Improvement on corrosion resistance of molten calcium-magnesium-alumina-silicate (CMAS) by Yb2O3-Y2O3 co-stabilized ZrO2 ceramic pellets
Source abstract
Abstract
Five types of ceramic pellets with different doping contents of Yb 2O 3-Y 2O 3 co-stabilized ZrO 2 (YbYSZ) (x mol.% Yb 2O 3 - (4.5-x) mol.% Y 2O 3-ZrO 2 ; X = 0 (YSZ), 1, 2, 3, 4) were designed to investigate corrosion behavior under CMAS attack. The results show that the corrosion resistance of YbYSZ increased with increasing Yb 2O 3 content, which was attributed to the excellent phase stability and lower diffusion of Yb 3+. More degradation with microstructural destruction was observed in the YSZ pellets, and less degradation was observed in YbYSZ with 4 mol.% Yb 2O 3 (YbYSZ-4). Further, YbYSZ-4 performs a larger contact angle than others, promoting CMAS resistance.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (78)
Show source-provided references
1. Role of Re in NiAl bond coating on isothermal oxidation behavior of a thermal barrier coating system at 1100 ℃10.1016/j.corsci.2023.111151 ↗
2. Study on the oxidation behavior of a novel thermal barrier coating system using the nanocrystalline coating as bonding coating on the single-crystal superalloy10.1016/j.corsci.2023.111591 ↗
3. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
4. Effect of pre-oxidation on the failure mechanisms of EB-PVD thermal barrier coatings with (Ni,Pt)Al bond coats10.1016/j.corsci.2021.109873 ↗
5. Column formation in suspension plasma-sprayed coatings and resultant thermal properties10.1007/s11666-011-9632-2 ↗
6. Highly durable thermal barrier coatings made by the solution precursor plasma spray process10.1016/j.surfcoat.2003.06.023 ↗
7. Thermal conductivity analysis and lifetime testing of suspension plasma-sprayed thermal barrier coatings10.3390/coatings4030630 ↗
8. Plasma spray-PVD: A new thermal spray process to deposit out of the vapor phase10.1007/s11666-011-9654-9 ↗
9. Vapor phase deposition using plasma spray-PVD (TM)10.1007/s11666-009-9428-9 ↗
10. YSZ/NiCrAlY interface oxidation of APS thermal barrier coatings10.1016/j.corsci.2018.06.035 ↗
11. A coupled theory for deformation and phase transformation due to CMAS infiltration and corrosion of thermal barrier coatings10.1016/j.corsci.2021.109690 ↗
12. Evolution of the microstructure and mechanisms of performance degradation in EB-PVD YSZ thermal barrier coatings corroded by volcanic ash at 1150 °C10.1016/j.corsci.2022.110626 ↗
13. Thermal cyclic behavior of air plasma sprayed thermal barrier coatings sprayed on stainless steel substrates10.1016/j.surfcoat.2006.10.022 ↗
14. Effect of neck formation on the sintering of air-plasma-sprayed thermal barrier coating system10.1016/j.jeurceramsoc.2016.08.033 ↗
15. Effects of sintering and mixed oxide growth on the interface cracking of air-plasma-sprayed thermal barrier coating system at high temperature10.1016/j.apsusc.2015.10.037 ↗
16. Hot corrosion behavior of plasma sprayed La2Ce2O7/YSZ thermal barrier composite coating in the presence of Sulfate and Vanadate molten Salts
17. Hot corrosion behavior of solution precursor and atmospheric plasma sprayed thermal barrier coatings10.1016/j.corsci.2015.05.034 ↗
18. Hot corrosion of high-entropy hafnate for thermal barrier coating material subjected to molten CMAS10.1016/j.corsci.2022.110714 ↗
19. Effect of TGO creep on top-coat cracking induced by cyclic displacement instability in a thermal barrier coating system10.1016/j.surfcoat.2014.06.052 ↗
20. Local stress evolution in thermal barrier coating system during isothermal growth of irregular oxide layer10.1016/j.surfcoat.2012.11.052 ↗
21. Bending-driven failure mechanism and modelling of double-ceramic-layer thermal barrier coating system10.1016/j.ijsolstr.2017.10.024 ↗
22. Competition mechanism of interfacial cracks in thermal barrier coating system10.1016/j.matdes.2017.07.018 ↗
23. Modelling of TBC system failure: Stress distribution as a function of TGO thickness and thermal expansion mismatch10.1016/j.engfailanal.2004.12.027 ↗
24. Corrosion behavior and thermos-physical properties of a promising Yb2O3 and Y2O3 co-stabilized ZrO2 ceramic for thermal barrier coatings subject to calcium-magnesium-aluminum-silicate (CMAS) deposition: Experiments and first-principles calculation10.1016/j.corsci.2020.109230 ↗
25. 9.Research on aggressiveness of CMAS+NaVO3 mixtures towards thermal barrier coatings from the perspective of physical and chemical characteristics10.1016/j.corsci.2023.111463 ↗
26. CMAS + sea salt corrosion to thermal barrier coatings10.1016/j.corsci.2023.111172 ↗
27. Effect of CMAS infiltration on radiative transport through an EB-PVD thermal barrier coating10.1111/j.1744-7402.2008.02225.x ↗
28. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
29. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
30. Mechanisms of cracking and delamination within thick thermal barrier systems in aero-engines subject to calcium-magnesium-alumino-silicate (CMAS) penetration10.1016/j.msea.2008.01.006 ↗
31. CMAS penetration-induced cracking behavior in the ceramic top coat of APS TBCs10.1016/j.ceramint.2019.04.152 ↗
32. Corrosion resistance and thermal-mechanical properties of ceramic pellets to molten calcium-magnesium-alumina-silicate (CMAS)10.1016/j.ceramint.2019.06.223 ↗
33. CMAS corrosion behavior of a novel high entropy (Nd0.2Gd0.2Y0.2Er0.2Yb0.2)2Zr2O7 thermal barrier coating materials10.1016/j.corsci.2023.111529 ↗
34. 5.Investigating the interface cracking mechanism of CMAS-corroded thermal barrier coatings based on the cohesive zone model10.1016/j.corsci.2022.110337 ↗
35. High-temperature degradation of the in-situ laser-glazed plasma sprayed LaMgAl11O19 thermal barrier coating exposed to Ca-Mg-Al-silicate deposits10.1016/j.corsci.2020.108934 ↗
36. Thermal cycling performance of La2Ce2O7/50 vol% YSZ composite thermal barrier coating with CMAS corrosion10.1016/j.jeurceramsoc.2018.02.025 ↗
37. Effects of Er stabilization on thermal property and failure behavior of Gd2Zr2O7 thermal barrier coatings10.1016/j.corsci.2021.109418 ↗
38. CMAS resistance characteristics of LaPO4/YSZ thermal barrier coatings at 1250 ℃-1350 ℃10.1016/j.corsci.2019.04.014 ↗
39. Corrosion resistance of GdPO4 thermal barrier coating candidate in the presence of CMAS+NaVO3 and CMAS10.1016/j.corsci.2022.110628 ↗
40. Plasma-sprayed thermal barrier coatings with enhanced splat bonding for CMAS and corrosion protection10.1007/s11666-015-0345-9 ↗
41. Lifetime and failure modes of plasma sprayed thermal barrier coatings in thermal gradient rig tests with simultaneous CMAS injection10.1016/j.surfcoat.2017.04.071 ↗
42. Adsorbability and spreadability of calcium-magnesium-alumino-silicate (CMAS) on Al-modified 7YSZ thermal barrier coating10.1016/j.ceramint.2016.09.106 ↗
43. EB-PVD alumina (Al2O3) as a top coat on 7YSZ TBCs against CMAS/VA infiltration: Deposition and reaction mechanisms10.1016/j.jeurceramsoc.2018.03.027 ↗
44. In situ synthesis of alpha-alumina layer on thermal barrier coating for protection against CMAS (CaO-MgO-Al2O3-SiO2) corrosion10.1016/j.surfcoat.2014.11.064 ↗
45. Protectiveness of Pt and Gd2Zr2O7 layers on EB-PVD YSZ thermal barrier coatings against calcium-magnesium-alumina-silicate (CMAS) attack10.1016/j.ceramint.2015.05.128 ↗
46. Corrosion resistant plasma sprayed (Y0.8Gd0.2)(3)Al5O12/YSZ thermal barrier coatings towards molten calcium-magnesium-alumina-silicate10.1016/j.ceramint.2019.01.114 ↗
47. An interpretation of glass chemistry in terms of the optical basicity concept10.1016/0022-3093(76)90027-2 ↗
48. 10.2ZrO2·Y2O3 Thermal barrier coatings resistant to degradation by molten CMAS: Part I, Optical basicity considerations and processing10.1111/jace.13210 ↗
49. Hot corrosion behavior of BaLa2Ti3O10 exposed to calcium-magnesium-alumina-silicate at elevated temperatures10.1016/j.ceramint.2018.03.021 ↗
50. Composition effects of thermal barrier coating ceramics on their interaction with molten Ca-Mg-Al-silicate (CMAS) glass10.1016/j.actamat.2012.06.053 ↗
51. Calcium-magnesium aluminosilicate (CMAS) reactions and degradation mechanisms of advanced environmental barrier coatings10.1016/j.surfcoat.2013.08.036 ↗
52. Interaction between Yb2O3-Y2O3 co-stabilized ZrO2 ceramic powder and molten silicate deposition, and its implication on thermal barrier coating application10.1016/j.matchar.2021.111418 ↗
53. Coprecipitation synthesis and thermal conductivity of La2Zr2O710.1016/j.jallcom.2009.02.081 ↗
54. Air plasma-sprayed yttria and yttria-stabilized zirconia thermal barrier coatings subjected to calcium-magnesium-alumino-silicate (CMAS)10.1007/s11666-014-0107-0 ↗
55. Deposition and properties of a multilayered thermal barrier coating10.1016/j.surfcoat.2016.01.001 ↗
56. Pore filling behavior of YSZ under CMAS attack: Implications for designing corrosion-resistant thermal barrier coatings10.1111/jace.15790 ↗
57. Novel thermal barrier coatings that are resistant to high-temperature attack by glassy deposits10.1016/j.actamat.2007.08.028 ↗
58. 14.Volcanic ash melting under conditions relevant to ash turbine interactions10.1038/ncomms10795 ↗
59. Structural study of metastable tetragonal YSZ powders produced via a sol-gel route10.1016/j.jallcom.2006.10.155 ↗
60. Volcanic ash melting under conditions relevant to ash turbine interactions10.1038/ncomms10795 ↗
61. Interaction between ceramic powder and molten calcia-magnesia-alumino-silicate (CMAS) glass, and its implication on CMAS-resistant thermal barrier coatings10.1016/j.scriptamat.2015.09.027 ↗
62. The tetragonal-monoclinic transformation in zirconia: Lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
63. 2ZrO2•Y2O3 thermal barrier coatings resistant to degradation by molten CMAS: part II, interactions with sand and fly ssh10.1111/jace.13209 ↗
64. Equimolar YO1.5 and TaO2.5 co-doped ZrO2 as a potential CMAS-resistant material for thermal barrier coatings10.1111/jace.17514 ↗
65. Comparative study of EB-PVD gadolinium-zirconate and yttria-rich zirconia coatings performance against Fe-containing calcium-magnesium-aluminosilicate (CMAS) infiltration10.1016/j.corsci.2021.109660 ↗
66. Environmental-barrier coating ceramics for resistance against attack by molten calcia-magnesia-aluminosilicate (CMAS) glass: Part II, β-Yb2Si2O7 and β-Sc2Si2O710.1016/j.jeurceramsoc.2018.03.010 ↗
67. Influence of rare earth oxides on kinetics and reaction mechanisms in CMAS silicate melts10.1016/j.jeurceramsoc.2019.06.036 ↗
68. Corrosion behavior and thermos-physical properties of a promising Yb2O3 and Y2O3 co-stabilized ZrO2 ceramic for thermal barrier coatings subject to calcium-magnesium-aluminum-silicate (CMAS) deposition: Experiments and first-principles calculation10.1016/j.corsci.2020.109230 ↗
69. Interaction between Yb2O3-Y2O3 co-stabilized ZrO2 ceramic powder and molten silicate deposition, and its implication on thermal barrier coating application10.1016/j.matchar.2021.111418 ↗
70. Preparation and conductivity of Yb2O3-Y2O3 and Gd2O3-Y2O3 co-doped zirconia ceramics10.1016/j.ssi.2008.03.003 ↗
71. Effect of scandia content on the thermal shock behavior of SYSZ thermal sprayed barrier coatings10.1016/j.ceramint.2016.04.018 ↗
72. Nonisothermal viscous sintering of volcanic ash10.1002/2014JB011453 ↗
73. Volcanic sintering: Timescales of viscous densification and strength recovery10.1002/2013GL058105 ↗
74. Propagation of capillary waves and ejection of small droplets in rapid droplet spreading10.1017/jfm.2012.49 ↗
75. Review of non-reactive and reactive wetting of liquids on surfaces10.1016/j.cis.2007.04.009 ↗
76. Novel thermal barrier coatings repel and resist molten silicate deposits10.1016/j.scriptamat.2018.12.028 ↗
77. Preparation and CMAS wettability investigation of CMAS corrosion resistant protective layer with micro-nano double scale structure10.3390/coatings12050648 ↗
78. Hot corrosion behavior and wettability of calcium–magnesium–alumina–silicate (CMAS) on LaTi2Al9O19 ceramic