic electrolytes promoting the dissolution of Al 2O 3 part and adjacent matrix. The radial diffusion and hydrolysis of Al 3+ acidified the pit solution, resulting in the propagation of circular pit. Finally, the pitting propagation decelerated with the depletion of inclusion.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. On the mechanical heterogeneity in dual phase steel grades: Activation of slip systems and deformation of martensite in DP80010.1016/j.actamat.2019.11.002 ↗
2. Dissolution kinetics of the sulfide-oxide complex inclusion and resulting localized corrosion mechanism of X70 steel in deaerated acidic environment10.1016/j.corsci.2020.108815 ↗
3. Localized attack at inclusions in 42CrMo4 QT steel10.1016/j.electacta.2023.142754 ↗
4. Insight into TiN inclusion induced pit corrosion of interstitial free steel exposed to aerated NaCl solution10.1016/j.jmrt.2021.04.046 ↗
5. Pitting corrosion behavior in advanced high strength steels10.1016/j.jallcom.2014.08.243 ↗
6. Cerium addition to CaS inclusions in stainless steel: Insolubilizing water-soluble inclusions and improving pitting corrosion resistance10.1016/j.corsci.2020.109222 ↗
7. Pit initiation at single sulfide inclusions in stainless steel: I. electrochemical microcell measurements10.1149/1.1474430 ↗
8. Effect of inclusions modified by rare earth elements (Ce, La) on localized marine corrosion in Q460NH weathering steel10.1016/j.corsci.2017.10.001 ↗
9. Pitting and sulphide inclusions in steel10.1016/S0010-938X(74)80047-8 ↗
10. Initial microzonal corrosion mechanism of inclusions associated with the precipitated (Ti, Nb)N phase of Sb-containing weathering steel10.1016/j.corsci.2019.108232 ↗
11. In situ characterization by localized electrochemical impedance spectroscopy of the electrochemical activity of microscopic inclusions in an X100 steel10.1016/j.corsci.2010.11.026 ↗
12. Correlation between active/inactive (Ca, Mg, Al)-Ox-Sy inclusions and localised marine corrosion of EH36 steels10.1016/j.jmrt.2021.06.030 ↗
13. Role of Al2O3 inclusions on the localized corrosion of Q460NH weathering steel in marine environment10.1016/j.corsci.2018.04.007 ↗
14. Stainless-steel corrosion and MnS inclusions10.1038/424389b ↗
15. Pitting corrosion behavior of cerium treated HSLA steel induced by sulfide inclusions in 3.5 wt% NaCl solution10.1016/j.jre.2020.06.015 ↗
16. Mechanism of pitting corrosion induced by inclusions in Al-Ti-Mg deoxidized high strength pipeline steel10.1016/j.micron.2020.102898 ↗
17. New insights into the mechanism of localised corrosion induced by TiN-containing inclusions in high strength low alloy steel10.1016/j.jmst.2021.12.075 ↗
18. In-situ characterization of initial marine corrosion induced by rare-earth elements modified inclusions in Zr-Ti deoxidized low-alloy steels10.1016/j.jmrt.2019.11.080 ↗
19. Influence of inclusions on initiation of pitting corrosion and stress corrosion cracking of X70 steel in near-neutral pH environment10.1016/j.corsci.2018.11.007 ↗
20. Correlation of micro-galvanic corrosion behavior with corrosion rate in the initial corrosion process of dual phase steel10.1016/j.jmrt.2021.09.123 ↗
21. Microstructural influence on the electrochemical corrosion behaviour of dual-phase steels in 3.5% NaCl solution10.1016/j.matlet.2005.03.030 ↗
22. Mechanical and corrosion behavior of plain low carbon dual-phase steels10.1016/j.matdes.2010.06.025 ↗
23. Relationship between microstructure and corrosion behavior in dual-phase steels with various Si content10.1002/srin.201900331 ↗
24. Mechanism of MnS-mediated pit initiation and propagation in carbon steel in an anaerobic sulfidogenic media10.1016/j.corsci.2013.06.049 ↗
25. Thermodynamics of chemical and electrochemical stability of corrosion active nonmetal inclusions10.1134/S0033173207010043 ↗
26. Investigation of inclusion formation in light-weight Fe–Mn–Al steels using automated scanning electron microscope equipped with energy-dispersive X-ray spectroscopy10.1002/srin.201900477 ↗
27. In situ observation on the heterogeneous nucleation of MnS in heavy rail steels with varied aluminum content10.1002/srin.202200684 ↗
28. Correction of artefacts associated with large area EBSD10.1016/j.ultramic.2021.113315 ↗
29. Experimental and numerical study on geometrically necessary dislocations and non-homogeneous mechanical properties of the ferrite phase in dual phase steels10.1016/j.actamat.2011.03.062 ↗
30. Corrosion performance of additively manufactured stainless steel parts: a review
31. A critical review of the recent advances in inclusion-triggered localized corrosion in steel10.1038/s41529-022-00294-6 ↗
32. Formation mechanisms and three-dimensional characterization of composite inclusion of MnS-Al2O3 in high speed wheel steel10.1016/j.matchar.2023.112669 ↗
33. 3D crystal plasticity analyses on the role of hard/soft inclusions in the local slip formation10.1016/j.ijfatigue.2020.105518 ↗
34. Effects of LaAlO3 and La2O2S inclusions on the initialization of localized corrosion of pipeline steels in NaCl solution10.1016/j.scriptamat.2019.10.025 ↗
35. Mechanism of Yttrium composite inclusions on the localized corrosion of pipeline steels in NaCl solution10.1016/j.micron.2019.102820 ↗
36. Ex situ characterization of metallurgical inclusions in X100 pipeline steel before and after immersion in a neutral pH bicarbonate solution10.1016/j.jallcom.2016.02.224 ↗
37. Pitting corrosion of Type 430 stainless steel under chloride solution droplet10.1016/j.corsci.2010.02.031 ↗
38. On the removal of Mn2+ ions by adsorption onto natural and activated Chilean zeolites10.1016/j.mineng.2008.09.007 ↗
39. Occluded solution chemistry control and the role of alloy sulfur on the initiation of crevice corrosion in type 304ss10.1016/S0010-938X(98)00084-5 ↗
40. Localized corrosion of 304 stainless steel triggered by embedded MnS10.1016/j.corsci.2022.110860 ↗
41. SVET, AFM and AES study of pitting corrosion initiated on MnS inclusions by microinjection10.1016/S0010-938X(02)00222-6 ↗
42. Microelectrochemical measurements of the dissolution of single MnS inclusions, and the prediction of the critical conditions for pit initiation on stainless steel10.1149/1.1360205 ↗
43. Effect of MnS inclusion dissolution on carbon steel stress corrosion cracking in fuel-grade ethanol10.1016/j.corsci.2015.03.002 ↗
44. Local pH measurements during pitting corrosion at MnS inclusions on stainless steel10.1149/1.1391164 ↗
45. Influence of the dissolution of MnS inclusions under free corrosion and potentiostatic conditions on the composition of passive films and the electrochemical behaviour of stainless steels10.1016/j.electacta.2005.09.015 ↗
46. The stress corrosion cracking behavior of N80 carbon steel under a crevice in an acidic solution containing different concentrations of NaCl10.1016/j.corsci.2023.111068 ↗
47. SKPFM measured Volta potential correlated with strain localisation in microstructure to understand corrosion susceptibility of cold-rolled grade 2205 duplex stainless steel10.1016/j.corsci.2015.06.035 ↗
48. Effects of strain localization on the corrosion behavior of ultra-fine grained aluminum alloy AA606110.1016/j.corsci.2018.04.023 ↗
49. Pitting corrosion initiated by Al2O3–CaO–CaS inclusions in a 304 stainless steel10.1007/s11663-023-02793-6 ↗
50. Dissolution kinetics of nanodispersed γ-alumina in aqueous solution at different pH: Unusual kinetic size effect and formation of a new phase10.1016/j.jcis.2006.08.016 ↗
51. Pitting corrosion of bare stainless steel 304 under chloride solution droplets10.1149/1.3467850 ↗
52. Unmasking of the temperature window and mechanism for “loss of passivation” effect of a Cr-13 type martensite stainless steel10.1016/j.corsci.2020.108951 ↗
53. Effects of niobium and rare earth elements on microstructure and initial marine corrosion behavior of low-alloy steels10.1016/j.apsusc.2018.12.243 ↗
54. The pitting to uniform corrosion evolution process promoted by large inclusions in mooring chain steels10.1016/j.matchar.2021.111456 ↗
55. New understanding of the effect of hydrostatic pressure on the corrosion of Ni–Cr–Mo–V high strength steel10.1016/j.corsci.2013.04.013 ↗
56. Pitting behaviors of low-alloy high strength steel in neutral 3.5wt% NaCl solution based on in situ observations10.1016/j.jelechem.2020.114056 ↗
57. Role of inclusions in the pitting initiation of pipeline steel and the effect of electron irradiation in SEM10.1016/j.corsci.2017.10.029 ↗
58. Corrosion propagation monitoring using electrochemical noise measurements on carbon steel in hydrogenocarbonated solution containing chloride ions10.1016/j.corsci.2021.109885 ↗
59. Passivity breakdown, pit initiation and propagation of pits in metallic materials – Review10.1016/j.corsci.2014.10.006 ↗
60. Feasible route for the recovery of strategic metals from mixed lithium-ion batteries cathode materials by precipitation and carbonation10.1016/j.cej.2020.127561 ↗
61. Cobalt recovery from mixed Co-Mn hydroxide precipitates by ammonia-ammonium carbonate leaching10.1016/j.mineng.2010.03.006 ↗
62. Transport processes in passivity breakdown-II. Full hydrolysis of the metal ions10.1016/0010-938X(81)90009-3 ↗
63. Ferrous and ferric ion generation during iron electrocoagulation10.1021/es8036669 ↗
64. The initiation of pitting corrosion of stainless steels at oxide inclusions10.1016/0010-938X(92)90137-R ↗