Corrosion and scaling as interrelated phenomena in an operating geothermal power plant
Source abstract
Abstract
This study refers to an experimental research and contributes to a better understanding of corrosion and scaling in an operating geothermal power plant (Soultz-sous-Forets, France). An in situ physicochemical monitoring program has been performed in order to characterise the processed brine. In situ and laboratory corrosion experiments were performed using conventional and candidate metals (mild steels, CrNiMo alloys, and non-ferrous metals). Mild steels exhibit long-term corrosion rates below 0.2 mm/year, accompanied by scaling formation offering protection. Conventional stainless steels 430F and 316L undergo pitting corrosion, while higher alloyed materials were identified to be suited for geothermal service.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Calcium Carbonate Crystallization and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Chemistry and materials in geothermal systems
2. The use of potential-pH diagrams for the interpretation of corrosion phenomena in high salinity geothermal brines10.5006/0010-9312-35.1.1 ↗
3. Ellis · 1977
4. D.W. DeBerry, P.F. Ellis, C.C. Thomas, Material Selection Guidelines for Geothermal Power Systems, first ed., ALO-3904-1, EG-77-C-04-3904, US Department of, Energy, 1978.10.2172/6356102 ↗
5. J.P. Carter, S.D. Cramer, Materials of Construction for High-Salinity Geothermal Brines, U.S. Department of the Interior, Report of Investigations 8792, 1992.
6. R.K. Conrad, J.P. Carter, S.D. Cramer, Corrosion of Selected Metals and a High-Temperature Thermoplastic in Hypersaline Geothermal Brine, U.S. Department of the Interior, Report of Investigations 8792, 1983.
7. Titanium in the geothermal industry10.1016/j.geothermics.2003.08.004 ↗
8. On-line corrosion monitoring in geothermal district heating systems. I. General corrosion rates10.1016/j.corsci.2005.06.019 ↗
9. Corrosion resistance of different steel grades in the geothermal fluid of Molasse Basin
10. R. Bäßler, A. Burkert, R. Kirchheiner, A. Saadat, M. Finke, Proceedings of NACE Corrosion 2009, Paper No. 09377, NACE International, Atlanta 2009.
11. Effect of CO2 and H2S on the composition and stability of passive film on iron alloys in geothermal water10.1016/j.electacta.2007.01.086 ↗
12. F.X. McCawley, S.D. Cramer, W.D. Riley, J.P. Carter, P.B. Needham, Corrosion of Materials and Scaling in Low-Salinity East Mesa Geothermal Brines, U.S. Department of the Interior, Report of Investigations 8504, 1981.10.2172/6883071 ↗
13. F. Baticci, A. Genter, P. Huttenloch, R. Zorn, Corrosion and Scaling Detection in the Soultz EGS Power Plant, Upper Rhine Graben (France), in: Proceedings World Geothermal Congress 2010, Bali, Indonesia, 25–29 April 2010.
14. Metal corrosion in geothermal brine environments in the upper rhine graben - laboratory and in-situ studies -10.1016/j.geothermics.2012.10.006 ↗
15. Treatment methods for geothermal brines
16. Geochemistry of geothermal fluids and well scales, and potential for mineral recovery10.1016/S0169-1368(98)00004-3 ↗
17. Characteristics of corrosions scales on steels in a CO2-saturated NaCl brine10.5006/1.3585227 ↗
18. A. Genter, D. Fritsch, N. Cuenot, J. Baumgaertner, J.-J. Graff, Overview of the current activities of the European EGS Soultz project: from exploration to electricity production, in: Proceedings 34th Workshop on Geothermal Reservoir Engineering, Stanford University, California, 2009.
19. J. Scheiber, F. Nitschke, A. Seibt, A. Genter, Geochemical and mineralogical monitoring of the geothermal power plant in Soultz-sous-Forêts (France), in: Proceedings 37th Workshop on Geothermal Reservoir Engineering, Stanford University, California, 2012.
20. Material selection guidelines for geothermal power systems – An overview
21. The chemistry of geothermal waters: its effects on exploitation10.1111/j.1365-3121.1991.tb00183.x ↗
22. Chemistry and isotopes of deep geothermal saline fluids in the Upper Rhine Graben: origin of compounds and water-rock interactions10.1016/0016-7037(93)90387-C ↗
23. Main characteristics of the deep geothermal brine (5km) at Soultz-sous-Forêts (France) determined using geochemical and tracer test data10.1016/j.crte.2009.10.009 ↗
24. Reactions of pipeline steels in carbon dioxide solutions10.1016/S0010-938X(98)00104-8 ↗
25. The influence of microstructure and chemical composition of carbon and low alloy steels in CO2 corrosion: a state-of-the-art appraisal10.1016/S0261-3069(03)00158-4 ↗
26. Formation Characteristic of CO2 corrosion product layer of API P110 steel investigated by SEM and electrochemical techniques10.1016/S1006-706X(09)60067-4 ↗
27. Corrosion of API N80 carbon steel in oil field formation water containing CO2 in the absence and presence of acetic acid10.1016/j.corsci.2011.05.059 ↗
28. Corrosion of unalloyed and low alloyed steels in carbonic acid solution10.1002/maco.19780290402 ↗
29. C. De Warrd, U. Lozt, Prediction of CO2 corrosion of carbon steel, Corrosion/93 NACE, Paper No. 69, NACE International, Houston, TX, 1993.10.5006/C1993-93069 ↗
30. An XPS characterization of FeCO3 films from CO2 corrosion10.1016/S0010-938X(98)00180-2 ↗
31. Solubility product of siderite10.1016/j.chemgeo.2009.03.015 ↗
32. A. Roine, Outokumpu HSC Chemistry®6.0 User’s Guide Volume 1/2 – Chemical Reaction and Equilibrium Software with Extensive Thermochemical Database and Flowsheet Simulation Outokumpu Research Finland, 2006.
33. J. Han, Galvanic Mechanism of Localized Corrosion for Mild Steel in Carbon Dioxide Environments, Ph.D Thesis, Department of Chemical and Biomolecular Engineering, Russ College of Engineering and Technology of Ohio University, 2009.
34. Chemistry and structure of the passive film on mild steel in CO2 corrosion environments10.1021/ie801819y ↗
35. Effect of temperature in CO2 corrosion of carbon steel10.1002/sia.3057 ↗
36. M.R. Hoffmann, Brine Chemistry – Scaling and Corrosion, Geothermal Research Study in the Salton Sea Region of California, California Institute of Technology, 1975.10.2172/7364728 ↗
37. Sedriks · 1979
38. G.T. Burstein, Electrochemistry of Pit Formation, Electrochemical Society Joint International Meeting, Honolulu, 2004.
39. Pitting corrosion of stainless steels10.1002/maco.19960470104 ↗
40. A general model for the repassivation potential as a function of multiple aqueous solution species10.1016/j.corsci.2003.10.002 ↗
41. B. Sanjuan, Soultz EGS Pilot Plant Exploitation – Phase III: Scientific Program about In-situ Operations of Geochemical Monitoring and Tracing (2010–2013). First Yearly Progress Report BRGM/RP-59902-FR, 2011, 92 pp.
42. B. Sanjuan, Soultz EGS Pilot Plant Exploitation – Phase III: Scientific Program about In-situ Operations of Geochemical Monitoring and Tracing (2010–2013). Second Yearly Progress Report BRGM/RP-61030-FR, 2012, 48 pp.
43. S. Gentier, X. Rachez, M. Peter, A. Blaisonneau, B. Sanjuan, Transport and Flow Modelling of the Deep Geothermal Exchanger Between Wells at Soultz-sous-Forêts (France), in, Proceedings of the Geothermal Research Council (GRC) Annual Meeting, San Diego, USA, 2011, 12 pp.
44. H. Surbeck, Assessment of Radiological Risks at the Geothermal Pilot Plant Soultz-sous-Forêts. First results. CHYN technical report, University of Neuchâtel, Switzerland, 2008.
45. ASTM G 1-03: Standard practice for preparing, cleaning, and evaluating corrosion test specimens, in: G.S. Haynes, R. Baboian (Eds.) Laboratory Corrosion Tests and Standards. ASTM Committee G-1 on Corrosion of Metals, ASTM Special Technical Publication, vol. 866, 1985.10.1520/STP866-EB ↗
46. C. Thornton, C. Cooper, Overmatching Superalloy Consumable Inco-weld® 686CPT® Broadens its Applications to Include Welding Super Austenitic and Super Duplex Stainless Steels, Stainless Steel World 2004 © 2004 KCI Publishing BV. .
47. Corrosion degradation of pipeline carbon steels subjected to geothermal plant conditions10.1108/00035591011058165 ↗
48. Microelectrochemical heterogeneity of Ferritic–Pearlitic structures
49. Iron corrosion by novel anaerobic microorganisms10.1038/nature02321 ↗
50. Effect of CO2 on the stability of steels with 1% and 13% Cr in saline water10.1016/j.corsci.2009.01.025 ↗
51. A mechanistic model for carbon dioxide corrosion of mild steel in the presence of protective iron carbonate films—Part III: The film growth model10.5006/1.3277592 ↗
52. S.N. Karlsdottir, Corrosion, scaling and material selection in geothermal power production, in: A. Sayigh (Ed.), Comprehensive Renewable Energy, vol. 7 Geothermal Energy, Elsevier Publishing, 2012, pp. 239–258.10.1016/B978-0-08-087872-0.00706-X ↗