A gradient NiCoCrAlYSiB coating was prepared on a Ni-base superalloy using arc ion plating (AIP) and subsequent gaseous phase aluminisation techniques. Hot corrosion of normal NiCoCrAlYSiB and the gradient coating in pure Na(2)SO(4) and Na(2)SO(4)/NaCl (75:25, wt./wt.) salts was performed at 900 degrees C in static air. The corrosion results indicated an enhanced corrosion resistance to both salts for the gradient NiCoCrAlYSiB coating, which the improved performance of it should be attributed to the beta aluminide "pool" at the surface layer. By partially sacrificing Al(2)O(3) (i.e. Al), the gradient NiCoCrAlYSiB coating specimen behaved excellently in the two kinds of salts. The grain growth during the gaseous phase aluminisation and the corrosion mechanism, including the role NaCl played in the mixture salt corrosion, are discussed. (C) 2009 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Whittle · 1978 · 109
2. Oxidation and hot corrosion behavior of sputtered nanocrystalline coating of superalloy K5210.1016/j.tsf.2007.07.131 ↗
3. The effect of an enamel coating on the oxidation and hot corrosion behavior of an HVOF-sprayed CoNi-CrAlY coating10.1023/A:1023619222906 ↗
4. Functionally gradient ceramic/metallic coatings for gas turbine components by high-energy beams for high-temperature applications10.1023/A:1004675900887 ↗
5. Alloy design strategies for promoting protective oxide-scale formation10.1007/s11837-000-0109-x ↗
6. Graded materials for resistance to contact deformation and damage10.1126/science.1059716 ↗
7. Oxidation and hot corrosion behavior of gradient NiCoCrAlYSiB coatings deposited by a combination of arc ion plating and magnetron sputtering techniques10.1016/j.corsci.2005.09.014 ↗
8. Smart overlay coatings — concept and practice10.1016/S0257-8972(01)01499-2 ↗
9. High-temperature oxidation and hot-corrosion behavior of a sputtered NiCrAlY coating with and without aluminizing10.1016/j.surfcoat.2005.10.042 ↗
10. Coatings for gas turbine materials and long term stability issues10.1016/j.matdes.2004.02.005 ↗
11. Aluminizing and chromizing bed treatment by CVD in a fluidized bed reactor on austenitic stainless steels10.1016/S0257-8972(99)00355-2 ↗
12. Preparation and cyclic oxidation of gradient NiCrAlYRe coatings on Ni-based superalloys10.1016/j.surfcoat.2008.04.049 ↗
13. NiCoCrAlY coatings with and without an Al2O3/Al interlayer on an orthorhombic Ti2AlNb-based alloy: Oxidation and interdiffusion behaviors10.1016/j.actamat.2006.09.044 ↗
14. Hot corrosion behavior of MCrAlY coatings on IN738LC10.1016/j.surfcoat.2006.03.043 ↗
15. Hot corrosion behavior of AIP NiCoCrAlY(SiB) coatings on nickel base superalloys10.1016/j.surfcoat.2003.12.020 ↗
16. Goward · Oxid. Met. · 1971 · 3 · 47510.1007/BF00604047 ↗
17. Thermodynamic assessment of the Al---Ni system10.1016/S0925-8388(96)02652-7 ↗
18. The control of the composition and structure of aluminide layers formed by vapour aluminising10.1016/S0257-8972(99)00347-3 ↗
19. Corrosion behaviour of AIP NiCoCrAlYSiB coating in salt spray tests10.1016/j.corsci.2007.09.004 ↗
20. Hot corrosion in gas turbine components10.1016/S1350-6307(00)00035-2 ↗
21. Vanadic and chloride attack of superalloys10.1080/02670836.1987.11782265 ↗
22. Evaluation of arc ion plated NiCoCrAlYSiB coatings after oxidation at 900–1100 °C10.1016/j.surfcoat.2005.04.055 ↗
23. Structure and hot - corrosion resistance properties of M38 superalloy in laser- irradiated zones
24. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
25. Synergistic dissolution of oxides in molten sodium sulfate10.1149/1.2086647 ↗
26. Rapp · Whitney Award Lecture, Corrosion-NACE · 1986 · 42 · 56810.5006/1.3583026 ↗
27. Identification of hot corrosion resistant MCrAlY based bond coatings for gas turbine engine applications10.1016/S0257-8972(00)01156-7 ↗
28. A comparative study of oxidation and hot corrosion of a cast nickel base superalloy in different corrosive environments10.1016/S0167-577X(96)00109-7 ↗
29. Accelerated oxidation rate of chromium induced by. sodium chloride10.1007/BF00659274 ↗
30. Jianting · 1982
31. Morphological development of subscale formation in Fe–Cr–(Ni) alloys with chloride and sulfates coating10.1023/A:1020119107724 ↗