journal article·2024-05

Role of hygroscopic chloride salts on corrosion performance and hydrogen absorption of steel under cyclic wet-dry conditions

Xiaole Han, Masatoshi Sakairi

Corrosion Science· Volume 231
Publisher page

Abstract

The corrosion morphology of steel under aqueous NaCl, MgCl 2 , and ZnCl 2 droplets and the corresponding hydrogen permeation behaviour were investigated using surface characterization techniques and electrochemical methods. Under cyclic wet -dry conditions, Mg 2 + and Zn 2 + -containing surface layers were formed on steel and the latter presented a high corrosion resistance. The most active hydrogen entry occurred under ZnCl 2 during drying, while it happened under MgCl 2 at low humidity. The effects of chloride salts on the formation of rust layers and hydrogen entry into steel during wet -dry cycles were discussed based on the hardness of metal cations and the deliquescence properties of salts.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Function of hydrogen in embrittlement of high-strength steels10.2355/isijinternational.41.590 ↗
2. Hydrogen entry into steel by atmospheric corrosion10.2355/isijinternational.43.470 ↗
3. Hydrogen entry into steel during atmospheric corrosion process10.1016/j.corsci.2004.10.006 ↗
4. Understanding and mitigating hydrogen embrittlement of steels: a review of experimental, modelling and design progress from atomistic to continuum10.1007/s10853-017-1978-5 ↗
5. Atmospheric Corrosion
6. Physical and chemical properties of sea salt deliquescent brines as a function of temperature and relative humidity10.1016/j.scitotenv.2022.154462 ↗
7. Marine atmospheric corrosion of carbon steel: a review10.3390/ma10040406 ↗
8. The mechanism of the so-called “dry corrosion” of metals10.1039/TF9231900201 ↗
9. Mechanism of atmospheric rusting10.1016/S0010-938X(72)90671-3 ↗
10. Phase transitions of aqueous atmospheric particles10.1021/cr990034t ↗
11. A study of the wetting of metal surfaces in order to understand the processes controlling atmospheric corrosion10.1149/1.1809596 ↗
12. Wetting phenomena and time of wetness in atmospheric corrosion: a review
13. Corrosion mechanisms of Zn (Mg, Al) coated steel in accelerated tests and natural exposure: 1. The role of electrolyte composition in the nature of corrosion products and relative corrosion rate10.1016/j.corsci.2014.05.014 ↗
14. Atmospheric corrosion of ZnAlMg coated steel during long term atmospheric weathering at different worldwide exposure sites10.1016/j.corsci.2018.12.033 ↗
15. Effect of surface conditions and relative humidity on hydrogen permeation behavior of zinc coated steels during wet and dry corrosion10.2355/isijinternational.ISIJINT-2015-247 ↗
16. Hydrogen Permeation Behavior of Scratch Formed on Zn Coated Steels in Simulated Atmospheric Corrosion Environment10.2355/isijinternational.ISIJINT-2020-302 ↗
17. A database for deliquescence and efflorescence relative humidities of compounds with atmospheric relevance10.1016/j.fmre.2021.11.021 ↗
18. The influence of CO2, AlCl3·6H2O, MgCl2·6H2O, Na2SO4 and NaCl on the atmospheric corrosion of aluminum10.1016/j.corsci.2005.05.027 ↗
19. T. Herzog, W. Müller, W. Spiegel, J. Brell, D. Molitor, D. Schneider, Corrosion caused by dew point and deliquescent salts in the boiler and flue gas cleaning, K.J. Thomé-Kozmiensky, S. Thiel (Eds.), Waste Management, 3, Recycling and Recovery, TK Verlag, Neuruppin (2012), pp. 343-358.
20. Effect of relative humidity on corrosion of steel under sea salt aerosol proxies: II. MgCl2, artificial seawater
21. The promotion effect of aluminium ion on hydrogen entry into steel during atmospheric corrosion10.1016/j.electacta.2023.142505 ↗
22. Effect of Humidity of Air on Hydrogen Absorption into Fe with Rust Layer Containing MgCl2 during Atmospheric Corrosion10.2355/isijinternational.ISIJINT-2020-426 ↗
23. Transport processes and the mechanism of pitting of metals10.1149/1.2132857 ↗
24. Hydrogen entry into Fe and high strength steels under simulated atmospheric corrosion10.1016/j.electacta.2010.09.043 ↗
25. Evaluation of hydrogen absorption into steel in automobile moving environments10.1016/j.corsci.2015.05.049 ↗
26. Hydrogen Absorption Behavior of Pre-Rusted Steels under an NaCl Droplet10.1149/2.0591910jes ↗
27. Hydrogen permeation behavior of steel under wet/dry corrosion with changes in relative humidity at the dry period10.2355/isijinternational.ISIJINT-2020-555 ↗
28. Effect of cations on corrosion of zinc and carbon steel covered with chloride deposits under atmospheric conditions10.1016/j.corsci.2006.11.004 ↗
29. Inhibition of Cathodic Kinetics by Zn2+ and Mg2+ on AA7050-T745110.1149/2.0551906jes ↗
30. Hard and soft acids and bases10.1021/ja00905a001 ↗
31. Inhibition effect of metal cations to intergranular stress corrosion cracking of sensitized Type 304 stainless steel10.1016/j.corsci.2004.06.014 ↗
32. Passivity breakdown and stress corrosion cracking of stainless steel10.1016/j.corsci.2006.05.031 ↗
33. Evaluation of metal cation effects on galvanic corrosion behavior of the A5052 aluminum alloy in low chloride ion containing solutions by electrochemical noise impedance10.1016/j.electacta.2014.02.010 ↗
34. Effects of metal cations on corrosion of mild steel in model fresh water10.1016/j.corsci.2016.05.020 ↗
35. A new dual parameter scale for the strength of Lewis acids and bases with the evaluation of their softness10.1016/0022-1902(67)80006-X ↗
36. Evaluation of softness from the stability constants of metal-ion complexes10.1246/bcsj.43.3680 ↗
37. Effects of metal cations on mild steel corrosion in 10 mM Cl− aqueous solution10.1016/j.corsci.2017.11.015 ↗
38. Passive film of 18-8 stainless steel structure and its function10.1016/0010-938X(73)90031-0 ↗
39. The adsorption and diffusion of electrolytic hydrogen in palladium10.1098/rspa.1962.0205 ↗
40. Hydrogen Absorption Mechanism into Iron in Aqueous Solution Including Metal Cations by Laser Ablation Tests and First-principles Calculations10.2355/isijinternational.ISIJINT-2020-065 ↗
41. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
42. Corrosion resistance of zinc–magnesium coated steel10.1016/j.corsci.2007.03.032 ↗
43. XPS and FT-IR characterization of selected synthetic corrosion products of zinc expected in neutral environment containing chloride ions
44. (Deceased), Electrochemical Mechanism
45. Stability of passive stainless steel in relation to the potential of passivation treatment10.1016/S0010-938X(70)80027-0 ↗
46. Effect of Cl- and rust layer on stress corrosion cracking behavior of X100 steel base metal and heat-affected zone in marine alternating wet/dry environment10.1016/j.matchemphys.2021.124826 ↗
47. The role of rusts in corrosion and corrosion protection of iron and steel10.1016/j.corsci.2008.03.008 ↗