journal article·2022-01

Antioxidation enhancement and siliconization mitigation for SiC coated C/C composites via a nano-structural SiC porous layer

Tao Li, Yulei Zhang, Yanqin Fu, Jia Sun

Corrosion Science· Volume 194
Publisher page

Abstract

Abstract A reactive nano-structural SiC porous layer on C/C surface was pre-prepared via a slurry-dipping and reaction-sintering method, using Si, C and Al2O3 powders as raw materials. Pre-introduction of nano-structural SiC porous layer helped to form a dense sintered SiC coating by the pack cementation (PC), which provided excellent oxidation protection for C/C substrate under different conditions at 1773 K and mitigated the siliconization reaction of free silicon during the PC process. Results showed that the modified SiC coating had a mass loss of only ~0.03% after 50 thermal cycles between room temperature and 1773 K in air. And the mass loss reduced by ~4.31 and ~2.25 times after isothermal oxidation in dry air and wet oxygen atmosphere at 1773 K, respectively. Furthermore, because of the delaying effect of SiC porous layer on free silicon infiltrating into C/C substrate, the bending strength of modified SiC-coated C/C composites has increased by 93.0%.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Thermal properties of materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Oxidation microstructure studies of reinforced carbon/carbon10.1016/j.carbon.2005.11.013 ↗
2. Mechanical and thermal properties of C/C composites modified with SiC nanofiller10.1016/j.msea.2018.01.048 ↗
3. Carbon-carbon composites: oxidation behavior and coatings protection
4. Effects of thermal and thermomechanical induced mechanical changes of C/C composites10.1016/j.carbon.2010.04.040 ↗
5. Oxidation protective multilayer coatings for carbon-carbon composites10.1016/S0008-6223(01)00151-8 ↗
6. An oxidation protective Si-Mo-Cr coating for C/SiC coated carbon/carbon composites10.1016/j.carbon.2007.10.022 ↗
7. Tailored macro-pores during the formation of C/C-SiC via liquid phase pyrolysis10.1016/j.jeurceramsoc.2020.10.006 ↗
8. Coating effects on thermal properties of carbon carbon and carbon silicon carbide composites for space thermal protection systems10.1016/j.actaastro.2014.02.007 ↗
9. Erosion protective coatings for low density, highly porous carbon/carbon composites10.1016/j.carbon.2009.01.045 ↗
10. Multilayer and multi-component oxidation protective coating system for carbon/carbon composites from room temperature to 1873 K10.1016/j.corsci.2013.03.006 ↗
11. Characterization of the oxidation of C/C/SiC composites by X-ray microtomography10.1016/j.jeurceramsoc.2020.06.042 ↗
12. SiC/MoSi2 based coatings for Cf/C composites by two step pack cementation10.1016/j.jeurceramsoc.2018.01.024 ↗
13. ZrB2-SiC based composites for thermal protection by reaction sintering of ZrO2+B4C+Si10.1007/s40145-017-0244-2 ↗
14. Preparation of an oxidation protection coating for C/C composites by low pressure chemical vapor deposition10.1016/S0008-6223(00)00086-5 ↗
15. Oxidation through coating cracks of SiC-protected carbon/carbon10.1016/j.surfcoat.2008.09.013 ↗
16. Resistance to oxidation and ablation of SiC coating on graphite prepared by chemical vapor reaction10.1016/j.corsci.2013.05.009 ↗
17. Silicon carbide based plasma sprayed coatings10.1016/j.surfcoat.2012.06.062 ↗
18. Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites10.1016/j.carbon.2004.01.066 ↗
19. Influence of preparation temperature on the oxidation resistance and mechanical properties of C/SiC coated C/C composites10.1016/j.corsci.2014.05.009 ↗
20. Oxidation and mechanical properties of SiC/SiC-MoSi2-ZrB2 coating for Carbon/Carbon composites10.1016/j.jmst.2013.09.006 ↗
21. TaxHf1−xB2-SiC multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.corsci.2014.07.016 ↗
22. coating providing oxidation and ablation protection over 1973 K for SiC coated C/C composites10.1016/j.corsci.2020.108536 ↗
23. The oxidation behavior and mechanical properties of MoSi2-CrSi2-SiC-Si coated carbon/carbon composites in high-temperature oxidizing atmosphere10.1016/j.corsci.2011.08.018 ↗
24. Oxidation and ablation resistance of ZrB2-SiC-Si/B-modified SiC coating for carbon/carbon composites10.1016/j.corsci.2012.10.041 ↗
25. A C/SiC gradient oxidation protective coating for carbon/carbon composites10.1016/j.surfcoat.2006.07.239 ↗
26. Bamboo-shaped SiC nanowire-toughened SiC coating for oxidation protection of C/C composites10.1016/j.corsci.2012.12.009 ↗
27. Influence of SiC nanowires on the properties of SiC coating for C/C composites between room temperature and 1500 °C10.1016/j.corsci.2011.05.046 ↗
28. High strength retention and improved oxidation resistance of C/C composites by utilizing a layered SiC ceramic coating10.1016/j.ceramint.2021.01.208 ↗
29. Single-crystal SiC nanowires with a thin carbon coating for stronger and tougher ceramic composites10.1002/adma.200500104 ↗
30. SiC nanowire-induced fabrication of fine-grained and highly-density SiC coating by pressure-less reactive sintering10.1016/j.jallcom.2018.05.001 ↗
31. Simple approach to fabricate SiC-SiO2 composite nanowires and their oxidation resistance10.1016/j.mseb.2010.01.042 ↗
32. Preparation and characterization of SiO2 thin film and SiC nanofibers to improve of graphite oxidation resistance10.1016/j.jeurceramsoc.2016.06.046 ↗
33. Silicon carbide coating by reactive pack cementation—part II: silicon monoxide/carbon reaction10.1002/(SICI)1521-3862(200002)6:1<41::AID-CVDE41>3.0.CO;2-8 ↗
34. Effects of pyrocarbon on morphology stability of SiC nanowires at high temperatures10.1111/jace.15524 ↗
35. Sintering behavior, microstructural evolution, and mechanical properties of ultra-fine grained alumina synthesized via in-situ spark plasma sintering10.1016/j.ceramint.2015.11.106 ↗
36. Aluminum composite reinforced with multiwalled carbon nanotubes from plasma spraying of spray dried powders10.1016/j.surfcoat.2008.12.004 ↗
37. Thermal shock resistance and isothermal oxidation behavior of C/SiC-SiCnano functionally gradient coating on graphite produced via reactive melt infiltration (RMI)10.1016/j.matchemphys.2016.07.004 ↗
38. SiC coating toughened by SiC nanowires to protect C/C composites against oxidation10.1016/j.ceramint.2011.05.159 ↗
39. Toughening by SiC nanowires in a dense SiC-Si ceramic coating for oxidation protection of C/C composites10.1111/j.1551-2916.2012.05412.x ↗
40. Oxidation protection of C/C composites with a multilayer coating of SiC and Si + SiC + SiC nanowires10.1016/j.carbon.2011.10.048 ↗
41. A SiC-ZrB2-ZrC coating toughened by electrophoretically-deposited SiC nanowires to protect C/C composites against thermal shock and oxidation10.1016/j.apsusc.2015.05.028 ↗
42. SiC nanoparticles toughened-SiC/MoSi2-SiC multilayer functionally graded oxidation protective coating for carbon materials at high temperatures10.1007/s11665-017-2725-4 ↗
43. Nanowire-toughened transition layer to improve the oxidation resistance of SiC-MoSi2-ZrB2 coating for C/C composites10.1016/j.corsci.2016.05.013 ↗
44. A SiCnw/PyC-toughened ZrB2-SiC coating for protecting Si-SiC coated C/C composites against oxidation10.1016/j.apsusc.2018.06.246 ↗
45. Improved thermal shock resistance of SiCnw/PyC core-shell structuretoughened CVD-SiC coating10.1016/j.jeurceramsoc.2018.02.017 ↗
46. Oxidation pre-treatment and electrophoretic deposition of SiC nanowires to improve the thermal shock resistance of SiC coating for C/C composites10.1016/j.jallcom.2015.02.075 ↗
47. Nanowire-toughened CVD-SiC coating for C/C composites with surface pre-oxidation10.1080/02670844.2017.1292705 ↗
48. Effect of carbon nanotubes on the toughness, bonding strength and thermal shock resistance of SiC coating for C/C-ZrC-SiC composites10.1016/j.jallcom.2015.04.223 ↗
49. Surface dissolution and diffusion of oxygen molecules in SiO2 glass10.2109/jcersj.112.559 ↗
50. Effects of ZrB2 and SiC dual addition on the oxidation resistance of graphite at 1600–2000 °C10.1016/j.corsci.2013.06.041 ↗
51. Oxidation of liquid silicon in air atmospheres containing water vapor10.1021/acs.iecr.9b00313 ↗