Abstract
The crevice corrosion behavior of 316 L stainless steel in NaCl solution was investigated under constant potential conditions. Once crevice corrosion initiates at a given site, it propagates from the initiation site toward the crevice mouth. Upon reaching the crevice mouth, corrosion spreads circumferentially along the crevice mouth. This behavior occurs because the potential decreases rapidly before reaching the corrosion initiation site due to the IR drop, resulting in higher potential at the crevice mouth than at the bottom. Additionally, the distribution of solution concentration within the crevice does not differ significantly regardless of the location of the corrosion initiation site. This potential gradient leads to an increase in the corrosion current within the crevice, which accelerates crevice corrosion. From an equipment maintenance perspective, this study suggests that crevice corrosion predominantly propagates in the direction of crevice depth near the crevice mouth. When crevice corrosion is detected, even if the crevice length is significant, propagation in the direction of crevice depth is limited near the bottom. Therefore, priority should be given to inspecting and maintaining the area near the crevice mouth.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. The composition of the surface during passivation of stainless steels10.5006/1.3577318 ↗
2. J.W. Oldfield, Crevice corrosion of stainless steel in seawater, ACOM Report No. 1, Avesta AB, Avesta, Sweden, 1998.
3. X-ray photoelectron spectroscopy and scanning tunneling microscopy study of passive films formed on (100) Fe-18Cr-13Ni single-crystal surfaces10.1149/1.1838366 ↗
4. Passive film of 18-8 stainless steel structure and its function10.1016/0010-938X(73)90031-0 ↗
5. An XPS Study of the passivity of a series of iron-chromium alloys in sulphuric acid10.1016/S0010-938X(78)80085-7 ↗
6. A review of passivity breakdown on metal surfaces: influence of chloride- and sulfide-ion concentrations, temperature, and pH, Emergent
7. The role of micro pit in the initiaion process of crevice corrosion of SUS304 stainless steel in aqueous chloride solution10.3323/jcorr.70.32 ↗
8. Response to the Seawater Contamination Event at Hamaoka Unit 5 and the Effects of Corrosion by Seawater
9. Crevice corrosion of stainless steels: I. a mathematical model10.1179/000705978798358671 ↗
10. Crevice corrosion of stainless steels: II. Experimental studies10.1179/000705978798276258 ↗
11. The role of inclusions on initiation of crevice corrosion of stainless steel: I. experimental studies10.1149/1.2096896 ↗
12. The role of inclusions on initiation of crevice corrosion of stainless-steel. 2. Theoretical studies10.1149/1.2096434 ↗
13. On the mechanism of localized corrosion of iron and stainless steel
14. On the mechanism of localized corrosion of iron and stainless steel
15. Susceptibility to crevice corrosion and metastable pitting of stainless steels10.4028/www.scientific.net/MSF.44-45.313 ↗
16. Effects of hydrogen on the crevice corrosion behaviors of duplex stainless steel 220510.1016/j.jmrt.2022.05.026 ↗
17. The crevice corrosion behavior of N80 carbon steel in acidic NaCl solution: the effect of O210.1002/maco.202112595 ↗
18. Distribution of sulfate-reducing bacteria in the crevice and its effect on the initial corrosion behavior of 2205 stainless steel in artificial seawater10.1002/maco.202112759 ↗
19. Corrosion of alloy 690 in simulated steam generator crevices: effect of applied potential, pH and Pb
20. A critical crevice solution and IR drop crevice corrosion model10.1016/j.corsci.2008.02.020 ↗
21. Measurement of pH gradients in the crevice corrosion of Iron using a Palladium Hydride microelectrode10.1149/1.1851053 ↗
22. Pitting on the crevice wall prior to crevice corrosion: iron in sulfate/chromate solution10.1016/j.electacta.2010.10.013 ↗
23. In situ investigation of crevice corrosion on UNS S32101 duplex stainless steel in sodium chloride solution10.1016/j.corsci.2013.06.039 ↗
24. In situ monitoring of crevice corrosion morphology of Type 316L stainless steel and repassivation behavior induced by sulfate ions10.1016/j.corsci.2017.08.005 ↗
25. Introduction of Cu2+ to the inside of the crevice by chelation and its effect on crevice corrosion of Type 316L stainless steel10.1016/j.corsci.2022.110850 ↗
26. The crevice corrosion behaviour of stainless steel in sodium chloride solution10.1016/j.corsci.2011.08.012 ↗
27. Propagation analysis of crevice corrosion on SUS304 stainless steel under potentiostatic condition in artificial sea water10.3323/jcorr.64.51 ↗
28. Crevice corrosion of stainless steels - initiation & propagation mechanism and its evaluation tests-10.3323/jcorr.70.77 ↗
29. Simultaneous visualization of pH and Cl- distributions inside the crevice of stainless steel10.1016/j.corsci.2016.01.028 ↗
30. Visualization of pH and pCl distributions: initiation and propagation criteria for crevice corrosion of stainless steel10.1149/2.019207jes ↗
31. NH4+ Generation: the role of NO3- in the crevice corrosion repassivation of type 316L Stainless Steel10.1149/2.0501910jes ↗
32. The geometric characterization of crevice corrosion part for inside crevice10.3323/jcorr.65.307 ↗
33. A multiphysics model for studying transient crevice corrosion of stainless steel10.1016/j.jmst.2020.06.008 ↗
34. S.K. Karandros, A numerical model of crevice corrosion for passive and active metals10.1016/0010-938X(96)00107-2 ↗
35. An arbitrary Lagrangian-Eulerian model for modelling the time-dependent evolution of crevice corrosion10.1016/j.corsci.2013.10.003 ↗
36. Effect of ionic interactions on the initiation of crevice corrosion in passive metals10.1149/1.1852433 ↗
37. A mathematical model of crevice and pitting corrosion—I. The physical model10.1016/0010-938X(88)90027-3 ↗
38. Mathematical modeling of mass transport and chemical reaction in crevice and pitting corrosion10.1016/0010-938X(90)90013-U ↗
39. Calculating chemical concentrations during the initiation of crevice corrosion10.1016/S0010-938X(99)00097-9 ↗
40. The numerical analysis of potential / current density distribution in crevice corrosion propagation stage10.3323/jcorr.65.350 ↗
41. Estimation of the critical potential for crevice corrosion by measuring metastable pitting potential of stainless steel in aqueous chloride solution10.3323/jcorr.70.302 ↗
42. Experimental and modeling studies on the oxygen ingression behavior at the crevices of stainless steels in high-temperature water10.1016/j.corsci.2025.112897 ↗
43. An experimental study of crevice corrosion behaviour of 316L stainless steel in artificial seawater10.1016/j.corsci.2010.05.040 ↗
44. The effect of crevice-opening dimension on the stability of crevice corrosion for nickel in sulfuric acid10.1149/1.1838632 ↗
45. Effect of crevice gap on crevice corrosion initiation and development of 2205 duplex stainless steel in NaCl
46. Effect of the crevice gap on the initiation of crevice corrosion in passive metals10.5006/1.3287850 ↗
47. Critical characteristic dimension or geometry for determining the susceptibility of a crevice to crevice corrosion10.5006/1.3287849 ↗
48. Role of the thermodynamic properties of concentrated aqueous solutions in corrosion processes
49. Densities of aqueous solutions of inorganic substances
50. Electrochemical studies of the passive film on 316 stainless steel in chloride media10.1149/1.2113954 ↗
51. Passivity and its breakdown on stainless steels and alloys10.1002/sia.1460 ↗
52. Moire method to measure penetration depth profiles on unevenly corroded metal surfaces10.1016/0010-938X(93)90216-4 ↗
53. The electrochemical behavior, including hydrogen overvoltage, of iron in acid environments10.1149/1.2429923 ↗
54. M. Yamamoto, Analysis of corrosion phenomena using Multiphysics calculations, kindaikagaku-sha digita (2022).
55. Pourbaix · 1966
56. Qualitative inorganic analysis Ⅱ
57. Effect of Applied potential on changes in solution chemistry inside crevices on Type 304L stainless steel and Alloy 82510.5006/1.3293476 ↗
58. Temperature and potential dependence of crevice corrosion of AISI 316 stainless steel10.1016/S0010-938X(00)00167-0 ↗
59. Numerical simulation of crevice corrosion of stainless steels and nickel alloys in chloride solutions10.5006/1.3585142 ↗
60. The significance of the local electrode potential within pits, crevices and cracks10.1016/0010-938X(89)90039-5 ↗
61. Corrosion behaviour of 13Cr stainless steel under stress and crevice in 3.5 wt% NaCl solution10.1016/j.corsci.2019.108290 ↗
62. The influence of the crevice induced IR drop on polarization measurement of localized corrosion behavior of 316L stainless steel10.1016/j.corsci.2019.04.030 ↗
63. Influence of pH and chloride concentration on the pitting and crevice corrosion behavior of high-alloy stainless steels10.5006/1.3280545 ↗