In situ microscopy and electrochemical characteristics of initiation of intergranular corrosion of aging-treated Al–1Mg–0.65Si–0.8Cu alloy in 0.1 M NaCl
Source abstract
Abstract
This study investigated the initiation site of intergranular corrosion (IGC) in aging-treated Al–1Mg–0.65Si–0.8Cu alloy in 0.1 M NaCl. Polarization and open-circuit potential measurements were performed. Further, in situ observations were made using a small electrode area of 300 µm × 300 µm. In potentiodynamic polarization, the breakdown potential was −0.4 V vs. SHE, leading to pitting corrosion, which in turn initiated IGC. The OCP under naturally aerated conditions increased from approximately −1.2 to −0.4 V over time, and IGC was initiated at −0.4 V. Even in the case of the small electrode area (300 µm × 300 µm), IGC occurred at −0.4 V in potentiostatic polarization; high-spatial-resolution in situ observations were then performed. IGC initiated from randomly distributed Mg 2 Si particles and generation of gas bubbles. Moreover, the Mg 2 Si particles at the initiation site of IGC were located on or near the grain boundaries, and trenching was observed at the Mg 2 Si/alloy matrix boundaries. In addition to the exposure of the bare alloy surface by trenching, the acidification inside the trench likely contributed to the initiation of IGC. The role of Mg 2 Si in the initiation of IGC was examined based on the results of in situ observations and the polarization behavior. • Mg 2 Si particles (≥1 µm) were randomly distributed in Al–1Mg–0.65Si–0.8Cu alloy. • Intergranular corrosion (IGC) initiated at Mg 2 Si located on or near grain boundary. • Trenching between Mg 2 Si and alloy matrix provided the sites for IGC. • An acid in the trench likely dissolves the Cu-depleted zone and leads to IGC. • Corrosion tunnels around the Mg 2 Si might also be related to the IGC initiation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Corrosion of aluminum alloys
2. Mechanism of intergranular corrosion of Al–Cu alloys10.1016/S0010-938X(70)80003-8 ↗
3. The intergranular corrosion susceptibility of a heavily overaged Al–Mg–Si–Cu alloy10.1016/j.corsci.2016.02.025 ↗
4. Influence of the grain boundary chemistry on the intergranular corrosion mechanisms of a high-strength Al–Mg–Si alloy10.1002/sia.5859 ↗
5. Comparing intergranular corrosion in Al-Mg-Si-Cu alloys with and without α-Al(Fe, Mn, Cu)Si particles10.1002/maco.202011954 ↗
6. Understanding the origins of intergranular corrosion in copper-containing Al–Mg–Si alloys10.1007/s11661-015-3296-3 ↗
7. Effects of grain boundary chemistry and precipitate structure on intergranular corrosion in Al–Mg–Si alloys doped with Cu and Zn10.1016/j.corsci.2024.112227 ↗
8. Influence of grain boundary precipitates on intergranular corrosion behavior of 7050 Al alloys10.3390/coatings12020249 ↗
9. Microconstituent-induced pitting corrosion in aluminum alloy 2024-T310.5006/1.3292099 ↗
10. In-situ monitoring of pitting corrosion in aluminum alloy 202410.5006/1.3284873 ↗
11. The Effects of Microstructure and composition on Al alloy corrosion10.5006/1887 ↗
12. Mechanism for the morphological change from trenching to pitting around intermetallic particles in AA1050 aluminum10.1149/2.0331902jes ↗
13. Galvanic corrosion of AA5083/Fe in diluted synthetic seawater: effect of anodizing on local electrochemistry on and around Al6(Fe,Mn) on Al-matrix10.1149/1945-7111/ac5301 ↗
14. Corrosion of AA2024-T3 part II: Co-operative corrosion10.1016/j.corsci.2010.09.030 ↗
15. Difference in the precursory process of the intergranular corrosion of aged Al–Cu and Al–Cu–Mg alloys in 0.1 M NaCl10.1149/1945-7111/ad0666 ↗
16. Stability analysis of the Mg2Si phase in AA 6061 aluminum alloy10.1016/j.mspro.2012.06.074 ↗
17. Electrochemical behavior and localized corrosion associated with Mg2Si particles in Al and Mg alloys10.1149/2.002201eel ↗
18. Elucidation of the trigger for trenching around Al6(Fe, Mn) on AA5083 aluminum alloy in diluted synthetic seawater10.1016/j.corsci.2024.112362 ↗
19. SVET study of galvanic corrosion of Al/Mg2Si couple in aqueous solutions at different pH10.1149/2.0671706jes ↗
20. Clarifying the dissolution mechanisms and electrochemistry of Mg2Si as a function of solution pH10.1149/2.1061809jes ↗
21. Clarifying the role of Mg2Si and Si in localized corrosion of aluminum alloys by quasi in situ transmission electron microscopy10.5006/3457 ↗
22. Corrosion study of AA2024-T3 by scanning Kelvin probe force microscopy and in situ atomic force microscopy scratching10.1149/1.1838634 ↗
23. Integrated AFM and SECM for in situ studies of localized corrosion of Al alloys10.1016/j.electacta.2006.12.073 ↗
24. Real-time corrosion monitoring of aluminum alloy using scanning Kelvin probe force microscopy10.1149/1945-7111/ab8826 ↗
25. Corrosion susceptibility of passive films on 1060, 2024, and 5083 aluminum alloys: Experimental study and first-principles calculations10.1149/1945-7111/accab8 ↗
26. Understanding the effect of microstructure and composition on localized corrosion susceptibility of 6xxx aluminum alloys10.1038/s41529-024-00461-x ↗
27. Pit initiation mechanism at MnS inclusions in stainless steel: Synergistic effect of elemental sulfur and chloride ions10.1149/2.081310jes ↗
28. Micro-electrochemical aspects of the effects of temperature on pit initiation at MnS inclusion in Type 304 stainless steel10.1149/1945-7111/ac9d6c ↗
29. Morphological characteristics of trenching around MnS inclusions in Type 316 stainless steel: the role of molybdenum in pitting corrosion resistance10.1149/2.0131911jes ↗
30. Role of MnS in the intergranular corrosion and depassivation of sensitized Type 304 stainless steel10.1038/s41529-023-00419-5 ↗
31. Pitting at inclusions of the equiatomic CoCrFeMnNi alloy and improving corrosion resistance by potentiodynamic polarization in H2SO410.1016/j.corsci.2021.109748 ↗
32. Real-time microelectrochemical observations of very early stage pitting on ferrite-pearlite steel in chloride solutions10.1149/2.0801706jes ↗
33. Fabrication of a model specimen for understanding micro-galvanic corrosion at the boundary of α-Mg and β-Mg17Al1210.1016/j.jma.2022.10.020 ↗
34. In situ confocal laser scanning microscopy of AA 2024-T3 corrosion metrology: I. Localized corrosion of particles10.1149/1.1764780 ↗
35. Reducing subjectivity in EIS interpretation of corrosion and corrosion inhibition processes by in-situ optical analysis10.1016/j.electacta.2018.10.018 ↗
36. Transport processes and the mechanism of pitting of metals10.1149/1.2132857 ↗
37. Local corrosion chemistry–A review10.5006/2246 ↗
38. Sudden pH and Cl- concentration changes during the crevice corrosion of Type 430 stainless steel10.1149/1945-7111/ac9bda ↗
39. Microelectrochemical measurements of dissolution of MnS inclusions and morphological observation of metastable and stable pitting on stainless steel10.1149/1.2745639 ↗
40. A microelectrochemical system for in situ high-resolution optical microscopy: Morphological characteristics of pitting at MnS inclusion in stainless steel10.1149/2.054208jes ↗
41. Morphological change and open-circuit potential of single metastable Pit on AA1050 aluminum in NaCl solution10.1149/1945-7111/abdee9 ↗
42. Processing and precipitation strengthening of 6xxx series aluminium alloys: A review10.22271/27078221.2020.v1.i1a.10 ↗
43. Equilibrium composition variation of Q-phase precipitates in aluminum alloys10.1016/j.actamat.2017.07.048 ↗
44. Grain boundary structures and their correlation with intergranular corrosion in an extruded Al-Mg-Si-Cu alloy10.1016/j.matchar.2020.110695 ↗
45. K.A.Q. O'Reilly, Influence of Al grain structure on Fe bearing intermetallics during DC casting of an Al–Mg–Si alloy10.1016/j.matchar.2016.09.017 ↗
46. Effect of Cu content on corrosion behavior of 7xxx series aluminum alloys10.1149/1.1695385 ↗
47. Cerium addition to CaS inclusions in stainless steel: Insolubilizing water-soluble inclusions and improving pitting corrosion resistance10.1016/j.corsci.2020.109222 ↗
48. Micro-electrochemical insights into pit initiation site on aged UNS S32750 super duplex stainless steel10.1038/s41529-023-00335-8 ↗
49. Pitting corrosion characteristics of sintered Type 316 L stainless steel: relationship between pores and MnS10.1038/s41529-024-00482-6 ↗
50. Electrochemical properties of MnSe inclusions and improving the pitting corrosion resistance of stainless steel via Se microalloying10.1038/s41598-024-57995-y ↗
51. The contribution of hydrogen evolution processes during corrosion of aluminium and aluminium alloys investigated by potentiodynamic polarisation coupled with real-time hydrogen measurement10.1038/s41529-017-0011-4 ↗
52. On the electrochemical and quasi in situ corrosion response of the Q-Phase (AlxCuyMgzSiw) intermetallic particle in 6xxx series aluminum alloys10.5006/2249 ↗
53. Alkaline etching and desmutting of aluminium alloy: the behaviour of Mg2Si particles10.1016/j.jallcom.2020.155834 ↗