Flow, chloride, and pH effects on carbon steel corrosion in BWR cold shutdown: Development of a 4-STEP corrosion model

Gaku Yamazaki, Kazutoshi Fujiwara

Corrosion Science· Volume 253

Abstract

The corrosion behavior of carbon steel in Boiling Water Reactor (BWR) plants during cold shutdown was investigated under flow velocities of 0.1 and 2.0 m/s, chloride ion (Cl - ) concentrations of 0.01, 0.1, 1, and 10 mg/L, and pH of 6.3, 7.6, and 8.5. Experiments over 800 h demonstrated that a high flow velocity (2.0 m/s) promotes rapid passivation , while a low flow velocity (0.1 m/s) results in sustained corrosion. Cl - damaged protective films, accelerating corrosion, particularly under high flow velocity. Higher pH and/or electric conductivity increased uniform corrosion . The newly developed 4-STEP corrosion model successfully reproduced the experimental results.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Metallurgical Processes and Thermodynamics · Erosion and Abrasive Machining

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Revie · 2008
2. Iron pipe corrosion in distribution systems10.1002/j.1551-8833.2001.tb09246.x ↗
3. Prediction of corrosion rate for carbon steel using regression model with commercial LPR sensor data10.3390/app142310836 ↗
4. The effect of corrosion on the structural reliability of steel offshore structures10.1016/j.corsci.2005.04.004 ↗
5. Effect of velocity on corrosion of steel under water10.1021/ie50205a019 ↗
6. The effect of velocity on the corrosion of steel in sulfuric acid10.1021/ie50163a005 ↗
7. Corrosion of several materials for pump in flowing water containing chloride ion10.3323/jcorr1974.32.1_31 ↗
8. Corrosion behavior of carbon steel piping in flowing diluted seawater10.5006/3557 ↗
9. Effect of pH and chloride on the micro-mechanism of pitting corrosion for high strength pipeline steel in aerated NaCl solutions10.1016/j.apsusc.2015.05.053 ↗
10. Pitting corrosion on Fe-Cr alloys10.1016/S0010-938X(69)80051-X ↗
11. The role of chloride ions in pitting of carbon steel studied by the statistical analysis of electrochemical noise10.1016/S0169-4332(99)00328-1 ↗
12. Unmasking chloride attack on the passive film of metals10.1038/s41467-018-04942-x ↗
13. Characterization and prediction of carbon steel corrosion in diluted seawater containing pentaborate10.1016/j.jnucmat.2017.10.032 ↗
14. Passivity–the key to our metals-based civilization10.1351/pac199971060951 ↗
15. Influence of pH on corrosion behavior of carbon steel in simulated cooling water containing scale and corrosion inhibitors10.1002/maco.202011516 ↗
16. Corrosion of carbon steel in aqueous solution10.3323/jcorr.63.109 ↗
17. Effect of seawater salinity, pH, and temperature on external corrosion behavior and microhardness of offshore oil and gas pipeline: RSM modelling and optimization10.1038/s41598-024-67463-2 ↗
18. Effect of hydrogen-ion concentration on the submerged corrosion of steel10.1021/ie50175a002 ↗
19. Measurement of the Instantaneous Corrosion Rate By Means of Polarization Data10.5006/0010-9312-13.2.69 ↗
20. Corrosion film formation on carbon steels in bicarbonate solutions10.3323/jcorr.58.274 ↗
21. Atomic Energy Society of Japan, Water Chemistry Guidelines for Boiling Water Reactors: 2019, 2019..
22. Modeling of marine immersion corrosion for mild and low-alloy steels—part 1: phenomenological model10.5006/1.3277564 ↗
23. Film formation on mild steel and low alloy steels in aerated sea water10.2355/isijinternational1966.9.239 ↗
24. Metallographische mitteilungen aus dem institut für physikalische chemie der universität göttingen. CV. Die Geschwindigkeit der Einwirkung von Sauerstoff, Schwefelwasserstoff und Halogenen auf Metalle10.1002/zaac.19221230115 ↗
25. Initial oxidation rate of metals and the logarithmic equation10.1016/0001-6160(56)90051-7 ↗
26. The Rate of Film Formation on Metals10.1149/1.3071385 ↗
27. author_in_Japanese, room temperature oxidation of iron at low pressures10.3323/jcorr1954.14.2_72 ↗
28. Crack-heal mechanism of the growth of invisible films on metals10.1038/157732a0 ↗
29. Oxide film growth kinetics on metals and alloys: I. physical model10.1149/2.036306jes ↗
30. Low-temperature oxidation10.1007/BF00603582 ↗
31. Measurement of the anodic oxide film growth on iron for hours10.1149/1.2426654 ↗
32. A point defect model for anodic passive films: I. film growth kinetics10.1149/1.2127591 ↗
33. On the concentration at the electrodes in a solution, with special reference to the liberation of hydrogen by electrolysis of a mixture of copper sulphate and sulphuric acid10.1080/14786440109462590 ↗
34. Über anlauffarben von metallen10.1002/zaac.19201110107 ↗
35. Beitrag zur theorie des anlaufvorgangs10.1515/zpch-1933-2105 ↗
36. Theory of the oxidation of metals10.1088/0034-4885/12/1/308 ↗
37. Development of corrosion rate measuring apparatus for carbon steel under reducing environment10.3323/jcorr.60.374 ↗
38. Oxide film growth kinetics on metals and alloys: II. Numerical simulation of transient behavior10.1149/2.037306jes ↗
39. N.F. Mott, R.W. Gurney, Electronic Processes in Ionic Crystals, 2nd Eds., 1964.
40. A note on the theory of surface diffusion reactions10.1039/tf9484400796 ↗
41. Pitting corrosion of metals: a review of the critical factors10.1149/1.1838615 ↗
42. Passivity breakdown, pit initiation and propagation of pits in metallic materials – Review10.1016/j.corsci.2014.10.006 ↗
43. A review of trends for corrosion loss and pit depth in longer-term exposures10.3390/cmd1010004 ↗
44. A fundamental study of flow-accelerated corrosion in feedwater systems
45. External reference electrodes for use in high temperature aqueous systems10.1149/1.2129192 ↗
46. Fougerite and FeII–III hydroxycarbonate green rust; ordering, deprotonation and/or cation substitution; structure of hydrotalcite-like compounds and mythic ferrosic hydroxide Fe(OH)(2+x)10.1016/j.solidstatesciences.2005.02.001 ↗
47. Python Software Foundation, Python Language Reference, 2024. 〈https://www.python.org/〉.
48. others, SciPy 1.0: fundamental algorithms for scientific computing in python10.1038/s41592-019-0686-2 ↗
49. Bard · 2000
50. The interaction of oxygen with clean metal surfaces
51. Adsorption and oxide formation on aluminium films
52. The theory of the formation of protective oxide films on metals.—III10.1039/TF9474300429 ↗
53. Determination of kinetic parameters in the point defect model (PDM) for iron using electrochemical impedance spectroscopy and first-principles calculations10.1016/j.corsci.2025.112779 ↗
54. Model of physico-chemical effect on flow accelerated corrosion in power plant10.1016/j.corsci.2011.06.027 ↗
55. Japanese Standards Association, Japanese Industrial Standards (JIS) G 3456: 2024 -Carbon steel pipes for high temperature service-, (2024).
56. Physiochemical characterization of five iron tubercles from a single drinking water distribution system: possible new insights on their formation and growth10.1016/j.corsci.2008.05.005 ↗
57. Physico-chemical characteristics of corrosion scales in old iron pipes10.1016/S0043-1354(00)00591-1 ↗