The effect of surface grinding on the stress corrosion cracking initiation of 316LN stainless steel in 600 °C supercritical CO2
Source abstract
Abstract
The effect of surface grinding on the stress corrosion cracking initiation of 316LN stainless steel in 600 °C supercritical CO 2 was studied through constant extension rate tensile test. The ground surface exhibited much higher oxidation resistance than the polished surface as the deformation layer can greatly enhance the diffusion of active elements and promote the formation of more protective oxide scale. Moreover, the intergranular cracking was effectively suppressed on the ground surface as the ingress of oxidant along the original grain boundary was inhibited.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. A review of research and development of supercritical carbon dioxide Brayton cycle technology in nuclear engineering applications10.1016/j.nucengdes.2020.110767 ↗
2. State of the art overview material degradation in high-temperature supercritical CO2 environments10.1016/j.pmatsci.2023.101107 ↗
3. Review of supercritical CO2 power cycle technology and current status of research and development10.1016/j.net.2015.06.009 ↗
4. Corrosion of 9-12Cr ferritic–martensitic steels in high-temperature CO210.1016/j.corsci.2016.01.009 ↗
5. Carburisation of ferritic Fe–Cr alloys by low carbon activity gases10.1016/j.corsci.2011.05.013 ↗
6. Corrosion and carburization behaviour of Ni-xCr binary alloys in a high-temperature supercritical-carbon dioxide environment10.1007/s11085-017-9811-8 ↗
7. Mechanical and corrosion response of 316SS in supercritical CO210.1007/s11085-021-10026-x ↗
8. Corrosion and carburization behavior of chromia-forming heat resistant alloys in a high-temperature supercritical-carbon dioxide environment10.1016/j.corsci.2015.07.007 ↗
9. Corrosion of a stainless steel and nickel-based alloys in high temperature supercritical carbon dioxide environment10.1016/j.corsci.2012.11.041 ↗
10. Alloys SS316 and Hastelloy-C276 in supercritical CO2 at high temperature10.1007/s11085-015-9589-5 ↗
11. The role of active elements in the oxidation behaviour of high temperature metals and alloys
12. Initial oxidation and chromium diffusion. I. Effects of surface working on 9–20 % Cr steels10.1016/j.corsci.2003.09.004 ↗
13. High-resolution characterization of the internal and external oxidation of austenitic alloys in supercritical water10.1016/j.scriptamat.2021.113814 ↗
14. Effect of machining on oxide development in type 316L stainless steel in high-temperature hydrogenated water10.1016/j.corsci.2021.109444 ↗
15. Effect of surface preparation on the corrosion of austenitic stainless steel 304L in high temperature steam and simulated PWR primary water10.1016/j.corsci.2011.12.007 ↗
16. Effect of surface machining on the corrosion behaviour of 316 austenitic stainless steel in simulated PWR water10.1016/j.corsci.2017.06.019 ↗
17. A high-resolution study of the different surface state effects on the corrosion behaviors of a ferritic steel and an austenitic steel in supercritical water10.1016/j.corsci.2022.110757 ↗
18. Effect of surface modification on the corrosion resistance of austenitic stainless steel 316L in supercritical water conditions10.1016/j.supflu.2013.05.002 ↗
19. Effect of shot-peening on the oxidation of alloy 800H exposed to supercritical water and cyclic oxidation10.1016/j.corsci.2008.04.008 ↗
20. The surface grinding-induced oxide scale exfoliation of an austenitic alloy in supercritical CO210.1016/j.corsci.2023.111615 ↗
21. Corrosion behavior of a new alumina-forming duplex stainless steel with different surface treatment in supercritical carbon dioxide10.1016/j.surfcoat.2023.129619 ↗
22. Effect of surface finish on high-temperature oxidation of steels in CO2, supercritical CO2, and air10.1007/s11085-019-09938-6 ↗
23. Effect of surface finishing on the oxidation characteristics of a Fe-21Cr-32Ni alloy in supercritical carbon dioxide10.1016/j.corsci.2021.110019 ↗
24. The effect of surface grinding and Si addition on the corrosion of Fe-12Cr ODS steels in supercritical CO210.1016/j.corsci.2023.111533 ↗
25. On the role of mechanical deformation in the environmental degradation of 310S stainless steels in supercritical carbon dioxide10.1016/j.corsci.2022.110537 ↗
26. Effect of shot-peening on corrosion behavior of austenitic steel in supercritical carbon dioxide at 700 °C10.1016/j.corsci.2022.110180 ↗
27. TEM investigation of intergranular stress corrosion cracking for 316 stainless steel in PWR environment10.1016/j.actamat.2005.10.011 ↗
28. Insights into the superior stress corrosion cracking resistance of FeCrAl alloy in high temperature hydrogenated water: the critical role of grain boundary oxidation10.1016/j.corsci.2022.110668 ↗
29. A high-resolution characterization of irradiation-assisted stress corrosion cracking of proton-irradiated 316L stainless steel in simulated pressurized water reactor primary water10.1016/j.corsci.2022.110187 ↗
30. Corrosion and creep behavior of a Ni-base alloy in supercritical-carbon dioxide environment at 650 °C10.1016/j.corsci.2020.108843 ↗
31. Understanding the stress corrosion cracking growth mechanism of a cold worked alumina-forming austenitic steel in supercritical carbon dioxide10.1016/j.corsci.2022.110179 ↗
32. Grain boundary oxidation behavior of Ni15Cr alloy in high temperature carbon dioxide10.1016/j.scriptamat.2022.114935 ↗
33. Effect of machining on stress corrosion crack initiation in warm-forged type 304L stainless steel in high temperature water10.1016/j.actamat.2018.11.046 ↗
34. Corrosion behavior of typical structural steels in 500 ℃, 600 ℃ and high pressure supercritical carbon dioxide conditions10.1016/j.corsci.2021.109801 ↗
35. Effect of silicon on the steam oxidation resistance of a 9 % Cr heat resistant steel10.1023/B:OXID.0000016280.81734.3f ↗
36. The effects of grain boundary structure and bulk Cr content on grain boundary degradation behavior of Ni-Cr binary alloys in high temperature CO210.1016/j.actamat.2023.119496 ↗
37. The effect of cold rolling on grain boundary structure and stress corrosion cracking susceptibility of twins in alloy 690 in simulated PWR primary water environment10.1016/j.corsci.2017.11.002 ↗
38. Crack initiation of neutron-irradiated 304 L stainless steel in PWR primary water10.1016/j.corsci.2021.109902 ↗
39. Creep of MARBN-type 9Cr martensitic steel in gaseous CO2 environment10.1016/j.msea.2021.141996 ↗
40. S. Palkó, F. Scenini, R. Ainsworth, Factors Affecting the Oxidation and Carburisation Behaviour of an Austenitic Stainless Steel Used in the UK Advanced Gas-Cooled Reactors, in: Pressure Vessels and Piping Conference, American Society of Mechanical Engineers, 2018, 51593: V01BT01A067.10.1115/PVP2018-84279 ↗