Abstract

The microstructural evolution of the oxide scales formed on FeCr(Al,Ni) alloys after breakaway oxidation was studied in 5% O2 + 20% H2O + N2 (Bal) + KCl(s)/KCl(g) at 600 °C for 168, 1000 and 8000 hours. The SEM/EDS, SEM/EBSD and XRD investigation show that all alloys experience breakaway oxidation and form multi-layered scales. Experimental results, thermodynamic modelling and kinetic simulations show that FeCrAl and FeCrNi alloys form chromium-rich spinel oxide in inward-growing scales which transform into a protective corundum-type oxide as the oxidation progresses, while FeCr alloy experiences fast oxidation and maintains a non-protective spinel oxide/internal oxidation after long exposures.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (68)

Show source-provided references
1. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
2. K.O. Davidsson, L.-E. Åmand, B. Leckner, B. Kovacevik, M. Svane, M. Hagström, J.B.C. Pettersson, J. Pettersson, H. Asteman, J.-E. Svensson, L.-G. Johansson, Potassium, Chlorine, and Sulfur in Ash, Particles, Deposits, and Corrosion during Wood Combustion in a Circulating Fluidized-Bed Boiler, (2007). 〈https://doi.org/10.1021/ef060306c〉.10.1021/ef060306c ↗
3. High-temperature corrosion of HVAF-sprayed Ni-based coatings for boiler applications10.1007/s11085-019-09906-0 ↗
4. Corrosion of furnace wall materials in waste-wood fired power plant10.1179/1743278214Y.0000000228 ↗
5. Alkali induced high temperature corrosion of stainless steel-experience from laboratory and field
6. A pilot plant study of the effect of alkali salts on initial stages of the high temperature corrosion of alloy 304L10.4028/www.scientific.net/MSF.461-464.965 ↗
7. Field exposure of FeCrAl model alloys in a waste‐fired boiler at 600°C: The influence of Cr and Si on the corrosion behaviour10.1002/maco.201810618 ↗
8. J. Eklund, M. Dolores Paz, B. Jönsson, Jesper Liske, J.-E. Svensson, T. Jonsson, Field Exposure of FeCrAl Model Alloys in A Waste-fired Boiler at 600°C: the influence of Cr and Si on the Corrosion Behaviour, (2019). 〈https://doi.org/10.1002/maco.201810618〉.10.1002/maco.201810618 ↗
9. Oxidation after breakdown of the chromium-rich scale on stainless steels at high temperature: internal oxidation10.1007/s11085-016-9610-7 ↗
10. Continuous KCl addition in high temperature exposures of 304 L – a way to mimic a boiler environment10.1016/j.corsci.2020.108511 ↗
11. Effect of flue gas composition on deposit induced hightemperature corrosion under laboratory conditionsmimicking biomass firing. Part I: exposures in oxidizingand chlorinating atmospheres10.1002/maco.201609173 ↗
12. Cr diffusion coatings on a ferritic-martensitic steel for corrosion protection in KCl-rich biomass co-firing environments10.1016/j.corsci.2019.108343 ↗
13. Breakdown mechanism of γ-Al2O3 on Ni2Al3 coatings exposed in a biomass fired power plant10.1016/j.corsci.2020.108583 ↗
14. Chlorine-induced high temperature corrosion of Inconel 625 sprayed coatings deposited with different thermal spray techniques10.1016/j.surfcoat.2016.12.086 ↗
15. Enhanced internal oxidation as trigger for breakaway oxidation of Fe–Cr alloys in gases containing water vapor10.1016/j.scriptamat.2007.06.058 ↗
16. Breakaway corrosion of austenitic steel induced by fireside corrosion10.1016/j.corsci.2020.108765 ↗
17. Beyond breakaway corrosion – influence of chromium, nickel and aluminum on corrosion of iron-based alloys at 600 °C10.1016/j.corsci.2020.108961 ↗
18. Effect of molybdenum addition on oxidation behavior and secondary protection mechanism of FeCrAl coatings10.1016/j.matchar.2023.113221 ↗
19. Secondary corrosion protection of FeCr(Al) model alloys at 600 °C – The influence of Cr and Al after breakaway corrosion10.1016/j.corsci.2021.109584 ↗
20. Oxidation of a Fe–18Cr–8Ni austenitic stainless steel at 850 °C in O2: microstructure evolution during breakaway oxidation10.1016/j.corsci.2016.10.029 ↗
21. KCl-induced corrosion of Ni-based alloys containing 35–45 wt% Cr10.1002/maco.201810658 ↗
22. Grain-size effects on the high-temperature oxidation of modified 304 austenitic stainless steel10.1007/s11085-012-9347-x ↗
23. High temperature corrosion behavior of FeCrAlSi model alloys in the presence of water vapor and KCl at 600 °C – the influence of Cr content10.1016/j.corsci.2022.110114 ↗
24. Super VM12 - a new 12% Cr Boiler Steel
25. High temperature corrosion resistance of FeCr(Ni, Al) alloys as bulk/overlay weld coatings in the presence of KCl at 600 °C10.1016/j.corsci.2022.110896 ↗
26. ASTM international, Standard Test Methods for Determining Average Grain Size, PA 19428–2959, 2013. https://doi.org/Designation: E112–12.
27. B. Sedigheh, R. Naraghi, A. Harihara Subramonia Iyer, T. Jonsson, Thermodynamic and Kinetic Assessment of Binary Cr-O: Case Study for Effect of Grain Size in the Oxide Growth Rate, n.d.
28. Thermo-Calc & DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
29. Corrosion behaviour of iron and nickel aluminide coatings under the synergistic effect of NaCl and water vapour10.1016/j.corsci.2021.109484 ↗
30. Microstructural investigation using advanced TEM techniques of inner oxide layers formed on T92 steel in oxyfuel environment10.1016/j.corsci.2018.12.008 ↗
31. Strategies for high-temperature corrosion simulations of Fe-based alloys using the Calphad approach: part I10.1007/s11669-021-00893-x ↗
32. T. Olszewski, Oxidation Mechanisms of Materials for Heat Exchanging Components in CO2/H2O-containing Gases Relevant to Oxy-fuel Environments, Forschungszentrum, Zentralbibliothek, 2012. 〈https://books.google.se/books?id=rKA0_6HmjMwC〉.
33. High temperature oxidation behavior of APM and APMT under dry air/steam condition10.1557/adv.2016.514 ↗
34. High temperature oxidation of the austenitic (35Fe27Cr31Ni) alloy Sanicro 28 in O2 + H2O environment10.1007/s11085-010-9199-1 ↗
35. The effects of KCl, NaCl and K2CO3 on the high-temperature oxidation onset of Sanicro 28 steel10.1007/s11085-016-9613-4 ↗
36. KCl-induced high-temperature corrosion behavior of HVAF-sprayed Ni-based coatings in ambient air10.1007/s11666-017-0684-9 ↗
37. The influence of a KCl-rich environment on the corrosion attack of 304 L: 3D FIB/SEM and TEM investigations10.1016/j.corsci.2021.109315 ↗
38. Oxidation of iron at 400–600 °C in dry and wet O210.1016/j.corsci.2010.01.002 ↗
39. Oxidation of binary FeCr alloys (Fe–2.25Cr, Fe–10Cr, Fe–18Cr and Fe–25Cr) in O2 and in O2 + H2O environment at 600 °C10.1007/s11085-010-9229-z ↗
40. High temperature corrosion behavior of FeCrAlSi model alloys in the presence of water vapor and KCl at 600 °C – the influence of Cr content10.1016/j.corsci.2022.110114 ↗
41. H.J. Grabke, E. Reese, M. Spiegel, The Effects of Chlorides, Hydrogen Chloride, and Sulfur Dioxide in the Oxidation of Steels below Deposits, 1995.10.1016/0010-938X(95)00011-8 ↗
42. Influence of KCl and HCl on a laser clad FeCrAl alloy: In-Situ SEM and controlled environment high temperature corrosion10.1016/j.corsci.2019.07.003 ↗
43. Impacts of temperature and KCl on corrosion behavior of 12Cr1MoVG and T91 in HCl-containing atmosphere10.1007/s11085-018-9864-3 ↗
44. Point defects and cation tracer diffusion in (CrxFe1 − x)3 − δO4 spinels10.1016/0167-2738(95)00190-H ↗
45. Oxidation of Fe–10Cr in O2 and in O2+H2O environment at 600°C: a microstructural investigation10.1016/j.corsci.2013.06.016 ↗
46. High-temperature oxidation of FeCr(Ni) alloys: the behaviour after breakaway10.1007/s11085-017-9731-7 ↗
47. KCl-induced high temperature corrosion of selected commercial alloys10.1002/maco.201408213 ↗
48. Oxidation of iron at 600 °C – experiments and simulations10.1002/maco.201508781 ↗
49. The effect of oxide grain structure on the high-temperature oxidation of Fe, Ni and Cr10.1179/cmq.1979.18.3.283 ↗
50. Modelling of the effect of grain boundary diffusion on the oxidation of Ni-Cr alloys at high temperature10.1016/j.corsci.2018.03.001 ↗
51. A quantitative demonstration of the grain boundary diffusion mechanism for the oxidation of metals10.1080/01418618208239905 ↗
52. XXX. The structure of the spinel group of crystals10.1080/14786440808635400 ↗
53. The valence and site occupancy of substituting metals in magnetite spinel structure Fe3−xMxO4 (M = Cr, Mn, Co and Ni) and their influence on thermal stability: An XANES and TG-DSC investigation10.1016/j.solidstatesciences.2012.10.005 ↗
54. The influence of alloying elements on the chlorine-induced high temperature corrosion of Fe-Cr alloys in oxidizing atmospheres10.1002/(SICI)1521-4176(199910)50:10<561::AID-MACO561>3.0.CO;2-L ↗
55. High temperature corrosion mechanisms and effect of alloying elements for materials used in waste incineration environment10.1016/S0010-938X(01)00058-0 ↗
56. The long-term corrosion behavior of FeCrAl(Si) alloys after breakaway oxidation at 600 °C10.1016/j.corsci.2023.111155 ↗
57. Efficacy of an external chromia layer in reducing nitridation of high temperature alloys10.1016/j.corsci.2021.110050 ↗
58. A microstructural and kinetic investigation of the KCl-induced corrosion of an FeCrAl alloy at 600 °C10.1007/s11085-015-9546-3 ↗
59. In situ ESEM investigation of KCl-induced corrosion of a FeCrAl and a model FeNiCrAl alloy in lab air at 450°C10.1149/2.0581514jes ↗
60. Cyclic corrosion and chlorination of an FeCrAl alloy in the presence of KCl10.1007/s11085-015-9554-3 ↗
61. Factors affecting the nitridation behavior of Fe-base, Ni-base, and Co-base alloys in pure nitrogen
62. Aluminium nitride in steel10.1179/imr.1988.33.1.221 ↗
63. Effect of grain refinement on the resistance of 304 stainless steel to breakaway oxidation in wet air10.1016/j.actamat.2005.07.019 ↗
64. Grain-size effects on the high-temperature oxidation behaviour of chromium steels10.1007/s11085-010-9192-8 ↗
65. Effect of alloy grain size on the high-temperature oxidation behavior of the austenitic steel TP 34710.1590/S1516-14392005000400003 ↗
66. Effect of alloy grain size and silicon content on the oxidation of austenitic Fe-Cr-Ni-Mn-Si alloys in pure O210.1007/BF00662967 ↗
67. High temperature oxidation of the austenitic (35Fe27Cr31Ni) alloy Sanicro 28 in O2 + H2O environment10.1007/s11085-010-9199-1 ↗
68. Depletion and voids formation in the substrate during high temperature oxidation of Ni–Cr alloys10.1007/s11085-012-9328-0 ↗