Environmental degradation of electroplated nickel and copper coated SS316H in molten FLiNaK salt

Matthew Weinstein, Cody Falconer, William Doniger, Louis Bailly-Salins, Raphaelle David, Kumar Sridharan, Adrien Couet

Corrosion Science· Volume 191

Abstract

Abstract Corrosion of nickel and copper electroplated coatings on SS316H in molten FLiNaK salt was studied. 500- and 1000-hour static corrosion tests were performed in molten FLiNaK at 700 degrees Celsius. Characterization of the coatings following corrosion indicated that they did not degrade in the molten salt during the corrosion experiment and fully protected the underlying SS316H from chromium dissolution. Interdiffusion between the copper coating and SS316H was extremely limited, interdiffusion between the nickel coating and SS316H. Diffusion modelling revealed that the nickel coatings still significantly reduced chromium dissolution over 60 years despite the interdiffusion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Molten salt chemistry and electrochemical processes · Metallurgical Processes and Thermodynamics · Thermodynamic and Structural Properties of Metals and Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Molten-salt reactors. History, status, and potential
2. Method for identification of redox control parameters for corrosion mitigation in molten fluoride salts10.1016/j.jnucmat.2020.152624 ↗
3. Corrosion of structural alloys in high-temperature molten fluoride salts for applications in molten salt reactors10.1007/s11837-018-2981-2 ↗
4. Corrosion in the molten fluoride and chloride salts and materials development for nuclear applications10.1016/j.pmatsci.2018.05.003 ↗
5. Optimization of dissolved hydrogen concentration for control of primary coolant radiolysis in pressurized water reactors10.1080/18811248.2004.9715523 ↗
6. PWR steam generators10.1016/0301-9322(95)00016-Q ↗
7. Busby · 2019
8. Division 5—High temperature reactors
9. Materials corrosion in molten Lif_Naf_KF salt10.1016/j.jfluchem.2008.05.008 ↗
10. P.M. [Georgia I. of T. Singh Atlanta, GA (United States)], K.J. [Georgia I. of T. Chan Atlanta, GA (United States)], C.S. [Georgia I. of T. Deo Atlanta, GA (United States)], V. [Haynes I.I. Deodeshmukh Kokomo, IN (United States)], J.R. [Oak R.N.L. (ORNL) Keiser Oak Ridge, TN (United States)] (ORCID:0000000347187776), W. [Oak R.N.L. (ORNL) Ren Oak Ridge, TN (United States)] (ORCID:0000000281262832), T.L. [Argonne N.L. (ANL) Sham Argonne, IL (United States)], D.F. [ThorCon P. Wilson Jakarta (Indonesia)], J. Yoder Graydon [Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)] (ORCID:0000000170803034), J. [Virginia P.I. and S.U. (Virginia T. Zhang Blacksburg, VA (United States)], Phenomena Identification and Ranking Table (PIRT) study for metallic structural materials for advanced High-Temperature reactor, (2018). https://doi.org/10.1016/j.anucene.2018.08.036.10.1016/j.anucene.2018.08.036 ↗
11. Investigating corrosion behavior of Ni and Ni-20Cr in molten ZnCl210.1016/j.corsci.2020.109105 ↗
12. Corrosion behavior and elements interdiffusion between a Ni coating and GH3535 alloy with and without a CrN barrier in molten fluoride salts10.1016/j.jnucmat.2018.12.018 ↗
13. Non-galvanic mass transport in molten fluoride salt isothermal corrosion cells10.1016/j.corsci.2020.108955 ↗
14. Microstructural characterization of Ni-201 weld cladding onto 304 stainless steel10.1016/j.surfcoat.2017.11.023 ↗
15. Nickel-plating for active metal dissolution resistance in molten fluoride salts10.1016/j.jnucmat.2011.01.032 ↗
16. Corrosion of Incoloy 800H alloys with nickel cladding in FLiNaK salts at 850 °C10.1016/j.corsci.2018.01.026 ↗
17. Ni coating on 316L stainless steel using cage plasma treatment: feasibility and swelling studies10.1016/j.jnucmat.2020.152385 ↗
18. Effects of SO42− ions on the corrosion of GH3535 weld joint in FLiNaK molten salt10.1016/j.jnucmat.2017.05.020 ↗
19. Effect of SO42− ion impurity on stress corrosion behavior of Ni-16Mo-7Cr alloy in FLiNaK salt10.1016/j.jnucmat.2021.152809 ↗
20. Effect of SO42− on the corrosion of 316L stainless steel in molten FLiNaK salt10.1016/j.corsci.2018.08.057 ↗
21. Influences of corrosive sulfur on copper wires and oil-paper insulation in transformers10.3390/en4101563 ↗
22. Bulk diffusion of iron in copper10.1134/S0031918X12030106 ↗
23. The diffusion and solubility of copper in iron10.1063/1.323934 ↗
24. Application of nickel electroplating for PWR reactor pressure vessel cladding repair
25. In-situ nuclear steam generator repair using electrodeposited nanocrystalline nickel10.1016/S0965-9773(97)00160-8 ↗
26. R.A. [Ontario H.T. Barton Toronto, ON (Canada)], T.E. [Framatome T.I. Moran Lynchburg, VA (United States)], E. [Babcock and W.I.L. Renaud Cambridge, ON (Canada)], Electrosleeve process for in-situ nuclear steam generator repair, in: Canada, 1997. https://www.osti.gov/etdeweb/servlets/purl/20043865.