Ablation behavior and mechanism of (PyC-Csf)/ZrB2-SiC-ZrC ceramics sintered by reactive spark plasma sintering at low temperature
Source abstract
Abstract
The (PyC-C sf)/ZrB 2 -SiC-ZrC ceramics are fabricated by reactive spark plasma sintering (RSPS) at 1200 °C. The sample has a low density and intact pyrolytic carbon modified carbon fiber (PyC-C sf). After three cycles of ablation (heat flux = 2.38 MW/m 2, t = 120 s), samples demonstrate excellent resistance to oxidative ablation. The mass recession rate and linear recession rate for the sample are 3.41 g/m 2 ∙s and 0.68 µm/s, respectively. Excessive content of carbon destroys the oxide layer by forming large amounts of CO 2 during the ablation process. The inner layer of intact PyC-C sf aggregates around the borosilicate which are denser in the oxide layer. Finally, a porous ZrO 2-SiO 2 layer and a dense ZrO 2-SiO 2-C sf layer are formed on the surface of the sample which resists ablation.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. On the thermal shock resistance and mechanical properties of novel unidirectional UHTCMCs for extreme environments10.1038/s41598-018-27328-x ↗
2. Selection, processing, properties and applications of ultra-high temperature ceramic matrix composites, UHTCMCs – a review10.1080/09506608.2019.1652006 ↗
3. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
4. Inherent anisotropy in transition metal diborides and microstructure/property tailoring in ultra-high temperature ceramics—a review10.1016/j.jeurceramsoc.2017.09.012 ↗
5. Ultra-high temperature ceramics: materials for extreme environments10.1016/j.scriptamat.2016.10.018 ↗
6. Advances in ultra-high temperature ceramics, composites, and coatings10.1007/s40145-021-0550-6 ↗
7. In situ formation of oxidation resistant refractory coatings on SiC-reinforced ZrB2 ultra high temperature ceramics10.1111/j.1551-2916.2011.05032.x ↗
8. Pressureless sintering and physical properties of ZrB2-based composites with ZrSi2 additive10.1016/j.scriptamat.2007.11.019 ↗
9. A novel microstructural design to improve the oxidation resistance of ZrB2-SiC ultra-high temperature ceramics (UHTCs)10.1016/j.jallcom.2019.01.208 ↗
10. Contact-mechanical properties at intermediate temperatures of ZrB2 ultra-high-temperature ceramics pressureless sintered with Mo, Ta, or Zr disilicides10.1016/j.jeurceramsoc.2015.04.023 ↗
11. Changed oxidation behavior of ZrB2–SiC ceramics with the addition of ZrC10.1016/j.ceramint.2015.02.150 ↗
12. Oxidation behavior of zirconium diboride–silicon carbide at 1800 °C10.1016/j.scriptamat.2007.07.009 ↗
13. Initial oxidation behaviors of ZrB2-SiC-ZrC ternary composites above 2000 °C10.1016/j.jallcom.2017.10.034 ↗
14. Oxidation behavior of ZrB2-SiC-ZrC at 1700 °C10.1016/j.jeurceramsoc.2016.10.034 ↗
15. Oxidation behavior of carbon fiber-dispersed ZrB2-SiC-ZrC triple phase matrix composites in an oxyhydrogen torch environment10.1016/j.ceramint.2018.02.031 ↗
16. Ablation behavior of three-dimensional Cf/SiC-ZrC-ZrB2 composites prepared by a joint process of sol-gel and reactive melt infiltration10.1016/j.corsci.2018.02.011 ↗
17. Improved microstructure and fracture properties of short carbon fiber-toughened ZrB2-based UHTC composites via colloidal process10.1016/j.ijrmhm.2016.07.010 ↗
18. Development of short- and continuous carbon fiber-reinforced ZrB2-SiC-ZrC matrix composites for thermal protection systems10.1016/j.ceramint.2018.05.268 ↗
19. Characteristics of spark plasma sintered ZrB2-SiC-SCFs composites10.1016/j.ceramint.2018.12.109 ↗
20. Enhanced oxidation properties of ZrB2–SiC composite with short carbon fibers at 1600 °C10.1016/j.ceramint.2021.02.114 ↗
21. Pressureless sintering and ablation behavior of PyC-Csf/ZrB2-SiC-ZrC ceramics doped with B4C
22. Carbon fiber reinforced ultra-high temperature ceramic matrix composites: a review10.1016/j.ceramint.2019.05.065 ↗
23. Continuous carbon fiber reinforced ZrB2-SiC composites fabricated by direct ink writing combined with low-temperature hot-pressing10.1016/j.jeurceramsoc.2022.03.045 ↗
24. Starting from essence to reveal the ablation behavior and mechanism of 3D PyC Cf/ZrC-SiC composite10.1016/j.corsci.2022.110261 ↗
25. Carbon fiber reinforced CMC for high-performance structures
26. Ablation behavior of ZrC-SiC-ZrB2 and ZrC-SiC inhibited carbon/carbon composites components under ultrahigh temperature conditions10.1016/j.corsci.2021.109598 ↗
27. Spark plasma sintering of quadruplet ZrB2–SiC–ZrC–Cf composites10.1016/j.ceramint.2019.08.243 ↗
28. Microstructure characteristic, mechanical properties and sintering mechanism of nanocrystalline copper obtained by SPS process10.1016/j.msea.2009.07.016 ↗
29. The ablation behavior and mechanical property of C/C-SiC-ZrB2 composites fabricated by reactive melt infiltration10.1016/j.ceramint.2017.02.008 ↗
30. Ablation behavior of sharp-shape C/C-SiC-ZrB2 composites under oxyacetylene flame10.1016/j.jallcom.2017.04.188 ↗
31. Ablation resistance of wedge-shaped C/C-ZrB2-ZrC-SiC composites exposed to an oxyacetylene torch10.1016/j.corsci.2016.08.010 ↗
32. Effect of heat flux on ablation behaviour and mechanism of C/C–ZrB2–SiC composite under oxyacetylene torch flame10.1016/j.corsci.2013.04.052 ↗
33. Long-term and cyclic ablation behavior of La2O3 modified Cf/ZrB2-SiC composites at 2500℃10.1016/j.corsci.2022.110538 ↗
34. Oxidation-resistant ZrB2–SiC composites at 2200 °C10.1016/j.compscitech.2007.08.017 ↗
35. ZrB2-based "Brick-and-Mortar" composites achieving the synergy of superior damage tolerance and ablation resistance10.1021/acsami.0c08206 ↗
36. Multi-cycle and long-term ablation behavior of Cf/ZrB2-SiC composites at 2500 °C10.1016/j.corsci.2021.109385 ↗
37. Long-term ablation behavior and mechanisms of 2D-Cf/ZrB2-SiC composites at temperatures up to 2400 °C10.1016/j.corsci.2020.108967 ↗
38. Enhancement of oxidation resistance via a self-healing boron carbide coating on diamond particles10.1038/srep20198 ↗
39. Enhanced tensile strength and thermal conductivity in copper diamond composites with B4C coating
40. Oxidation behaviour of a continuous carbon fibre reinforced ZrB2–SiC composite10.1016/j.corsci.2017.04.012 ↗
41. Using flexible hydrothermal carbon-coated continuous carbon fiber to fabricate Cf/ZrB2-SiC composites by fused deposition modeling and precursor infiltration pyrolysis
42. Effect of pyrolytic carbon coating on the microstructure and fracture behavior of the Cf/ZrB2-SiC composite10.1016/j.ceramint.2018.07.210 ↗
43. Ablation behaviour of Csf/ZrB2-SiC composites fabricated by direct ink writing and reactive melt infiltration10.1016/j.jeurceramsoc.2023.02.034 ↗
44. Ablation behavior and mechanisms of 3D Cf/ZrB2-SiC composite applied in long-term temperature up to 2400 °C10.1016/j.corsci.2021.109706 ↗
45. Ablation behavior of Cf/ZrC-SiC-based composites fabricated by an improved reactive melt infiltration10.1016/j.jeurceramsoc.2019.07.007 ↗
46. Achieving the synergy of superior damage tolerance and oxidation resistance of 2D Cf/ZrB2-SiC composites via fiber heat treatment10.1016/j.apsusc.2021.149807 ↗
47. Oxidation of SiC-based ceramics at high temperature10.2320/materia.52.434 ↗
48. Use of volume element methods to understand experimental differences in active/passive transitions and active oxidation rates for SiC10.1111/jace.12141 ↗
49. Thermochemical and mechanical stabilities of the oxide scale of ZrB2+SiC and oxygen transport mechanisms10.1111/j.1551-2916.2008.02319.x ↗
50. High-temperature active/passive oxidation and bubble formation of CVD SiC in O2 and CO2 atmospheres10.1016/S0955-2219(02)00139-5 ↗
51. Arc-jet wind tunnel characterization of ultra-high-temperature ceramic matrix composites10.1016/j.corsci.2018.12.039 ↗