journal article·2008-01

Recession behavior of Yb2Si2O7 phase under high speed steam jet at high temperatures

Shunkichi Ueno, Tatsuki Ohji, Hua-Tay Lin

Corrosion Science· Volume 50· Issue 1
Publisher page

Abstract

Abstract Recession behavior of Yb 2 Si 2 O 7 phase was examined under high speed steam jet environment between 1300 °C and 1500 °C. Yb 2 SiO 5 phase was formed on the bulk surface by the decomposition of Yb 2 Si 2 O 7 phase and the elimination of silica component at elevated temperatures. The phase ratio of Yb 2 SiO 5 /Yb 2 Si 2 O 7 increased up to 1400 °C and then decreased above 1400 °C. The relative intensity of 2 2 0 peak for Yb 2 Si 2 O 7 phase increased with increasing the temperatures. Fine grains were generated on the bulk surface at 1300 °C. The phase decomposition caused on the grain interior. A porous structure was formed on the bulk surface during the test at 1400 °C. Surface cracks were generated for 1400 °C test sample. A smooth surface was generated on the surface of 1500 °C test sample. The triple points of the grains were bridged with a glassy phase.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Engineering and Material Science Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Water vapor effects on high-temperature oxidation and volatilization of ceramics10.1111/j.1151-2916.2003.tb03458.x ↗
2. Additive effects on Si3N4 oxidation/volatilization in water vapor10.1111/j.1151-2916.2003.tb03462.x ↗
3. High-temperature stability of SiC-based composites in high-water-vapor-pressure environments10.1111/j.1151-2916.2003.tb03463.x ↗
4. T. Fukudome, S. Tsuruzono, W. Karasawa, Y. Ichikawa, Development and evaluation of ceramic components for gas turbine, in: Proceedings of 2002 ASME TURBO EXPO, Power for Land, Sea and Air, GT2002-30627.10.1115/GT2002-30627 ↗
5. Mechanical reliability evaluation of silicon nitride ceramic components after exposure in industrial gas turbines10.1016/S0955-2219(02)00146-2 ↗
6. H.T. Lin, M.K. Ferber, Evaluation of mechanical reliability of silicon nitride vanes after field tests in an industrial gas turbine, in: Proceedings of 2002 ASME TURBO EXPO, Power for Land, Sea and Air, GT2002-30629.10.1115/GT2002-30629 ↗
7. Characterization of first-stage silicon nitride components after expose to an industrial gas turbine10.1111/j.1551-2916.2005.00678.x ↗
8. S. Ueno, N. Kondo, D.D. Jayaseelan, T. Ohji, S. Kanzaki, High temperature hydro corrosion resistance of silica based oxide ceramics, in: Proceedings of 2003 ASME TURBO EXPO, Power for Land, Sea and Air, GT2003-38878.10.1115/GT2003-38878 ↗
9. Development of oxide-based EBC for silicon nitride10.1111/j.1744-7402.2004.tb00187.x ↗
10. Environmental characterization of monolithic ceramics for gas turbine applications10.4028/www.scientific.net/KEM.287.367 ↗
11. Water vapor corrosion of mullite containing small amount of sodium10.1016/j.ceramint.2004.03.044 ↗
12. Corrosion and oxidation behavior of ASiO4 (A=Ti, Zr and Hf) and silicon nitride with an HfSiO4 environmental barrier coating
13. S. Ueno, D.D. Jayaseelan, T. Ohji, Water vapor corrosion of lutetium silicates at high temperature, Ceram. Int., in press.
14. I. Yuri, T. Hisamatsu, Recession rate prediction for ceramic materials in combustion gas flow, in: Proceedings of 2003 ASME TURBO EXPO, Power for Land, Sea and Air, GT2003-38886.10.1115/GT2003-38886 ↗