Abstract
Internal nitridation of IN617 was investigated during creep rupture at 1000 °C. The results indicated that internal nitridation seriously deteriorated creep properties. Various nitrides including π phase, AlN , Cr 2 N and TiN were found. Stable AlN and TiN precipitated inside grains and distributed widely. Less stable π phase and Cr 2 N only precipitated at the high-energy boundaries with sufficient N and Cr concentrations. Nitridation occurred all over the cross-section (8.9 mm thick) near the fracture surface of the creep specimen ruptured under 16 MPa. It suggested that creep aggravated internal nitridation because of providing continuous crack paths for nitrogen penetration.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Nuclear Materials and Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Assessment of the design effects on the structural performance of the Printed Circuit Heat Exchanger under very high temperature condition10.1016/j.nucengdes.2020.110713 ↗
2. Creep deformation behavior of inconel 617 alloy in the temperature range of 650 °C to 800 °C10.1007/s11661-020-06066-8 ↗
3. Image-based creep-fatigue damage mechanism investigation of Alloy 617 at 950 °C10.1016/j.msea.2016.10.050 ↗
4. Creep crack growth behavior of alloys 617 and 800H in air and impure helium environments at high temperatures
5. Hydrogen production using high temperature nuclear reactors: efficiency analysis of a combined cycle10.1016/j.ijhydene.2015.11.190 ↗
6. Cyclic stress response and fracture behaviors of alloy 617 base metal and weld joints under LCF loading10.1155/2015/207497 ↗
7. Temperature effect on the creep behavior of alloy 617 in air and helium environments10.1016/j.nucengdes.2013.11.050 ↗
8. Oxidation behaviour of an Alloy 617 in very high-temperature air and helium environments10.1016/j.ijpvp.2007.11.010 ↗
9. K. Natesan, A. Purohit, S.W. Tam. Materials Behavior of in HTGR Environments, Argonne National Laboratory (ANL), 2003. Report; NUREC/CR-6824.
10. Corrosion of high temperature metallic materials in VHTR10.1016/j.jnucmat.2009.03.029 ↗
11. Microstructural investigation of Alloy 617 corroded in high-temperature helium environment10.1016/j.nucengdes.2013.11.051 ↗
12. The effect of helium environment on the creep rupture properties of Inconel 617 at 1000°C10.1007/BF02658525 ↗
13. Effects of grain refinement on internal oxidation of Alloy 61710.1016/j.jnucmat.2010.05.013 ↗
14. Microstructure and phase-stability of INCONEL alloy 61710.1007/BF02643879 ↗
15. Microstructural Investigation of alloy 617 creep-ruptured at high temperature in a helium environment10.1016/j.jmst.2013.09.024 ↗
16. Material characterization of Ni base alloy for very high temperature reactor10.1016/j.jmst.2013.09.022 ↗
17. Effect of alloying element on mechanical and oxidation properties of Ni-Cr-Mo-Co alloys at 950 °C10.1016/j.nucengdes.2016.09.025 ↗
18. Oxidation and creep failure of alloy 617 foils at high temperature10.1016/j.jnucmat.2008.04.021 ↗
19. Assessment of creep damage models in the prediction of high-temperature creep behaviour of Alloy 61710.1016/j.ijpvp.2019.103974 ↗
20. Tensile deformation behavior and microstructure evolution of Ni-based superalloy 61710.1016/j.jnucmat.2014.08.003 ↗
21. Oh, Chang H. Development of a Supercritical Carbon Dioxide Brayton Cycle: Improving VHTR Efficiency and Testing Material Compatibility, Idaho National Laboratory (INL), 2006. Report; INL/EXT-06–01271.10.2172/911276 ↗
22. ANTARES: the HTR/VHTR project at framatome ANP10.1016/j.nucengdes.2005.10.030 ↗
23. Surface recrystallization and its effect on oxidation of superalloy C26310.1016/j.corsci.2017.09.020 ↗
24. Formation and compensation of internal stresses during internal nitridation of nickel-base alloys10.1016/S0921-5093(00)01670-1 ↗
25. Internal nitridation of Ni-based alloys during high-temperature corrosion by nitrogen10.1002/(SICI)1527-2648(199912)1:3/4<194::AID-ADEM194>3.0.CO;2-N ↗
26. Internal nitridation of nickel-base alloys. Part I: behavior of binary and ternary alloys of the Ni-Cr-Al-Ti system10.1023/A:1018843612011 ↗
27. Internal nitridation of nickel-base alloys. Part II: behavior of quaternary Ni-Cr-Al-Ti alloys and computer-based description10.1023/A:1018895628849 ↗
28. Internal nitridation of Ni-Cr-Al alloys
29. High-temperature nitridation of Ni-Cr alloys10.1007/BF02647747 ↗
30. Thermodynamic characteristics and numerical modeling of internal nitridation of nickel base alloys10.1002/maco.200303727 ↗
31. Oxidation-nitridation of Ni-Cr-Al alloys10.1590/S1516-14392004000100003 ↗
32. Damage mechanisms during very high cycle fatigue of a coated and grit-blasted Ni-based single-crystal superalloy10.1016/j.ijfatigue.2020.105962 ↗
33. Creep behavior and microstructure evolution of Ni-based alloy IN617 at 1000 °C10.1016/j.matchar.2022.111837 ↗
34. Creep deformation of alloys 617 and 276 at 750–950 ◦C10.1016/j.msea.2009.05.029 ↗
35. Effect of thermo-mechanical processing on microstructure and creep properties of the foils of alloy 61710.1016/j.jnucmat.2009.02.029 ↗
36. Morphological changes of carbides during creep and their effects on the creep properties of Inconel 617 at 1000 ◦C10.1007/BF02654716 ↗
37. Creep behaviour and long-term creep life extrapolation of alloy 617 for a very high temperature gas-cooled reactor
38. Effect of trace impurities in helium on the creep behavior of Alloy 617 for very high temperature reactor applications10.1016/j.jnucmat.2006.12.028 ↗
39. Biaxial thermal creep of Inconel 617 and Haynes 230 at 850 and 950°C10.1016/j.jnucmat.2013.12.016 ↗
40. Creep deformation and rupture behavior of Alloy 61710.1016/j.engfailanal.2015.07.041 ↗
41. Investigation of creep rupture properties in air and He environments of alloy 617 at 800 °C10.1016/j.nucengdes.2016.04.042 ↗
42. Effects of Zr and Co on the microstructure and mechanical properties of NiAl-based alloys10.1016/j.jallcom.2021.160815 ↗
43. Microstructure and mechanical properties of FeCoCrNiMnAlx high-entropy alloys prepared by mechanical alloying and hot-pressed sintering10.1016/j.jallcom.2018.10.168 ↗
44. Enhanced strength and ductility in a high-entropy alloy via ordered oxygen complexes10.1038/s41586-018-0685-y ↗
45. Formation and stability of a nitride with the structure of beta manganese in Ni-Cr-N ternary system10.1007/BF02647321 ↗
46. Internal nitridation behavior during long-term creep in a nickel-base superalloy10.1016/S1359-6462(01)00953-8 ↗
47. Influence of Ti addition on oxidation behavior of Ni-Cr-W-based superalloys10.1016/j.corsci.2021.109882 ↗
48. High temperature oxidation behavior of conventional and Nb-modified MAR-M246 Ni-based superalloy10.1007/s11661-021-06252-2 ↗
49. Simultaneous internal oxidation and nitridation of Ni-Cr-Al alloys10.1023/A:1010304026026 ↗
50. Oxidation behavior of a single-crystal Ni-base superalloy in air at 900, 1000 and 1100°C10.1007/s11085-006-9016-z ↗
51. Influence of Nb addition on the oxidation behavior of novel Ni-base superalloy10.1016/j.corsci.2021.109436 ↗
52. (n.d.). 8.2 Diffusion tables for C, N, and O in metals10.1007/10390457_90 ↗
53. The transport of oxygen to the advancing internal oxide front during internal oxidation of nickel-base alloys at high temperature10.1016/0167-2738(84)90166-8 ↗
54. Passivity and inhibition during the oxidation of metals at elevated temperatures10.1016/S0010-938X(65)80003-8 ↗
55. High temperature aging and corrosion study on alloy 617 and alloy 23010.1115/1.4002819 ↗
56. Effect of composition and process variables on Nb(C,N) precipitation in niobium microalloyed austenite10.1179/mst.1987.3.3.197 ↗