journal article·2024-05

In-situ observation and kinetics study on shrinkage defect corrosion of ductile iron in NaCl solution

Tianqi Chen, Liang Sun, Taike Zhang, Chao Liu, Xuequn Cheng, Xiaogang Li

Corrosion Science· Volume 232
Publisher page

Abstract

The corrosion propagation and kinetics of shrinkage defects in ductile iron in NaCl solution were investigated by in-situ observation based on time-lapse microscopy and confocal laser scanning microscopy. Immersion experiments reveal that shrinkage defects endure notably harsher corrosion compared to the matrix, exhibiting an average depth increase of 52.38μm within a single day. The depth loss rate, a crucial indicator for corrosion kinetics, inversely correlates with the square root of immersion time, underscoring the substantial role of shrinkage defects in expediting early-stage corrosion. The corrosion process predominantly involves longitudinal extension, with sharply shaped defects experiencing the most significant depth increases.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Non-Destructive Testing Techniques · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Corrosion behavior of nickel alloyed and austempered ductile irons in 3.5% sodium chloride10.1016/j.corsci.2010.05.006 ↗
2. In-situ monitoring of the corrosion behaviour of austempered ductile iron (ADI) under cyclic salt spray exposure10.1016/j.corsci.2021.109437 ↗
3. Improved corrosive wear resistance of carbidic austempered ductile iron by addition of Cu10.1016/j.matchar.2020.110577 ↗
4. Wear resistance enhancement of QT700-2 ductile iron crankshaft processed by laser hardening10.1016/j.optlastec.2023.109519 ↗
5. New approach to develop ductile cast iron digital grade for automotive components
6. Microelectrode evaluation of in situ oxidant reactivity and pH variability at new ductile iron and copper coupon surfaces10.1016/j.watres.2023.120352 ↗
7. Failure analysis in buried ductile iron pipelines: a study of leakage in drinking water distribution systems10.1016/j.engfailanal.2023.107361 ↗
8. Long solidification time effect on solution strengthened ferritic ductile iron fatigue properties10.1016/j.ijfatigue.2020.106137 ↗
9. Control of surface graphite degeneration in ductile iron for windmill applications
10. Failure analysis of a clutch wheel for wind turbines with the use of casting process simulation10.1016/j.engfailanal.2022.106159 ↗
11. Graphite compactness degree and nodularity of high-si ductile iron produced via permanent mold versus sand mold casting10.3390/ma15082712 ↗
12. Fatigue life distribution and size effect in ductile cast iron for wind turbine components10.1016/j.engfailanal.2010.07.001 ↗
13. Metallurgical quality of cast iron made from steel scrap and possibilities of its improvement10.3390/met13010027 ↗
14. The importance of SiC in the process of melting ductile iron with a variable content of charge materials10.3390/ma13051231 ↗
15. Influence of chemical composition and cooling rate on chunky graphite formation in thick-walled ductile iron castings
16. The effects of holding time in the heating/pouring unit on the metallurgical quality of spheroidal graphite iron
17. Mechanical and fatigue properties of pearlitic ductile iron castings characterized by long solidification times10.1016/j.engfailanal.2017.06.007 ↗
18. Microscopic characterization of different shrinkage defects in ductile irons and their relation with composition and inoculation process
19. Study of shrinkage porosity in spheroidal graphite cast iron10.1080/13640461.2015.1106783 ↗
20. Fatigue strength estimation of ductile cast irons containing solidification defects10.3390/met13010083 ↗
21. Engineering HEterogeneous Nucleation during Solidification of Multiphase Cast Alloys: an Overview10.3390/met13071154 ↗
22. Study on the austemperability of thin-wall ductile cast iron produced by high-pressure die-casting10.1007/s11665-021-06252-8 ↗
23. Fatigue failure of suspension arm: experimental analysis and multiaxial criterion10.1016/j.engfailanal.2003.12.001 ↗
24. Microscale fatigue mechanisms in high silicon alloyed nodular cast iron10.1016/j.ijfatigue.2022.107402 ↗
25. Research on solution strengthened ferritic ductile iron (SSFDI) structure and properties using different treatment and inoculation materials
26. Analysis of ductile cast iron tensile tests to relate ductility variation to casting defects and material microstructure10.1016/j.msea.2008.09.082 ↗
27. A new energy based highly stressed volume concept to investigate the notch-pores interaction in thick-walled ductile cast iron subjected to uniaxial fatigue10.1016/j.ijfatigue.2022.107491 ↗
28. Effect of the porosity on the fatigue strength of metals10.1111/ffe.13783 ↗
29. Influence of casting defects on the fatigue limit of nodular cast iron10.1016/S0142-1123(03)00141-5 ↗
30. Mechanism of shrinkage in compacted graphite iron and prediction of shrinkage tendency10.3390/ma15238413 ↗
31. Macro-defects characterization in cast CA-6NM martensitic stainless steel10.1016/j.matchar.2016.11.040 ↗
32. A study of the mechanisms and kinetics of the localized corrosion aggravation of ductile iron in a harsh water quality environment10.3390/met12122103 ↗
33. Influence of microshrinkage cavities on the plastic deformation and fracture under tensile loading in ferritic ductile iron
34. The origin of graphite morphology in cast iron10.1016/j.actamat.2022.117660 ↗
35. A structure metric for quantitative assessment of fracture surfaces in 3D conceived based on confocal laser scanning microscopy data10.1016/j.matchar.2022.112369 ↗
36. Confocal laser scanning microscopy: applications in material science and technology10.1007/BF02744951 ↗
37. Compressive, shear, and fracture behavior of CNT reinforced Al matrix composites manufactured by severe plastic deformation10.1016/j.matdes.2016.05.109 ↗
38. Hot oxidation and corrosion behaviour of boiler steel fabricated by wire arc additive manufacturing10.1016/j.matchar.2023.113113 ↗
39. Corrosion of the Fe–25Ni–15Cr superalloy under the combined effects of marine atmospheric exposure and high-temperature oxidation10.1016/j.matchar.2023.112885 ↗
40. Comprehensive analysis of corrosion failure of blast furnace gas pipeline in a steel plant10.1016/j.engfailanal.2023.107651 ↗
41. Modeling the environmental dependence of pit growth using neural network approaches10.1016/j.corsci.2010.05.027 ↗
42. G.S. Frankel, Errata: “pitting corrosion of metals. a review of the critical factors” [J. Electrochem. Soc., 145, 2186 (1998)], J. Electrochem. Soc., 145 (1998) 2970a-2970.10.1149/1.1838748 ↗
43. In situ monitoring of the microstructural corrosion mechanisms of zinc–magnesium–aluminium alloys using time lapse microscopy10.1016/j.corsci.2011.02.043 ↗
44. Pseudo-passive films on cast irons: a strategy to mitigate corrosion by acting directly on microstructure10.1016/j.corsci.2022.110480 ↗
45. Influence of the secondary phase on micro galvanic corrosion of low carbon bainitic steel in NaCl solution10.1016/j.matchar.2018.03.021 ↗
46. Modeling the effect of insoluble corrosion products on pitting corrosion kinetics of metals10.1038/s41529-019-0090-5 ↗
47. Effect of chloride ion content on pitting corrosion of dispersion-strengthened-high-strength steel10.1016/j.corcom.2022.03.005 ↗
48. Influence of cementite coarsening on the corrosion resistance of high strength low alloy steel10.1038/s41529-023-00358-1 ↗
49. Correlation between microstructural evolution and corrosion resistance of hypoeutectic Al–Si–Mg alloy: influence of corrosion product layer10.1016/j.matchar.2022.112276 ↗
50. Time-lapse observation of pitting corrosion in ferritic stainless steel under bipolar electrochemistry control10.1016/j.jelechem.2021.115599 ↗
51. Pitting behavior of SLM 316L stainless steel exposed to chloride environments with different aggressiveness: pitting mechanism induced by gas pores10.1016/j.corsci.2020.108520 ↗
52. The coupling mechanism of shrinkage defects and graphite on the corrosion resistance of ductile iron10.1016/j.corsci.2023.111798 ↗
53. Influence of alloy sulfur content and bulk electrolyte composition on crevice corrosion initiation of austenitic stainless steel10.5006/1.3284838 ↗
54. Passivity breakdown, pit initiation and propagation of pits in metallic materials – review10.1016/j.corsci.2014.10.006 ↗
55. Transport processes in passivity breakdown—II. Full hydrolysis of the metal ions10.1016/0010-938X(81)90009-3 ↗
56. Self-accelerated corrosion of nuclear waste forms at material interfaces10.1038/s41563-019-0579-x ↗