Stress corrosion cracking behavior of selected stainless steels in saturated potash brine solution at different temperatures
Source abstract
Abstract
Abstract The susceptibility of UNS S31603, UNS S32550, UNS S32760, and UNS S32205 to stress corrosion cracking (SCC) in saturated potash brine (KCl) solution was studied using the slow strain rate testing (SSRT) method. Two strain rates (10−6 s-1 and 5 × 10-7 s-1) and three temperatures (25, 50, and 80 °C) were used. UNS S31603 steel showed significant susceptibility to SCC, the severity of which increased with temperature, while the duplex steels exhibited considerable resistance to SCC in KCl solution for all the test conditions. Examination of surfaces of failed specimens suggests a mixture of ductile and brittle fractures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (74)
Show source-provided references
1. Stress corrosion cracking of duplex and super duplex stainless steels in sour environments10.1016/S0010-938X(98)00022-5 ↗
2. Chloride induced stress corrosion cracking of type 304 and 304L stainless steels in air, Zair. to Kankyo10.3323/jcorr1991.52.166 ↗
3. Shirazi · 1996
4. Correlation between electrochemical properties and stress corrosion cracking of super 13Cr under an HTHP CO2 environment10.1039/C8RA04222E ↗
5. In situ pH measurements during localised corrosion of type 316LN stainless steel using scanning electrochemical microscopy10.1023/A:1006517503049 ↗
6. The effect of test temperature on SCC behavior of austenitic stainless steels in boiling saturated magnesium chloride solution10.1016/j.corsci.2006.01.014 ↗
7. Brittle behavior of ductile metals during stress-corrosion cracking
8. Microstructure and stress corrosion cracking behavior of the weld metal in alloy 52-A508 dissimilar welds10.2320/matertrans.M2010294 ↗
9. Design of a novel Mn-based 1 GPa duplex stainless TRIP steel with 60% ductility by a reduction of austenite stability10.1016/j.actamat.2011.04.011 ↗
10. The dependency of the crack growth rate on the loading pattern and temperature in stress corrosion cracking of strain-hardened 316L stainless steels in a simulated BWR environment10.1016/j.corsci.2007.08.022 ↗
11. Stress corrosion cracking of austenitic stainless steels in chloride environment
12. Pit to crack transition in stress corrosion cracking of a steam turbine disc steel10.1016/j.corsci.2003.09.017 ↗
13. Parkins · 2013 · 8
14. SCC evaluation of type 304 and 316 austenitic stainless steels in acidic chloride solutions using the slow strain rate technique10.1016/j.corsci.2003.08.001 ↗
15. Stress corrosion cracking behavior of cold-worked and sensitized type 304 stainless steel using the slow strain rate test10.5006/1.3287668 ↗
16. Stress corrosion cracking of type 321 stainless steels in simulated petrochemical process environments containing hydrogen sulfide and chloride10.1016/j.msea.2005.07.011 ↗
17. Stress corrosion cracking susceptibility of 304L Substrate and 308L weld metal exposed to a salt spray10.3390/ma10020187 ↗
18. Welding corrosion resistant alloys – stainless steel10.1016/B978-0-12-391916-8.00018-2 ↗
19. Effect of weld metal chemistry on stress corrosion cracking behavior of AISI 444 ferritic stainless steel weldments in boiling chloride solution10.1002/maco.201106186 ↗
20. Influence of the heat input and aging treatment on microstructure and mechanical properties of AISI 317 L steel weldments using 0020 robotic–pulsed GMAW10.1007/s00170-019-04621-1 ↗
21. Influence of microstructure on the corrosion resistance of AISI 317L (UNS S31703)10.1590/1980-5373-mr-2016-1107 ↗
22. Gunn · 1997
23. Selection of materials for corrosive environment10.1016/B978-075065924-6/50010-6 ↗
24. Overview Super duplex stainless steels10.1179/mst.1992.8.8.685 ↗
25. Determination of susceptibility to intergranular corrosion of UNS 31803 type duplex stainless steel by electrochemical reactivation method10.1155/2012/478508 ↗
26. Stress corrosion cracking behaviour of dissimilar welding of AISI 310S austenitic stainless steel to 2304 duplex stainless steel
27. A. International · 2005
28. ASTM International · 2004
29. A. International · 2004
30. A. International · 2000
31. Stress corrosion cracking susceptibility of nickel-molybdenum alloys by slow strain rate and immersion testing
32. NACE · 2004 · 1
33. Modeling of the critical pitting temperature between the laboratory-scale specimen and the large-scale specimen10.1149/2.0521807jes ↗
34. Effect of pitting nucleation on critical pitting temperature of 316L stainless steel by nitric acid passivation10.1016/j.corsci.2014.11.018 ↗
35. Study of temperature and chloride concentration effect on pitting corrosion of AISI 316L with immersion method
36. Effect of chromium content and sweep rate on passive film growth on iron-chromium alloys studied by EQCM and XPS10.1016/S0010-938X(01)00126-3 ↗
37. Effect of nitrogen on the corrosion behavior of austenitic stainless steel in chloride solutions10.1016/j.matlet.2005.05.063 ↗
38. Bui · 1986 · 26 · 769
39. Molybdenum effects on pitting corrosion resistance of FeCrMnMoNC austenitic stainless steels10.3390/met8080653 ↗
40. Effect of temperature change rate on the critical pitting temperature for duplex stainless steel10.1007/s10800-009-9863-9 ↗
41. Critical pitting and repassivation temperatures for duplex stainless steel in chloride solutions10.1016/j.electacta.2008.02.047 ↗
42. Loto · 2016 · 147
43. In situ fluorescence imaging of localized corrosion with a pH-sensitive imaging fiber10.1021/ac961025c ↗
44. Direct observation of pitting corrosion evolutions on carbon steel surfaces at the nano-to-micro- scales
45. 2012
46. Syaranamual · 2018
47. Pre-exposure embrittlement and stress corrosion failure in AlZnMg alloys10.1016/0010-938X(76)90065-2 ↗
48. Influence of ferrite phase content on the electrochemical properties of duplex stainless steels10.1590/1980-5373-mr-2016-0546 ↗
49. Relationship of localized corrosion and SCC in oil and gas production environments
50. Chloride stress corrosion cracking in austenitic stainless steel: Assessing susceptibility and structural integrity
51. An ATEM study of oxidation behavior of SCC crack tips in 304L stainless steel in high temperature oxygenated water10.1016/j.jnucmat.2005.07.006 ↗
52. Characterization and perspective of stress corrosion cracking of austenitic stainless steels (type 304 and type 316) in acid solutions using constant load method10.1016/j.corsci.2006.05.011 ↗
53. Discontinuous surface cracks during stress corrosion cracking of stainless steel single crystal10.1016/j.corsci.2011.06.019 ↗
54. Effect of plastic deformation on the corrosion resistance of ferritic stainless steel as a bipolar plate for polymer electrolyte membrane fuel cells10.1016/j.ijhydene.2012.02.127 ↗
55. Film-rupture mechanism of stress corrosion
56. A theory of transgranular stress-corrosion cracking10.1016/0956-7151(91)90138-Q ↗
57. Corrosion behavior of austenitic and duplex stainless steels in thiosulfate- and chloride-containing environments10.5006/1694 ↗
58. Stress corrosion resistance of duplex grades
59. Microstructural simulation of grain growth in two-phase polycrystalline materials
60. Johansson · 1999
61. Effect of heat treatment and microstructure on the corrosion and SCC of duplex stainless steels in H 2 S/Cl − environments10.5006/1.3593951 ↗
62. Influence of the solution-treatment temperature and short aging times on the electrochemical corrosion behaviour of UNS S32520 super duplex stainless steel
63. Effects of nitrogen and tensile direction on stress corrosion cracking susceptibility of ni-free FeCrMnC-based duplex stainless steels10.3390/ma10030294 ↗
64. Comparison of stress corrosion cracking susceptibility of austenitic and ferritic stainless steels in small punch testing10.1016/0022-3115(91)90162-Z ↗
65. The effect of deposition parameters on the structure and mechanical properties of chromium oxide coatings deposited by reactive magnetron sputtering10.3390/coatings8030111 ↗
66. Non-destructive rapid analysis discriminating between chromium(VI) and chromium(III) oxides in electrical and electronic equipment using Raman spectroscopy10.2116/analsci.21.197 ↗
67. Analysis of initial oxidation process of 2205 duplex stainless steel in closed container at high temperature
68. Defect and stress characterization of AlN films by Raman spectroscopy10.1063/1.2404938 ↗
69. Corrosion of stainless steels in chloride solution: an XPS investigation of passive films10.1007/BF00618720 ↗
70. Ford · 2015
71. Corrosion behavior of 304 stainless steel in high temperature, hydrogenated water10.1016/j.corsci.2005.10.014 ↗
72. The mechanism and kinetics of corrosion product release from stainless steel in lithiated high temperature water10.1016/0010-938X(87)90068-0 ↗
73. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
74. Microstructural characterization of SCC crack tip and oxide film for SUS 316 stainless steel in simulated PWR primary water at 320°C10.1080/18811248.2005.9726383 ↗