The cyclic oxidation behavior of fourth-generation nickel-based single crystal superalloys with 2–4 wt% Mo content were studied at 900 ℃ and 1100 ℃. At 900 ℃, with the increase of Mo content, the oxide layer accumulates more growth stress, resulting in the interface between the outer oxide layer and the inner oxide layer more prone to crack initiation. At 1100 ℃, the oxidation layer accumulates more growth stress and thermal stress, so the oxidation layer occurs large scale spalling, which is more severe in 4Mo alloy. The results show that the increase of Mo content of alloy promotes the oxidation of containing W-Re alloy, which promotes the volatilization of oxides and the spalling of oxide, decreases the protection of oxide layer, and deteriorates the oxidation resistance of the alloy.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. High-temperature tensile and creep behaviour of Inconel 625 superalloy sheet and its associated deformation-failure micromechanisms10.1016/j.msea.2021.142152 ↗
2. Creep behavior and deformation mechanisms of a novel directionally solidified Ni-base superalloy at 900 degrees C10.1016/j.matchar.2018.12.023 ↗
3. High-temperature creep-deformation behavior of the Ni-based superalloy M96310.1007/s11661-005-0111-6 ↗
4. Fabrication of of single-crystal superalloy hollow blade based on integral ceramic mold10.1016/j.jmatprotec.2019.04.037 ↗
5. Study on creep properties of nickel-based superalloy blades based on microstructure characteristics10.1016/j.jallcom.2021.161710 ↗
6. Oxidation behavior characteristics of an aluminized Ni-based single crystal superalloy CM186LC between 900 degrees C and 1100 degrees C in air10.1016/j.jiec.2013.02.039 ↗
7. Oxidation behavior and mechanism of a Ni-based single crystal superalloy with single alpha-Al2O3 film at 1000 degrees C10.1016/j.apsusc.2017.03.116 ↗
8. Oxidation behavior in static air and its effect on tensile properties of a powder metallurgy EP962NP nickel-based superalloy10.1016/j.jallcom.2022.167795 ↗
9. Effect of surface treatment on high-temperature oxidation behavior of IN 713C10.1007/s11665-018-3621-2 ↗
10. The effect of long-term thermal exposures on the microstructure and properties of CMSX-10 single crystal Ni-base superalloys10.1016/j.msea.2004.04.001 ↗
11. Creep behaviour of Ni-base single-crystal superalloys with various gamma ' volume fraction10.1016/j.actamat.2004.04.028 ↗
12. Microstructure stability of 4th generation single crystal superalloy, PWA 1497, during high temperature creep deformation10.2320/matertrans.MB201003 ↗
13. Creep of CMSX-4 superalloy single crystals: effects of rafting at high temperature10.1016/S1359-6454(99)00217-7 ↗
14. Influence of Mo and Ru additions on the creep behavior of Ni-based single crystal superalloys at 1100 degrees C10.1016/j.msea.2018.04.026 ↗
15. Influence of molybdenum on the creep-properties of nickel-base superalloy single-crystals10.1007/BF02782418 ↗
16. Effect of Mo content on microstructure and stress-rupture properties of a Ni-base single crystal superalloy10.1016/j.pnsc.2016.01.006 ↗
17. The effect of alloying elements on the dislocation climbing velocity in Ni: a first-principles study10.1016/j.actamat.2009.08.019 ↗
18. The effect of volatilisation of refractory metal oxides on the cyclic oxidation of Ni-base superalloys10.1007/s11085-013-9440-9 ↗
19. High temperature oxidation behavior of a novel Ni-Cr-W-Al-Ti superalloy10.1016/j.corsci.2022.110141 ↗
20. Characterization of the oxides formed at 1000 degrees C on the AISI 316L stainless steel - role of molybdenum10.1016/j.matchemphys.2008.04.054 ↗
21. Microstructure and oxidation behavior of Nb-Mo-Si-B alloys10.1016/j.intermet.2005.03.007 ↗
22. Statistics of oxidation resistance of Ni-(0-15)Co-(8-15)Cr-(0-5)Mo-(0-10)W-(3-8)Al-(0-5)Ti-(0-10)Ta-0.1C-0.01B superalloys at 1000 degrees C by compositional variations10.1007/s12598-018-1063-5 ↗
23. Role of volatilization of molybdenum oxides during the cyclic oxidation of high-Mo containing Ni-based single crystal superalloys10.1016/j.corsci.2017.08.025 ↗
24. Oxidation properties for 2nd-5th generation Ni-base single-crystal superalloys at 1023, 1173 and 1373 K10.2320/jinstmet.71.313 ↗
25. Oxidation behavior of the nickel-based superalloy DZ125 at 980 degrees C10.1007/s40195-017-0598-z ↗
26. Effect of Re element on oxidation resistance of Ni3Al-Mo based alloys at 1150 degrees C10.1016/S1003-6326(11)61206-5 ↗
27. Effect of Mo, Ta, and Re on high-temperature oxidation behavior of minor HI doped beta-NiAl alloy10.1016/j.corsci.2015.10.011 ↗
28. High temperature oxidation behavior of Ni-based superalloy Nimonic95 and the effect of pre-oxidation treatment10.1016/j.vacuum.2021.110582 ↗
29. High temperature oxidation behavior of a novel cobalt-nickel-base superalloy10.1016/j.jallcom.2018.06.275 ↗
30. Effect of trace impurity elements on the high-temperature oxidation resistance of a high-purity nickel-based superalloy10.1016/j.corsci.2022.110904 ↗
31. F. Fan, et al., Effect of Mo on the high temperature oxidation behavior of Co-Al-W based alloys, in: Proceedings of the Chinese Materials Congress (CMC 2012), Taiyuan, PR China, 2012.
32. Effect of Al and Cr on the oxidation behavior of nanocrystalline coatings at 1050 degrees C
33. Oxidation of rhenium and a thenium-8 percent titanium alloy in flow environments at oxygen pressures of 1-10 torr and at 800 degrees -1400 degrees C10.1016/0022-5088(68)90117-3 ↗
34. In situ atomic-scale imaging of the metal/oxide interfacial transformation10.1038/s41467-017-00371-4 ↗
35. Effect of Cr content on interdiffusion and Kirkendall pore formation during homogenization of pack-aluminized Ni and Ni-Cr wires10.1016/j.intermet.2018.07.007 ↗
36. Pilling-Bedworth ratio for oxidation of alloys10.1007/s100190050008 ↗
37. The oxidation of metals at high temperatures
38. On the growth strain origin and stress evolution prediction during oxidation of metals10.1016/j.apsusc.2005.07.075 ↗
39. Investigations on the growing, cracking and spalling of oxides scales of powder metallurgy Rene95 nickel-based superalloy10.1016/j.apsusc.2011.06.005 ↗
40. Oxidation of Ni-Cr-Co-Al-Mo-Ti-Re-Ta-W-Ru single crystals at 1000 degrees C in air10.3365/KJMM.2020.58.4.234 ↗
41. The mechanical properties and breakdown of surface oxide films at elevated temperatures
42. Oxidation-induced rhenium evaporation in Ni-based single crystal superalloy thin lamella10.1016/j.scriptamat.2021.114106 ↗
43. Selective oxidation of nanoscale nickel-based superalloys revealed by multi-dimensional electron tomography10.1016/j.matchar.2021.111219 ↗
44. J. Yang, et al., Oxidation behavior of a new ni-base superalloy in air at 850 degrees cand 950 degrees C, in: Proceedings of the International Conference on Materials and Manufacturing (ICMM 2011), Jinzhou, PR China, 2011.10.4028/www.scientific.net/AMR.299-300.466 ↗
45. Effect of Ti addition on high-temperature oxidation behavior of Co-Ni-based superalloy10.1007/s42243-020-00379-z ↗
46. Role of Re in NiAl bond coating on isothermal oxidation behavior of a thermal barrier coating system at 1100 ℃10.1016/j.corsci.2023.111151 ↗
47. Improved oxidation resistance and diffusion barrier behaviors of gradient oxide dispersed NiCoCrAlY coatings on superalloy10.1016/j.vacuum.2010.09.006 ↗
48. Effects of Ni and Cr on the high-temperature oxidation behavior and mechanisms of Co- and CoNi-base superalloys
49. Microstructural evolution of oxidation film on a single crystal nickel-based superalloy at 980 A degrees C10.1007/s11085-017-9787-4 ↗
50. Characterisation of subsurface oxidation damage in Ni based superalloy, RR100010.1179/1743284714Y.0000000541 ↗
51. Oxidation behavior of a cast polycrystalline Ni-base superalloy in air: at 900 and 1000 degrees C10.1007/s11085-007-9066-x ↗
52. High temperature oxidation behavior and mechanism of a new Ni-Co-based superalloy10.1016/j.vacuum.2021.110219 ↗