Effect of hot corrosion on cycle deformation and fracture behavior of Ti-6Al-4V alloy under salt coating
Source abstract
Abstract
The effect of NaCl deposition on the deformation and fracture behavior during the cycle loading of dwell fatigue of Ti-6Al-4V alloy at 500 °C was investigated. Experimental results show that the hot corrosion reduces the dwell fatigue life of the alloy by up to 79 % compared with the bare (without salt) sample, and the degree of hot corrosion damage increase with the decrease of dwell stress. Comprehensive microstructural analysis suggests that the reduction of dwell fatigue life of the salt-coated sample is related to the crack initiation from surface corrosion pits/spalling pits and rapid crack propagation. Moreover, hot corrosion and creep damage are considered to exist competitive relationship during the failure process.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Nuclear Materials and Properties · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Feasibility of producing Ti-6Al-4V alloy for engineering application by powder compact extrusion of blended elemental powder mixtures10.1016/j.jallcom.2016.10.282 ↗
2. Effect of stress ratio on VHCF behavior for a compressor blade titanium alloy10.1016/j.ijfatigue.2016.05.004 ↗
3. An investigation of the effects of microstructure on dwell fatigue crack growth in Ti-624210.1016/j.msea.2005.05.097 ↗
4. Dwell sensitive fatigue in a near alpha titanium alloy at ambient temperature10.1016/S0142-1123(97)00020-0 ↗
5. Effects of α + β phase deformation on microstructure, fatigue and dwell fatigue behavior of a near alpha titanium alloy10.1016/j.ijfatigue.2016.05.023 ↗
6. A comparative study on dwell fatigue of Ti-6Al-2Sn-4Zr-xMo (x=2 to 6) alloys on a microstructure-normalized basis10.1007/s11661-014-2541-5 ↗
7. Effect of temperature and dwell time on fatigue crack growth behavior of CP-Ti10.3390/met8121031 ↗
8. Effect of dwell time on creep-fatigue life of a high-Nb TiAl alloy at 750°C10.1016/j.scriptamat.2015.07.018 ↗
9. Influence of complex LCF and dwell load regimes on fatigue of Ti–6Al–4V10.1016/j.actamat.2015.09.014 ↗
10. R.L. Ashbrook. A survey of salt deposits in compressors of flight gas turbine engines. NASA-TN-D-4999, 1969.
11. Corrosion behavior of Ti60 alloy under a solid NaCl deposit in wet oxygen flow at 600 °C
12. NaCl induced corrosion of Ti-6Al-4V alloy at high temperature10.1016/j.corsci.2016.04.016 ↗
13. Effect of streaming water vapor on the corrosion behavior of Ti60 alloy under a solid NaCl deposit in water vapor at 600 °C10.1016/j.corsci.2019.108177 ↗
14. The mechanisms of hot salt stress corrosion cracking in titanium alloy Ti-6Al-2Sn-4Zr-6Mo10.1016/j.corsci.2018.02.025 ↗
15. AgCl-induced hot salt stress corrosion cracking in a titanium alloy10.1016/j.corsci.2021.109497 ↗
16. The mechanism of thermal corrosion fatigue (TCF) on nickel-based single crystal superalloy and the corresponding structure shape effect10.1016/j.corsci.2020.109142 ↗
17. The effect of salt composition on the stress-free and corrosion-fatigue performance of a fine-grained nickel-based superalloy10.1016/j.corsci.2022.110113 ↗
18. Effects of tensile load hold time on the fatigue and corrosion-fatigue behavior of turbine blade materials10.1016/j.ijfatigue.2021.106448 ↗
19. Frequency and stress ratio effects in high cycle fatigue of Ti–6Al–4V10.1016/S0142-1123(99)00030-4 ↗
20. The influence of near service environmental conditions on the corrosion and LCF behaviour of a beta-stabilized γ-TiAl alloy10.1016/j.corsci.2020.108885 ↗
21. Effect of pre-hot salt corrosion on hot salt corrosion fatigue behavior of the TC11 titanium alloy at 500 °C
22. High-temperature cycle deformation and fracture behavior of advanced austenitic heat-resistant steel Sanicro25 alloy for A-USC power plants10.1007/s11661-022-06628-y ↗
23. Comparative investigation of oxidation behavior and hot corrosion behavior in NaCl–Na2SO4 mixture for a Ti2AlNb based alloy at 1023 K
24. Hot corrosion-creep interaction in IN718 under simulated marine environment: Introducing strain-associated-time (SAT) plots for comprehensive understanding10.1016/j.corsci.2021.109667 ↗
25. Effect of NaCl-rich environment on internal corrosion for Ti60 alloy at 600 °C10.1016/j.corsci.2023.111307 ↗
26. Internal crack initiation in high cycle fatigue at cryogenic temperatures10.1016/0013-7944(91)90257-2 ↗
27. Degradation mechanism of Ti-6Al-2Sn-4Zr-2Mo-Si alloy exposed to solid NaCl deposit at high temperature10.1016/j.corsci.2020.108611 ↗
28. A review of dwell sensitive fatigue in titanium alloys: the role of microstructure, texture and operating conditions10.1016/S0142-1123(03)00145-2 ↗
29. Influence of saline environment on creep rupture life of Nimonic-263 for marine turbine application10.1016/j.msea.2012.12.081 ↗
30. Enhanced creep properties of Y2O3-bearing Ti-48Al-2Cr-2Nb alloys10.1016/j.msea.2021.140952 ↗
31. Microstructure and high temperature oxidation behavior of the Al2O3 CPED coating on TiAl alloy10.1016/j.jallcom.2020.154271 ↗
32. The stress-corrosion cracking susceptibility of near-α titanium alloy IMI834 in presence of hot salt10.1016/j.corsci.2014.01.013 ↗
33. Hot corrosion damage mechanism of Ti6Al4V alloy in marine environment10.1016/j.vacuum.2021.110350 ↗
34. A new insight into the NaCl-induced hot corrosion mechanism of TiN coatings at 500°C10.1016/j.corsci.2020.108794 ↗
35. High temperature oxidation and hot corrosion behaviors of Ti2AlNb alloy at 923 K and 1023 K10.1016/j.corsci.2021.109336 ↗
36. Comparative study of corrosion-fatigue in aircraft materials10.2514/2.1308 ↗
37. Hertzberg · 2020
38. Effect of high temperature hot corrosion on the compression creep behavior of 12Cr1MoV alloys10.1515/htmp-2016-0027 ↗
39. High-temperature hot-corrosion effects on the creep-fatigue behavior of a directionally solidified nickel-based superalloy: Mechanism and lifetime prediction10.1177/1056789519891765 ↗