Oxide scale growth behavior of alumina-forming austenitic stainless steel exposed to supercritical water
Source abstract
Abstract
The corrosion characteristics of a novel alumina-forming austenitic (AFA) steel exposed to 600 ℃/25 MPa deaerated supercritical water (SCW) were investigated. The results show that the weight gain curves of the AFA steel follow parabolic law. A chromium-rich oxide scale containing reticular alumina is formed in the AFA steel, which contributes to the high corrosion resistance of the AFA steel. No continuous alumina scale is formed on the AFA steel with 2.5 wt% Al addition, which is attributed to the negative effects of B2-NiAl, Laves and σ-FeCr precipitates on the continuity of alumina scale.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Subcritical and Supercritical Water Processes · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. The hotter the engine, the better10.1126/science.1179327 ↗
2. The role of new energy in carbon neutral10.1016/S1876-3804(21)60039-3 ↗
3. Current status and future developments in nuclear-power industry of the world10.1115/1.4042194 ↗
4. Optimization of a fuel assembly for supercritical water-cooled reactor CSR100010.3389/fenrg.2021.678741 ↗
5. Supercritical water-cooled reactor materials– summary of research and open issues10.1016/j.pnucene.2014.02.008 ↗
6. Conceptual fuel channel designs for CANDU-SCWR10.5516/NET.2008.40.2.139 ↗
7. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
8. Materials for future nuclear energy systems10.1016/j.jnucmat.2019.151837 ↗
9. Supercritical water-cooled reactor materials – summary of research and open issues10.1016/j.pnucene.2014.02.008 ↗
10. Cycle chemistry and its effect on materials in a supercritical water-cooled reactor: a synthesis of current understanding10.1016/j.corsci.2012.08.006 ↗
11. Creep-resisitant, Al2O3-forming austenitic stainless steels10.1126/science.1137711 ↗
12. Corrosion behavior of an alumina forming austenitic steel exposed to supercritical carbon dioxide10.1016/j.corsci.2013.12.023 ↗
13. The influence of Y and Nb addition on the corrosion resistance of Fe-Cr-Al-Ni model alloys exposed to oxygen-containing molten Pb10.1016/j.corsci.2020.109152 ↗
14. Microstructure and mechanical properties of Ni-Fe-Cr-Al wrought alumina forming superalloy heat-treated at 600–1100 °C10.1016/j.matchar.2020.110737 ↗
15. Oxidation behavior and microstructure evolution of alumina-forming austenitic & high entropy alloys in steam environment at 1200 °C10.1016/j.corsci.2020.108654 ↗
16. Chromium evaporation and oxidation characteristics of alumina-forming austenitic stainless steels for balance of plant applications in solid oxide fuel cells10.1016/j.ijhydene.2021.04.002 ↗
17. Alumina Scale Formation: A New Perspective
18. Corrosion behavior of alumina-forming and oxide dispersion strengthened austenitic 316 stainless steel in supercritical water10.1016/j.corsci.2018.04.026 ↗
19. Microstructure and mechanical properties of Ni-Fe-Cr-Al wrought alumina forming superalloy heat-treated at 600–1100 °C10.1016/j.matchar.2020.110737 ↗
20. Comprehensive review of chromium deposition and poisoning of solid oxide fuel cells (SOFCs) cathode materials10.1016/j.rser.2020.110320 ↗
21. Corrosion of alumina-forming austenitic steel Fe–20Ni–14Cr–3Al–0.6Nb–0.1Ti in supercritical water10.1016/j.jnucmat.2010.01.025 ↗
22. Oxidation behavior of 9Cr-4.5Al ODS steel in 600 °C supercritical water and the effect of pre-oxidation10.1016/j.corsci.2019.108380 ↗
23. The corrosion and stress corrosion cracking behavior of a novel alumina-forming austenitic stainless steel in supercritical water10.1016/j.jnucmat.2016.10.039 ↗
24. The nature of the third-element effect in the oxidation of Fe-xCr-3 at% Al alloys in 1 atm O2 at 1000 °C10.1016/j.corsci.2007.06.019 ↗
25. The influence of alloying elements on the development and maintenance of protective scales10.1007/BF01046725 ↗
26. Measurement of oxidation rate of metal
27. The influence of alloying elements on the development and maintenance of protective scales10.1007/BF01046725 ↗
28. The nature of the third-element effect in the oxidation of Fe-xCr-3 at% Al alloys in 1 atm O2 at 1000°C10.1016/j.corsci.2007.06.019 ↗
29. Criteria for the formation of protective Al2O3 scales on Fe–Al and Fe–Cr–Al alloys10.1016/j.corsci.2005.01.012 ↗
30. Effects of silicon additions on the oxide scale formation of an alumina-forming austenitic alloy10.1016/j.corsci.2012.08.039 ↗
31. Reason for negative effect of Nb addition on oxidation resistance of alumina-forming austenitic stainless steel at 1323 K10.1016/j.corsci.2021.109754 ↗
32. Effects of Nb/Ti/V/Ta on phase precipitation and oxidation resistance at 1073 K in alumina-forming austenitic stainless steels10.1016/j.matchar.2018.07.007 ↗
33. Mo-rich Laves phase in a 9.5Cr-1.5MoCoVNbNB heat-resistant steel during long-term aging at 620 °C10.1016/j.matchar.2021.111588 ↗
34. Elucidating the grain-orientation dependent corrosion rates of austenitic stainless steels10.1016/j.matdes.2020.108583 ↗
35. The role of (FeCrSi)2(MoNb)-type Laves phase on the formation of Mn-rich protective oxide scale on ferritic stainless steel10.1016/j.corsci.2017.12.026 ↗
36. Alumina-Forming Austenitic Stainless Steels Strengthened by Laves Phase and MC Carbide Precipitates10.1007/s11661-007-9319-y ↗
37. Study of the effect of sigma phase precipitation on the sliding wear and corrosion behavior of duplex stainless steel AISI 220510.1016/j.wear.2017.12.019 ↗
38. Corrosion and stress corrosion cracking susceptibility of type 347H stainless steel in supercritical water10.5006/2459 ↗
39. Overview of Strategies for High-Temperature Creep and Oxidation Resistance of Alumina-Forming Austenitic Stainless Steels10.1007/s11661-010-0295-2 ↗
40. Precipitate characteristics and their effects on the high-temperature creep resistance of alumina-forming austenitic stainless steels10.1016/j.msea.2014.11.013 ↗
41. Co-strengthening of dislocations and precipitates in alumina-forming austenitic steel with cold rolling followed by aging10.1016/j.msea.2021.142181 ↗
42. Corrosion behavior of a 14Cr-ODS steel in supercritical water10.1016/j.jnucmat.2013.02.002 ↗
43. A study on the corrosion and stress corrosion cracking susceptibility of 310-ODS steel in supercritical water10.1016/j.jnucmat.2018.11.016 ↗
44. Corrosion behavior of alloy 800H (Fe-21Cr-32Ni) in supercritical water10.1016/j.corsci.2010.10.021 ↗
45. Alloy oxidation II: internal oxidation
46. Design of alumina-forming austenitic stainless steel using genetic algorithms10.1016/j.matdes.2019.108198 ↗
47. Micro-structural evolution of oxide scales formed on a Nb-Stabilizing heat-resistant steel at the initial stage in high-temperature water vapor10.1016/j.matchemphys.2019.122443 ↗
48. Oxidation behavior of Ni-25Cr-10Fe-3Si-χNb alloys at 1000 °C in ambient air: Role of Laves phase10.1016/j.corsci.2021.109475 ↗
49. Microstructures of oxidized primary carbides on superalloy inconel 71810.4028/www.scientific.net/MSF.502.249 ↗
50. The oxidation behaviour of NiAl-I. Phase transformations in the alumina scale during oxidation of NiAl and NiAl-Cr alloys10.1016/0010-938X(92)90002-K ↗
51. Corrosion characteristics and mechanisms of typical Ni-based corrosion-resistant alloys in sub- and supercritical water10.1016/j.supflu.2020.105138 ↗
52. Early oxidation mechanism of austenitic stainless steel TP347H in supercritical water10.1016/j.corsci.2017.09.023 ↗
53. Transmission electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb-Bi eutectic10.1016/j.corsci.2018.10.018 ↗
54. Formation of a well-ordered aluminium oxide overlayer by oxidation of NiAl (110)10.1016/0039-6028(91)90555-7 ↗
55. Overview of Strategies for High-Temperature Creep and Oxidation Resistance of Alumina-Forming Austenitic Stainless Steels10.1007/s11661-010-0295-2 ↗
56. The formation mechanism, growth, and effect on the mechanical properties of precipitate free zones in the alumina-forming austenitic stainless steel Fe-20Cr-30Ni-2Nb-5Al during creep10.1016/j.msea.2021.141561 ↗
57. Effects of Si, Mn on the corrosion behavior of ferritic-martensitic steels in supercritical water (SCW) environments10.1016/j.corsci.2020.108432 ↗
58. Diffusion of iron in Cr2O3: polycrystals and thin films10.1016/j.msea.2004.09.033 ↗
59. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
60. High Temperature Oxidation and Corrosion of Metals · 2016 · 719
61. Theoretical and experimental analysis of selective oxide and nitride formation in Fe–Al alloys10.1016/j.corsci.2014.10.024 ↗
62. Air-oxidation of FeCoNiCr-based quinary high-entropy alloys at 700–900 °C10.1016/j.corsci.2017.02.008 ↗
63. Mehrer · 1990 · vol. 26
64. Internal oxidation and formation of Si/Al-enriched oxide bands in the scale of electrical steel grades10.1016/j.corsci.2021.109502 ↗