Abstract

The susceptibility of multipass flux-cored arc welds of STSs 308 L and 316 L to hydrogen embrittlement (HE) was investigated at various temperatures. Cracks predominantly initiated and propagated along the δ-ferrite in the interdendritic region at 25 °C. δ-ferrite served as preferred hydrogen trap sites, and the δ/γ boundary became the stress concentration site. At −100 °C, STSs 308 L and 316 L exhibited high susceptibility to HE owing to strain-induced martensite formation, providing additional hydrogen trap sites and dislocation accumulation. Despite strain-induced martensite actively transformed at −196 °C, the HE disappeared owing to the sluggish diffusion of hydrogen to stress-concentrated areas.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Effect of low-temperature on mechanical behavior for an AISI 304 austenitic stainless steel10.1016/j.msea.2017.11.003 ↗
2. Low-temperature fatigue of 316L and 316LN austenitic stainless steels10.1007/BF02665004 ↗
3. Hydrogen environment embrittlement of stable austenitic steels10.1016/j.ijhydene.2012.08.071 ↗
4. Effects of shielding gases on the weldability of laser welded austenitic stainless steel10.5781/JWJ.2022.40.6.8 ↗
5. T-joint fillet laser welding of high-strength stainless steel for curtain wall frames10.5781/JWJ.2022.40.6.4 ↗
6. Effects of hydrogen on fatigue crack growth behavior of austenitic stainless steels10.1016/j.ijhydene.2008.02.067 ↗
7. Influence of machining-induced martensite on hydrogen-assisted fracture of AISI type 304 austenitic stainless steel10.1016/j.ijhydene.2011.05.133 ↗
8. Hydrogen embrittlement of catholically hydrogen-precharged 304L austenitic stainless steel: Effect of plastic pre-strain10.1016/j.ijhydene.2014.04.122 ↗
9. Hydrogen effects in austenitic stainless steels10.1016/0921-5093(90)90348-7 ↗
10. Hydrogen embrittlement and hydrogen diffusion behavior in interstitial nitrogen-alloyed austenitic steel10.1016/j.ijhydene.2021.07.084 ↗
11. Effect of strain-induced martensite on hydrogen environment embrittlement of sensitized austenitic stainless steels at low temperatures10.1016/S1359-6454(98)00136-0 ↗
12. Hydrogen-assisted fatigue crack growth of AISI 316L stainless steel weld10.1016/j.corsci.2008.08.016 ↗
13. Effect of ultrasonic power on the microstructure and properties of 304 stainless steel welded joints through cold metal transfer welding assisted with ultrasonication10.1007/s12540-023-01419-5 ↗
14. Growth morphologies and primary solidification modes in a dissimilar weld between a low-alloy steel and an austenitic stainless steel10.3390/met8040284 ↗
15. Precipitation of sigma and chi phases in δ-ferrite of Type 316FR weld metals10.1016/j.matchar.2013.10.003 ↗
16. Kinetic model to investigate the effect of cooling rate on δ-ferrite behavior and its application in continuous casting of AISI 304 stainless steel10.1007/s12540-021-01118-z ↗
17. Enhancement of hardness and yield strength induced by cu-rich phase and its effect at cryogenic temperature on gas tungsten arc welds of ferrous medium-entropy alloy10.1007/s12540-022-01376-5 ↗
18. Development and evaluation of stainless steel-base flux-cored wires for 9% nickel steel10.5781/JWJ.2022.40.5.1 ↗
19. Effect of hydrogen on the microstructure, mechanical properties and phase transformations in austenitic steels10.1016/0022-3115(89)90530-8 ↗
20. The effect of pre-straining and δ-ferrite on the embrittlement of 304L stainless steel by hydrogen10.1016/0010-938X(93)90261-E ↗
21. Effects of delta ferrite on hydrogen embrittlement of austenitic stainless steel welds10.1016/S0010-938X(98)00083-3 ↗
22. Effect of δ-ferrite in welded ER308 and ER316 microstructure on hydrogen embrittlement10.1016/j.ijhydene.2023.01.025 ↗
23. Fatigue crack growth of AISI 304 stainless steel welds in air and hydrogen10.1016/j.msea.2004.02.018 ↗
24. Hydrogen induced ductility losses in austenitic stainless steel welds10.1007/BF02655194 ↗
25. Tensile behaviour of type 304 austenitic stainless steels in hydrogen atmosphere at low temperatures10.1179/026708301773002509 ↗
26. Effect of nickel equivalent on hydrogen gas embrittlement of austenitic stainless steels based on type 316 at low temperatures10.1016/j.actamat.2008.03.022 ↗
27. Role of hydrogen and temperature in hydrogen embrittlement of equimolar CoCrFeMnNi high-entropy alloy10.1007/s12540-020-00752-3 ↗
28. Hydrogen uptake in 316L stainless steel: Consequences on the tensile properties10.1016/j.corsci.2005.11.004 ↗
29. Temperature dependency of hydrogen embrittlement in thermally H-precharged STS 304 austenitic stainless steel10.1007/s12540-022-01232-6 ↗
30. A study on mechanical properties of austenitic stainless steel welds using arctig welding10.5781/JWJ.2022.40.4.7 ↗
31. Tensile and microstructural behaviors of austenitic stainless steel GTA welds for cryogenic application10.5781/JWJ.2020.38.4.10 ↗
32. Mechanism of (Mg,Al,Ca)-oxide inclusion-induced pitting corrosion in 316L stainless steel exposed to sulphur environments containing chloride ion10.1016/j.corsci.2012.09.044 ↗
33. Effect of Prestrain on Hydrogen Embrittlement Susceptibility of EH 36 Steels Using In Situ Slow-Strain-Rate Testing10.1007/s12540-018-00221-y ↗
34. The detrimental effect of hydrogen at dislocations on the hydrogen embrittlement susceptibility of Fe-CX alloys: An experimental proof of the HELP mechanism10.1016/j.ijhydene.2017.12.109 ↗
35. Impact of precipitates on the hydrogen embrittlement behavior of a V-alloyed medium-manganese austenitic stainless steel10.1016/j.jmrt.2020.09.085 ↗
36. Dieter · 1976
37. Stacking fault energies of seven commercial austenitic stainless steels10.1007/BF02641927 ↗
38. Stacking fault energy and deformation mechanisms in Fe-xMn-0.6C-yAl TWIP steel10.1016/j.msea.2016.08.106 ↗
39. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe–Mn–C alloys10.1016/j.msea.2004.01.059 ↗
40. Temperature dependent deformation mechanisms of a high nitrogen-manganese austenitic stainless steel
41. The effect of strain-induced martensite transformation on strain partitioning and damage evolution in a duplex stainless steel with metastable austenite10.1016/j.msea.2021.141173 ↗
42. Low cycle fatigue behavior and failure mechanism of a dual-phase steel10.1016/j.msea.2008.09.011 ↗
43. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe-18Mn-1.5AI-0.6C TWIP steel10.2355/isijinternational.49.1952 ↗
44. Observation of hydrogen diffusion channel and hydrogen trap in 304 austenitic stainless steel10.1016/j.matlet.2021.129453 ↗
45. Effect of hydrogen trapping on hydrogen permeation in a 2205 duplex stainless steel: role of austenite–ferrite interface10.1016/j.corsci.2022.110332 ↗
46. Effect of pre-strain on microstructure and hydrogen embrittlement of K-TIG welded austenitic stainless steel10.1016/j.corsci.2018.12.018 ↗
47. Effects of hydrogen and microstructure on tensile properties and failure mechanism of 304L K-TIG welded joint10.1016/j.msea.2018.08.045 ↗
48. Study of the hydrogen diffusion and segregation into Fe–C–Mo martensitic HSLA steel using electrochemical permeation test10.1016/j.jpcs.2010.07.017 ↗
49. Effective hydrogen diffusion coefficient for CoCrFeMnNi high-entropy alloy and microstructural behaviors after hydrogen permeation10.1016/j.ijhydene.2020.02.012 ↗
50. Hydrogen-induced cracking at grain and twin boundaries in an Fe–Mn–C austenitic steel10.1016/j.scriptamat.2011.12.015 ↗
51. Criteria for determining hydrogen compatibility and the mechanisms for hydrogen-assisted, surface crack growth in austenitic stainless steels10.1016/j.engfracmech.2015.12.023 ↗