Oxidation behaviour of austenitic stainless steel 304HCu in Advanced Ultra Supercritical (AUSC) steam and the efficacy of shot-peening treatment
Source abstract
Abstract
Effect of shot-peening on the oxidation behaviour of alloy 304HCu in controlled advanced ultra-supercritical (AUSC) steam at 650 ◦ C, 31 MPa for 600 h was investigated. Non-shot peened surfaces form thick Fe-rich oxides, undergo internal oxidation, and suffer oxide spallation sooner than those reported in literature. Shot-peened surfaces form a thin, external chromia scale with Mn(Cr,Fe) 2O 4 and MnCr 2O 4 spinels growing above and below it respectively. Shot-peening enhances Cr and Mn diffusivity through grain refinement and increased dislocation density, which aids in resisting chromia scale breakdown, eliminating iron oxides, and preventing oxide spallation. Oxide growth mechanism in AUSC steam is discussed.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Subcritical and Supercritical Water Processes · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. A. Di GianfrancescoThe fossil fuel power plants technology, in: Mater. Ultra-Supercritical Adv Elsevier , Ultra-Supercritical Power Plants , 2017, , 1–49, 10.1016/B978-0-08-100552-1.00001-4.10.1016/B978-0-08-100552-1.00001-4 ↗
2. Advanced ultra-supercritical coal-fired power plant with post-combustion carbon capture: analysis of electricity penalty and CO2 emission reduction
3. Materials research and opportunities in thermal (coal-based) power sector including advanced ultra super critical power plants10.16943/ptinsa/2015/v81i4/48294 ↗
4. Boiler materials for ultra-supercritical coal power plants - steamside oxidation10.1361/105994906X108756 ↗
5. Materials technology for advanced coal power plants
6. Di Gianfrancesco · 2017
7. Development and qualification of materials for Indian advanced ultra-supercritical coal-fired power plant10.1520/MPC20200189 ↗
8. Long term creep properties and microstructure of SUPER304H, TP347HFG and HR3C for A-USC boilers10.1179/174892408X382860 ↗
9. The Development of a new 18-8 austenitic stainless steel (0.lC-18Cr-9Ni-3Cu-Nb, N) with high elevated temperatures strength for fossil power boilers
10. History of power plants and progress in heat resistant steels10.2355/isijinternational.41.612 ↗
11. Coherent precipitation of copper in Super304H austenite steel10.1016/j.msea.2013.06.082 ↗
12. The precipitation strengthening behavior of Cu-rich phase in Nb contained advanced Fe-Cr-Ni type austenitic heat resistant steel for USC power plant application10.1016/j.pnsc.2012.05.002 ↗
13. Effect of Cu content on aging precipitation behaviors of Cu-rich phase in Fe-Cr-Ni alloy10.1016/S1006-706X(10)60101-X ↗
14. Oxidation behaviour of Super 304H stainless steel in supercritical water10.1080/1478422X.2018.1459064 ↗
15. Early oxidation of Super304H stainless steel and its scales stability in supercritical water environments10.1016/j.ijhydene.2016.04.144 ↗
16. The oxidation behaviour of an austenitic steel in deaerated supercritical water at 600–700 °C10.1016/j.matchar.2017.07.023 ↗
17. Investigation on oxidation behavior of super304H and HR3C steel in high temperature steam from a 1000 MW ultra-supercritical coal-fired boiler
18. Theoretical and experimental investigation of the thermochemistry of CrO2(OH)2(g)10.1021/jp0647380 ↗
19. Indication of chromium oxide hydroxide evaporation during
20. M. Yunhai, W. Haibo, F. Rui, L. Qiang, S. KexianThe Effect of Shot Peening on the Oxidation Resistance of Super304H Steels in Water Vapor Cham , Springer International Publishing , 2014 in: Energy Mater2014, , 251–259, 10.1007/978-3-319-48765-6_28..10.1002/9781119027973.ch28 ↗
21. Effect of shot-peening on the oxidation of alloy 800H exposed to supercritical water and cyclic oxidation10.1016/j.corsci.2008.04.008 ↗
22. Managing steam-side oxidation and exfoliation in USC boiler tubes10.31399/asm.amp.2013-01.p023 ↗
23. High-temperature corrosion in fossil fuel power generation: present and future10.1007/s11837-013-0642-z ↗
24. B.A. Pint, The Effect of Shot Peening on Steam Oxidation of Stainless Steel at 600°-650°C, Corros. 2017. (2017) NACE-2017-9426.
25. O. Vohringer, Changes in the state of the material by Shotpeening, in: 3rd Int. Conf. Shotpeening, 1987: pp. 185–204.
26. Review of shot peening processes to obtain nanocrystalline surfaces in metal alloys10.1179/026708408X334087 ↗
27. Effects of surfaces nanocrystallization induced by shot peening on material properties: a review10.3221/IGF-ESIS.07.01 ↗
28. Correlation between the surface coverage of severe shot peening and surface microstructural evolutions in AISI 321: A TEM, FE-SEM and GI-XRD study10.1016/j.surfcoat.2017.11.062 ↗
29. Effect of shot-peening on the oxidation behaviour of boiler steels10.1007/s11085-011-9250-x ↗
30. Dislocation engineering and its effect on the oxidation behaviour10.3184/096034012X13322687148749 ↗
31. High temperature oxidation behaviour of AISI 321 stainless steel with an ultrafine-grained surface at 800 °C in Ar–20 vol% O210.1016/j.corsci.2019.108282 ↗
32. New insights into the effects of surface nanocrystallization on the oxidation of 321 austenitic stainless steel in a humid oxygen environment at 1000 °C10.1016/j.corsci.2018.11.024 ↗
33. M.I. Bass, Steam Oxidation of Shot Peened Austenitic Stainless Steel, University of Birmingham, 2018.
34. Effect of shot peening on the oxidation resistance of TP304H and HR3C steels in water vapor10.1007/s11085-011-9270-6 ↗
35. steam oxidation of super 304h and shot-peened super 304H10.3184/096034012X13316633785757 ↗
36. The effect of shot peening on steam oxidation of 304H stainless steel10.1007/s11085-019-09951-9 ↗
37. S. Yli-Olli, S. Tuurna, S. Penttilä, P. Auerkari, E.C. Zabetta, K. Vänskä, Evaluation of supercritical oxidation resistance of boiler tube materials, in: 7th Int. Conf. Adv. Mater. Technol. Foss. Power Plants, ASM Int., 2014: pp. 791–802.10.31399/asm.cp.am-epri-2013p0791 ↗
38. Oxidation Behavior of Austenitic Steels in Supercritical Water Containing Dissolved Oxygen10.1007/s11665-018-3809-5 ↗
39. Steam oxidation and chromia evaporation in ultrasupercritical steam boilers and turbines10.1149/1.3155442 ↗
40. Chromium volatilization rates from Cr2O3 scales into flowing gases containing water vapor10.1007/s11085-006-9030-1 ↗
41. A review of the oxidation behaviour of structural alloys in steam10.1179/095066010X12646898728165 ↗
42. Theoretical study of steam grown oxides as a function of temperature, pressure and p(O2)10.3184/096034005782750455 ↗
43. Oxidation behaviour of Ni-base superalloy 617 in simulated advanced ultra supercritical (AUSC) steam10.1016/j.corsci.2023.111503 ↗
44. The powder diffraction file: a quality materials characterization database10.1017/S0885715619000812 ↗
45. A review of strain analysis using electron backscatter diffraction10.1017/S1431927611000055 ↗
46. Assessment of local deformation using EBSD: quantification of accuracy of measurement and definition of local gradient10.1016/j.ultramic.2011.02.004 ↗
47. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
48. Geometrically necessary dislocations and strain-gradient plasticity: a few critical issues10.1016/S1359-6462(02)00335-4 ↗
49. The indentation size effect: a critical examination of experimental observations and mechanistic interpretations10.1146/annurev-matsci-070909-104456 ↗
50. Indentation hardness measurements at macro-, micro-, and nanoscale: a critical overview10.1007/s11249-016-0805-5 ↗
51. Comparison of nano-indentation hardness to microhardness10.1016/j.surfcoat.2004.07.108 ↗
52. Revealing the mechanism of extraordinary hardness without compensating the toughness in a low alloyed high carbon steel10.1038/s41598-019-55803-6 ↗
53. Raman spectroscopy of iron oxides and (oxy)hydroxides at low laser power and possible applications in environmental magnetic studies10.1111/j.1365-246X.2009.04122.x ↗
54. Raman spectroscopic study of solid solution spinel oxides, UNLV theses
55. Raman microspectroscopy of some iron oxides and oxyhydroxides10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO;2-B ↗
56. Microstructural understanding of the oxidation of an austenitic stainless steel in high-temperature steam through advanced characterization10.1016/j.actamat.2020.05.010 ↗
57. A high-resolution study of the different surface state effects on the corrosion behaviors of a ferritic steel and an austenitic steel in supercritical water10.1016/j.corsci.2022.110757 ↗
58. H. Tripathy, Measurement And Modelling Of Phase Stability, Thermophysical Properties And Recrystallization Behavior Of Advanced Austenitic Steels, Homi Bhabha National Institute, 2018.
59. On the modeling of the static recrystallization considering the initial grain size effects10.1016/j.msea.2007.08.071 ↗
60. Recrystallization and related annealing phenomena
61. Quantitative study of microstructure evolution and the effect on mechanical properties of Super304H during aging10.1080/09603409.2019.1632508 ↗
62. Interaction of recrystallization and precipitation: the effect of Al3Sc on the recrystallization behaviour of deformed aluminium10.1016/S1359-6454(03)00002-8 ↗
63. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
64. Oxidation of binary FeCr alloys (Fe-2.25Cr, Fe-10Cr, Fe-18Cr and Fe-25Cr) in O 2 and in O 2 + H 2O environment at 600 °c10.1007/s11085-010-9229-z ↗
65. Enhanced internal oxidation as trigger for breakaway oxidation of Fe-Cr alloys in gases containing water vapor10.1016/j.scriptamat.2007.06.058 ↗
66. The effect of water vapor on selective oxidation of Fe-Cr alloys10.1007/s11085-007-9090-x ↗
67. Growth and adherence of chromia based surface scales on Ni-base alloys in high- and low-pO2 gases10.1016/j.msea.2007.05.035 ↗
68. Correlation of high-temperature steam oxidation with hydrogen dissolution in pure iron and ternary high-chromium ferritic steel10.2355/isijinternational.45.1066 ↗
69. Hydrogen in chromium: influence on the high-temperature oxidation kinetics in H2O, oxide-growth mechanisms, and scale adherence10.1023/A:1004610626903 ↗
70. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600 °C10.1016/j.corsci.2005.08.012 ↗
71. Characterization of oxide scales grown on alloy 310S stainless steel after long term exposure to supercritical water at 500 °C10.1016/j.matchar.2016.09.013 ↗
72. Thermodynamics of gas phase chromium species: the chromium oxides, the chromium oxyhydroxides, and volatility calculations in waste incineration processes10.1016/0010-2180(93)90087-J ↗
73. The oxidation of alloys10.1088/0034-4885/39/5/001 ↗
74. Point defects and cation tracer diffusion in (CrxFe1 - x)3 - δO4 spinels10.1016/0167-2738(95)00190-H ↗
75. B.J. SkinnerSection 6: THERMAL EXPANSION, in: 3 Geological Society of America , 1966, , 75–96, 10.1130/MEM97-p75.10.1130/MEM97-p75 ↗
76. Diffusion of iron in Cr2O3: polycrystals and thin films10.1016/j.msea.2004.09.033 ↗
77. The influence of manganese on the High-temperature oxidation of iron-chromium alloys10.1002/maco.19890400403 ↗
78. The effect of manganese additions on the reactive evaporation of chromium in Ni-Cr alloys10.1016/j.scriptamat.2006.01.026 ↗
79. Chromium vaporization from high-temperature alloys10.1149/1.2434690 ↗
80. Effective reduction of chromium-oxy-hydroxide evaporation from Ni-base alloy 69010.1007/s11085-019-09935-9 ↗
81. Corrosion in high-temperature and supercritical water and aqueous solutions: a review10.1016/S0896-8446(03)00031-7 ↗
82. Cycle chemistry and its effect on materials in a supercritical water-cooled reactor: a synthesis of current understanding10.1016/j.corsci.2012.08.006 ↗
83. Evidence for chromium evaporation influencing the oxidation of 304L: the effect of temperature and flow rate10.1023/A:1014877600235 ↗
84. Effect of pressure on the rate of corrosion of metals in high subcritical and supercritical aqueous systems10.1016/j.supflu.2003.09.004 ↗
85. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
86. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
87. L. Qiu, D.A. Guzonas, Prediction of metal oxide stability in supercritical water reactors - Pourbaix versus Ellingham, in: 3rd Canada-China JointWorkshop Supercrit. Water-Cooled React. CCSC-2012, Zian, China, 2012. http://inis.iaea.org/search/search.aspx?orig_q=RN:49101514.
88. Oxidation kinetics and phase evolution of a Fe-16Cr alloy in simulated SOFC cathode atmosphere10.1016/j.jpowsour.2005.09.056 ↗
89. Diffusion in Fe-Ni-Cr alloys with an F.C.C. lattice10.1016/0025-5416(85)90069-2 ↗
90. Self-diffusion in austenitic Fe-Cr-Ni alloys10.1088/0305-4608/10/3/009 ↗
91. Influence of temperature on the oxidation behavior of an austenitic steel in deaerated supercritical water10.1002/maco.201709705 ↗
92. Alloy oxidation III: multiphase scales10.1016/B978-0-08-100101-1.00007-8 ↗
93. Thermodynamic assessment of high-temperature oxidation of Fe-Cr alloys in air10.1007/s10789-005-0087-z ↗
94. Cracking and spalling of protective oxide layers10.1016/0921-5093(89)90731-4 ↗
95. J. Armitt, R. Holmes, M.I. Manning, D.B. Meadowcroft, E. Metcalfe, Spalling of steam-grown oxide from superheater and reheater tube steels. Technical planning study 76-655. Final report, U.S. Department of Energy, 1978. https://doi.org/10.2172/5047517.10.2172/5047517 ↗
96. Effects of grain size, cold working, and surface finish on the metal-dusting resistance of steels10.1023/A:1018888321213 ↗
97. On the role of dislocations in bulk diffusion10.1016/0001-6160(57)90127-X ↗
98. Oxidation of alloys I
99. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
100. First study of manganese diffusion in Cr2O3 polycrystals and thin films by SIMS10.1080/14786430601120462 ↗