journal article·2023-11

The hydrogen embrittlement mechanisms and hydrogen induced cracking process of selective laser-melted GH4169

Zhao Xu, Saiyu Liu, Pu Geng, Rongjian Shi, Kewei Gao, Xiaolu Pang

Corrosion Science· Volume 224
Publisher page

Abstract

This study investigates the hydrogen embrittlement sensitivity and brittle failure mechanism of selective laser-melted GH4169 alloy under hydrogen precharged conditions. Fractographic analysis reveals that a high concentration of hydrogen facilitates the formation of small quasi-cleavage steps near the fracture edge. Additionally, hydrogen promotes the migration of {111} planar dislocations, resulting in shear failure of the δ phases and the nucleation of microvoids. These microvoids then propagate, leading to the development of hydrogen-assisted transgranular cracks along the dislocation slip bands. The deformation behaviors of the δ and γ" phases were characterized using high-resolution transmission electron microscopy.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Scanning strategy dependent tensile properties of selective laser melted GH416910.1016/j.msea.2020.139616 ↗
2. Effect of heat treatment on strain hardening ability of selective laser melted precipitation-hardened GH4169 superalloy10.1016/j.matchar.2022.112064 ↗
3. Effect of building direction on anisotropy of mechanical properties of GH4169 alloy fabricated by laser powder bed fusion10.1016/j.msea.2022.144430 ↗
4. Progress in the research and manufacture of GH4169 alloy10.1016/S1006-706X(15)30054-6 ↗
5. Superior creep strength of a nickel-based superalloy produced by selective laser melting10.1016/j.msea.2016.07.061 ↗
6. Investigation of hydrogen embrittlement properties of Ni-based alloy 718 fabricated via laser powder bed fusion10.1016/j.ijhydene.2022.04.045 ↗
7. Effect of heat treatment on microstructural evolution and hardness homogeneity in laser powder bed fusion of alloy 718
8. Effect of trapping and temperature on the hydrogen embrittlement susceptibility of alloy 71810.1016/j.msea.2014.06.015 ↗
9. Effect of δ phase on size effect in microtensile deformation of a nickel-based superalloy10.1016/j.msea.2019.138405 ↗
10. Dependence of creep fracture of inconel 718 on grain boundary precipitates10.1016/S1359-6454(96)00399-0 ↗
11. δ Phase precipitation in Inconel 718 and associated mechanical properties10.1016/j.msea.2016.09.114 ↗
12. Hydrogen-assisted failure of laser melting additive manufactured IN718 superalloy10.1016/j.corsci.2019.108171 ↗
13. Improving the hydrogen embrittlement resistance of a selective laser melted high-entropy alloy via modifying the cellular structures10.1016/j.corsci.2021.109695 ↗
14. Effect of different microstructural features on the hydrogen embrittlement susceptibility of alloy 71810.1016/j.ijhydene.2018.02.088 ↗
15. Hydrogen diffusion coefficients through Inconel 718 in different metallurgical conditions10.1016/j.corsci.2013.11.002 ↗
16. Hydrogen embrittlement in nickel-based superalloy 718: relationship between γ' + γ'' precipitation and the fracture mode10.1016/j.ijhydene.2015.07.053 ↗
17. Multi-scale and spatially resolved hydrogen mapping in a Ni-Nb model alloy reveals the role of the 8 phase in hydrogen embrittlement of alloy 71810.1016/j.actamat.2016.02.053 ↗
18. Hydrogen embrittlement behavior of selective laser-melted Inconel 718 alloy
19. Hydrogen assisted crack initiation and propagation in a nickel-based superalloy10.1016/j.actamat.2016.05.003 ↗
20. In-situ observation of hydrogen induced crack initiation in a nickel-based superalloy10.1016/j.scriptamat.2017.07.006 ↗
21. Tensile mechanical properties and fracture behaviors of nickel-based superalloy 718 in the presence of hydrogen10.1016/j.ijhydene.2018.08.179 ↗
22. Hydrogen-assisted failure in Inconel 718 fabricated by laser powder b e d fusion: the role of solidification substructure in the embrittlement10.1016/j.scriptamat.2021.114308 ↗
23. The combined and interactive effects of orientation, strain amplitude, cycle number, stacking fault energy and hydrogen doping on microstructure evolution of polycrystalline high-manganese steels under low-cycle fatigue10.1016/j.ijplas.2020.102803 ↗
24. Pronounced transition of crack initiation and propagation modes in the hydrogen-related failure of a Ni-based superalloy 718 under internal and external hydrogen conditions10.1016/j.corsci.2019.108186 ↗
25. Meyers · 2008
26. Influence of additive manufacturing by laser powder bed fusion on the susceptibility of Alloy 718 to hydrogen embrittlement10.1080/1478422X.2021.1921336 ↗
27. Effect of homogenization and solution treatments time on the elevated-temperature mechanical behavior of Inconel 718 fabricated by laser powder bed fusion10.1038/s41598-021-81618-5 ↗
28. Effect of heat treatment on the microstructure evolution and mechanical behaviour of a selective laser melted Inconel 718 alloy10.1016/j.jallcom.2021.158613 ↗
29. Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloy10.1016/j.msea.2015.06.021 ↗
30. Microstructural evolution and mechanical properties of Inconel 718 alloy manufactured by selective laser melting after solution and double aging treatments10.1016/j.jallcom.2022.164988 ↗
31. Investigations of MX and γ′/γ″ precipitates in the nickel-based superalloy 718 produced by electron beam melting10.1016/j.msea.2007.07.012 ↗
32. Overlapping of γ′ precipitate variants in Inconel 71810.1016/1044-5803(93)90062-Z ↗
33. Microstructure evolution during thermal aging of Inconel 718
34. Effect of gaseous hydrogen embrittlement on the mechanical properties of additively manufactured CrMnFeCoNi high-entropy alloy strengthened by in-situ formed oxide10.1016/j.msea.2020.140039 ↗
35. Hydrogen enhances strength and ductility of an equiatomic high-entropy alloy
36. Energies de défaut d′empilement et mécanismes de déformation dans les alliages nickel-chrome
37. Stacking fault energies of Ni–Co–Cr alloys
38. Stacking‐fault energy at room temperature of the γ matrix of the MC2 Ni‐based superalloy10.1080/01418619508236228 ↗
39. Hydrogen embrittlement and failure mechanisms of multi-principal element alloys: a review10.1016/j.jmst.2022.01.008 ↗
40. Effect of electrochemical charging on the hydrogen embrittlement susceptibility of alloy 71810.1016/j.actamat.2019.08.020 ↗
41. On the hydrogen embrittlement behavior of nickel-based alloys: alloys 718 and 72510.1016/j.msea.2020.139785 ↗
42. Effects of alloy 718 microstructure on hydrogen embrittlement susceptibility for oil and gas environments10.1080/02670836.2016.1139225 ↗
43. The influence of the processing route on the fragmentation of (Nb,Ti)C stringers and its role on mechanical properties and hydrogen embrittlement of nickel based alloy 71810.1016/j.ijhydene.2021.02.127 ↗
44. On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels10.1016/j.actamat.2010.11.024 ↗
45. The effect of hydrogen on crack propagation behavior and microstructures around cracks in austenitic stainless steels10.2355/isijinternational1966.19.170 ↗
46. Deformation behaviour of γ″ strengthened inconel 71810.1016/0001-6160(88)90139-3 ↗
47. Stacking fault formation in perovskite Ti3AlC carbides in a TiAl based alloy during creep at 800 degrees C10.1016/j.scriptamat.2022.115034 ↗
48. Excellent strength-ductility combination of Cr26Mn20Fe20Co20Ni14 high-entropy alloy at cryogenic temperatures10.1016/j.jmst.2023.01.023 ↗
49. Excellent strength-ductility synergy properties of gradient nano-grained structural CrCoNi medium-entropy alloy10.1016/j.jmst.2021.09.058 ↗
50. X-Ray diffraction measurement of the stacking fault energy reduction induced by hydrogen in an AISI 304 steel10.1016/S1359-6462(97)00332-1 ↗
51. Stacking fault energy decrease in austenitic stainless steels induced by hydrogen pairs formation10.1016/S1359-6462(98)00285-1 ↗
52. Hydrogen-assisted failure of laser melting additive manufactured IN718 superalloy10.1016/j.corsci.2019.108171 ↗
53. Hydrogen transport in nickel-base alloys10.1007/BF02663432 ↗
54. The trapping and transport phenomena of hydrogen in nickel10.1007/BF02643893 ↗
55. Hydrogen trapping phenomena in metals with B.C.C. and F.C.C. crystals structures by the desorption thermal analysis technique10.1016/0257-8972(86)90087-3 ↗
56. Hydrogen-assisted failure in Ni-based superalloy 718 studied under in situ hydrogen charging: the role of localized deformation in crack propagation10.1016/j.actamat.2017.02.059 ↗
57. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
58. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
59. Hydrogen induced grain boundary fracture in high purity nickel and its alloys—Enhanced hydrogen diffusion along grain boundaries10.1016/0001-6160(88)90109-5 ↗