Improved corrosion resistance of AA5083 after 2 years of exposure in seawater splash and tidal zones: Formation of a protective surface film

Yuanyuan Ji, Yuheng Wu, Weimin Qin, Weixian Jin, Wenbin Hu, Xinjie Yao, Hongqiang Fan, Da-Hai Xia, Bernard Tribollet

Corrosion Science· Volume 260
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Aluminum Alloy Microstructure Properties · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (63)

Show source-provided references
1. Overview of intergranular corrosion mechanisms, phenomenological observations, and modeling of AA508310.5006/1818 ↗
2. Damage micromechanisms of stress corrosion cracking in Al-Mg alloy with high magnesium content10.1016/j.corsci.2021.109343 ↗
3. Elucidation of the trigger for trenching around Al6(Fe, Mn) on AA5083 aluminum alloy in diluted synthetic seawater10.1016/j.corsci.2024.112362 ↗
4. Clarifying the role of Mg2Si and Si in localized corrosion of aluminum alloys by quasi in situ transmission electron microscopy10.5006/3457 ↗
5. SVET study of galvanic corrosion of Al/Mg2Si couple in aqueous solutions at different pH10.1149/2.0671706jes ↗
6. SVET and ToF-SIMS Studies on the galvanic corrosion of β-phase/aluminum couple in aqueous solutions as a function of pH10.1149/1945-7111/ab6a66 ↗
7. A closer inspection of a grain boundary immune to intergranular corrosion in a sensitised Al-Mg alloy10.1016/j.corsci.2018.01.009 ↗
8. Long-term corrosion behavior of the 7A85 aluminum alloy in an industrial-marine atmospheric environment10.1016/j.jmrt.2021.03.085 ↗
9. Corrosion evolution and quantitative corrosion monitoring of Q355 steel for offshore wind turbines in multiple marine corrosion zones10.1016/j.oceaneng.2024.119044 ↗
10. Corrosion and pitting of 6060 series aluminium after 2 years exposure in seawater splash, tidal and immersion zones10.1016/j.corsci.2018.05.036 ↗
11. The effect of dry/wet ratios on the corrosion process of the 6061 Al alloy in simulated Nansha marine atmosphere10.1016/j.corsci.2022.110840 ↗
12. Progress in corrosion science at atomic and nanometric scales10.1016/j.pmatsci.2018.03.001 ↗
13. Effect of dry/wet ratio and pH on the stress corrosion cracking behavior of rusted X100 steel in an alternating dry/wet environment10.1016/j.conbuildmat.2020.120478 ↗
14. On the localized corrosion of AA5083 in a simulated dynamic seawater/air interface—Part 2: effects of wetting time10.1016/j.corsci.2023.111367 ↗
15. Effect of splash amount on corrosion of low-alloy steel in marine splash zone
16. Enhancing the corrosion resistance of low-density steels via Al-rich oxide film formation by grain size optimization10.1016/j.corsci.2025.113331 ↗
17. Localized corrosion in anodized aluminium alloys: The role of constituent particle-induced defects in anodic films10.1016/j.corsci.2025.112961 ↗
18. A study on corrosion of X80 steel in a simulated tidal zone10.1016/j.jmrt.2021.04.014 ↗
19. Corrosion protection of aluminium by ultra-thin atomic layer deposited alumina coatings10.1016/j.corsci.2016.01.021 ↗
20. Micro- and nano-scale intermetallic phases in AA2070-T8 and their corrosion behavior10.1016/j.electacta.2019.05.028 ↗
21. Dealloying-driven local corrosion by intermetallic constituent particles and dispersoids in aerospace aluminium alloys10.1016/j.corsci.2020.108947 ↗
22. Effect of major intermetallic particles on localized corrosion of AA2060-T810.5006/2867 ↗
23. Delamination of near-surface layer on cold rolled AlFeSi alloy during sheet forming10.1016/j.matchar.2014.11.011 ↗
24. The corrosion behaviour of machined AA7150-T651 aluminium alloy10.1016/j.corsci.2017.07.008 ↗
25. Near-surface microstructure on twin-roll cast 8906 aluminum alloy10.1007/s11661-015-2877-5 ↗
26. The effect of manufacturing process induced near-surface deformed layer on the corrosion behaviour of AA2198-T851 Al–Cu–Li alloy10.1080/1478422X.2018.1558932 ↗
27. Intermetallic particles trigger streaking corrosion in AA7075-T610.1038/s41529-025-00631-5 ↗
28. Influence of the altered surface layer on the corrosion of AA508310.1149/2.0321506jes ↗
29. Physical properties obtained from measurement model analysis of impedance measurements10.1016/j.electacta.2020.136747 ↗
30. F. Huet, P. Rousseau, H. Takenouti, SIMAD v.4.1[software], CNRS-Sorbonne Université UMR8235, 〈https://lise-www.sorbonne-universite.fr/en/simad〉, 2024.
31. Unraveling the pressure-induced microstructural origin of enhanced corrosion resistance in a high-strength Al-Si-Cu-Mg alloy10.1016/j.corsci.2025.112972 ↗
32. Rare earth addition powered corrosion resistance of the surface oxide film on GCr15 bearing steel substrate10.1016/j.corsci.2024.112490 ↗
33. Combined electrochemical impedance spectroscopy and X-ray photoelectron spectroscopy analysis of the passive films formed on 5083 aluminium alloy10.1016/j.corsci.2023.111337 ↗
34. Unraveling the role of tensile stress in corrosion and the formation of oxide films on sensitized Al-Mg alloys10.1016/j.corsci.2025.113306 ↗
35. Study on influence of native oxide and corrosion products on atmospheric corrosion of pure Al10.1016/j.corsci.2013.11.027 ↗
36. Electrical properties of the oxide layers formed in simulated primary water environment on steam generator tubes made in Ni based alloy: An EIS analysis10.1016/j.corsci.2025.113206 ↗
37. Application of the impedance model of de Levie for the characterization of porous electrodes10.1016/S0013-4686(02)00081-6 ↗
38. EIS Technique in Passivity Studies: Determination of the Dielectric Properties of Passive Films
39. Constant-phase-element behavior caused by resistivity distributions in films: I. Theory10.1149/1.3499564 ↗
40. Constant-phase-element behavior caused by resistivity distributions in films: II. Applications10.1149/1.3499565 ↗
41. Measurement model for analysis of electrochemical impedance data10.1007/s10008-023-05755-9 ↗
42. Investigation of the passive behavior of a Ni–Cr binary alloy using successive electrochemical impedance measurements10.1016/j.electacta.2020.136531 ↗
43. On the localized corrosion of AA5083 in a simulated dynamic seawater/air interface—Part 1: Corrosion initiation mechanism10.1016/j.corsci.2023.110985 ↗
44. Near-atomic-scale study of the oxide films on the grain boundaries of Al-Mg alloys at the initial stage of corrosion: Experimental investigations and DFT calculations10.1016/j.corsci.2024.112640 ↗
45. On the localized corrosion of AA5083 in a simulated dynamic seawater/air interface—Part 3: effects of sensitization10.1016/j.corsci.2024.111821 ↗
46. Influence of micro-structure on corrosion behavior of a Ni-based superalloy in 3.5% NaCl10.1016/j.electacta.2007.05.043 ↗
47. Localized corrosion of an ultrafine grained Al–4Zn–2Mg alloy produced by cryorolling10.1016/j.corsci.2012.04.009 ↗
48. Nanoscale corrosion investigation of surface nanocrystallized 7150 Al alloy in 3.5 wt% NaCl solution by using FIB-TEM techniques10.1016/j.corsci.2021.110021 ↗
49. Understanding electrochemical behavior and localized corrosion susceptibility in cold sprayed Al-Mg binary deposits with varying Mg contents10.1149/1945-7111/ad97e0 ↗
50. Influence of long-term immersion tests on the electrochemical corrosion behavior of an ultrafine-grained aluminum alloy10.3390/met14121417 ↗
51. Stress corrosion cracking resistant nanostructured Al-Mg alloy with low angle grain boundaries10.1016/j.actamat.2021.117607 ↗
52. Atomistic mechanisms of water vapor–induced surface passivation10.1126/sciadv.adh5565 ↗
53. Characterization of atmospheric corrosion of 2A12 aluminum alloy in tropical marine environment10.1007/s11665-009-9506-7 ↗
54. Study on the free corrosion potential at an interface between an Al electrode and an acidic aqueous NaCl solution through density functional theory combined with the reference interaction site model10.1016/j.electacta.2021.138121 ↗
55. SVET and SIET study of galvanic corrosion of Al/MgZn2 in aqueous solutions at different pH10.1149/2.0861803jes ↗
56. Density functional theory study of influence of oxide thickness and surface alloying on Cl migration within α-Al2O310.1149/1945-7111/ac1cc4 ↗
57. Corrosion susceptibility of passive films on 1060, 2024, and 5083 aluminum alloys: experimental study and first-principles calculations10.1149/1945-7111/accab8 ↗
58. Intermetallic phases in aluminum alloys and their roles in localized corrosion10.1149/2.0931811jes ↗
59. Anodising as pre-treatment before organic coating of extruded and cast aluminium alloys10.1016/j.corsci.2003.10.021 ↗
60. Quasi-“In Situ” analysis of the reactive liquid-solid interface during magnesium corrosion using cryo-atom probe tomography10.1002/adma.202401735 ↗
61. Effect of the chloride on passivity breakdown of Al-Zn-Mg alloy10.1016/j.corsci.2019.108254 ↗
62. Change in oxygen reduction reactivity of intermetallics: a mechanism of the difference in trenching around Al–Fe and Al–Fe–Si particles on AA1050 in NaCl10.1149/1945-7111/acb6ba ↗
63. A review of the electrochemical and galvanic corrosion behavior of important intermetallic compounds in the context of aluminum alloys10.1039/D4RA06070A ↗