Effect of inhomogeneous microstructures on stress corrosion cracking sensitivity of 2050-T84 Al-Li alloy thick plate
Source abstract
Abstract
Inhomogeneous microstructures in the thickness direction and stress corrosion cracking of 2050-T84 Al-Li alloy thick plate was investigated. The quarter layer of alloy thick plate exhibited the highest stress corrosion cracking sensitivity, which was related to AlCuMnFe IMPs, subgrains, orientation, T 1 phase and dislocation density. In the quarter layer, the obstruction of subgrains to deformation bands resulted in significant stress concentration. Cracks originated from corrosion pits caused by AlCuMnFe IMPs around subgrains. The dealloying corrosion of T 1 phase and the presence of Goss texture increased the brittleness of the alloy, further accelerating the stress corrosion cracking of the quarter layer.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Nanoporous metals and alloys · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Wanhill · 2013
2. Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al-Li alloys: a review10.1016/j.jare.2017.12.004 ↗
3. Recent developments in advanced aircraft aluminium alloys10.1016/j.matdes.2013.12.002 ↗
4. Development and characterization of Al-Li alloys10.1016/j.msea.2006.01.045 ↗
5. Fabrication methods to manufacture isotropic Al-Li alloys and products for space and aerospace applications10.1016/S0921-5093(98)00827-2 ↗
6. Aluminum-copper-lithium alloy 2050 developed for medium to thick plate10.1007/s11665-009-9554-z ↗
7. The evolution of Al-Li base products for aerospace and space applications10.1007/s11661-012-1155-z ↗
8. Corrosion-induced mechanical properties degradation of Al-Cu-Li (2198-T351) aluminium alloy and the role of side-surface cracks10.1016/j.corsci.2021.109330 ↗
9. Enhanced strength and corrosion resistance of creep-aged AA2050 Al-Li alloy by pre-rolling deformation10.1016/j.matdes.2023.111621 ↗
10. Effect of aging treatment on the exfoliation corrosion and stress corrosion cracking behaviors of 2195 Al-Li alloy10.1016/j.matdes.2014.11.007 ↗
11. Stress-corrosion cracking characterisation of the advanced aerospace Al-Li 2099-T86 alloy10.1016/j.msea.2016.07.013 ↗
12. Coupling effect on corrosion behavior of multi-phase AlCuMnFe IMPs in 2050-T84 Al-Li alloy10.1016/j.corsci.2023.111462 ↗
13. Insights on the Al-Cu-Fe-Mn intermetallic particles induced pitting corrosion of Al-Cu-Li alloy10.1016/j.corsci.2020.109040 ↗
14. Corrosion of AA2024-T3 Part I: Localised corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
15. Study of localized corrosion in AA2024 aluminium alloy using electron tomography10.1016/j.corsci.2012.02.001 ↗
16. The effect of inhomogeneous microstructures on strength and fatigue properties of an Al-Cu-Li thick plate10.1016/j.msea.2018.06.033 ↗
17. Effect of average pass reduction ratio on thickness-oriented microstructure and properties homogeneity of an Al-Zn-Mg-Cu aluminum alloy thick plate10.1007/s00339-019-2683-9 ↗
18. Influence of multi-microstructural alterations on tensile property inhomogeneity of 7055 aluminum alloy medium thick plate10.1016/j.matchar.2016.01.020 ↗
19. Influence of microstructural and crystallographic inhomogeneity on tensile anisotropy in thick-section Al-Li-Cu-Mg plates10.1016/j.msea.2021.142135 ↗
20. Through-thickness inhomogeneity of precipitate distribution and pitting corrosion behavior of Al-Li alloy thick plate10.1016/S1003-6326(19)65087-9 ↗
21. Improving the strength and SCC resistance of an Al-5Mg-3Zn alloy with low-angle grain boundary structure10.1016/j.jmst.2023.02.063 ↗
22. Simultaneously improving tensile properties and stress corrosion cracking resistance of 7075-T6 aluminum alloy by USRP treatment10.1016/j.corsci.2023.111211 ↗
23. Enhancing the stress corrosion cracking resistance of a low-Cu containing Al-Zn-Mg-Cu aluminum alloy by step-quench and aging heat treatment10.1016/j.corsci.2019.108184 ↗
24. Some effects of alloy composition on stress corrosion cracking in Al–Zn–Mg–Cu alloys10.1016/j.corsci.2015.05.016 ↗
25. SCC susceptibility of RRA treated high-zinc 7068 aluminum alloy10.1016/j.corsci.2023.111257 ↗
26. Dislocation-aided electrochemical behavior of precipitates in stress corrosion cracking of Al-Zn-Mg-Cu alloys
27. SCC evaluation of a 2297 Al-Li alloy rolled plate using the slow-strain rate technique10.1016/j.cja.2019.01.022 ↗
28. Effects of critical defects on stress corrosion cracking of Al-Zn-Mg-Cu-Zr alloy10.1016/j.jmrt.2021.03.070 ↗
29. Effects of microstructure and local mechanical fields on intergranular stress corrosion cracking of a friction stir welded aluminum–copper–lithium 2050 nugget10.1016/j.corsci.2014.05.001 ↗
30. Through-thickness inhomogeneity of localized corrosion in 7050-T7451 Al alloy thick plate10.1007/s11771-015-2769-2 ↗
31. Effects of heat treatment and pre-stretching on the mechanical properties and microstructure evolution of extruded 2050 Al–Cu–Li alloy10.1016/j.msea.2022.143236 ↗
32. SVET, SKP and EIS study of the corrosion behaviour of high strength Al and Al–Li alloys used in aircraft fabrication10.1016/j.corsci.2014.03.001 ↗
33. Enhanced corrosion resistance of AZ31 Mg alloy by one-step formation of PEO/Mg-Al LDH composite coating10.1016/j.corcom.2022.05.001 ↗
34. Evaluation of dislocation density for 1100 aluminum with different grain size during tensile deformation by using in-situ x-ray diffraction technique10.2320/matertrans.L-M2015803 ↗
35. Corrosion and anodizing behavior of T1 (Al2CuLi) precipitates in Al-Cu-Li alloy10.1149/2.0891912jes ↗
36. Precipitation of T1 phase in 2198 Al-Li alloy studied by atomic-resolution HAADF-STEM10.1557/jmr.2019.136 ↗