Stress corrosion behavior and mechanism of Ti6321 alloy with different microstructures in stimulated deep-sea environment
Source abstract
Abstract
The stress corrosion cracking (SCC) behaviors of Ti-6Al-3Nb-2Zr-1Mo (Ti6321, in wt %) alloy samples with equiaxed microstructure (EM), bimodal microstructure (BM) and Widmanstätten microstructure (WM) in simulated 3000 m deep sea environment were investigated using electrochemical tests, electron backscattered diffraction (EBSD), and so on. WM exhibits the best SCC resistance, which is attributed to its best self-healing ability, and is beneficial for the re-passivation of fresh metal at the crack tip. Besides, there is no obvious micro-texture region in WM with higher β phase, and α phase colonies hinder the dislocation movement, resulting in the lowest crack growth rate.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. A stochastic analysis of the effect of hydrostatic pressure on the pit corrosion of Fe-20Cr alloy10.1016/j.electacta.2009.02.010 ↗
2. New understanding of the effect of hydrostatic pressure on the corrosion of Ni-Cr-Mo-V high strength steel10.1016/j.corsci.2013.04.013 ↗
3. The performance of Al-Zn-In-Mg-Ti sacrificial anode in simulated deep water environment10.1016/j.corsci.2013.07.029 ↗
4. Effect of hydrostatic pressure on the corrosion behavior of a low alloy steel10.1149/2.040303jes ↗
5. A review of studies on corrosion of metals and alloys in deep-sea environment10.1016/j.oceaneng.2014.05.003 ↗
6. Hydrostatic pressure effects on stress corrosion cracking of X70 pipeline steel in a simulated deep-sea environment10.1016/j.ijhydene.2017.09.061 ↗
7. Influence of hydrostatic pressure on the corrosion behavior of 90/10 copper-nickel alloy tube under alternating dry and wet condition10.1016/j.corsci.2018.10.036 ↗
8. Stress corrosion cracking (SCC) and hydrogen-assisted cracking in titanium alloys
9. The effect of strain rate on stress corrosion performance of Ti6Al4V alloy produced by additive manufacturing process10.1016/j.jmrt.2020.02.035 ↗
10. Influence of NaCl environment on stress corrosion cracking of additive manufactured Ti-6Al-4V alloy10.1016/j.engfailanal.2021.105515 ↗
11. Crack size effects on the chemical driving force for aqueous corrosion fatigue10.1007/BF02814848 ↗
12. Stress corrosion cracking facet crystallography of Ti-8Al-1Mo-1V10.1016/j.corsci.2010.05.046 ↗
13. Effect of hydrogen and strain rate upon the ductility of mill-annealed Ti6Al4V10.1016/S0010-938X(98)00109-7 ↗
14. Influence of microstructure on corrosion behavior of Ti-5%Ta-1.8%Nb alloy10.1007/s10853-007-1773-9 ↗
15. Effects of microtexture and Ti3Al (α2) precipitates on stress-corrosion cracking properties of a Ti-8Al-1Mo-1V alloy10.1016/j.corsci.2016.12.012 ↗
16. Selection of optimum microstructure for improved corrosion resistance in a Ti-5%Ta-1.8%Nb alloy10.1016/j.jnucmat.2005.05.007 ↗
17. Influence of microstructure and alloying elements on corrosion behavior of Ti–13Nb–13Zr alloy10.1016/S0010-938X(03)00186-0 ↗
18. Annealed microstructure dependent corrosion behavior of Ti-6Al-3Nb-2Zr-1Mo alloy10.1016/j.jmst.2020.05.058 ↗
19. Influence of phase composition on stress-corrosion cracking of ti-6mo-5v-3al-2fe-2zr alloy in 3.5% NaCl solution10.3390/cryst12121794 ↗
20. The relationship between crystallographic texture and salt water cracking susceptibility in Ti6Al4V10.1016/0921-5093(95)09820-8 ↗
21. Stress corrosion characteristics of electron beam welded titanium alloys joints in NaCl solution10.1016/j.matchar.2022.112126 ↗
22. A primary study of the effect of hydrostatic pressure on stress corrosion cracking of Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2019.108402 ↗
23. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗
24. Chemical composition and semiconducting behaviour of stainless steel passive films in contact with artificial seawater10.1016/S0010-938X(98)00016-X ↗
25. Semiconducting properties of passive films formed on stainless steels: influence of the alloying elements10.1149/1.1838880 ↗
26. Electrochemical and semiconducting properties of thin passive film formed on titanium in chloride medium at various pH conditions10.1016/j.tsf.2015.12.025 ↗
27. Microstructural evolution and corrosion behavior of Ti-6Al-4V alloy fabricated by laser metal deposition for dental applications10.1016/j.jmrt.2021.07.006 ↗
28. The potential distribution at the tio2 aqueous electrolyte interface10.1149/1.2129316 ↗
29. Role of electrolyte chemistry on electronic and in vitro electrochemical properties of micro-arc oxidized titania films on Cp Ti10.1016/j.electacta.2013.05.032 ↗
30. Corrosion behavior and passive film characteristics formed on Ti, Ti3SiC2, and Ti4AlN3 in H2SO4 and HCl10.1149/1.1637897 ↗
31. Effects of dissolved oxygen on electrochemical and semiconductor properties of 316L stainless steel10.1016/j.jnucmat.2010.10.010 ↗
32. In vitro electrochemical behavior of aged ti-6al-4v alloy: a trial of the point defect model
33. Understanding the “blue spot.10.1016/j.engfailanal.2015.06.008 ↗
34. Effect of lamellar α on the stress corrosion cracking of Ti-6Al-4 V alloy in simulated oilfield brine10.1016/j.matchar.2021.111000 ↗
35. Fatigue crack growth mechanisms in Ti6242 lamellar microstructures: Influence of loading frequency and temperature10.1007/s11661-003-0016-1 ↗
36. Microstructure and fatigue crack growth mechanisms in high temperature titanium alloys10.1016/j.ijfatigue.2010.02.001 ↗
37. Influence of phase composition on stress-corrosion cracking of ti-6mo-5v-3al-2fe-2zr alloy in 3.5% NaCl solution10.3390/cryst12121794 ↗
38. The mechanism of aqueous stress-corrosion cracking of α+β titaniumalloys10.1016/j.corsci.2017.05.025 ↗
39. Stress corrosion cracking of TC4 ELI alloy with different microstructure in 3.5% NaCl solution10.1016/j.matchar.2022.112357 ↗