Insights into the effect of Cr on interfacial and grain boundaries oxidation in Fe-Mn-Si-based alloys
Source abstract
Abstract
Grain-boundary oxides formed in advanced high-strength steels during hot-rolled coil can seriously impair the formability and the surface quality of coatings. In this paper, the effect of Cr addition on interfacial and internal oxidation of Fe-Mn-Si based alloys was investigated. The experimental results show that the internal oxidation of Cr-containing alloys decreases significantly, while the interfacial oxidation increases significantly. This is attributed to the formation of dispersed Mn-Si and Mn-Cr oxides at the interface and depletion of solute elements near grain boundaries. In addition, Cr enhanced the driving force for Mn and Si migration to the oxide scale/substrate interface.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Strategies for third-generation advanced high-strength steel development
2. Selective oxidation of a medium-Mn third generation advanced high strength steel during austenitizing and intercritical annealing10.1149/1945-7111/ac790a ↗
3. The surface and sub-surface structure of continuously annealed sheet steel: implications for galvanizing and galvannealing
4. Galvanizability of high-strength steels for automotive applications10.1007/s11661-001-1042-5 ↗
5. On the reactive wetting of a medium-Mn advanced high-strength steel during continuous galvanizing10.1016/j.surfcoat.2018.10.028 ↗
6. Effect of dew point on the reactive wetting of a C-2Mn-1.3Si (wt%) advanced high strength steel during continuous galvanizing10.1016/j.surfcoat.2018.06.060 ↗
7. Effect of carbon on isothermal reduction of high-strength steel oxide scale in 30% H2–N2 atmosphere10.1016/j.jclepro.2020.123681 ↗
8. Influence of Si content on selective oxidation and oxide scale phase transition during hot-rolled coiling10.1016/j.jmrt.2023.06.163 ↗
9. Insight into internal oxidation mechanism of hot rolled Si–Mn added high strength steel: Pure iron layer formation10.1016/j.vacuum.2023.111828 ↗
10. Formation of a dark streaky edge defect on galvannealed ultra-high strength steel10.1016/j.surfcoat.2022.128162 ↗
11. Effect of internal oxidation of the hot-rolled sheet steel, on the suppression of the Si and Mn selective surface oxidation in recrystallization annealing, after cold rolling10.4139/sfj.55.48 ↗
12. Effect of process atmosphere dew point and tin addition on oxide morphology and growth for a medium-Mn third generation advanced steel during intercritical annealing10.1007/s11661-018-4855-1 ↗
13. Influence of Al addition on the grain boundary oxidation of ultra high strength steels during hot coiling10.1016/j.corsci.2022.110863 ↗
14. New insights into the effect of Al on the selective oxidation of advanced high-strength steels prior to hot-dip galvanizing10.1016/j.actamat.2024.119651 ↗
15. Thermodynamic consideration on selective surface oxidation of high strength steels prior to hot-dip galvanizing10.1007/s11998-011-9334-1 ↗
16. J. Vrieze, A. Dekker, H. Winter, R. Zwetsloot, Cold rolled hot dip galvanised multi phase steel with 600–900 MPa tensile strengths, Proc. Galvanised Sheet Steel Forum–Automotive, London, (2000) 17–26.
17. Influence of Cr addition on selective oxidation behavior of Mn-added high-strength steel sheet10.2355/isijinternational.ISIJINT-2018-075 ↗
18. S. Maekawa R. Otomo, A. Kawakami, Internal oxidation of Fe-Si-Mn-Cr alloy under oxide scales formed during hot rolling process, 13th Int. Conf. on Zinc and Zinc Alloy Coated Steel Sheet (Galvatech’23), Seoul, (2023) 1267–1274.
19. Kubaschewski · 1967
20. Oxygen solubility in austenitic Fe-Ni alloys at high temperatures10.1016/j.jallcom.2017.10.226 ↗
21. Internal oxidation of austenitic Fe-Ni-Cr alloys at high temperatures: deduction of oxygen permeability and the influence of carbon-bearing gases10.1016/j.corsci.2023.111465 ↗
22. Effect of alloying elements, water vapor content, and temperature on the oxidation of interstitial-free steels10.1007/s11663-009-9238-y ↗
23. Investigation of selective oxidation during cooling of hot-rolled iron-manganese-silicon alloys10.1016/j.corsci.2021.109466 ↗
24. Surface oxidation and wettability of Fe–Mn and Fe–Mn–Si-alloyed steel after annealing10.1007/s11661-022-06847-3 ↗
25. Internal oxidation in dry and wet conditions for oxygen permeability of Fe–Ni alloys at 1150 and 1100 °C10.1007/s11085-017-9724-6 ↗
26. Role of interface structure and interfacial defects in oxide scale growth10.1007/BF01046723 ↗
27. Influence of oxidation temperature and Cr content on the adhesion and microstructure of scale on low Cr steels10.1007/s11085-009-9167-9 ↗
28. Oxidation behavior and scale properties on the Si containing steels10.4028/www.scientific.net/MSF.522-523.477 ↗
29. The effect of temperature and water vapor on the initial stage of high temperature oxidation of an Fe-1.5 mass% Si alloy10.2355/tetsutohagane1955.86.8_526 ↗
30. Comparative oxidation behaviour of Fe-9Cr steel in CO2 and H2O at 550 °C: detailed analysis of the inner oxide layer10.1016/j.corsci.2015.07.032 ↗
31. Oxidation of Fe–10Cr in O2 and in O2 + H2O environment at 600 °C: a microstructural investigation10.1016/j.corsci.2013.06.016 ↗
32. Morphologies of oxide growth and exfoliation in superheater and reheater tubing of steam boiler10.3184/096034011X12982937656387 ↗
33. Carbon transport through oxide scales on Fe-Cr alloys10.1007/BF00751801 ↗
34. D.J. Young, High Temperature Oxidation and Corrosion of Metals, 2nd edition, Elsevier, 2016.10.1016/B978-0-08-100101-1.00001-7 ↗
35. Retaining meta-stable fcc-Cr phase by restraining nucleation of equilibrium bcc-Cr phase in CuCrZrTi alloys during ageing10.1016/j.jallcom.2018.03.238 ↗
36. Segregation and precipitation at grain boundaries of weathering steels without/with Sb addition10.1016/j.matchemphys.2019.121783 ↗
37. Interfacial segregation of Sn during the continuous annealing and selective oxidation of Fe-Mn-Sn alloys10.3390/ma17061257 ↗
38. Grain boundary segregation engineering in metallic alloys: a pathway to the design of interfaces10.1016/j.cossms.2014.06.002 ↗
39. On the chemistry of grain boundary segregation and grain boundary fracture10.1007/BF02646981 ↗
40. Grain boundary activity measurements by auger electron spectroscopy10.1016/0036-9748(72)90162-7 ↗
41. Use of a “BET” analogue equation to describe grain boundary segregation10.1016/0036-9748(73)90124-5 ↗
42. Segregation to interfaces10.1179/imr.1977.22.1.262 ↗
43. On the interaction between Mn, Sb and O during the annealing and selective oxidation of Fe-Mn-Sb alloy10.1016/j.scriptamat.2022.115096 ↗
44. Birks · 2006
45. Lejcek · 2010
46. Dowben · 1990
47. Internal oxidation of Fe–3% Si alloys annealed under H2O–H2 atmosphere10.1002/maco.201005862 ↗