journal article·2023-07

Simultaneously enhancing strength and hydrogen embrittlement resistance of pure iron via gradient microstructure

Xinfeng Li, Canyu Wang, Hui Feng, Tang Gu, Jin Zhang, Yong Zhang, Xuechong Ren

Corrosion Science· Volume 218
Publisher page

Abstract

Hydrogen embrittlement (HE) of gradient-structured pure iron was studied by slow strain rate tensile tests, microstructural analysis and time-of-flight secondary ion mass spectrometry. As pre-torsion angles increase from 0° to 1400°, yield strength of alloys monotonically increases, but the HE susceptibility first decreases and then increases, with optimal match of improved strength and HE-resistance for pre-torsioned sample at 400°. This correlates with gradient distributions of grain boundary and dislocation hydrogen traps. These results indicate that the construction of suitable gradient structure in alloys is a promising strategy to maximize the strength and HE-resistance synergy.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Review of hydrogen embrittlement in metals: Hydrogen diffusion, hydrogen characterization, hydrogen embrittlement mechanism and prevention10.1007/s40195-020-01039-7 ↗
2. Applications of phase field fracture in modelling hydrogen assisted failures10.1016/j.tafmec.2020.102837 ↗
3. Hydrogen embrittlement resistance of pre-strained ultra-high-strength low alloy TRIP-aided steel10.1007/s10704-020-00451-5 ↗
4. Failure analysis of high strength steel bar used in a wind turbine foundation10.1007/s11668-015-9929-4 ↗
5. Hydrogen embrittlement induced fracture of 17-4 PH stainless steel valve stem10.1016/j.engfailanal.2020.104576 ↗
6. Effect of heat treatment on hydrogen-assisted fracture behavior of PH13-8Mo steel10.1016/j.corsci.2017.09.018 ↗
7. Electrochemical and hydrogen embrittlement of a micro-alloy steel coated with nanocrystalline nickel by pulse electrodeposition10.1080/09500839.2020.1736356 ↗
8. Hydrogen absorption, desorption and embrittlement of Zn and ZnNi-electrodeposited bolts10.1016/j.jmrt.2021.02.006 ↗
9. Niobium coating applied by HVOF as protection against hydrogen embrittlement of API 5CT P110 steel10.1016/j.surfcoat.2017.05.017 ↗
10. Graphene coating on nickel as effective barriers against hydrogen embrittlement10.1016/j.surfcoat.2019.06.044 ↗
11. Effect of CrxCy–NiCr coating on the hydrogen embrittlement of 17-4 PH stainless steel using the smooth bar tensile test10.1007/s10853-019-03356-4 ↗
12. Effect of Diamond-Like Carbon Coating on Preventing the Ingress of Hydrogen into Bearing Steel10.1080/10402004.2020.1815919 ↗
13. Effects of surface coating on cylinder rods prepared using sputtering deposition method with modulated magnetic field10.1143/JJAP.49.08JF01 ↗
14. Coatings to reduce hydrogen environment embrittlement of 304 austenitic stainless steel10.1016/j.surfcoat.2009.01.013 ↗
15. Effect of hydrogen on the integrity of aluminium–oxide interface at elevated temperatures
16. Grain refinement effect on hydrogen embrittlement resistance of an equiatomic CoCrFeMnNi high-entropy alloy10.1016/j.ijhydene.2019.04.280 ↗
17. Effect of grain refinement on hydrogen embrittlement behaviors of high-Mn TWIP steel10.1016/j.msea.2015.11.017 ↗
18. Effect of nano Nb and V carbides on the hydrogen interaction in tempered martensitic steels10.1016/j.ijhydene.2021.10.051 ↗
19. Comparative study on the effects of Cr, V, and Mo carbides for hydrogen-embrittlement resistance of tempered martensitic steel, Scientific reports
20. Atomistic simulation study of the grain-size effect on hydrogen embrittlement of nanograined Fe10.1016/j.ijhydene.2019.11.131 ↗
21. Effect of pre-strain on hydrogen embrittlement of high strength steels10.1016/j.msea.2014.07.085 ↗
22. Effect of dislocation cell walls on hydrogen adsorption, hydrogen trapping and hydrogen embrittlement resistance10.1016/j.corsci.2020.108428 ↗
23. Effect of loading mode on blistering in iron submitted to plastic prestrain before hydrogen cathodic charging10.1016/j.ijhydene.2017.02.048 ↗
24. Hydrogen permeation through deformed and heat-treated Armco pure iron10.1080/02670836.2017.1342015 ↗
25. Effect of gradient microstructure on the strength and ductility of medium-entropy alloy processed by severe torsion deformation10.1016/j.msea.2020.140429 ↗
26. Simultaneously enhancing strength and ductility of a high-entropy alloy via gradient hierarchical microstructures10.1016/j.ijplas.2019.07.017 ↗
27. Strengthening and toughening austenitic steel by introducing gradient martensite via cyclic forward/reverse torsion10.1016/j.matdes.2018.01.058 ↗
28. Dual gradient microstructure to simultaneously improve strength and electrical conductivity of aluminum wire10.1016/j.msea.2020.139308 ↗
29. Effect of gradient microstructure induced by pre-torsion on hydrogen embrittlement of pure iron10.1016/j.corsci.2021.109821 ↗
30. Effect of surface roughness on hydrogen-induced blister behavior in pure iron10.3390/met10060745 ↗
31. Numerical analysis of hydrogen transport into a steel after shot peening10.1016/j.rinp.2018.08.030 ↗
32. Effect of mechanical deformation on permeation of hydrogen in iron10.2355/isijinternational.43.548 ↗
33. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
34. The cleavage strength of polycrystals
35. On peierls nabarro stress in iron10.1016/j.commatsci.2011.12.033 ↗
36. G.I. Taylor, The mechanism of plastic deformation of crystals. Part I.—Theoretical, Proceedings of the Royal Society of London. Series A, Containing Papers of a Mathematical and Physical Character 145(855) (1934) 362–387.10.1098/rspa.1934.0106 ↗
37. Revisiting the role of prestrain history in the mechanical properties of ultrafine-grained CoCrFeMnNi high-entropy alloy10.1016/j.msea.2020.140398 ↗
38. Microstructural and micromechanical investigations of surface strengthening mechanisms induced by repeated impacts on pure iron10.1016/j.matdes.2018.03.014 ↗
39. On the origins of ultra-high hardness and strain gradient plasticity in multi-phase nanocrystalline MoNbTaTiW based refractory high-entropy alloy10.1016/j.msea.2021.141098 ↗
40. Constitutive modeling of deformation behavior of high-entropy alloys with face-centered cubic crystal structure10.1080/21663831.2017.1292325 ↗
41. Evolution of dislocation densities and the critical conditions for the Portevin-Le Chatelier effect10.1016/0956-7151(90)90021-8 ↗
42. Effect of pre-compression on microstructural evolution, mechanical property and strengthening mechanism of AZ31 alloy10.1007/s10853-020-04724-1 ↗
43. Determination of the critical hydrogen concentration for delayed fracture of high strength steel by constant load test and numerical calculation10.1016/j.corsci.2005.07.010 ↗
44. Critical hydrogen concentration for hydrogen-induced cracking of type 321 stainless steel10.5006/1.3293639 ↗
45. Stress-induced hydrogen redistribution and corresponding fracture behavior of Q960E steel at different hydrogen content10.1016/j.msea.2020.138963 ↗
46. Failure analysis of pre‐stressed high strength steel bars used in a wind turbine foundation: experimental and FE simulation10.1002/maco.201508506 ↗
47. Critical hydrogen concentration for hydrogen-induced blistering on AISI 430 stainless steel10.1016/S0254-0584(03)00084-1 ↗
48. The detrimental effect of hydrogen at dislocations on the hydrogen embrittlement susceptibility of Fe-CX alloys: an experimental proof of the HELP mechanism10.1016/j.ijhydene.2017.12.109 ↗
49. Effect of deformation and charging conditions on crack and blister formation during electrochemical hydrogen charging10.1016/j.actamat.2017.01.013 ↗
50. Unraveling the effect of dislocations and deformation-induced boundaries on environmental hydrogen embrittlement behavior of a cold-rolled Al–Zn–Mg–Cu alloy10.1016/j.ijhydene.2020.12.028 ↗
51. Mechanical properties and deformation mechanisms of gradient nanostructured metals and alloys10.1038/s41578-020-0212-2 ↗
52. The effect of hydrogen content and yield strength on the distribution of hydrogen in steel: a diffusion coupled micromechanical FEM study10.1016/j.actamat.2021.116799 ↗