journal article·2006-03

Thermodynamic and kinetic consideration on the corrosion of Fe, Ni and Cr beneath a molten KCl–ZnCl2 mixture

Andreas Ruh, Michael Spiegel

Corrosion Science· Volume 48· Issue 3
Publisher page

Abstract

Abstract Thermogravimetric (TG) experiments have been carried out to study the kinetics of hot corrosion of Fe, Cr and Ni, covered by a molten KCl–ZnCl 2 mixture of a composition close to the eutectic (50 mol% KCl–50 mol% ZnCl 2 ). Furthermore binary and ternary phase diagrams were calculated in order to describe the corrosion process. The tests were conducted at a temperature of 320 °C in an atmosphere consisting of argon and oxygen. For iron different stages are observed in a TG curve. They can be attributed to the different reaction steps of iron chloride formation (incubation phase), oxide precipitation (linear stage) and scale formation (parabolic or logarithmic stage). Based on these observations a model, described by Spiegel [A. Spiegel, Molten Salt Forum 7 (2003) 253], is confirmed. For Cr and Ni these stages are not observed. At 8 vol% O 2 only slight oxidation of Cr and Ni was observed accompanied by evaporation of the salt deposit. At 16 vol% O 2 the rate of oxidation increases and the experiments yield a curve that is either parabolic or logarithmic for both Ni and Cr. As a result it is shown that the solubility of iron chloride in the KCl–ZnCl 2 melt is higher than the solubility of nickel chloride and chromium (III) chloride in the KCl–ZnCl 2 melt. This enables a higher diffusibility of iron chloride to the upper region of the melt where a higher oxygen partial pressure ( p (O 2 )) is present leading to a higher oxidation rate of iron.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Molten salt chemistry and electrochemical processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. Spiegel · Molten Salt Forum · 2003 · 7 · 253
2. Sorrell · Mater. High Temp. · 1997 · 14 · 20710.1080/09603409.1997.11689546 ↗
3. Kofstad · 1988
4. Rapp · Metall. Mater. Trans. A · 2000 · 31A · 210510.1007/s11661-000-0128-9 ↗
5. Reese · Mater. Corros. · 1992 · 43 · 54710.1002/maco.19920431202 ↗
6. Reese · Mater. Corros. · 1993 · 44 · 4110.1002/maco.19930440204 ↗
7. Lee · Metall. Trans. · 1987 · 18A · 109910.1007/BF02668559 ↗
8. Li · High Temp. Corros. Protect. Mater. · 2004 · 6 · 1047
9. Shu · Oxid. Met. · 2000 · 54 · 45710.1023/A:1004690518225 ↗
10. Li · Mater. Sci. Eng. A · 2003 · 345 · 6410.1016/S0921-5093(02)00386-6 ↗
11. Ruh · High Temp. Corros. Protect. Mater. · 2004 · 6 · 61
12. Bale · Calphad · 2002 · 26 · 18910.1016/S0364-5916(02)00035-4 ↗