Abstract

Corrosion pits preferentially initiate in the bainitic regions of Q420qNH steel against the simulated marine atmospheric environment, where a high initial dislocation density is present. This occurs in addition to the initiation sites associated with nonmetallic inclusions that exhibit significant lattice distortion. The formation of corrosion the corrosion-induced non elastic buckling exacerbates the cyclic softening effect and significantly reduces fatigue strength. At a strain amplitude of 0.4 %, the fatigue life decreases by 73.2 % after 60 days of pre-corrosion treatment. Layered segregation of Cr and Cu alloying elements could develop the formation of dense rust layer to inhibit further surface degradation.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Material Properties and Failure Mechanisms · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (67)

Show source-provided references
1. Murata · 2000
2. Influence of carbon content and microstructure on corrosion behaviour of low alloy steels in a cl− containing environment10.1016/j.corsci.2008.10.025 ↗
3. Rust layer adhesion capability and corrosion behavior of weathering steel under tension during initial stages of simulated marine atmospheric corrosion10.1016/j.conbuildmat.2019.117393 ↗
4. Corrosion characteristics of Q690qE high-strength bridge steel in simulated coastal–industrial environment and its influence on mechanical and corrosion fatigue behaviors10.1016/j.conbuildmat.2022.127830 ↗
5. Estimating the effects of corrosion pits on the fatigue life of steel plate based on the 3D profile10.1016/j.ijfatigue.2014.11.003 ↗
6. Tensile and low cycle fatigue behavior of corroded reinforcing steel bars S40010.1016/j.conbuildmat.2005.12.012 ↗
7. Experimental study on fatigue strength of corroded bridge wires10.1061/(ASCE)BE.1943-5592.0000366 ↗
8. Corrosion pit size distributions and fatigue lives—a study of the EIFS technique for fatigue design in the presence of corrosion10.1016/S0142-1123(03)00069-0 ↗
9. Corrosion fatigue life prediction of a steel shaft material in seawater10.1016/j.engfailanal.2013.08.004 ↗
10. ISO 14993:2018, Corrosion of metals and alloys accelerated testing involving cyclic exposure to salt mist, dry and wet condition, (2018). 〈https://www.antpedia.com/standard/7951388.html〉.
11. New insights into the corrosion behaviour of medium manganese steel exposed to a NaCl solution spray10.1016/j.conbuildmat.2020.119908 ↗
12. ASTM G 31-21, Standard Guide for Laboratory Immersion Corrosion Testing of Metals, (2021). 〈https://www.cssn.net.cn/cssn/productDetail/0fbd50d4da5c1fb76187f22f9fe4e3ac〉.
13. ASTM E606, Standard Test Method for Strain-Controlled Fatigue Testing, (2021). 〈https://www.cssn.net.cn/cssn/productDetail/b02fd6e16dfa3cafb0334c74a89e84b7〉.
14. Atmospheric corrosion data of weathering steels. a review10.1016/j.corsci.2013.08.021 ↗
15. Insight into the corrosion behaviour and degradation mechanism of pure zinc in simulated body fluid10.1016/j.corsci.2020.109071 ↗
16. Accelerated corrosion behavior of weathering steel Q345qDNH for bridge in industrial atmosphere10.1016/j.conbuildmat.2021.124864 ↗
17. Fundamental understanding on the effect of Cr on corrosion resistance of weathering steel in simulated tropical marine atmosphere10.1016/j.corsci.2021.109427 ↗
18. Experiments on static and fatigue behaviour of corroded Q235B and 42CrMo steels10.1016/j.jcsr.2022.107535 ↗
19. A study on the initial corrosion behavior of carbon steel exposed to a simulated coastal-industrial atmosphere
20. Effect of small content of chromium on wet-dry acid corrosion behavior of low alloy steel10.1007/s40195-016-0513-z ↗
21. Structure analysis of cation selective cr-goethite as protective rust of weathering steel10.2320/matertrans.46.337 ↗
22. Effects of alloyed Cr and Cu on the corrosion behavior of low-alloy steel in a simulated groundwater solution10.1016/j.corsci.2015.09.025 ↗
23. Influence of carbon content and microstructure on corrosion behaviour of low alloy steels in a Cl− containing environment10.1016/j.corsci.2008.10.025 ↗
24. Control of Fe(O,OH)6 nano-network structures of rust for high atmospheric-corrosion resistance10.1016/j.corsci.2005.04.005 ↗
25. Mechanistic modelling of atmospheric corrosion of carbon steel in port-louis by electrochemical characterisation of rust layers10.1016/j.matchemphys.2022.126694 ↗
26. Benefit of the corrosion product film formed on a new weathering steel containing 3% nickel under marine atmosphere in maldives10.1016/j.corsci.2019.108416 ↗
27. Structure of the rust layer of weathering steel in a high chloride environment: a detailed characterization via HRTEM, STEM-EDS, and FIB-SEM10.1016/j.corsci.2020.108997 ↗
28. Atmospheric corrosion of weathering steels. overview for engineers. part I: basic concepts10.1016/j.conbuildmat.2019.03.334 ↗
29. In situ observation of initial rust formation process on carbon steel under Na2SO4 and NaCl solution films with wet/dry cycles using synchrotron radiation X-rays10.1016/j.corsci.2004.10.021 ↗
30. Comparison of the rusting behaviors of S450EW weathering steel under continuous spray and wet/dry cycling10.1016/j.conbuildmat.2021.125211 ↗
31. A study for corrosion behavior of a new-type weathering steel used in harsh marine environment10.1016/j.conbuildmat.2020.119760 ↗
32. Role of climatic conditions on corrosion characteristics of structural steels10.1016/j.corsci.2007.06.026 ↗
33. The mechanism of atmospheric rusting and the effect of Cu and P on the rust formation of low alloy steels10.1016/S0010-938X(71)80072-0 ↗
34. The mechanism of atmospheric rusting and the protective amorphous rust on low alloy steel10.1016/S0010-938X(74)80037-5 ↗
35. Long-term atmospheric corrosion of mild steel10.1016/j.corsci.2010.10.007 ↗
36. Advances in understanding atmospheric corrosion of iron. I. Rust characterisation of ancient ferrous artefacts exposed to indoor atmospheric corrosion10.1016/j.corsci.2003.09.027 ↗
37. An empirical stress-intensity factor equation for the surface crack10.1016/0013-7944(81)90116-8 ↗
38. Effect of inclusions modified by rare earth elements (ce, la) on localized marine corrosion in Q460NH weathering steel10.1016/j.corsci.2017.10.001 ↗
39. Effect of MnS inclusion dissolution on carbon steel stress corrosion cracking in fuel-grade ethanol10.1016/j.corsci.2015.03.002 ↗
40. Mechanism of (mg,al,ca)-oxide inclusion-induced pitting corrosion in 316L stainless steel exposed to sulphur environments containing chloride ion10.1016/j.corsci.2012.09.044 ↗
41. Local corrosion characteristics of CaS/CaO–MgO–Al2O3 inclusions in low-alloy steel under multi-factor mechanisms10.1016/j.jmrt.2023.03.113 ↗
42. The mechanoelectrochemical effect on the electrochemical corrosion of austenitic stainless steel10.1016/j.jmrt.2023.03.030 ↗
43. The mechanochemical behavior of type 316L stainless steel10.1016/0010-938X(96)00008-X ↗
44. Insight into the triggering effect of (Al, Mg, Ca, Mn)-oxy-sulfide inclusions on localized corrosion of weathering steel10.1016/j.jmst.2020.06.031 ↗
45. Unraveling the effect of sulfide-oxide complex inclusions on the localized corrosion mechanism for carbon steel10.1016/j.corsci.2023.111555 ↗
46. Corrosion behavior and mechanism of cr–mo alloyed steel: Role of ferrite/bainite duplex microstructure10.1016/j.jallcom.2019.151787 ↗
47. Effect of grain size and twins on corrosion behaviour of AZ31B magnesium alloy10.1016/j.corsci.2009.10.018 ↗
48. In-situ SEM/EBSD investigation of tensile deformation-driven microstructural changes in low-carbon HSLA steels with ferrite-bainite microstructures10.1016/j.matchar.2023.113418 ↗
49. Insight into the localized strain effect on micro-galvanic corrosion behavior in AA7075-T6 aluminum alloy10.1016/j.corsci.2020.109174 ↗
50. Strength degradation of a ferrite-bainite weathering steel subjected to corrosion fatigue environment10.1016/j.corsci.2022.110690 ↗
51. Corrosion behavior and mechanism of cr–mo alloyed steel: role of ferrite/bainite duplex microstructure10.1016/j.jallcom.2019.151787 ↗
52. Corrosion behavior and mechanism of Cr–Mo alloyed steel: role of ferrite/bainite duplex microstructure10.1016/j.jallcom.2019.151787 ↗
53. About the fatigue crack propagation threshold of metals as a design criterion – a review10.1016/j.engfracmech.2015.12.002 ↗
54. Experimental investigation into corrosion effect on buckling and low-cycle fatigue performance of high-strength steel bars10.1016/j.engstruct.2024.118230 ↗
55. Nonlinear stress–strain behaviour of corrosion-damaged reinforcing bars including inelastic buckling10.1016/j.engstruct.2012.09.034 ↗
56. Phenomenological hysteretic model for corroded reinforcing bars including inelastic buckling and low-cycle fatigue degradation10.1016/j.compstruc.2015.04.005 ↗
57. The impact of corrosion and inelastic buckling on low cycle fatigue life of steel bars10.1016/j.prostr.2018.09.008 ↗
58. Impact of corrosion on low-cycle fatigue degradation of reinforcing bars with the effect of inelastic buckling10.1016/j.ijfatigue.2015.03.013 ↗
59. A study of the effects of cyclic thermal stresses on a ductile metal
60. Low cycle fatigue behaviour study of a nano precipitate strengthened ferrite-bainite 780 steel10.1016/j.ijfatigue.2022.107294 ↗
61. Microstructure and deformation behavior of a novel steel rebar: effect of the heterogeneous microstructure of soft ferrite and hard bainite10.1016/j.jmrt.2020.08.085 ↗
62. A study on fatigue crack growth in dual phase martensitic steel in air environment10.1007/BF02719909 ↗
63. Exploring factors controlling pre-corrosion fatigue of 316L austenitic stainless steel in hydrofluoric acid10.1016/j.engfailanal.2020.104556 ↗
64. Ralph · 2000
65. In-situ SEM/EBSD investigation of tensile deformation-driven microstructural changes in low-carbon HSLA steels with ferrite-bainite microstructures10.1016/j.matchar.2023.113418 ↗
66. Doherty · Curr. Issues Recryst.: A Rev. · 1997 · 238 · 219
67. δ-ferrite dynamic recrystallization behavior during thermal deformation in fe–32Mn–11Al-0.9C low density steel10.1016/j.jmrt.2022.02.129 ↗