Effect of CrN coating on the hot salt corrosion fatigue behavior of titanium alloy
Source abstract
Abstract
The dwell fatigue behavior of CrN coated titanium alloys were carried out in air and hot salt corrosive environment at 500 ℃. The results indicate that the decrease of the elastic modulus difference between the coating and the substrate alleviates the deformation mismatch issue at high temperature. Stress relaxation at the crack tip caused by Cr transition layer oxidation can improve the fatigue properties of the coated samples. Furthermore, the CrN coating enhances the corrosion fatigue properties, which is related to the barrier effect of the coating on the corrosive medium. The crack growth mode in the substrate transition from stress corrosion crack to fatigue damage crack.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Hydrogen embrittlement and corrosion behaviors in metals · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Effect of streaming water vapor on the corrosion behavior of Ti60 alloy under a solid NaCl deposit in water vapor at 600 °C10.1016/j.corsci.2019.108177 ↗
2. Effect of NaCl-rich environment on internal corrosion for Ti60 alloy at 600 °C10.1016/j.corsci.2023.111307 ↗
3. Study of NaCl-induced hot-corrosion behavior of TiN single-layer and TiN/Ti multilayer coatings at 500°C10.1016/j.corsci.2021.109838 ↗
4. The influence of TiAlN and enamel coatings on the corrosion behavior of Ti6Al4V alloy in the presence of solid NaCl deposit and water vapor at 450 °C10.1016/j.surfcoat.2006.10.038 ↗
5. Effects Ti/TiAlN composite multilayer coatings on corrosion resistance of titanium alloy in solid NaCl-H2O-O2 at 600°C10.1016/j.jallcom.2017.11.035 ↗
6. W.H Liu. NaCl-induced hot-corrosion behavior and mechanism of TiSiCN/Ag nanocomposite coatings by arc ion plating10.1016/j.corsci.2023.111406 ↗
7. Effects of tensile load hold time on the fatigue and corrosion-fatigue behavior of turbine blade materials10.1016/j.ijfatigue.2021.106448 ↗
8. Effect of high-temperature hot corrosion on the low cycle fatigue behavior of a directionally solidified nickel-base superalloy10.1016/j.ijfatigue.2014.08.011 ↗
9. Effect of hot corrosion on low cycle fatigue behavior of superalloy IN71810.1016/j.ijfatigue.2013.08.009 ↗
10. The effect of salt composition on the stress-free and corrosion-fatigue performance of a fine-grained nickel-based superalloy10.1016/j.corsci.2022.110113 ↗
11. Effect of pre-hot salt corrosion on hot salt corrosion fatigue behavior of the TC11 titanium alloy at 500°C10.1016/j.ijfatigue.2022.107055 ↗
12. Influence of hot corrosion on low cycle fatigue behavior of nickel base superalloy SU 26310.1016/j.ijfatigue.2013.02.006 ↗
13. The mechanism of thermal corrosion fatigue (TCF) on nickel-based single crystal superalloy and the corresponding structure shape effect10.1016/j.corsci.2020.109142 ↗
14. Effect of hot corrosion on cycle deformation and fracture behavior of Ti-6Al-4V alloy under salt coating10.1016/j.corsci.2023.111545 ↗
15. X.J Li. Erosion behavior of CrN, CrAlN and CrAlN/CrN multilayer coatings deposited on Ti6Al4V10.1016/j.surfcoat.2022.128284 ↗
16. R. Franz. Correlating high temperature mechanical and tribological properties of CrAlN and CrAlSiN hard coatings10.1016/j.surfcoat.2019.05.044 ↗
17. Cyclic oxidation behaviour of Ti/TiAlN composite multilayer coatings deposited on titanium alloy10.1016/j.corsci.2020.108476 ↗
18. Fatigue and wear properties of Ti–6Al–4V alloy with Cr/CrN multilayer coating10.1016/j.surfcoat.2015.05.014 ↗
19. Structure, hardness and corrosion behavior of a gradient CrNx thick coating applied to turbine blades[J]10.1016/j.apsusc.2009.04.009 ↗
20. Fatigue behavior of PVD coated Ti–6Al–4V alloy10.1016/j.ijfatigue.2010.11.007 ↗
21. Fatigue behavior of AA7075-T6 aluminum alloy coated with ZrN by PVD10.1016/j.ijfatigue.2007.09.001 ↗
22. Fatigue fracture behavior of Ti-6Al-4V PVD coated10.1016/j.proeng.2010.03.200 ↗
23. Stress-sensitive fatigue crack initiation mechanisms of coated titanium alloy10.1016/j.actamat.2021.117179 ↗
24. Failure and deformation mechanisms during indentation in nanostructured Cr/CrN multilayer coatings10.1016/j.surfcoat.2013.12.006 ↗
25. Effect of plasma electrolytic oxidation on the hot salt corrosion fatigue behavior of the TC17 titanium alloy10.1002/maco.202112756 ↗
26. Effect of the ultrasonic surface rolling process and plasma electrolytic oxidation on the hot salt corrosion fatigue behavior of TC11 alloy10.1016/j.ijfatigue.2022.107443 ↗
27. Hot corrosion and low cycle fatigue of a Cr2AlC-coated superalloy10.1016/j.msea.2017.10.098 ↗
28. F.H Wang. Studies on corrosion resistance of thick TiN/Ti multilayer coatings under solid NaCl-H2O-O2 at 450°C10.1016/j.ceramint.2020.04.267 ↗
29. High-temperature cycle deformation and fracture behavior of advanced austenitic heat-resistant steel Sanicro25 alloy for A-USC power plants10.1007/s11661-022-06628-y ↗
30. Brittle coating effects on fatigue cracks behavior in Ti alloys10.1016/j.ijfatigue.2019.04.017 ↗
31. Attempt to design a strong solid10.1103/PhysRevB.2.547 ↗
32. Surface strengthening in aluminium single crystals coated with evaporated films10.1016/0001-6160(76)90027-4 ↗
33. Deformation behaviors and cyclic strength assessment of AZ31B magnesium alloy based on steady ratcheting effect10.1016/j.msea.2018.03.023 ↗
34. In-situ SEM analysis of brittle plasma electrolytic oxidation coating bonded to plastic aluminum substrate: microstructure and fracture behaviors10.1016/j.matchar.2019.109851 ↗
35. Brittle film-induced cracking of ductile substrates10.1016/j.actamat.2015.07.059 ↗
36. The effect of NaCl-induced corrosion on Ti60′ s hot salt stress corrosion cracking10.1016/j.corsci.2023.111677 ↗
37. Corrosion behavior of pure Cr with a solid NaCl deposit in O2 plus water vapor10.1023/A:1004690518225 ↗