Nano-scale evidence for coupled interfacial dissolution-reprecipitation (CDR) controlling corrosion of alumina-forming austenitic (AFA) steel in static lead-bismuth eutectic (LBE) at 600°C
Source abstract
Abstract
Despite extensive research on dissolution corrosion, whether element dissolution is selective or non-selective remains unclear, due to limitations of past characterization technologies. Using nano-scale characterization, we investigated AFA steel exposed to LBE with 10 −8 wt.% oxygen at 600°C for 1700 h, found that alloying elements dissolve non-selectively into LBE and then reprecipitate, forming penetrable corrosion zone that inherits substrate crystallographic information and comprises ferrite, river-like NiAl, and NiAl nanoparticles. The ferrite and river-like NiAl exhibit complete elemental segregation due to liquid-phase diffusion, while NiAl nanoparticles form via reaction-diffusion. This supports that coupled dissolution-reprecipitation mechanism primarily controls dissolution corrosion at 600°C.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Opportunities and challenges for a sustainable energy future10.1038/nature11475 ↗
2. Nuclear power for sustainable development: current status and future prospects10.1016/j.enpol.2009.07.052 ↗
3. A high-density and high-confinement tokamak plasma regime for fusion energy10.1038/s41586-024-07313-3 ↗
4. Generation IV International Forum: A decade of progress through international cooperation10.1016/j.pnucene.2014.02.010 ↗
5. Multi-purpose hybrid research reactor for high-tech applications a multipurpose fast spectrum research reactor10.1002/er.1891 ↗
6. Status of Pb-16Li technologies for European DEMO fusion reactor10.1016/j.fusengdes.2019.04.083 ↗
7. Thermodynamic properties and equation of state of liquid lead and lead–bismuth eutectic10.1016/j.jnucmat.2008.02.030 ↗
8. A review of steel corrosion by liquid lead and lead–bismuth10.1016/j.corsci.2009.03.013 ↗
9. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
10. Liquid metal corrosion10.5006/0010-9312-9.3.78 ↗
11. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
12. Influence of liquid lead and lead-bismuth eutectic on tensile, fatigue and creep properties of ferritic/martensitic and austenitic steels for transmutation systems10.1016/j.jnucmat.2011.04.047 ↗
13. The effects of cold working on the corrosion behavior of an austenitic stainless steel in liquid lead-bismuth eutectic under vacuum at 873 K10.1016/j.jnucmat.2018.07.034 ↗
14. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500C10.1016/j.jnucmat.2017.04.004 ↗
15. Long-term corrosion of austenitic steels in flowing LBE at 400°C and 10−7 mass% dissolved oxygen in comparison with 450 and 550°C10.1016/j.jnucmat.2015.09.027 ↗
16. Dissolution and oxidation behaviour of various austenitic steels and Ni rich alloys in lead-bismuth eutectic at 520°C10.1016/j.jnucmat.2015.11.005 ↗
17. Twin boundary-accelerated ferritization of austenitic stainless steels in liquid lead-bismuth eutectic10.1016/j.scriptamat.2016.02.029 ↗
18. Corrosion behavior of austenitic steels 1.4970, 316L and 1.4571 in flowing LBE at 450 and 550°C with 10−7 mass% dissolved oxygen10.1016/j.jnucmat.2014.08.024 ↗
19. Selective leaching of nickel and chromium from Type 316 austenitic steel in oxygen-containing lead-bismuth eutectic (LBE)10.1016/j.corsci.2014.03.016 ↗
20. Corrosion behavior of austenitic steels in liquid lead bismuth containing 10−6 wt% and 10−8 wt% oxygen at 400-500°C10.1016/j.jnucmat.2014.01.046 ↗
21. Liquid metal corrosion of T91 and A316L materials in Pb–Bi eutectic at temperatures 400-600°C10.1016/j.corsci.2005.04.001 ↗
22. Comparison of the corrosion behavior of austenitic and ferritic/martensitic steels exposed to static liquid Pb-Bi at 450 and 550°C10.1016/j.jnucmat.2004.07.064 ↗
23. Dissolution mechanism of 316L in lead-bismuth eutectic at 500 °C10.1016/j.corsci.2011.05.031 ↗
24. Models of liquid metal corrosion10.1016/j.jnucmat.2010.05.024 ↗
25. Analysis on liquid metal corrosion–oxidation interactions10.1016/j.corsci.2007.05.012 ↗
26. Corrosion of T91 and pure iron in flowing and static Pb-Bi alloy between 450 °C and 540 °C: experiments, modelling and mechanism10.1016/j.corsci.2020.108897 ↗
27. Mechanism of aqueous dissolution of silicate glasses yielded by fission tracks10.1038/319485a0 ↗
28. Unifying natural and laboratory chemical weathering with interfacial dissolution-reprecipitation: A study based on the nanometer-scale chemistry of fluid-silicate interfaces10.1016/j.chemgeo.2011.12.002 ↗
29. Supernormal enrichment of cadmium in sphalerite via coupled dissolution-reprecipitation process10.1038/s43247-023-01025-8 ↗
30. Mineral dissolution and reprecipitation mediated by an amorphous phase10.1038/s41467-018-03944-z ↗
31. Nanometre-scale evidence for interfacial dissolution-reprecipitation control of silicate glass corrosion10.1038/nmat4172 ↗
32. Textural and compositional complexities resulting from coupled dissolution–reprecipitation reactions in geomaterials10.1016/j.earscirev.2015.08.013 ↗
33. Coupled dissolution and precipitation at mineral-fluid interfaces10.1016/j.chemgeo.2014.06.007 ↗
34. Research results on the corrosion effects of liquid heavy metals Pb, Bi and Pb-Bi on structural materials with and without corrosion inhibitors10.1016/S0029-5493(02)00158-9 ↗
35. Creep-Resistant, Al₂O₃-forming austenitic stainless steels10.1126/science.1137711 ↗
36. Effect of variation in oxygen concentration in static Pb-Bi eutectic on long-term corrosion performance of Al-alloyed austenitic steels at 500°C10.1016/j.corsci.2021.109963 ↗
37. Corrosion behaviour of Al-added high Mn austenitic steels in molten lead bismuth eutectic with saturated and low oxygen concentrations at 450°C10.1016/j.corsci.2020.108864 ↗
38. The influence of Y and Nb addition on the corrosion resistance of Fe-Cr-Al-Ni model alloys exposed to oxygen-containing molten Pb10.1016/j.corsci.2020.109152 ↗
39. Corrosion resistance and microstructural stability of austenitic Fe-Cr-Al-Ni model alloys exposed to oxygen-containing molten lead10.1016/j.jnucmat.2019.06.043 ↗
40. Long term corrosion resistance of alumina forming austenitic stainless steels in liquid lead10.1016/j.jnucmat.2015.03.011 ↗
41. Effect of oxygen on corrosion of an alumina-forming duplex steel in static liquid lead-bismuth eutectic at 550 °C10.1016/j.corsci.2021.109591 ↗
42. Temperature effect on the corrosion mechanism of austenitic and martensitic steels in lead-bismuth10.1016/S0022-3115(01)00723-1 ↗
43. Oxygen concentration measurement and control of lead-bismuth eutectic in a small, static experimental facility10.1080/00223131.2019.1700842 ↗
44. Synergistic effects of Si and Y on corrosion behavior of cast cladding steels by pre-laying Y powder for nuclear applications in static liquid LBE10.1016/j.jnucmat.2022.153781 ↗
45. The influence of Y addition on oxide layers of 15-15Ti-Y steel exposed to static Pb-Bi alloys with containing oxygen10.1016/j.jnucmat.2023.154806 ↗
46. Dissolution corrosion of FeCrAl alloy exposed to oxygen-depleted lead-bismuth eutectic containing Ni impurities at 600°C
47. Ultrahigh stability and strong precipitation strengthening of nanosized NbC in alumina-forming austenitic stainless steels subjecting to long-term high-temperature exposure10.1016/j.msea.2018.09.081 ↗
48. Precipitation sequence and its effect on age hardening of alumina-forming austenitic stainless steel10.1016/j.msea.2015.08.005 ↗
49. Development of L12-ordered Ni3(Al,Ti)-strengthened alumina-forming austenitic stainless steel alloys10.1016/j.scriptamat.2013.09.005 ↗
50. Variety of yield strength caused by precipitations of L12-Ni3Al and B2-NiAl phases in alumina-forming austenitic steel
51. Effect of deformation twinning on dissolution corrosion of 316L stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.jnucmat.2018.08.030 ↗
52. Corrosion behavior of steels in liquid lead-bismuth with low oxygen concentrations10.1016/j.jnucmat.2007.05.051 ↗
53. Orientation relationship of the austenite-to-ferrite transformation in austenitic stainless steels due to dissolution corrosion in contact with liquid Pb-Bi eutectic10.1016/j.scriptamat.2019.03.035 ↗
54. Corrosion behaviour of steels in lead-bismuth at 823 K10.1016/j.jnucmat.2004.07.013 ↗
55. Experimental investigation on corrosion of structural steels in molten Pb-Mg and LBE
56. Superior radiation tolerance via reversible disordering–ordering transition of coherent superlattices10.1038/s41563-022-01260-y ↗
57. Microstructural evolution and mechanical properties of an Fe-18Ni-16Cr-4Al base alloy during aging at 950°C10.1007/s12613-016-1240-1 ↗
58. Prediction of high-entropy stabilized solid-solution in multi-component alloys10.1016/j.matchemphys.2011.11.021 ↗
59. High-strength steels hardened mainly by nanoscale NiAl precipitates10.1016/j.scriptamat.2014.05.006 ↗
60. Aging characteristics and mechanical properties of 1600 MPa body-centered cubic Cu and B2-NiAl precipitation-strengthened ferritic steel10.1016/j.actamat.2014.03.051 ↗
61. Effects of increased alloying element content on NiAl-type precipitate formation, loading rate sensitivity, and ductility of Cu- and NiAl-precipitation-strengthened ferritic steels10.1016/j.actamat.2015.11.041 ↗
62. Structure and dynamics of water at a clay surface from molecular dynamics simulation10.1039/b807288d ↗
63. Effects of substrate structure and composition on the structure, dynamics, and energetics of water at mineral surfaces; a molecular dynamics modeling study10.1016/j.gca.2005.10.006 ↗
64. A new mode of mineral replacement reactions involving the synergy between fluid-induced solid-state diffusion and dissolution-reprecipitation: a case study of the replacement of bornite by copper sulfides10.1016/j.gca.2021.04.017 ↗
65. Analysis of kinetics of reactive diffusion in a hypothetical binary system10.1016/j.actamat.2003.10.047 ↗