Enhanced oxidation resistance of additively manufactured Inconel 718 superalloy by surface mechanical attrition treatment
Source abstract
Abstract
This study investigated the effects of surface mechanical attrition treatment (SMAT) on the antioxidation performance of additively manufactured Inconel 718 parts. The results show that SMAT generated a nanograin layer near the part surface with high densities of low-angle grain boundaries, plastic strain and lattice distortion. Oxidation resistance was improved owing to that a continuous oxide scale was quickly formed to protect the underlying materials at the early stage of oxidation by the nanosized microstructure. Moreover, adhesion between the oxide scale and the parent alloy was enhanced because of a high level of compressive residual stress induced by SMAT. • The IN718 superalloy processed by PBF-LB was treated using SMAT. • SMAT produced a hardness-enhanced layer with large compressive residual stress. • The part treated using SMAT had a better oxidation resistance at 850 ℃. • Nano-sized microstructure and high residual stress were the main contributions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Surface Treatment and Residual Stress · Additive Manufacturing Materials and Processes · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Microstructural characterization and oxidation performance of solution-annealed and precipitation hardened wire-arc additively manufactured Inconel 718 superalloys
2. Review on fatigue of additive manufactured metallic alloys: microstructure, performance, enhancement, and assessment methods
3. Interfacial microstructure and mechanical properties of forging and SLM hybrid manufacturing Ti-6Al-4V parts10.1016/j.matlet.2023.134101 ↗
4. Influence of laser power and scanning speed on microstructure evolutions and mechanical properties of the SLM fabricated Al–Mg–Mn–Sc–Zr alloy10.1016/j.jmrt.2024.10.134 ↗
5. Tailoring the microstructure and mechanical property of additively manufactured AlCrCuFeNi3.0 high-entropy alloy through heat treatment10.1016/j.msea.2022.143192 ↗
6. Single-track investigation of IN738LC superalloy fabricated by laser powder bed fusion: track morphology, bead characteristics and part quality10.1016/j.jmatprotec.2020.117000 ↗
7. A comparing study of defect generation in IN738LC superalloy fabricated by laser powder bed fusion: continuous-wave mode versus pulsed-wave mode10.1016/j.jmst.2021.03.006 ↗
8. A review on metallurgical aspects of laser additive manufacturing (LAM): stainless steels, nickel superalloys, and titanium alloys10.1016/j.jmrt.2021.12.039 ↗
9. Heterogeneous structures in a Ni-based superalloy with tailoring mechanical properties produced by a twin laser powder bed fusion system10.1016/j.jallcom.2022.166983 ↗
10. Effect of processing parameters on surface roughness, porosity and cracking of as-built IN738LC parts fabricated by laser powder bed fusion10.1016/j.jmatprotec.2020.116788 ↗
11. Cracking mechanism of GH5188 alloy during laser powder bed fusion additive manufacturing10.1016/j.matchar.2023.113548 ↗
12. Preferential interdendritic oxidation of laser additively manufactured Inconel 71810.1016/j.corsci.2020.109144 ↗
13. Intergranular oxidation of Ni-base alloy 718 with a focus on additive manufacturing10.1016/j.corsci.2020.108684 ↗
14. Investigations of the effects of combination treatments on the fretting fatigue resistance of GH4169 superalloy at an elevated temperature10.1016/j.surfcoat.2021.127758 ↗
15. Fatigue behaviors of AISI 316L stainless steel with a gradient nanostructured surface layer10.1016/j.actamat.2014.12.057 ↗
16. Thermal oxidation behaviour of bulk titanium with nanocrystalline surface layer10.1016/j.corsci.2012.03.005 ↗
17. Influence of surface mechanical attrition treatment on the oxidation behaviour of 316L stainless steel10.1016/j.corsci.2018.03.007 ↗
18. High-temperature oxidation behaviour of nanostructure surface layered austenitic stainless steel10.1016/j.apsusc.2022.152437 ↗
19. Effects of post-processing route on fatigue performance of laser powder bed fusion Inconel 718
20. Fatigue life extension of additively manufactured nickel-base 718 alloy by nanostructured surface10.1016/j.msea.2021.142041 ↗
21. Subsurface grain refinement in electron beam-powder bed fusion of Alloy 718: surface texture and oxidation performance10.1016/j.matchar.2020.110567 ↗
22. Literature review on the mechanical properties of materials after surface mechanical attrition treatment (SMAT)10.1016/j.nanoms.2020.04.002 ↗
23. Mechanical properties and deformation mechanisms of gradient nanostructured metals and alloys10.1038/s41578-020-0212-2 ↗
24. Effect of laser power on the microstructure and mechanical properties of heat treated Inconel 718 superalloy by laser solid forming10.1016/j.jallcom.2018.02.268 ↗
25. Evolution of texture and microstructure in pulsed electro-deposited Cu treated by surface mechanical attrition treatment (SMAT)10.1016/j.jallcom.2010.04.040 ↗
26. Fatigue life improvement through surface nanostructuring of stainless steel by means of surface mechanical attrition treatment10.1016/j.scriptamat.2006.01.049 ↗
27. High-temperature oxidation behaviour of a Co-based superalloy fabricated through laser powder bed fusion10.1016/j.corsci.2023.111703 ↗
28. Study of oxide layer formation on Inconel 718 during isothermal oxidation between 800 °C and 1200 °C in hot air10.1016/j.ceramint.2022.07.187 ↗
29. Selective laser melting additive manufactured Inconel 718 superalloy parts: high-temperature oxidation property and its mechanisms10.1016/j.optlastec.2014.03.008 ↗
30. Healing cracks in selective laser melting by 3D laser shock peening
31. Effect of shot peening on fatigue performance of Ti2AlNb intermetallic alloy10.1016/j.ijfatigue.2019.05.034 ↗
32. Surface post-treatments for metal additive manufacturing: progress, challenges, and opportunities
33. A direct comparison in the fatigue resistance enhanced by surface severe plastic deformation and shot peening in a C-2000 superalloy10.1016/j.msea.2009.10.028 ↗
34. Strengthening via deformation twinning in a nickel alloy10.1016/j.msea.2007.06.072 ↗
35. The effects of shot peening, laser shock peening and ultrasonic nanocrystal surface modification on the fatigue strength of Inconel 71810.1016/j.msea.2021.141029 ↗
36. Deforming TC6 titanium alloys at ultrahigh strain rates during multiple laser shock peening10.1016/j.msea.2013.04.070 ↗
37. Predicting surface deformation during mechanical attrition of metallic alloys10.1038/s41524-019-0171-6 ↗
38. Analysis of shot-peening and residual stress relaxation in the nickel-based superalloy RR100010.1016/j.actamat.2013.01.031 ↗
39. Enhanced high-cycle fatigue resistance of 304 austenitic stainless steel with nanotwinned grains10.1016/j.ijfatigue.2020.105994 ↗
40. Influence of stacking-fault energy on the accommodation of severe shear strain in Cu-Al alloys during equal-channel angular pressing10.1557/jmr.2009.0426 ↗
41. Mechanical behavior of structurally gradient nickel alloy10.1016/j.actamat.2018.02.021 ↗
42. The influence of strain rate on the microstructure transition of 304 stainless steel10.1016/j.actamat.2011.03.005 ↗
43. Formation of nano-laminated structure in nickel by means of surface mechanical grinding treatment10.1016/j.actamat.2015.06.014 ↗
44. Improving the hot corrosion resistance of additively manufactured Inconel 718 via recrystallization-based grain boundary engineering induced by its residual stress
45. Creep property of Inconel 718 superalloy produced by selective laser melting compared to forging10.1016/j.msea.2020.139947 ↗
46. Effect of local treatment temperature of ultrasonic nanocrystalline surface modification on tribological behavior and corrosion resistance of stainless steel 316L produced by selective laser melting10.1016/j.surfcoat.2020.126080 ↗
47. Oxidation10.1016/B978-0-12-804622-7.00004-8 ↗
48. Giggins · J. Electrochem. Soc. · 1971 · 118 · 178210.1149/1.2407837 ↗
49. Comparative study on mechanical properties and high temperature oxidation behaviour of Hastelloy X and Inconel 718 fabricated by laser directed energy deposition10.1016/j.jmrt.2023.12.199 ↗
50. High temperature oxidation and oxychlorination behaviors of cold sprayed Inconel 718 deposits at 700 °C10.1016/j.corsci.2022.110536 ↗
51. Effects of helium ion irradiation on the high temperature oxidation resistance of Inconel 718 alloy10.1016/j.surfcoat.2019.02.021 ↗
52. Effect of Cr addition on the evolution of protective alumina scales and the oxidation properties of a Ta stabilized γ'-strengthened Co-Ni-Al-Mo-Ta-Ti alloy10.1016/j.corsci.2020.108683 ↗
53. Contribution of Mg addition to the high temperature cyclic oxidation resistance of NiAlCr alloys10.1016/j.corsci.2018.08.004 ↗
54. The effect of alloying elements on oxide scale spallation of multicomponent Co-based superalloys10.1016/j.corsci.2021.109787 ↗
55. On the dwell-fatigue crack propagation behavior of a high strength superalloy manufactured by electron beam melting10.1016/j.msea.2019.06.013 ↗
56. Sub-scale depletion and enrichment processes during high temperature oxidation of the nickel base alloy 625 in the temperature range 900–1000 °C10.1007/s11085-010-9225-3 ↗
57. SEM-EDS and XPS studies of the high temperature oxidation behaviour of inconel 71810.1007/s006040050027 ↗
58. Influence of thermal post treatments on microstructure and oxidation behavior of EB-PBF manufactured alloy 71810.1016/j.matchar.2019.02.016 ↗
59. Effect of post-treatment on the microstructure and high-temperature oxidation behaviour of additively manufactured inconel 718 alloy10.1016/j.corsci.2019.06.030 ↗
60. Influence of the density of oxide on oxidation kinetics10.1016/j.intermet.2013.11.024 ↗
61. Oxides spallation/cracking and oxidation kinetics behaviours of microstructurally different regions of TIG joint in Cr-Mo (T11) boiler steel under cyclic environment10.1016/j.matlet.2022.133485 ↗
62. Cracking and spalling of protective oxide layers10.1016/0921-5093(89)90731-4 ↗
63. Laser shock peening of AlCoCrCuFeNi high-entropy alloy fabricated by laser powder bed fusion: an enhanced oxidation-resistance mechanism at high-temperature10.1016/j.corsci.2023.111667 ↗