journal article·2025-04

Corrosion behaviour of magnesia-carbon refractories by high manganese steel melts

Jianhua Chu, Ziyi Cheng, Panjun Dou, Xi Pan, Ziming Wang, Yutong Li, Na Tao, Qiang Yue, Lizhong Chang

Corrosion Science· Volume 246
Publisher page

Abstract

The corrosion behaviour of MgO-C refractories by high manganese steel melt was investigated. The results demonstrated that corrosion mechanism of MgO-C refractories by manganese steel with a manganese content of less than 20 % is mainly decarburization reaction, while the corrosion for manganese content of 30 % is mainly reduction reaction of MgO by C and [Mn] as well as the penetration of Fe-Mn-Si melt, and the number of the MgO-rich inclusions significantly increase. The aluminium addition promotes the decarburization reaction, and the [Al] react with MgO directly to form Al 2O 3, follow by MgO·Al 2O 3 was generated at around the periclase in MgO-C refractories, and the inclusions mainly transform from TiN-AlN to TiN-MgO-AlN with MgO core.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors · Advanced Power Generation Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. A sustainable ultra-high strength Fe18Mn3Ti maraging steel through controlled solute segregation and alpha-Mn nanoprecipitation10.1038/s41467-022-30019-x ↗
2. Effect of solute atoms (C, Al and Si) on hydrogen embrittlement resistance of high-Mn TWIP steels10.1016/j.corsci.2022.110376 ↗
3. Insights into the role of grain refinement on high-temperature initial oxidation phase transformation and oxides evolution in high aluminium Fe-Mn-Al-C duplex lightweight steel10.1016/j.corsci.2017.07.002 ↗
4. Simultaneously enhancing strength-ductility synergy and strain hardenability via Si-alloying in medium-Al FeMnAlC lightweight steels10.1016/j.actamat.2022.118611 ↗
5. Achievement of high strength and plasticity product of the nugget zone in friction stir welded high-Mn steel via controlling stacking fault energy10.1016/j.msea.2022.144427 ↗
6. A reaction between high Mn-high Al steel and CaO-SiO2-type molten mold flux: Part I. Composition evolution in molten mold flux10.1007/s11663-012-9770-z ↗
7. Effects of Al addition on the reaction between high-manganese steel and CaO-SiO2-Al2O3-MgO slag10.1002/srin.202000143 ↗
8. Grain size dependence of hot deformation behaviors and resultant hot ductility in cryogenic high-manganese steel10.1016/j.msea.2024.146466 ↗
9. Oxidation mechanism of high-manganese heat-resistant steels reinforced by in situ second-phase particles10.1016/j.corsci.2023.111720 ↗
10. New insights into the properties of high-manganese steel10.1007/s12613-020-2166-1 ↗
11. Post-mortem analysis of alumina-magnesia-carbon refractory bricks used in steelmaking ladles10.1016/j.ceramint.2018.09.150 ↗
12. Degradation behavior of MgO-based refractory by CaO-SiO2-Al2O3-MgO-TiO2 system ladle slags10.1007/s11663-023-02901-6 ↗
13. Wettability between 304 stainless steel and refractory materials10.1016/j.jmrt.2020.03.103 ↗
14. Slag corrosion-resistance mechanism of lightweight magnesia-based refractories under a static magnetic field10.1016/j.corsci.2020.108517 ↗
15. Corrosion and penetration behaviors of slag/steel on the corroded interfaces of Al2O3-C refractories: role of Ti3AlC210.1016/j.corsci.2018.08.022 ↗
16. Hot corrosion behavior of Al2O3-Cr2O3 refractory by molten glass at 1200 °C under static condition10.1016/j.corsci.2015.10.004 ↗
17. Dynamic interaction of refractory and molten steel: effect of alumina-magnesia castables on alloy steel cleanness10.1016/j.ceramint.2018.08.327 ↗
18. Physical properties and corrosion resistance of magnesia-calcium hexaaluminate refractories to molten steel10.1016/j.ceramint.2022.09.288 ↗
19. Phase analysis of complex non-metallic inclusions in Al-deoxidized 42CrMo4 steel after contact with MgO-C refractories
20. Effect of refractory on nonmetallic inclusions in Al-killed steel10.1007/s11663-016-0746-2 ↗
21. The Effect of Refining slag and refractory on inclusion transformation in extra low oxygen steels10.1007/s11663-016-0592-2 ↗
22. Effect of MgO-Cr2O3 and MgO-MgAl2O4-based refractories on refractory–steel interface reaction and cleanliness of pipeline steel10.1007/s42243-023-01043-y ↗
23. Effect of refractory on nonmetallic inclusions in Si–Mn-Killed steel10.1002/srin.201900268 ↗
24. Improved slag corrosion resistance of MgO-C refractories with calcium magnesium aluminate aggregate and silicon carbide: corrosion behavior and thermodynamic simulation10.1016/j.jeurceramsoc.2023.08.033 ↗
25. Wetting and corrosion behavior between magnesia-carbon refractory and converter slags with different MgO contents10.1007/s42243-021-00695-y ↗
26. Interactions of alumina-based and magnesia-based refractories with iron melts and slags: a review10.1007/s11663-018-1300-1 ↗
27. Corrosion mechanism of novel MgO-Al3BC3 refractories in contact with converter slag10.1016/j.corsci.2024.111833 ↗
28. Reaction behaviors of Al-killed medium-manganese steel with glazed MgO refractory10.1007/s11663-018-1390-9 ↗
29. Corrosion behavior of CaO-Al2O3-SiO2-MgO-Cr2O3 slag on MgO refractory brick for smelting of chromite10.1016/j.jeurceramsoc.2023.09.019 ↗
30. Oxidizing decarbonization characteristics of MgO-C refractories for electric arc furnace steelmaking with CO2 utilization10.1016/j.ceramint.2022.08.260 ↗
31. Dissolution behavior of Mg from magnesia-chromite refractory into Al-killed molten steel10.1007/s11663-018-1301-0 ↗
32. Cathodoluminescence imaging for rapid identification of low-melting CaO-MgO-SiO2 phases in MgO-based refractories involving the steelmaking process10.1016/j.jeurceramsoc.2022.08.031 ↗
33. Impact of antioxidants in MgO-C refractory on steel cleanliness and refractory degradation
34. Steel/refractory/slag interfacial reaction and its effect on inclusions in high-Mn high-Al steel10.1016/j.ceramint.2021.09.194 ↗
35. Reaction mechanism between MgO crucible and AerMet100 steel during vacuum induction melting10.1016/j.ceramint.2022.04.257 ↗
36. Effect of Magnesia-Carbon Refractory on the Kinetics of MgO·Al2O3 spinel inclusion generation in extra-low oxygen steels10.1007/s11663-015-0540-6 ↗
37. Interaction of magnesia-carbon refractory with metallic iron under flash ironmaking conditions10.1016/j.jeurceramsoc.2019.09.019 ↗
38. Magnesia-carbon refractory dissolution in Al killed low carbon steel10.1179/174328106X113977 ↗
39. An experimental study of the interactions between liquid steel and a MgO-based tundish refractory
40. Corrosion behaviour of MgO-based refractories by different existence states of manganese-containing volatile phases10.1016/j.jeurceramsoc.2023.01.045 ↗
41. Corrosion of alumina-magnesia castable by high manganese steel with respect to steel cleanness10.1016/j.ceramint.2019.02.029 ↗
42. Transient evolution of non-metallic inclusions in molten high aluminum and high manganese steel contacting with slag and crucible: experimental investigation and FactSage macros modeling10.1016/j.jmrt.2023.06.025 ↗
43. reaction behaviors of Al-killed medium-manganese steel with different refractories10.1007/s11663-018-1223-x ↗
44. Raw materials, microstructure, and properties of MgO-C refractories: directions for refractory recipe development10.1016/j.jeurceramsoc.2022.09.032 ↗
45. Microstructure evolution and high-temperature oxidation behavior of low-carbon MgO-C refractories with TiB2 addition10.1016/j.ceramint.2024.10.338 ↗
46. High temperature mechanical and corrosion resistance of Fe-containing MgO-C refractory in oxidizing atmosphere10.1016/j.ceramint.2019.06.306 ↗
47. Liquid steel interaction with MgO-based refractories: a review functional materials2019, 26(2).10.15407/fm26.02.366 ↗
48. Study on the relationship between vacuum denitrification and manganese evaporation behaviours of manganese steel melts10.1016/j.vacuum.2021.110420 ↗
49. Mn evaporation and denitrification behaviors of molten Mn steel in the vacuum refining with slag process10.1007/s12613-021-2311-5 ↗
50. Characterization of nonmetallic inclusions in high-manganese and aluminum-alloyed austenitic steels10.1007/s11661-012-1088-6 ↗
51. Formation, evolution and remove behavior of manganese-containing inclusions in medium/high manganese steels10.1016/j.jmrt.2022.12.023 ↗
52. Effects of Mn content on the formation of inclusions in high aluminum steel10.1007/s11663-023-02866-6 ↗
53. Study of the formation of non-metallic inclusions by ladle glaze and the effect of slag on inclusion composition using tracer experiments
54. Effect of slag composition on the kinetics of formation of Al2O3-MgO inclusions in aluminum killed ferritic stainless steel10.2355/isijinternational.40.121 ↗
55. A study on the mechanism of reaction between refractory materials and aluminium deoxidised molten steel10.1002/srin.199700542 ↗