Chloride-induced pitting corrosion and stress corrosion cracking could present potential damage mechanisms in high activity waste (HAW) containers made of austenitic stainless steels operating at room temperature, elevated temperature, and humidity. In this paper, atmospheric corrosion tests were conducted on cold-rolled 316 L stainless steel (SS) specimens—both sensitised and non-sensitised—subjected to varying levels of applied stress (ranging from 0 to 1.5 times the yield strength, σ y ) in the presence of 0.546 mol/L artificial seawater droplets. A subset of the samples was thermally sensitised at 550°C for 150 hours. The experiments were conducted at room temperature (RT) and humidity levels, and at 50°C and 60% relative humidity (RH), using a custom-made environmental corrosion chamber for 672 hours. Stress was applied using a 4-point bending rig, and artificial seawater droplets were delivered via a SS 304 medical syringe needle. Correlative microscopy (SEM and EBSD), optical profilometry, and dry vapor etching techniques revealed pit initiation sites and growth predominantly occurring at grain boundaries along the rolling direction. Sensitisation and increased applied stress led to a rise in both the number and size of corrosion pits, as observed in experiments conducted both at room temperature and in the corrosion chamber.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (82)
Show source-provided references
1. World Nuclear Association, ‘Radioactive Waste Management’, 2022. Accessed: Aug. 22, 2022. [Online]. Available: 〈https://world-nuclear.org/information-library/nuclear-fuel-cycle/nuclear-wastes/radioactive-waste-management.aspx〉.
2. World Nuclear Association, ‘Radioactive Waste Management’, 2022. Accessed: Aug. 22, 2022. [Online]. Available: 〈https://world-nuclear.org/information-library/nuclear-fuel-cycle/nuclear-wastes/radioactive-waste-management.aspx〉.
3. SCC in PWRs: learning from a Bottom-Up Approach
4. S.Finsås Wika, ‘Pitting and Crevice Corrosion of Stainless Steel under Offshore Conditions’, MSc Thesis, Norwegian University of Science and Technology, Trondheim, 2012. [Online]. Available: 〈https://ntnuopen.ntnu.no/ntnu-xmlui/handle/11250/249144〉.
5. Corrosion behavior and mechanism of austenitic stainless steels in a new quaternary molten salt for concentrating solar power10.1016/j.solmat.2019.01.024 ↗
6. An efficient procedure for reducing in-line-inspection datasets for structural integrity assessments10.1016/j.tafmec.2017.07.005 ↗
7. J. Barrett et al., ‘The role of energy demand reduction in achieving net-zero in the UK’, the Centre for Research into Energy Demand Solutions, 2021.
8. A. Afanasyev, C.K. Anderson, J. Bergallo, K. Brammer, S.S. Kim, and P. Leister, ‘Basic Principles Objectives IAEA Nuclear Energy Series - Costing of Spent Nuclear Fuel Storage’, International Atomic Energy Agency, Vienna, 2009. [Online]. Available: 〈http://www.iaea.org/Publications/index.html〉.
9. J.D. Werner, ‘CRS Report for Congress U.S. Spent Nuclear Fuel Storage’, Congressional Research Service, 2012. [Online]. Available: 〈www.crs.gov〉.
10. Atmospheric stress corrosion cracking of stainless steel rock climbing anchors, Part 110.5006/3227 ↗
11. Corrosion cracking under main pipelines stress
12. Influence of pitting corrosion on fatigue and corrosion fatigue of ship and offshore structures, Part II: load - pit - crack interaction10.1515/pomr-2015-0057 ↗
13. Pitting corrosion of galvanized pipes in the hot water supply system10.1051/matecconf/201710603028 ↗
14. Stress corrosion cracking mechanism of AISI 316LN stainless steel rebars in chloride contaminated concrete pore solution using the slow strain rate technique10.1016/j.electacta.2019.135565 ↗
15. Bunn · 2022
16. Extended dry storage of used nuclear fuel: technical issues: a usa perspective10.5516/NET.2011.43.5.405 ↗
17. Annual average relative humidity value in Carlisle/Cumbria Region in the UK
18. WorldData, ‘Climate in Texas’, 2024. Accessed: May 10, 2024. [Online]. Available: 〈https://www.worlddata.info/america/usa/climate-texas.php〉.
19. Towards understanding stress corrosion cracking of austenitic stainless steels exposed to realistic sea salt brines10.1016/j.corsci.2024.111992 ↗
20. Physical and chemical properties of sea salt deliquescent brines as a function of temperature and relative humidity10.1016/j.scitotenv.2022.154462 ↗
21. Development of a consistent geochemical model of the Mg(OH)2–MgCl2–H2O system from 25°C to 120°C10.1016/j.apgeochem.2024.106032 ↗
22. Characterization of spent nuclear fuel canister surface roughness using surface replicating molds10.1038/s41598-024-71992-1 ↗
23. Variation of sea salt aerosol pH with relative humidity10.1029/2000GL012387 ↗
24. Localised dissolution kinetics, salt films and pitting potentials10.1016/S0010-938X(97)00049-8 ↗
25. Thermal stability of the passive film formed on 316L stainless steel surface studied by ToF-SIMS10.1016/j.corsci.2019.108395 ↗
26. Chloride-induced stress corrosion cracking of used nuclear fuel welded stainless steel canisters: a review10.1016/j.jnucmat.2015.07.043 ↗
27. Mechanical degradation of cold-worked 304 stainless steel in salt spray environments10.1016/j.jnucmat.2011.12.008 ↗
28. Mechanism of chlorine-induced stress corrosion cracking of two 304 SS heats in simulated marine environment through in situ X-ray tomography and diffraction: Role of deformation induced martensite and crack branching10.1016/j.matchar.2022.112020 ↗
29. Stress corrosion cracking of stainless-steel canister for concrete cask storage of spent fuel10.1016/j.jnucmat.2008.06.005 ↗
30. Low-temperature stress corrosion cracking of stainless steels in the atmosphere in the presence of chloride deposits10.5006/1.3319115 ↗
31. Toward understanding the effects of strain and chloride deposition density on atmospheric chloride-induced stress corrosion cracking of type 304 austenitic stainless steel under MgCl2 and FeCl3:MgCl2 droplets10.5006/3026 ↗
32. Standard guide for drying behavior of spent nuclear fuel
33. A study of dynamic nanoscale corrosion initiation events using HS-AFM10.1039/C8FD00017D ↗
34. Stress corrosion cracking in stainless steels
35. Smart · 2008
36. Applicability of the competition concept in determining the stress corrosion cracking behavior of austenitic stainless steels in chloride solutions10.3323/jcorr1991.46.313 ↗
37. Monitoring the degradation of nuclear waste packages induced by interior metallic corrosion using synchrotron X-ray tomography10.1016/j.conbuildmat.2019.04.178 ↗
38. Analogues for the Corrosion-induced Expansion of Iron in HLW containers10.1557/PROC-807-A73 ↗
39. Chloride induced stress corrosion cracking of type 304 and 304L stainless steels in air10.3323/jcorr1991.52.166 ↗
40. Effect of salt composition and microstructure on stress corrosion cracking of 316L austenitic stainless steel for dry storage canisters10.1016/j.jnucmat.2020.152572 ↗
41. Effect of grain size on corrosion: a review10.5006/1.3462912 ↗
42. Mechanical and electrochemical behavior of nanocrystalline surface of 304 stainless steel10.1016/S0013-4686(02)00365-1 ↗
43. Mechanical, electrochemical and tribological properties of nano-crystalline surface of 304 stainless steel10.1016/S0043-1648(03)00055-3 ↗
44. The effect of cold-rolling on the microstructure and corrosion behaviour of 316L alloy in FLiNaK molten salt10.1016/j.corsci.2018.07.006 ↗
45. Assessment of intergranular corrosion in AISI Type 316L stainless steel weldments10.1179/000705902225004419 ↗
46. Quantitative evaluation of aged AISI 316L stainless steel sensitization to intergranular corrosion: comparison between microstructural electrochemical and analytical methods10.1007/s11661-007-9114-9 ↗
47. Metastable pitting and the critical pitting temperature10.1149/1.1838691 ↗
48. Effect of temperature and salinity on the localized corrosion of stainless steel 316L10.4028/www.scientific.net/AMM.660.130 ↗
49. On the origin of passive film breakdown and metastable pitting for stainless steel 316L10.1016/j.corsci.2024.111911 ↗
50. H.F. Ebling and M.A. Scheil, ‘Time-Temperature-Sensitization (TTS) Diagrams for Types 347, 304L, and 316L Stainless Steels’, in Advances in the Technology of Stainless Steels and Related Alloys, ASTM International 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA 19428-2959, 1965, pp. 275–284. doi: 10.1520/STP43752S.10.1520/STP43752S ↗
51. Emulation of neutron irradiation effects with protons: validation of principle10.1016/S0022-3115(01)00751-6 ↗
52. Was · 2017
53. Effects of ageing conditions on the precipitates evolution, chromium depletion and intergranular corrosion susceptibility of AISI 316L: experimental and modeling results10.1016/j.msea.2003.12.017 ↗
54. J. Eaton-Mckay, ‘Creep Mechanics of Carburised 316H Stainless Steel in Advanced Gas-Cooled Reactor Environments’, Ph.D., The University of Manchester (United Kingdom), England, 2023. Accessed: Apr. 19, 2025. [Online]. Available: 〈https://www.proquest.com/docview/2861185203/abstract/31B955AEB83D4128PQ/1〉.
55. Intergranular corrosion of AISI 316L steel10.1016/S1044-5803(01)00125-5 ↗
56. ASTM D1141-98 · 2021
57. ASTM G39-99(2021) · 2021
58. The initiation and propagation of chloride-induced transgranular stress-corrosion cracking (TGSCC) of 304L austenitic stainless steel under atmospheric conditions10.1016/j.corsci.2014.07.017 ↗
59. Experimental investigation and analytical prediction of sigma phase precipitation in AISI 316L austenitic stainless steel10.1007/s11661-013-1647-5 ↗
60. D. Williams, ‘Application of Nano-Scale Characterization Techniques in Failure Analysis of Stress Corrosion Cracking in an Alloy C276 Pull Rod’, M.A.Sc., Queen’s University (Canada), Canada -- Ontario, CA, 2020. Accessed: Apr. 19, 2025. [Online]. Available: 〈https://www.proquest.com/docview/2524749666/abstract/C815231622354F61PQ/1〉.
61. Prediction of fatigue crack initiation life based on pit growth10.5006/1.3577891 ↗
62. Corrosion-fatigue: a review of damage tolerance models10.1080/09506608.2017.1375644 ↗
63. The role of corrosion pit topography on stress concentration10.1016/j.engfailanal.2023.107900 ↗
64. Effect of machining processes on the residual stress distribution heterogeneities and their consequences on the stress corrosion cracking resistance of AISI 316L SS in chloride medium10.1007/s00170-019-04410-w ↗
65. The effects of cold rolling orientation and water chemistry on stress corrosion cracking behavior of 316L stainless steel in simulated PWR water environments10.1016/j.jnucmat.2016.01.018 ↗
66. The aspect ratio of surface grooves and metastable pitting of stainless steel10.1016/S0010-938X(01)00039-7 ↗
67. Sensitivity of stress corrosion cracking of stainless steel to surface machining and grinding procedure10.1016/j.corsci.2011.06.020 ↗
68. Modelling of the evolution of stress corrosion cracks from corrosion pits10.1016/j.scriptamat.2005.10.053 ↗
69. Pitting corrosion of metals10.1149/2.F03101if ↗
70. Decline in pitting corrosion resistance of 316 L stainless steel induced by Cr-depleted layer during tribocorrosion10.1038/s41529-025-00569-8 ↗
71. An in-situ corrosion small punch test for developing stress corrosion cracking in stainless steel10.1007/s11340-025-01177-y ↗
72. Failure analysis of stress corrosion cracking of 316L stainless steel bend pipe in the atmospheric tower10.1016/j.engfailanal.2025.109519 ↗
73. Mass transfer and electrochemical kinetic interactions in localized pitting corrosion10.1002/aic.690320605 ↗
74. Aaltonen · 2002
75. Pitting corrosion of metals: a review of the critical factors10.1149/1.1838615 ↗
76. The mechanism of lacy cover formation in pitting10.1016/S0010-938X(97)00043-7 ↗
77. A.G. Penders, ‘Microstructural investigation of irradiation assisted stress corrosion cracking mechanisms based on focused ion beam analysis of tested and industrial specimens’, PhD Thesis, University of Antwerp, Antwerp, 2022. Accessed: Dec. 24, 2024. [Online]. Available: 〈https://repository.uantwerpen.be/desktop/irua〉.
78. Reflections on early stages of environmentally assisted cracking from corrosion pits10.3390/cmd2040030 ↗
79. M. Hashim, ‘Influence of Pit Morphology on Crack Propagation’, PhD Thesis, The University of Manchester, 2019. Accessed: Mar. 27, 2025. [Online]. Available: 〈https://www.proquest.com/docview/2429440550?pq-origsite=gscholar&fromopenview=true〉.
80. Directional corrosion behavior of cold-rolled and annealed 304L stainless steel: role of residual stress and phase transformation
81. Dislocation substructure vs transgranular stress corrosion susceptibility of single phase alloys10.5006/0010-9312-19.3.102 ↗
82. High voltage electron metallography of stress corrosion cracking of austenitic stainless steels10.1016/0010-938X(78)90033-1 ↗