Corrosion behavior of high-pressure die-cast secondary AlSi9Cu3(Fe) alloy
Source abstract
Abstract
This research investigated the corrosion behavior and susceptibility to stress corrosion cracking (SCC) of a high-pressure die-cast secondary AlSi9Cu3(Fe) alloy in 3.5 % NaCl solution. Microstructural observations by scanning electron microscope, coupled to energy dispersion spectroscopy, polarization curve recording, electrochemical impedance spectroscopy tests and slow strain rate tests evidenced the presence of critical surface segregation zones, where strong corrosion attack occurs due to composition differences and peculiar morphology of noble Al2Cu phases. No SCC susceptibility was detected, but very strong localized corrosion attack and abundant hydrogen gas bubbling evolved from noble phase/α-Al matrix interphases, determining positive going potential transients.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Mechanical and microstructural characterization of diecast aluminium alloys
2. The influence of Sr, Mg and Cu addition on the microstructural properties of a secondary AlSi9Cu3(Fe) die casting alloy10.1016/j.matchar.2013.08.012 ↗
3. Effects of microstructure and casting defects on the fatigue behavior of the high-pressure die-cast AlSi9Cu3(Fe) alloy10.1016/j.prostr.2017.11.119 ↗
4. The effects of microstructure heterogeneities and casting defects on the mechanical properties of high-pressure die-cast AlSi9Cu3(Fe) alloys10.1007/s11661-014-2515-7 ↗
5. A new high-strength and corrosion-resistant Al–Si based casting alloy10.1016/j.matlet.2013.01.112 ↗
6. Age-hardening behavior of cast Al–Si base alloy10.1016/j.matlet.2003.12.027 ↗
7. The role of Cr additions and Fe-rich compounds on microstructural features and impact toughness of AlSi9Cu3(Fe) diecasting alloys10.1016/j.msea.2014.02.071 ↗
8. Effect of precipitate evolution on the pitting corrosion of friction stir welded joints of an Al-Cu alloy10.5006/2049 ↗
9. Mechanism of intergranular corrosion of Al-Cu alloys10.1016/S0010-938X(70)80003-8 ↗
10. Pitting potential of high purity binary aluminium alloys-I. Al-Cu alloys. Pitting and Intergranular corrosion10.1016/0010-938X(77)90044-0 ↗
11. Davis · 1999
12. Microelectrochemical studies of pit initiation at single inclusions in Al 2024-T310.1149/1.1344530 ↗
13. Stable pit formation on AA2024-T3 in a NaCl environment10.1016/j.corsci.2009.08.043 ↗
14. Electrochemical characteristics of intermetallic phases in aluminium alloys: an experimental survey and discussion10.1149/1.1869984 ↗
15. Electrochemical behaviour and localised corrosion associated with Al7Cu2Fe particles in aluminium alloy 7075-T65110.1016/j.corsci.2006.02.007 ↗
16. Electrochemical quartz crystal microbalance study of corrosion of phases in AA202410.1149/1.1524172 ↗
17. Understanding the origins of intergranular corrosion in copper-containing Al-Mg-Si alloys10.1007/s11661-015-3296-3 ↗
18. On the intergranular corrosion and hardness evolution of 6xxx series Al-alloys as a function of Si:Mg ratio, Cu content and ageing condition10.5006/2506 ↗
19. Effect of segregation and surface condition on corrosion of Rheo-HPDC Al–Si alloys10.3390/met8040209 ↗
20. Effect of silicon content on microstructure and electrochemical behavior of hypoeutectic Al–Si alloys10.1016/j.matlet.2007.05.051 ↗
21. A study of a non-conventional evaluation of results from salt spray test of aluminum high pressure die casting alloys for automotive components10.1002/maco.201810307 ↗
22. Influence of injection temperature and pressure on the microstructure, mechanical and corrosion properties of a AlSiCu alloy processed by HPDC10.1016/j.matdes.2015.09.095 ↗
23. Effect of heat treatments on the microstructure, hardness and corrosion behavior of nondendritic AlSi9Cu3(Fe) cast alloy
24. Standard E.N. 1706:2020 + A1:2021, Aluminium and aluminium alloys – Castings – Chemical composition and mechanical properties, 2020, pp. 1–35.
25. Standard · 2021 · 1
26. Stress corrosion cracking of 13 % Cr martensitic steels in sodium chloride solutions in the presence of thiosulphate10.1002/(SICI)1521-4176(200004)51:4<207::AID-MACO207>3.0.CO;2-7 ↗
27. The influence of Cr content on the microstructure and mechanical properties of AlSi9Cu3(Fe) die-casting alloys10.1016/j.msea.2010.08.079 ↗
28. Quench modification of aluminium-silicon eutectic alloys10.1007/BF00352787 ↗
29. Inverse surface macro-segregation in high-pressure die-cast AM60 magnesium alloy and its effects on fatigue behavior10.1016/j.scriptamat.2005.01.007 ↗
30. Feeding mechanisms in high-pressure die castings10.1007/s11661-010-0222-6 ↗
31. L. Bäckerud, G. Chai, J. Tamminen, Solidification Characteristics of Aluminum Alloys, first ed., Vol. 2: Foundry Alloys, American Foundrymen’s Society Inc., Des Plaines, IL, United States, 1990.
32. Pitting corrosion of rheocast A356 aluminium alloy in 3.5 wt% NaCl solution10.1016/j.corsci.2013.04.023 ↗
33. Influence of surface liquid segregation on corrosion behavior of semi-solid metal high pressure die cast aluminium alloys10.1016/S1003-6326(10)60591-2 ↗
34. Development of shear bands during deformation of partially solid alloys10.1016/j.scriptamat.2010.08.032 ↗
35. Microstructure formation in AlSi4MgMn and AlMg5Si2Mn high-pressure die castings10.1007/s11661-009-9841-1 ↗
36. Pitting corrosion of Al and Al–Cu single crystals10.1149/1.2086291 ↗
37. Study of Al alloy corrosion in neutral NaCl by the pitting scan technique10.1016/j.matchemphys.2010.02.022 ↗
38. Enhancing corrosion resistance of 7150 Al alloy using novel three-step aging process10.1016/S1003-6326(16)64192-4 ↗
39. Characterization of pitting behavior of pure Al and Al-7Zn-0.1Sn-0.015Ga alloy by cyclic polarization technique
40. Corrosion study of the friction stir lap joint of AA7050-T76511 on AA2024-T3 using the scanning vibrating electrode technique10.1016/j.corsci.2015.02.029 ↗
41. Effect of multipass friction stir processing on corrosion resistance of hypereutectic Al–30Si alloy10.1016/j.corsci.2014.02.013 ↗
42. Effects of strontium addition on the microstructure and corrosion behavior of A356 aluminum alloy10.1016/j.jallcom.2018.05.341 ↗
43. The effect of vacuum suction casting on the microstructure and corrosion behavior of aluminium alloy10.1016/j.mseb.2019.01.006 ↗
44. Analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
45. Evaluation of some phenothiazine derivatives as corrosion inhibitors for bronze in weakly acidic solution10.1016/j.corsci.2012.06.010 ↗
46. The effect of small addition of tin and indium on the corrosion behavior of aluminium in chloride solution10.1016/j.jallcom.2010.06.055 ↗
47. Organo-silane coatings for AZ31 magnesium alloy corrosion protection10.1016/j.matchemphys.2008.02.015 ↗
48. Mono-carboxylate conversion coatings for AZ31 Mg alloy protection10.1002/maco.200905615 ↗
49. Change of corrosion potential fluctuations with pits growing on aluminum surface
50. Corrosion of AA2024-T3 Part I: localised corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
51. Corrosion of AA2024-T3 Part II: co-operative corrosion10.1016/j.corsci.2010.09.030 ↗
52. In-situ monitoring of pitting corrosion in aluminium alloy 202410.5006/1.3284873 ↗
53. The effect of precipitate size on the yield strength-pitting corrosion correlation in Al–Cu–Mg alloys10.1016/j.actamat.2010.07.010 ↗