The corrosion behavior of 316Ti steel in Lead-Bismuth Eutectic (LBE) was studied in this work. It reveals a transition in external oxidation between 5×10 −6 wt% and 5×10 −7 wt% DOC. The columnar magnetite (Fe 3O 4) formed under 5×10 −6 wt% DOC grew via solid-state diffusion, while metal-dissolution/oxide-precipitation mechanism guided the external oxidation under 5×10 −7 wt% DOC, forming equiaxed magnetite. Internal oxidation is influenced by the Ni-dissolution which facilitates the inner oxide growth. The internal oxide layer formed under 5×10 −7 wt% DOC exhibit a better resistance to LBE penetration and oxide cracking. A corrosion model was proposed to elucidate the influence of DOC on the corrosion behavior of 316Ti steel.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Nuclear Physics and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. C. Fazio, V.P. Sobolev, A. Aerts, S. Gavrilov, K. Lambrinou, P. Schuurmans, A. Gessi, P. Agostini, A. Ciampichetti, L. Martinelli. Handbook on lead-bismuth eutectic alloy and lead properties, materials compatibility, thermal-hydraulics and technologies, 2015 ed, Organisation for Economic Co-Operation and Development, 2015.
2. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
3. Corrosion behavior of austenitic steels in liquid lead bismuth containing 10−6wt% and 10−8wt% oxygen at 400-500°C10.1016/j.jnucmat.2014.01.046 ↗
4. Early stages of dissolution corrosion in 316L and DIN 1.4970 austenitic stainless steels with and without anticorrosion coatings in static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.matchar.2021.111234 ↗
5. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb-Bi melt saturated by oxygen10.1016/j.corsci.2008.02.006 ↗
6. Dissolution mechanism of 316L in lead-bismuth eutectic at 500 °C10.1016/j.corsci.2011.05.031 ↗
7. Oxidation of steels in liquid lead bismuth: Oxygen control to achieve efficient corrosion protection10.1016/j.nucengdes.2010.07.039 ↗
8. Oxide layer stability in lead–bismuth at high temperature10.1016/j.jnucmat.2004.07.017 ↗
9. Corrosion of stainless steels in lead–bismuth eutectic up to 600 °C10.1016/j.jnucmat.2004.07.012 ↗
10. Corrosion behavior of T91 steel in liquid lead-bismuth eutectic at 550 °C: effects of exposure time and dissolved oxygen concentration10.1016/j.corsci.2022.110405 ↗
11. Dissolution and oxidation behaviour of various austenitic steels and Ni rich alloys in lead-bismuth eutectic at 520 °C10.1016/j.jnucmat.2015.11.005 ↗
12. Behavior of steels in flowing liquid PbBi eutectic alloy at 420–600 °C after 4000–7200h10.1016/j.jnucmat.2004.07.010 ↗
13. Corrosion scales on various steels after exposure to liquid lead-bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗
14. of Armco iron and model Fe-Cr-Al alloys in oxygen-containing lead melts10.1007/BF02538517 ↗
15. Transmission electron microscopy (TEM) on oxide layers formed on D9 stainless steel in lead bismuth eutectic (LBE)10.1016/j.corsci.2012.09.019 ↗
16. Characterization of oxide layers grown on D9 austenitic stainless steel in lead bismuth eutectic10.1016/j.jnucmat.2007.12.005 ↗
17. Development of aluminum-alloy coating on type 316SS for nuclear systems using liquid lead–bismuth10.1016/j.jnucmat.2012.03.018 ↗
18. Hydrogen emission during the steam oxidation of ferritic steels: Kinetics and mechanism10.1016/0010-938X(89)90086-3 ↗
19. Kinetics of oxidation of ferrous alloys by super-heated steam10.1007/BF00666721 ↗
20. Microstructural evolution of early-stage oxide film on 15–15Ti austenitic stainless steel under 500 ℃ steam10.1016/j.corsci.2022.110557 ↗
21. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
22. Mechanism of corrosion of carbon and low alloy ferritic steels by high temperature water10.5006/1.3577543 ↗
23. High-resolution characterization of the internal and external oxidation of austenitic alloys in supercritical water10.1016/j.scriptamat.2021.113814 ↗
24. A model for mild steel oxidation in CO210.1007/BF00610578 ↗
25. The surface grinding-induced oxide scale exfoliation of an austenitic alloy in supercritical CO210.1016/j.corsci.2023.111615 ↗
26. Microstructural evolution of duplex grain structure and interpretation of the mechanism for NiO scales grown on pure Ni- and Cr-doped substrates during high temperature oxidation10.1016/S0921-5107(00)00435-9 ↗
27. Stacking fault energies of seven commercial austenitic stainless steels10.1007/BF02641927 ↗
28. X. Gong. Corrosion resistance of 15–15Ti and 316Ti austenitic steels as fuel cladding in liquid lead-bismuth eutectic at 550 ℃: The dominant role of grain structure10.1016/j.corsci.2023.111169 ↗
29. Effects of pre-exposure and simulated corrosion “pits” on liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic at 350 °C10.1016/j.jnucmat.2022.153641 ↗
30. C. Schroer, J.Konys. Physical Chemistry of Corrosion and Oxygen Control in Liquid Lead and Lead-Bismuth Eutectic, Wissenschaftliche Berichte FZKA 7364, Forschungszentrum Karlsruhe, 2007.
31. Improving the oxidation resistance of SIMP steel to liquid Pb-Bi eutectic by shot peening treatments10.1016/j.apsusc.2021.151910 ↗
32. Criteria for formation of single layer, duplex, and breakaway scales on steels10.1179/mst.1988.4.12.1064 ↗
33. Enhanced corrosion resistance of 15–15Ti austenitic steel in liquid lead-bismuth eutectic at 550 ℃ by shot peening processing10.1016/j.corsci.2023.111640 ↗
34. Oxidation mechanism of a Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
35. Insights into the corrosion mechanism of a 12Cr F/M steel in oxygen-saturated liquid LBE10.1016/j.corsci.2023.111602 ↗
36. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
37. Corrosion of austenitic stainless steels and nickel-base alloys in supercritical water and novel control methods
38. Structural, electrical and magnetic measurements on oxide layers grown on 316L exposed to liquid lead–bismuth eutectic10.1016/j.jnucmat.2011.11.042 ↗
39. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
40. Early stages of liquid-metal corrosion on pre-oxidized surfaces of austenitic stainless steel 316L exposed to static Pb-Bi eutectic at 400 °C10.1016/j.corsci.2023.111680 ↗
41. A high-resolution study of the different surface state effects on the corrosion behaviors of a ferritic steel and an austenitic steel in supercritical water10.1016/j.corsci.2022.110757 ↗
42. Self-diffusion in austenitic Fe-Cr-Ni alloys10.1088/0305-4608/10/3/009 ↗
43. Microstructural investigation of the nodular corrosion of 304NG stainless steel in supercritical water10.1016/j.corsci.2020.108652 ↗
44. Microstructure understanding of high Cr-Ni austenitic steel corrosion in high-temperature steam10.1016/j.actamat.2022.117634 ↗
45. Microstructural evolution of early-stage oxide film on 15–15Ti austenitic stainless steel under 500 ℃ steam10.1016/j.corsci.2022.110557 ↗
46. F. Balbaud, L. Martinelli, 22 - Corrosion issues in lead-cooled fast reactor (LFR) and accelerator driven systems (ADS), In: Nuclear Corrosion Science and Engineering, Woodhead Publishing, 2012, pp. 807-841.10.1533/9780857095343.6.807 ↗
47. D. Schryvers. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.jnucmat.2017.04.004 ↗
48. J. Konys. Long-term service of austenitic steel 1.4571 as a container material for flowing lead–bismuth eutectic10.1016/j.jnucmat.2011.07.026 ↗
49. J. Vít. Mechanism of localized corrosion issues of austenitic steels exposed to flowing lead with 10−7wt% oxygen at 480°C up to 16,000h10.1016/j.jnucmat.2022.154045 ↗
50. Quantification of the long-term performance of steels T91 and 316L in oxygen-containing flowing lead-bismuth eutectic at 550℃10.1115/1.4000364 ↗