journal article·2024-08

High-temperature corrosion behavior of 316 H stainless steel in lead-bismuth eutectic containing cesium

Jinwei Zhao, Youbin Wang, Pincheng Zeng, Zhonghui Liao, Qing Zou, Xinpeng Wang, Yuezhou Wei

Corrosion Science· Volume 236
Publisher page

Abstract

The influence of Cs on the corrosion of 316 H stainless steel pipework when exposed to liquid lead–bismuth eutectic (LBE) coolant, specifically LBE containing 0.5 wt% Cs at high temperature, is investigated. The addition of Cs in LBE can significantly accelerate the corrosion of 316 H stainless steel. Cs in LBE first destroys the Cr 2O 3 film on the surface of the stainless steel and reacts with Cr 23C 6 enriched at grain boundaries. Finally, the reaction between Cs and FeCr 2O 4 creates pores in inner oxide layer (IOL), thus destroying the protection provided to 316 H stainless steel by the IOL.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Thermodynamic and Structural Properties of Metals and Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. A review of steel corrosion by liquid lead and lead–bismuth10.1016/j.corsci.2009.03.013 ↗
2. High corrosion resistance of twin boundaries in medium-entropy alloy exposed to liquid lead-bismuth eutectic at 500 ℃: mechanism exploration by both experiment and first-principles calculation10.1016/j.corsci.2022.110865 ↗
3. Influence of temperature on the microstructural evolution of SIMP and T91 steels in liquid lead-bismuth eutectic: experiments and molecular dynamics simulations10.1016/j.corsci.2023.111411 ↗
4. Liquid metal corrosion of T91 and A316L materials in Pb–Bi eutectic at temperatures 400–600 ℃10.1016/j.corsci.2005.04.001 ↗
5. Microstructure, mechanical properties and lead-bismuth eutectic corrosion behavior of FeCrAlTiNb high-entropy alloy coatings10.1016/j.corsci.2023.111407 ↗
6. Point Defect Model for the kinetics of oxide film growth on the surface of T91 steel in contact with lead–bismuth eutectic10.1016/j.corsci.2022.110829 ↗
7. Revealing fretting corrosion synergistic mechanism of 316 stainless steel in liquid lead-bismuth eutectic (LBE)10.1016/j.corsci.2023.111058 ↗
8. Synergy of stress and corrosion in a 12Cr ferritic/martensitic steel exposed to static liquid lead-bismuth eutectic at 550℃10.1016/j.corsci.2023.111404 ↗
9. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
10. Corrosion behavior of T91 steel in liquid lead-bismuth eutectic at 550 ℃: Effects of exposure time and dissolved oxygen concentration10.1016/j.corsci.2022.110405 ↗
11. Selective leaching of nickel and chromium from Type 316 austenitic steel in oxygen-containing lead–bismuth eutectic (LBE)10.1016/j.corsci.2014.03.016 ↗
12. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 ℃10.1016/j.jnucmat.2017.04.004 ↗
13. Active control of oxygen in molten lead–bismuth eutectic systems to prevent steel corrosion and coolant contamination10.1016/S0022-3115(01)00713-9 ↗
14. Analysis of corrosion scale structure of pre-oxidized stainless steel 316 in molten lead bismuth eutectic and the relation to impedance spectroscopy response10.1016/j.jnucmat.2009.10.029 ↗
15. Transmission electron microscopy (TEM) on oxide layers formed on D9 stainless steel in lead bismuth eutectic (LBE)10.1016/j.corsci.2012.09.019 ↗
16. Quantification of the Long-Term Performance of Steels T91 and 316L in Oxygen-Containing Flowing Lead-Bismuth Eutectic at 550 ℃10.1115/1.4000364 ↗
17. Performance of the new ferritic/martensitic steel SIMP against liquid lead-bismuth eutectic corrosion: comparison with T91 and 316L steels10.1002/maco.202213372 ↗
18. Effect of lead-bismuth eutectic oxygen concentration on the onset of dissolution corrosion in 316 L austenitic stainless steel at 450 ℃10.1115/1.4039598 ↗
19. Temperature effect on the corrosion mechanism of austenitic and martensitic steels in lead–bismuth10.1016/S0022-3115(01)00723-1 ↗
20. Corrosion of stainless steels in lead–bismuth eutectic up to 600 ℃10.1016/j.jnucmat.2004.07.012 ↗
21. T91 cladding tubes with and without modified FeCrAlY coatings exposed in LBE at different flow, stress and temperature conditions10.1016/j.jnucmat.2008.02.026 ↗
22. Corrosion behavior of 410 stainless steel in flowing lead-bismuth eutectic alloy at 550℃10.1016/j.jnucmat.2019.05.029 ↗
23. Degradation of HT9 under simultaneous ion beam irradiation and liquid metal corrosion10.1016/j.jnucmat.2016.06.039 ↗
24. In-situ proton irradiation/lead-bismuth eutectic corrosion synergistic effect on corrosion behaviour of 11Cr1W1Si ferritic/martensitic steel10.1016/j.jnucmat.2022.154097 ↗
25. The chemical state of the fission products in oxide fuels10.1016/0022-3115(85)90460-X ↗
26. The effects of stress on corrosion behavior of SIMP martensitic steel in static liquid lead-bismuth eutectic10.1016/j.corsci.2021.109477 ↗
27. Cesium corrosion process in Fe–Cr steel10.1016/j.jnucmat.2013.05.055 ↗
28. Cs–Te corrosion depth dependence on distribution of chromium carbide precipitation in high chromium steel10.1080/00223131.2016.1214628 ↗
29. A proposed mechanism for internal cladding corrosion in LMFBR mixed oxide fuel pins10.1016/0022-3115(78)90448-8 ↗
30. 5.22 - Behavior of spallation, activation and fission products in LBE
31. Characterization of oxide layers grown on D9 austenitic stainless steel in lead bismuth eutectic10.1016/j.jnucmat.2007.12.005 ↗
32. Oxidation of SUS-316 stainless steel for fast breeder reactor fuel cladding under oxygen pressure controlled by Ni/NiO oxygen buffer10.1016/0022-3115(85)90432-5 ↗
33. Oxidation behavior of modified SUS316 (PNC316) stainless steel under low oxygen partial pressure10.1016/S0022-3115(02)00872-3 ↗
34. Characterization of corrosion phenomena and kinetics on T91 ferritic/martensitic steel exposed at 450 and 550 ℃ to flowing Pb-Bi eutectic with 10−7 mass% dissolved oxygen10.1016/j.jnucmat.2017.07.031 ↗
35. Corrosion of metallic materials in flowing liquid lead-bismuth