Effect of NaCl-rich environment on internal corrosion for Ti60 alloy at 600 °C
Source abstract
Abstract
The morphologies and compositions of internal oxides on Ti60 alloy after corrosion under solid NaCl in H 2O+O 2 at 600 °C have been studied by TEM. The results show that microstructure has an effect on the internal corrosion process. The partial pressure of Cl 2 was found to be higher inside the β strip and at the β phase/α platelet boundary, which promotes the corrosion process in α s grains located inside the β strip. Our results confirm that the internal oxides do not originate from the oxidation of chlorides. Titanium depletion caused by the Cl attack promotes oxidation of the matrix.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Synergistic effect of NaCl and water vapor on the corrosion of 1Cr-11Ni-2W–2Mo-V steel at 500-700 degrees C10.1023/A:1018854202982 ↗
2. Corrosion behavior of pure Cr with a solid NaCl deposit in O-2 plus water vapor10.1023/A:1004690518225 ↗
3. Influence of Cr content on the corrosion of Fe-Cr alloys: the synergistic effect of NaCl and water vapor10.1023/A:1023083309041 ↗
4. Corrosion behavior of a sputtered K38G nanocrystalline coating with a solid NaCl deposit in wet oxygen at 600 to 700 degrees C10.1023/A:1016072726338 ↗
5. Experimental and chemo-mechanical analysis of hot corrosion influence on creep properties of DD6 single crystal superalloy in molten NaCl salt10.1016/j.engfracmech.2021.108194 ↗
6. Influence of the oxygen partial pressure on the high temperature corrosion of 38Ni–34Fe–25Cr alloy in presence of NaCl deposit10.1007/s11085-013-9397-8 ↗
7. Study of titanium alloy Ti6242S oxidation behaviour in air at 560 degrees C: effect of oxygen dissolution on lattice parameters10.1016/j.corsci.2019.06.004 ↗
8. Investigation on the oxidation mechanism of titanium10.3891/acta.chem.scand.12-0239 ↗
9. Effect of microstructure on oxygen rich layer evolution and its impact on fatigue life during high-temperature application of alpha/beta titanium10.1016/j.actamat.2016.01.058 ↗
10. Oxidation and oxygen diffusion in Ti-6al-4V alloy: improving measurements during sims analysis by rotating the sample10.1007/s11085-013-9360-8 ↗
11. Put, STEM-EELS identification of TiOXNY, TiN, Ti2N and O, N dissolution in the Ti2642S alloy oxidized in synthetic air at 650 °C10.1016/j.corsci.2019.03.037 ↗
12. Diffusion of H and D in TiO2:suppression of internal fields by isotope10.1063/1.322206 ↗
13. Influence of water vapour on the isothermal oxidation behaviour of TiAl at high temperatures10.1016/S0921-5093(00)01967-5 ↗
14. Influence of water vapour on the oxidation behaviour of titanium aluminides10.1016/S0966-9795(01)00104-2 ↗
15. On the influence of water vapour on the oxidation behaviour of pure Ti10.1016/j.corsci.2006.06.030 ↗
16. NaCl-induced accelerated oxidation of a Titanium alloy10.1007/BF00614242 ↗
17. Corrosion behavior of pure ti under a solid NaCl deposit in a wet oxygen flow at 600 degrees C10.3390/met6040072 ↗
18. Experimental and theoretical study for hot corrosion behavior of network structured TiBw/TA15 composite with NaCl film at 800 °C10.1016/j.corsci.2022.110540 ↗
19. Corrosion behavior of Ti60 alloy coated with a solid NaCl deposit in O-2 plus water vapor at 500-700 degrees C10.1023/A:1018864216554 ↗
20. Effect of streaming water vapor on the corrosion behavior of Ti60 alloy under a solid NaCl deposit in water vapor at 600 degrees C10.1016/j.corsci.2019.108177 ↗
21. Corrosion behavior of Ti60 alloy under a solid NaCl deposit in wet oxygen flow at 600 degrees C10.1038/srep29019 ↗
22. NaCl induced corrosion of Ti-6Al-4V alloy at high temperature10.1016/j.corsci.2016.04.016 ↗
23. Degradation mechanism of Ti-6Al-2Sn-4Zr-2Mo-Si alloy exposed to solid NaCl deposit at high temperature10.1016/j.corsci.2020.108611 ↗
24. NaCl-induced high-temperature corrosion of beta 21S Ti alloy10.1007/s11085-017-9775-8 ↗
25. The effects of chlorides hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
26. The mechanisms of hot salt stress corrosion cracking in titanium alloy Ti-6Al-2Sn-4Zr-6Mo10.1016/j.corsci.2018.02.025 ↗
27. Effect of powder surface state on microstructure and tensile properties of a novel near alpha-Ti alloy using hot isostatic pressing10.1016/j.msea.2017.08.096 ↗
28. A study of epitaxial growth behaviors of equiaxed alpha phase at different cooling rates in near alpha titanium alloy10.1016/j.actamat.2016.10.012 ↗
29. On the influence of processing parameters on microstructural evolution of a near alpha titanium alloy10.1016/j.msea.2011.09.064 ↗
30. Characterization of high-temperature deformation behavior of as-cast Ti60 titanium alloy using processing map10.1016/j.msea.2013.01.008 ↗
31. Effect of processing parameters on hot deformation behavior and microstructural evolution during hot compression of as-cast Ti60 titanium alloy10.1016/j.msea.2013.07.086 ↗
32. The role of crystallographic and geometrical relationships between alpha and beta phases in an alpha/beta titanium alloy10.1016/S1359-6454(03)00179-4 ↗
33. Effect of pre-hot salt corrosion on hot salt corrosion fatigue behavior of the TC11 titanium alloy at 500 °C10.1016/j.ijfatigue.2022.107055 ↗
34. AgCl-induced hot salt stress corrosion cracking in a titanium alloy10.1016/j.corsci.2021.109497 ↗
35. The influence of a KCl-rich environment on the corrosion attack of 304 L: 3D FIB/SEM and TEM investigations10.1016/j.corsci.2021.109315 ↗
36. Oxidation of Fe-2.25Cr-1Mo in presence of KCl(s) at 400 °C – crack formation and its influence on oxidation kinetics10.1016/j.corsci.2019.108234 ↗
37. One dimensional wormhole corrosion in metals10.1038/s41467-023-36588-9 ↗
38. Direct diffusion through interpenetrating networks: oxygen in titanium10.1103/PhysRevLett.107.045504 ↗
39. Initial stages of the HCl-induced
40. Estimation of grain boundary diffusivity in near-α titanium polycrystals10.1016/j.scriptamat.2011.06.015 ↗
41. Lütjering · 2007 · 45
42. Literature survey on diffusivities of oxygen, aluminum, and vanadium in alpha titanium, beta titanium, and in rutile10.1007/BF02628396 ↗