journal article·2025-04

Influence of Zr alloying on the corrosion behavior of Ti-Zr alloys in simulated hot HNO3 reprocessing conditions

C.C. Liu, L.M. Zhang, Z. Liu, D.C. Ren, A.L. Ma, Z.X. Liu, Y.G. Zheng

Corrosion Science· Volume 246
Publisher page

Abstract

Titanium and its alloys show considerable potential for spent fuel reprocessing characterized by high-temperature HNO 3 due to their enhanced corrosion resistance through alloying. This study investigated the effects of Zr alloying on the microstructure and corrosion behavior of Ti-Zr alloys, integrating experimental research with theoretical calculations. The results demonstrated that the addition of Zr increased microstructural disorder, which in turn improved the mechanical properties. Optimal levels of Zr significantly enhanced both the corrosion resistance and the mechanical properties of the alloys. These findings underscored the suitability of Ti-Zr alloys for extremely corrosive environments, making them promising candidates for advanced reprocessing applications.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (75)

Show source-provided references
1. 4.19 - Corrosion in nuclear fuel reprocessing plants: corrosion in boiling nitric acid
2. Chapter 21 - the nuclear fuel cycle
3. Corrosion issues in nuclear industry today10.1016/S1369-7021(08)70205-0 ↗
4. Corrosion and contamination study of nuclear plant steel in HNO3‑Based waste solution with Strontium under nuclear processing environment
5. Materials development and corrosion problems in nuclear fuel reprocessing plants10.1016/j.pnucene.2005.07.001 ↗
6. Some fundamental understandings of Zn-injection water chemistry on material corrosion in pressurized water reactor primary circuit10.1016/j.corcom.2021.12.004 ↗
7. Corrosion behaviour of AISI type 304L stainless steel in nitric acid media containing oxidizing species10.1016/j.corsci.2010.09.023 ↗
8. Estimating the corrosion rate of stainless steel R-SUS304ULC in nitric acid media under concentrating operation10.1016/j.jnucmat.2024.154914 ↗
9. Effect of oxidizing ions on the corrosion behavior of SiN stainless steel in high-temperature nitric acid solution10.1016/j.electacta.2023.141917 ↗
10. Application of surface response analysis to the optimisation of nitric passivation of cp titanium and Ti6Al4V10.1016/j.surfcoat.2005.09.034 ↗
11. Structure of the oxide film on Ti–6Ta alloy after immersion test in 8mol/L boiling nitric acid medium10.1016/j.elspec.2013.08.013 ↗
12. Critical firing conditions for titanium alloys by molten droplet ignition10.1016/j.corcom.2022.10.003 ↗
13. Understanding the effect of fluoride on corrosion behavior of pure titanium in different acids10.1016/j.corsci.2021.109812 ↗
14. Friction and wear behaviour of cp Ti and Ti6Al4V following nitric acid passivation10.1016/j.apsusc.2006.04.047 ↗
15. Wear behaviour of nitric acid passivated cp Ti and Ti6Al4V10.1016/j.jallcom.2008.11.138 ↗
16. Temperature induced cathode-anode reversal behavior of TA2–304 L galvanic couple in simulated spent fuel reprocessing media10.1016/j.electacta.2023.143168 ↗
17. Superior corrosion resistance of Ti-Al-Zr alloy in aggressive nitric acid environments10.1007/s11665-020-05300-z ↗
18. Effects of Zr addition on the microstructural evolution, mechanical properties, and corrosion behavior of novel biomedical Ti-Zr-Mo-Mn alloys10.1021/acsbiomaterials.3c01012 ↗
19. Refinement of as phase and formation of nano-twins of Ti-7Mo-4Al-3Nb-2Cr alloyed by Zr element10.1016/j.jmrt.2022.10.129 ↗
20. Influence of Zr content on microstructure and corrosion behavior of As-Cast Zr-modified Ti6Al7Nb alloy for biomedical applications10.1007/s11665-022-07777-2 ↗
21. Effect of Zr on microstructure and properties of TC4 alloy fabricated by laser additive manufacturing10.1016/j.jmrt.2023.05.137 ↗
22. Synergistic effect of Zr addition and grain refinement on corrosion resistance and pitting corrosion behavior of single α-phase Ti-Zr-based alloys10.1016/j.jallcom.2021.163013 ↗
23. Effect of Zr content on microstructure, mechanical properties and corrosion behaviour in hydrochloric acid for as-cast Ti-Zr alloy10.1016/j.corsci.2024.112136 ↗
24. Effect of zirconium content on the microstructure and corrosion behavior of Ti-6Al-4V-xZr alloys10.1016/j.corsci.2016.09.012 ↗
25. Effects of Zr content on microstructure and corrosion resistance of Ti-30Nb-Zr casting alloys for biomedical applications10.1016/j.electacta.2007.10.060 ↗
26. Effect of zirconium content on the microstructure and corrosion behavior of as-cast Ti-Al-Nb-Zr-Mo alloy10.1016/j.jmrt.2021.10.102 ↗
27. Influence of Zr content on immersion and electrochemical corrosion behavior of as-cast TiZr alloys10.1108/ACMM-04-2022-2648 ↗
28. Effect of zirconium content on the microstructure, physical properties and corrosion behavior of Ti alloys10.1016/j.msea.2014.08.010 ↗
29. Investigations of cathodic reactions using cyclic voltammetry and electrochemical behavior of Ti–Al–Zr alloy in nitric acid using electrochemical impedance spectroscopy10.1007/s10800-021-01628-z ↗
30. Exploring the impact of Al alloying on microstructure and hot nitric acid corrosion resistance of Ti-xAl (x=0, 1, 2, 3, 4, 5) alloys10.1016/j.corsci.2024.112010 ↗
31. Potential dependent mechanism of the composition and electrochemical property of oxide films of Ti-6Al-3Nb-2Zr-1Mo10.1016/j.corsci.2023.110978 ↗
32. Corrosion and biological behaviors of biomedical Ti-24Nb-4Zr-8Sn alloy under an oxidative stress microenvironment10.1021/acsami.4c00562 ↗
33. Solute segregation and its influence on the microstructure and electrochemical behavior of Ti-Nb-Zr alloys10.1016/j.jallcom.2008.11.030 ↗
34. A comparative study on the passive film and SCC behavior of Ti-6Al-3Nb-2Zr-1Mo alloy at various test temperatures in simulated seawater10.1016/j.corsci.2024.112066 ↗
35. Effect of chloride ion on the corrosion behavior of SiN stainless steel in concentrated hot nitric acid media10.1016/j.corsci.2023.111604 ↗
36. Comparison of the three-phase corrosion behavior of SiN and 304L stainless steels in 6 M nitric acid solution at different temperatures10.3390/met12060922 ↗
37. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set10.1016/0927-0256(96)00008-0 ↗
38. Ab initio molecular dynamics for liquid metals
39. From ultrasoft pseudopotentials to the projector augmented-wave method10.1103/PhysRevB.59.1758 ↗
40. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
41. Improved adsorption energetics within density-functional theory using revised Perdew-Burke-Ernzerhof functionals10.1103/PhysRevB.59.7413 ↗
42. Latent heat of TB18 titanium alloy during β to a phase transition by DSC and first-principles methods10.1007/s40195-023-01589-6 ↗
43. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗
44. Technical Note: concerning the conversion of the constant phase element parameter Y0 into a capacitance10.5006/1.3280607 ↗
45. Potential dependent mechanism of the composition and electrochemical property of oxide films of Ti-6Al-3Nb-2Zr-1Mo10.1016/j.corsci.2023.110978 ↗
46. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
47. Impedance analysis of electrochemical systems10.1021/acs.chemrev.1c00876 ↗
48. Electrochemistry at semiconductor and oxidized metal electrodes10.1016/0021-9797(82)90180-1 ↗
49. C.D. Wagner, A.V. Naumkin, A. Kraut-Vass, J.W. Allison, J.J.R. Rumble, NIST Standard Reference Database 20 version 4.1, 2003.
50. XPS analysis of adsorption of oxygen molecules on the surface of ti and tinx films in vacuum10.1016/0368-2048(92)80016-2 ↗
51. The NIST x-ray photoelectron spectroscopy database10.1002/sia.740190147 ↗
52. Microstructure and transformation texture evolution during α precipitation in polycrystalline α/β titanium alloys - a simulation study10.1016/j.actamat.2015.04.050 ↗
53. Correspondence of the aging behaviors and the phase constituents of the Ti-Mo-based alloys tailored by the Al and Zr additions10.1016/j.jallcom.2024.174509 ↗
54. First-principles study of the phase stability and elastic properties of Ti-X alloys (X = Mo, Nb, Al, Sn, Zr, Fe, Co, and O)10.1016/j.jallcom.2017.08.128 ↗
55. Preparation, structural and microstructural characterization of Ti-25Ta-10Zr alloy for biomedical applications10.1016/j.jmrt.2019.07.020 ↗
56. The influence of zirconium content on the microstructure, mechanical properties, and biocompatibility of in-situ alloying Ti-Nb-Ta based β alloys processed by selective laser melting10.1016/j.msec.2021.112486 ↗
57. Development and characterization of a new predominantly β Ti-15Mo-5In alloy for biomedical applications10.1007/s10853-023-09017-x ↗
58. Mechanisms of macrozone elimination and grain refinement of near α Ti alloy via the spheroidization of the Widmannstatten structure10.1016/j.actamat.2023.119339 ↗
59. Microstructure and mechanical properties of a novel β titanium metallic composite by selective laser melting10.1016/j.actamat.2014.01.018 ↗
60. Additive manufacturing of titanium alloys by electron beam melting: a review10.1002/adem.201700842 ↗
61. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
62. Optimized mechanical properties, corrosion resistance and bactericidal ability of Ti-15Zr-xCu biomedical alloys during aging treatment10.1007/s40195-021-01248-8 ↗
63. Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
64. Biomedical applications of titanium and its alloys10.1007/s11837-008-0031-1 ↗
65. Modification of alpha morphology in Ti-6Al-4V by thermomechanical processing10.1007/BF02644991 ↗
66. Passivity–the key to our metals-based civilization10.1351/pac199971060951 ↗
67. Electronic properties and defect structure of Fe and Fe-Cr passive films10.5006/1.3315929 ↗
68. Diffusivity of point defects in the passive film on a Ni16Cr13Co4Mo alloy in molten NaCl-Na2SO410.1016/j.corsci.2023.111456 ↗
69. Dean · 1999
70. Study of the passivation and repassivation behavior of pure titanium in 3.5 wt% NaCl solution and 6 M HNO3 solution10.1016/j.corsci.2023.111538 ↗
71. Nucleation of corrosion pits in Ringer's solution containing bovine serum10.1016/j.corsci.2007.05.018 ↗
72. Depassivation current transients measured between identical twin microelectrodes in open circuit10.1016/j.corsci.2006.06.036 ↗
73. The effect of temperature on the nucleation of corrosion pits on titanium in Ringer's physiological solution10.1016/j.biomaterials.2004.02.023 ↗
74. Effects of alloy and solution chemistry on the fracture of anodic films formed at metastable pitting potentials10.1179/174327805X46922 ↗
75. Correlation between passive film-induced stress and stress corrosion cracking of α-Ti in a methanol solution at various potentials10.1016/S0921-5093(02)00529-4 ↗