Insights into the stress corrosion cracking of M54 ultra-high-strength steel in the marine environments at varying temperatures by comparison of slow strain rate tensile and crack growth tests
Source abstract
Abstract
The stress corrosion cracking of M54 steel in marine environments at varying temperatures was investigated. The slow strain rate tensile tests show that increasing the temperature from 5 to 45°C leads to a 71.9 % and 77.4 % decrease in plastic elongation ratio and reduction in area ratio in full immersion environments, while only 7.8 % and 7.9 % in atmospheric environments. The da/dt II increases from 0.75 nm/s to 5.5 nm/s in atmospheric environments, but first decreases and then increases in full immersion environments. Compared to full immersion environments, the sufficient oxygen supply within the crack in atmospheric environments lowers da/dt II by 50–80 %.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. Hydrogen-assisted cracking
2. Hydrogen trap states in ultrahigh-strength AERMET 100 steel10.1007/s11661-004-0011-1 ↗
3. Technology, Improvement of toughness of ultrahigh strength steel AerMet 100
4. performance, Effect of hydrogen on mechanical properties of 23Co14Ni12Cr3Mo ultrahigh strength steel10.1007/s11665-013-0671-3 ↗
5. Fatigue and fracture behavior of laser clad repair of AerMet® 100 ultra-high strength steel10.1016/j.ijfatigue.2015.11.021 ↗
6. Microbiologically influenced corrosion of ferrium M54 maraging steel with different grain sizes induced by desulfovibrio vulgaris10.1016/j.corsci.2024.112302 ↗
7. The investigation on Johnson-Cook model and dynamic mechanical behaviors of ultra-high strength steel M5410.1016/j.msea.2022.142693 ↗
8. Influence of cooling rate during cryogenic treatment on the hierarchical microstructure and mechanical properties of M54 secondary hardening steel10.1016/j.msea.2022.143659 ↗
9. Controlling the MC and M2C carbide precipitation in Ferrium® M54® steel to achieve optimum ultimate tensile strength/fracture toughness balance10.1016/j.matchar.2018.03.041 ↗
10. Ausforming and tempering of a novel ultra-high strength steel10.1016/j.msea.2022.142750 ↗
11. Microstructure characterization and mechanical behaviour of laser additive manufactured ultrahigh-strength M54 steel10.1088/2053-1591/ac5955 ↗
12. Genomic materials design: The ferrous frontier10.1016/j.actamat.2012.10.045 ↗
13. On the characteristics of M2C carbides in the peak hardening regime of AerMet 100 steel10.1007/s11661-998-0280-1 ↗
14. The role of heat treatment and alloying elements on hydrogen uptake in Aermet 100 ultrahigh-strength steel10.1016/j.jelechem.2014.12.011 ↗
15. Revealing the evolution behavior of multiple carbides precipitation and mechanical response in M54 secondary hardening steel
16. Hydrogen embrittlement in different materials: A review10.1016/j.ijhydene.2018.09.201 ↗
17. A review of hydrogen embrittlement of martensitic advanced high-strength steels10.1515/corrrev-2016-0006 ↗
18. Mechanisms of hydrogen assisted cracking- a review
19. Hydrogen transport and embrittlement in 300 M and AerMet 100 ultra high strength steels10.1016/j.corsci.2010.01.001 ↗
20. Investigation of stress corrosion cracking behavior and mechanism analysis of a 1900 MPa-grade ultra-high-strength stainless steel10.1007/s42243-021-00710-2 ↗
21. Stress corrosion cracking behavior and mechanism of Fe-Mn-Al-C-Ni high specific strength steel in the marine atmospheric environment10.1016/j.corsci.2021.109760 ↗
22. Probabilistic fracture mechanics simulation of stress corrosion cracking using accelerated laboratory testing and multi-scale modeling10.5006/1920 ↗
23. Modelling of environment assisted cracking10.1016/0010-938X(93)90072-O ↗
24. Mechanisms and kinetics of environmentally assisted cracking: current status, lssues, and suggestions for further work10.1007/s11661-012-1359-2 ↗
25. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
26. Hydrogen environment assisted cracking of modern ultra-high strength martensitic steels10.1007/s11661-017-4156-0 ↗
27. The influence of microstructure on the hydrogen embrittlement susceptibility of martensitic advanced high strength steels10.1016/j.mtcomm.2018.07.011 ↗
28. Correlation between the microstructure and hydrogen embrittlement resistance in a precipitation-hardened martensitic stainless steel10.1016/j.corsci.2021.109260 ↗
29. Mechanistic and fractographic aspects of stress corrosion cracking10.1515/corrrev-2012-0501 ↗
30. Measurement and modeling of hydrogen environment–assisted cracking of ultra-high-strength steel10.1007/s11661-006-9051-z ↗
31. Pioszak · 2015
32. Study on the hydrogen embrittlement of AerMet 100 using hydrogen permeation and SSRT techniques10.1007/s11661-017-4159-x ↗
33. A. Arcari, J.P. Moran, D.J. Horton, E.J. Lemieux, R. McCoy, T.M. Newbauer, The effect of alternate immersion on stress corrosion cracking behavior of steel and nickel alloys in natural seawater, In: CORROSION 2021. Virtual, 2021, Paper Number: NACE-2021-16857. 〈https://onepetro.org/NACECORR/proceedings/CORR21/8-CORR21/D081S029R012/464004〉.
34. Studies of evaluation of hydrogen embrittlement property of high-strength steels with consideration of the effect of atmospheric corrosion10.1007/s11661-012-1403-2 ↗
35. Corrosion of pure magnesium under thin electrolyte layers10.1016/j.electacta.2008.05.074 ↗
36. Electrochemical methods for the evaluation of the degradation of structural steels intended for long-term operation10.1007/s11003-017-9994-9 ↗
37. Influence of rust layers on the corrosion behavior of ultra-high strength steel 300M subjected to wet–dry cyclic environment with chloride and low humidity10.1007/s40195-014-0174-8 ↗
38. Corrosion evolution and stress corrosion cracking behavior of a low carbon bainite steel in the marine environments: Effect of the marine zones10.1016/j.corsci.2022.110490 ↗
39. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel10.1016/j.corsci.2008.03.007 ↗
40. Stress corrosion cracking in the heat affected zone of a stainless steel 308L-316L weld joint in primary water10.1016/j.corsci.2016.02.030 ↗
41. Environmentally assisted crack growth in 308L stainless steel weld metal in simulated primary water10.1016/j.corsci.2016.12.011 ↗
42. Environmentally assisted cracking in the fusion boundary region of a SA508-Alloy 52M dissimilar weld joint in simulated primary pressurized water reactor environments10.1016/j.corsci.2021.109668 ↗
43. Mechanistic aspect of near-neutral pH stress corrosion cracking of pipelines under cathodic polarization10.1016/j.corsci.2011.10.002 ↗
44. A comparative study of the corrosion behavior of 30CrMnSiNi2A in artificial seawater and salt spray environments10.3390/met12091443 ↗
45. Effect of Ni on the oxidation behavior of corrosion products that form on low alloy steel exposed to a thin electrolyte layer environment10.1016/j.corsci.2022.110471 ↗
46. Electrochemical corrosion, hydrogen permeation and stress corrosion cracking behavior of E690 steel in thiosulfate-containing artificial seawater10.1016/j.corsci.2018.08.048 ↗
47. Interaction between hydrogen and cyclic stress and its role in fatigue damage mechanism10.1016/j.corsci.2019.05.028 ↗
48. An electrochemical study of phase-transitions in rust layers10.1016/0010-938X(83)90024-0 ↗
49. Influence of isothermal tempering on microstructures and hydrogen-environmentally embrittlement susceptibility of laser additively manufactured ultra-high strength AerMet 100 steel10.1016/j.msea.2023.145167 ↗
50. Assessment of sulfide corrosion cracking and hydrogen permeation behavior of ultrafine grain high strength steel10.1016/j.corsci.2022.110142 ↗
51. The effect of corrosion evolution on the stress corrosion cracking behavior of mooring chain steel10.1016/j.corsci.2022.110316 ↗
52. Correlation of microstructure and stress corrosion cracking initiation behaviour of the fusion boundary region in a SA508 Cl. 3-Alloy 52M dissimilar weld joint in primary pressurized water reactor environment10.1016/j.corsci.2017.12.011 ↗
53. Microstructure and intergranular stress corrosion cracking susceptibility of a SA508–52 M-316L dissimilar metal weld joint in primary water10.1016/j.jmst.2017.11.051 ↗
54. On the suitability of slow strain rate tensile testing for assessing hydrogen embrittlement susceptibility10.1016/j.corsci.2019.108291 ↗
55. Hydrogen environment assisted cracking of modern ultra-high strength martensitic steels10.1007/s11661-017-4156-0 ↗
56. Measurement and modeling of hydrogen environment–assisted cracking of ultra-high-strength steel10.1007/s11661-006-9051-z ↗
57. Jr, Hydrogen-induced intergranular fracture of steels10.1016/S0013-7944(00)00124-7 ↗
58. S.P. Lynch, Progress towards understanding mechanisms of hydrogen embrittlement and stress corrosion cracking, In: CORROSION 2007, Nashville, Tennessee, 2021, Paper Number: NACE-07493. 〈https://onepetro.org/NACECORR/proceedings/CORR07/All-CORR07/NACE-07493/118618〉.
59. Microstructure and cleavage in lath martensitic steels10.1088/1468-6996/14/1/014208 ↗
60. The nature of quasicleavage fracture in tempered 5.5 Ni steel after hydrogen charging, Metall10.1007/BF02645559 ↗
61. The effect of crack tip environment on crack growth behaviour of a low alloy steel at cathodic potentials in artificial seawater10.1016/j.jmst.2020.04.034 ↗
62. Comparative study on the crack growth behaviours of E690 steel and heat-affected zone microstructures under cathodic potential in artificial seawater based on mechano-electrochemical effect at crack tip10.1016/j.corsci.2022.110103 ↗
63. The role of oxygen on the stability of crevice corrosion10.1149/1.1470655 ↗
64. E. Tada, S. Ajito, A. Ooi, A. Nishikata, Effect of rust on hydrogen uptake into exposed steels during drying of nacl droplets, in: PRiME 2020, Virtual, 2020.10.1149/MA2020-02121290mtgabs ↗
65. Hydrogen absorption behavior of pre-rusted steels under an NaCl droplet10.1149/2.0591910jes ↗
66. Evaluation of hydrogen permeation into high-strength steel during corrosion in different marine corrosion zones10.3390/app12062785 ↗
67. High-pressure corrosion fatigue experiments employing diverse methodologies for assessing rates of crack propagation10.1016/j.jmrt.2024.07.058 ↗