journal article·2026-01

Hydrogen trapping and embrittlement of a high-carbon steel after quenching and high-temperature tempering

Jiahao Zhu, Xiaoyuan Li, Wenchao Yu, Xiaofei He, Yongming Yan, Jie Shi, Maoqiu Wang

Corrosion Science· Volume 258
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Economic and environmental competitiveness of multiple hydrogen production pathways in China10.1038/s41467-025-59412-y ↗
2. Atomic mechanism and prediction of hydrogen embrittlement in iron10.1038/nmat3479 ↗
3. Strategies for improving the sustainability of structural metals10.1038/s41586-019-1702-5 ↗
4. Further study of the hydrogen embrittlement of martensitic advanced high-strength steel in simulated auto service conditions10.1016/j.corsci.2018.02.037 ↗
5. The role of retained austenite against hydrogen embrittlement and White etching area formation in bearing steel under dynamic loading10.1016/j.ijhydene.2024.01.155 ↗
6. Unveiling the nature of hydrogen embrittlement in bearing steels employing a new technique10.1016/j.scriptamat.2012.11.018 ↗
7. Study on hydrogen embrittlement during low-temperature tempering process of high-strength steel10.1016/j.ijhydene.2025.02.092 ↗
8. Improving the hydrogen embrittlement resistance by straining the ferrite / cementite interfaces10.1016/j.actamat.2024.119850 ↗
9. L. Vandewalle, T. Depover, K. Verbeken, Current state-of-the-art of hydrogen trapping by carbides: From theory to experiment, Int. J. Hydrog. Energy. 03 (2024) 266, https://doi.org/10.1016/j.ijhydene.2024.03.266.10.1016/j.ijhydene.2024.03.266 ↗
10. Effect of Ti, Mo and Cr based precipitates on the hydrogen trapping and embrittlement of Fe–C–X Q&T alloys10.1016/j.ijhydene.2015.06.157 ↗
11. Quantitative analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗
12. The effect of TiC on the hydrogen induced ductility loss and trapping behavior of Fe-C-Ti alloys10.1016/j.corsci.2016.07.013 ↗
13. Thermal desorption spectroscopy evaluation of the hydrogen-trapping capacity of NbC and NbN precipitates10.1007/s11661-013-2181-1 ↗
14. Evaluation of the effect of V4C3 precipitates on the hydrogen induced mechanical degradation in Fe-C-V alloys10.1016/j.msea.2016.08.053 ↗
15. The effect of undissolved and temper-induced (Ti,Mo)C precipitates on hydrogen embrittlement of quenched and tempered Cr-Mo steel10.1016/j.corsci.2019.108421 ↗
16. A first-principles study on the hydrogen trap characteristics of coherent nano-precipitates in α-Fe10.1016/j.ijhydene.2020.07.123 ↗
17. Atomistic insight into hydrogen trapping at MC/BCC-Fe phase boundaries: the role of local atomic environment10.1016/j.actamat.2021.116744 ↗
18. Numerical analysis of hydrogen trap state by TiC and V4C3 in bcc-Fe10.2355/isijinternational.52.1693 ↗
19. Ab-initio investigation of hydrogen trap state by cementite in bcc-Fe10.2355/isijinternational.53.709 ↗
20. Investigation of the effect of carbon on the reversible hydrogen trapping behavior in lab-cast martensitic FeC steels10.1016/j.matchar.2021.111671 ↗
21. Hydrogen trapping phenomena in carbon steel10.1007/BF00540409 ↗
22. Thermal desorption spectroscopy study of the interaction of hydrogen with TiC precipitates10.1007/s12540-013-4013-7 ↗
23. Precise determination of the activation energy for desorption of hydrogen in two Ti-added steels by a single thermal-desorption spectrum10.1007/s11663-004-0057-x ↗
24. Response of hydrogen trapping capability to microstructural change in tempered Fe–0.2C martensite10.1016/j.scriptamat.2004.11.008 ↗
25. The interaction of hydrogen and the cementite-ferrite interface in carbon steel10.1007/BF00543835 ↗
26. Difference in hydrogen trapping behaviors between epsilon carbide and cementite in steels10.1016/j.matchar.2024.114557 ↗
27. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
28. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
29. The role of cementite on the hydrogen embrittlement mechanism in martensitic medium-carbon steels10.1016/j.msea.2022.144204 ↗
30. Ab initio simulation of hydrogen-induced decohesion in cementite-containing microstructures10.1016/j.actamat.2018.03.005 ↗
31. Effect of uniform distribution of fine cementite on hydrogen embrittlement of low carbon martensitic steel plates10.2355/isijinternational.52.213 ↗
32. Effects of vanadium carbides on hydrogen embrittlement of tempered martensitic steel10.1007/s12540-016-5631-7 ↗
33. M4C3 precipitation in Fe-C-Mo-V steels and relationship to hydrogen trapping10.1098/rspa.2006.1688 ↗
34. Effect of pre-strain on critical conditions for hydrogen-induced delayed cracking and crack nucleation characteristic of DP1180 steel10.1016/j.corsci.2023.111749 ↗
35. Retained austenite and its measurement by X-ray diffraction
36. Factors influencing austenite stability during Inter-critical annealing and effect on mechanical properties of low-density medium mn steels10.1016/j.matchemphys.2025.130877 ↗
37. Hydrogen microprint technique in the study of hydrogen in steels10.1007/BF00556094 ↗
38. Enhancement of hydrogen embrittlement resistance in 310S austenitic stainless steel through ribbon-like δ-ferrite10.1016/j.corsci.2024.112086 ↗
39. Microstructure evolution and hydrogen embrittlement mechanism of a 2200 MPa press-hardened steel with tempering treatment10.1016/j.matchar.2025.114955 ↗
40. The effect of quench cracks and retained austenite on the hydrogen trapping capacity of high carbon martensitic steels10.1016/j.ijhydene.2021.02.057 ↗
41. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
42. Reaction kinetics in differential thermal analysis10.1021/ac60131a045 ↗
43. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
44. The effect of hydrogen release at room temperature on the ductility of steel wire rods for pre-stressed concrete10.1016/j.msea.2010.04.042 ↗
45. Crank · 1975
46. Stress-induced hydrogen redistribution and corresponding fracture behavior of Q960E steel at different hydrogen content10.1016/j.msea.2020.138963 ↗
47. Investigation of damage mechanisms related to microstructural features of ferrite-cementite steels via experiments and multiscale simulations10.1016/j.ijplas.2023.103745 ↗
48. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and “quasi-cleavage” fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
49. Atomic-scale insights on hydrogen trapping and exclusion at incoherent interfaces of nanoprecipitates in martensitic steels10.1038/s41467-022-31665-x ↗
50. Carbon segregation and cementite precipitation at grain boundaries in quenched and tempered lath martensite10.1016/j.msea.2022.144369 ↗
51. Enhancing the hydrogen embrittlement resistance of medium‑carbon high-strength steel by optimizing the tempering temperature10.1016/j.matchar.2023.113530 ↗
52. Review of the hydrogen embrittlement and interactions between hydrogen and microstructural interfaces in metallic alloys: grain boundary, twin boundary, and nano-precipitate10.1016/j.ijhydene.2024.05.257 ↗
53. Model-based interpretation of thermal desorption spectra of Fe-C-Ti alloys10.1016/j.jallcom.2019.03.102 ↗
54. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
55. Modeling hydrogen transport by dislocations10.1016/j.jmps.2015.03.002 ↗
56. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
57. Influence of hydrogen-enhanced plasticity and decohesion mechanisms of hydrogen embrittlement on the fracture resistance of steel10.1016/j.engfailanal.2021.105312 ↗
58. Prediction of hydrogen-assisted fracture under coexistence of hydrogen-enhanced plasticity and decohesion10.1016/j.ijhydene.2023.06.033 ↗