Hydrogen absorption and embrittlement of martensitic medium-Mn steels
Source abstract
Abstract
In the present study, the H absorption and the H embrittlement (HE) resistance of medium (3–7 wt%) Mn martensitic steels were investigated. When the specimens were electrochemically H-charged, 7 wt% Mn specimen had the highest diffusible H content because of the highest reversible H trap density. When the diffusible H content was identical, HE resistance deterioration arose due to the Mn addition, probably caused by grain boundary decohesion and H segregation into the grain boundaries. However, this condition was improved by B addition due to the enhanced grain boundary cohesion and the suppression of H segregation into the grain boundaries.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. A review of the physical metallurgy related to the hot press forming of advanced high strength steel
2. A review on hot stamping10.1016/j.jmatprotec.2010.07.019 ↗
3. Hot stamping of ultra-high strength steel parts10.1016/j.cirp.2017.05.007 ↗
4. Critical review of automotive hot-stamped sheet steel from an industrial perspective10.1080/02670836.2018.1425239 ↗
5. An introduction to medium-Mn steel: metallurgy, mechanical properties and warm stamping process10.1016/j.matdes.2016.01.048 ↗
6. Introduction to a third-generation automobile steel and its optimal warm-stamping process10.1115/1.4031636 ↗
7. Comparison of the hot-stamped boron-alloyed steel and the warm-stamped medium-Mn steel on microstructure and mechanical properties10.1016/j.msea.2016.10.045 ↗
8. Investigation on microstructure and martensitic transformation mechanism for the warm-stamped third-generation automotive medium-Mn steel10.1115/1.4037017 ↗
9. Microstructure evolution and enhanced performance of a novel Nb-Mo Microalloyed medium Mn-fabricated by low-temperature rolling and warm stamping10.1016/j.matdes.2017.08.047 ↗
10. Research on the warm-hot forming process and its performance evaluation for the third-generation automobile steel
11. Warm stamping technology of the medium manganese steel10.1002/srin.201700360 ↗
12. Ultrahigh strength-ductile medium-Mn steel auto-parts combining warm stamping and quenching & partitioning10.1080/02670836.2019.1591029 ↗
13. The effects of process temperatures on the microstructure and tensile properties of warm-stamped nb-bearing medium-mn steel10.1007/s11661-019-05570-w ↗
14. Evaluations of tensile properties as a function of austenitizing temperature and springback by V-bending testing in medium-Mn steels10.1016/j.msea.2020.139534 ↗
15. Investigation of the thermo-mechanical properties of hot stamping steels10.1016/j.jmatprotec.2006.03.233 ↗
16. Investigation of the high strength steel Al-Si coating during hot stamping operations10.4028/www.scientific.net/KEM.410-411.289 ↗
17. Hot forming of boron steels using heated and cooled tooling for tailored properties10.1016/j.jmatprotec.2012.06.028 ↗
18. Description of microstructures and mechanical properties of boron alloy steel in hot stamping process10.1016/j.jmapro.2015.11.008 ↗
19. Hot stamping of boron steel sheets with tailored properties: a review10.1016/j.jmatprotec.2015.09.023 ↗
20. Comparative effects of Al-Si and galvannealed coatings on the properties of resistance spot welded hot stamping steel joints10.1016/j.jmatprotec.2016.03.021 ↗
21. Enhancing hydrogen embrittlement resistance of lath martensite by introducing nano-films of interlath austenite10.1007/s11661-015-3009-y ↗
22. The mechanism of hydrogen embrittlement in intecritically annealed medium Mn TRIP steel10.1016/j.actamat.2016.04.038 ↗
23. Effect of gaseous hydrogen charging on the tensile properties of standard and medium Mn X70 pipeline steels
24. Hydrogen embrittlement of intercritically annealed medium-Mn steel (0.1C–5Mn) under different rolling conditions
25. Effect of intercritical annealing time on hydrogen embrittlement of warm-rolled medium Mn steel10.1016/j.msea.2018.04.100 ↗
26. Austenite morphology and resistance to hydrogen embrittlement in medium Mn transformation-induced plasticity steel10.1016/j.scriptamat.2019.05.011 ↗
27. Effect of reverted austenite fraction on hydrogen embrittlement of TRIP-aided medium Mn steel (0.1C–5Mn)10.1016/j.engfailanal.2019.01.018 ↗
28. Enhancing the resistance to hydrogen embrittlement of Al-containing medium-Mn steel through heavy warm rolling10.1016/j.scriptamat.2019.02.009 ↗
29. Research progress and prospect of medium manganese steel
30. Hydrogen embrittlement behavior of high strength low carbon medium manganese steel under different heat treatments10.1016/j.ijhydene.2019.10.103 ↗
31. Hydrogen embrittlement susceptibility of 0.1C–5Mn medium-Mn steel under different treatment conditions
32. Influence of microstructural morphology on hydrogen embrittlement in a medium-Mn steel Fe-12Mn-3Al-0.05C
33. Insight into hydrogen effect on a duplex medium-Mn steel revealed by in-situ nanoindentation test10.1016/j.ijhydene.2019.04.290 ↗
34. Intercritical annealing temperature dependence of hydrogen embrittlement behavior of cold-rolled Al-containing medium-Mn steel10.1016/j.ijhydene.2019.06.204 ↗
35. Impact of precipitates on the hydrogen embrittlement behavior of a V-alloyed medium-manganese austenitic stainless steel10.1016/j.jmrt.2020.09.085 ↗
36. A review of research status of hydrogen embrittlement for automotive advanced high-strength steels
37. Homogeneous elasto-plastic deformation and improved strain compatibility between austenite and ferrite in a co-precipitation hardened medium Mn steel with enhanced hydrogen embrittlement resistance10.1016/j.ijplas.2020.102805 ↗
38. J. Wang, W. Hui, Z. Xie, Z. Wang, Y. Zhang, X. Zhao, Hydrogen embrittlement of a cold-rolled Al-containing medium-Mn steel: Effect of pre-strain, 45 (2020) 22080–22093. http://doi.org/10.1016/j.jihydene.2020.05.239.10.1016/j.ijhydene.2020.05.239 ↗
39. Influence of hydrogen and annealing process on the microstructural evolution and fracture micromechanisms of medium Mn steel: An in-situ TEM investigation10.1016/j.ijhydene.2020.05.142 ↗
40. Effect of relative humidity on mechanical degradation of medium Mn steels
41. Effect of prestrain on hydrogen-induced delayed cracking for medium Mn steels10.1007/s11665-020-04706-z ↗
42. Dependence of hydrogen embrittlement mechanisms on microstructure-driven hydrogen distribution in medium Mn steels10.1016/j.actamat.2019.11.029 ↗
43. Effect of heat treatment processes on hydrogen embrittlement in hot-rolled medium Mn steels10.1016/j.ijhydene.2020.04.241 ↗
44. Influence of microstructure on hydrogen embrittlement in hot-rolled medium Mn steels10.1016/j.msea.2020.139147 ↗
45. The possibility of enhanced hydrogen embrittlement resistance of medium-Mn steels by addition of micro-alloying elements10.1016/j.matchar.2020.110386 ↗
46. Critical role of Lüders banding in hydrogen embrittlement susceptibility of medium Mn steels10.1016/j.scriptamat.2020.08.025 ↗
47. Evaluation of hydrogen effect on the fatigue crack growth behavior of medium-Mn steels via in-situ hydrogen plasma charging in an environmental scanning electron microscope10.1016/j.jmst.2020.12.069 ↗
48. Hydrogen embrittlement of medium mn steels
49. Vanadium or copper alloyed duplex lightweight steel with enhanced hydrogen embrittlement resistance at room temperature10.1016/j.msea.2021.141347 ↗
50. Current challenges and opportunities toward understanding hydrogen embrittlement mechanisms in advanced high-strength steels: a review
51. The potential significance of tempering treatment in alleviating the hydrogen embrittlement susceptibility of a hot-rolled and intercritically annealed medium-Mn steel10.1016/j.engfailanal.2020.104969 ↗
52. Dependence of hydrogen embrittlement on annealing time in medium-Mn steels10.1108/ACMM-07-2021-2521 ↗
53. Effects of rolling and heat treatment on hydrogen embrittlement in medium-Mn steel10.1016/j.matlet.2021.130784 ↗
54. New Insights to Understand the Influence of Nb/Mo on Hydrogen Embrittlement Resistance of Warm-Rolled Medium-Mn Steels10.1007/s11665-021-06405-9 ↗
55. Interactions of nanoprecipitates, metastable austenite, and Lüders banding in an ultra-low carbon medium Mn steel with abnormal strength dependence of hydrogen embrittlement10.1016/j.mtla.2022.101380 ↗
56. Effect of Mo and Nb on mechanical properties and hydrogen embrittlement of hot-rolled medium-Mn steels10.1016/j.msea.2022.143108 ↗
57. Hydrogen embrittlement of steels10.1146/annurev.ms.08.080178.001551 ↗
58. The role of hydrogen and other interstitials in the mechanical behavior of metals
59. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
60. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and "quasi-cleavage" fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
61. Hydrogen embrittlement of automotive advanced high-strength steels10.1007/s11661-012-1280-8 ↗
62. Effect of prior austenite grain size on hydrogen delayed fracture of hot-stamped boron martensitic steel10.1007/s11661-019-05523-3 ↗
63. Effect of specific microstructures on hydrogen embrittlement susceptibility of a modified AISI 4130 steel10.1016/j.ijhydene.2021.08.147 ↗
64. Effect of grain size on the susceptibility of martensitic steel to hydrogen-related failure10.1080/09500830500482316 ↗
65. Effects of hydrogen pressure and prior austenite grain size on the hydrogen embrittlement characteristics of a press-hardened martensitic steel10.1016/j.ijhydene.2021.05.005 ↗
66. Development of a press-hardened steel suitable for thin slab direct rolling processing10.1007/s11661-014-2613-6 ↗
67. ASTM (2014). ASTM B962–13 Standard test methods for density of compacted or sintered powder metallurgy (PM) products using Archimedes' principle. https://dx.doi.org/10.1520/B0962–13.10.1520/B0962-13 ↗
68. Quantitative investigation on deep hydrogen trapping in tempered martensitic steel10.1016/j.jallcom.2020.157218 ↗
69. Comparison of the dislocation density in martensitic steels evaluated by some X-ray diffraction methods10.2355/isijinternational.50.875 ↗
70. Study of the electrochemical permeation of hydrogen in iron10.1016/j.corsci.2008.10.024 ↗
71. An overview on hydrogen uptake, diffusion and transport behavior of ferritic steel, and its susceptibility to hydrogen degradation
72. Effective hydrogen diffusion coefficient for CoCrFeMnNi high-entropy alloy and microstructural behaviors after hydrogen permeation10.1016/j.ijhydene.2020.02.012 ↗
73. Accelerated diffusion of hydrogen along grain boundaries in nickel10.1016/1359-6454(95)00446-7 ↗
74. Grain size and grain-boundary effects on diffusion and trapping of hydrogen in pure nickel10.1016/j.actamat.2012.09.004 ↗
75. ISO (2014). ISO 17081 Method of measurement of hydrogen permeation and determination of hydrogen uptake and transport in metals by an electrochemical technique. http://iso.org/standard/40480.html.
76. The effect of pre-strain on the resistance to hydrogen embrittlement in 316L austenitic stainless steel10.2320/matertrans.M2014036 ↗
77. Estimation of martensite feature size in a low-carbon alloys steel by microtexture analysis of boundaries10.1016/j.micron.2014.09.008 ↗
78. A model for the microstructure behaviour and strength evolution in lath martensite10.1016/j.actamat.2015.07.018 ↗
79. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
80. The thermodynamics of liquid dilute iron alloys10.1179/msc.1974.8.1.298 ↗
81. Impact of Mn on the solution enthalpy of hydrogen in austenitic Fe-Mn alloys: A first-principles study10.1002/jcc.23742 ↗
82. Effects of solid solution and grain-boundary segregation of Mo on hydrogen embrittlement in 32MnB5 hot-stamping steels10.1016/j.actamat.2021.116661 ↗
83. Machine learning assisted design of FeCoNiCrMn high-entropy alloys with ultra-low hydrogen diffusion coefficients10.1016/j.actamat.2021.117535 ↗
84. Cold cracks in fillet weldments of 600 MPa tensile strength low carbon steel and microstructural effects on hydrogen embrittlement sensitivity and hydrogen diffusion10.3365/KJMM.2021.59.1.21 ↗
85. Quantification of hydrogen trapping in multiphase steels: Part I - point traps in martensite10.1016/j.actamat.2020.05.007 ↗
86. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
87. Microstructural influence on hydrogen permeation and trapping in steels10.1016/j.matdes.2019.107605 ↗
88. Effect of Nb-Ti multi-microalloying on the hydrogen trapping efficiency and hydrogen embrittlement susceptibility of hot-stamped boron steel10.1016/j.msea.2019.138788 ↗
89. Mitigation of hydrogen embrittlement in ultra-high strength lath martensitic steel via Ta microalloying10.1016/j.matdes.2021.110090 ↗
90. Hydrogen trapping in high strength martensitic steel after austenitized at different temperatures10.1016/j.ijhydene.2013.08.121 ↗
91. Dislocation density within lath martensite in Fe-C and Fe-Ni alloys10.2355/isijinternational.43.1475 ↗
92. Determination of dislocation density by electron backscatter dfifraction and X-ray line profile analysis in ferrous lath martensite10.1016/j.matchar.2015.11.014 ↗
93. Determination of Ms temperature in steels: a Bayesian neural network model10.2355/isijinternational.42.894 ↗
94. Dependence of martensite start temperature on fine austenite grain size10.1016/j.scriptamat.2007.09.017 ↗
95. Austenite grain size and the martensite-start temperature10.1016/j.scriptamat.2008.11.043 ↗
96. Hydrogen trapping models in steel10.1007/s11663-000-0032-0 ↗
97. Effect of boron on the grain boundary segregation of phosphorus and intergranular fracture in high-purity Fe-0.2 pct P-B alloys10.1007/BF02660870 ↗
98. Effects of hot stamping and tempering on hydrogen embrittlement of a low-carbon boron-alloyed steel10.3390/ma11122507 ↗
99. Effects of titanium content on hydrogen embrittlement susceptibility of hot-stamped boron steels10.1016/j.jallcom.2017.12.004 ↗
100. Influence of inclusions on hydrogen-induced delayed cracking in hot stamping steels10.1007/s42243-019-00312-z ↗