Cerium tartrate as a corrosion inhibitor for AA 2024-T3
Source abstract
Abstract
Abstract A new corrosion inhibitor, cerium tartrate, was synthetized. The inhibition behavior of cerium tartrate for 2024-T3 aluminum alloy was investigated in 0.05 M NaCl solution. The immersion tests indicate that the corrosion of Al2CuMg phase was well inhibited. The electrochemical results show that both anodic and cathodic inhibitions are present during the corrosion process. The surface characterizations reveal that the protective film of cerium tartrate inhibits the dealloying of Al2CuMg phase in the initial stage, and then cerium ions transform to cerium oxide/hydroxides and appear at the Al2CuMg phase, blocking the further corrosion at those corrosion sites.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Anodic Oxide Films and Nanostructures · Nanoporous metals and alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Corrosion of AA2024-T3. Part I: localized corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
2. Local dissolution phenomena associated with S phase (Al2CuMg) particles in aluminum alloy 2024-T310.1149/1.1837874 ↗
3. Electrochemical techniques for practical evaluation of corrosion inhibitor effectiveness. Performance of cerium nitrate as corrosion inhibitor for AA2024T3 alloy10.1016/j.corsci.2010.06.012 ↗
4. Synthesis and characterization of cerium molybdate nanocontainers and their inhibitor complexes10.1111/j.1551-2916.2009.03310.x ↗
5. High effective organic corrosion inhibitors for 2024 aluminium alloy10.1016/j.electacta.2007.05.058 ↗
6. Double-doped zeolites for corrosion protection of aluminium alloys10.1016/j.micromeso.2014.01.004 ↗
7. 2-Hydroxy-4-methoxy-acetophenone as an environment-friendly corrosion inhibitor for AZ91D magnesium alloy10.1016/j.corsci.2013.04.005 ↗
8. Localized corrosion of 2024 T351 aluminium alloy in chloride media10.1016/S0010-938X(98)00116-4 ↗
9. Nanostructured sol–gel coatings doped with cerium nitrate as pre-treatments for AA2024-T3: corrosion protection performance10.1016/j.electacta.2005.04.021 ↗
10. Evaluation of corrosion inhibition in mild steel using cerium oxide nanoparticles10.1016/j.matlet.2012.09.051 ↗
11. Effect of ambient aging on inhibition of oxygen reduction by chromate conversion coatings10.5006/1.3277568 ↗
12. Improved corrosion performance of electrophoretic coatings by silane addition10.1016/j.corsci.2011.11.018 ↗
13. Inhibition of 5083 aluminium alloy and galvanised steel by lanthanide salts10.1016/S0010-938X(00)00051-2 ↗
14. Electrochemical noise applied to the study of the inhibition effect of CeCl3 on the corrosion behaviour of Al–Mg alloy AA5083 in seawater10.1016/S0013-4686(01)00871-4 ↗
15. Comparison between the inhibition efficiencies of Ce(III) and Ce(IV) ammonium nitrates against corrosion of AA2024 aluminum alloy in solutions of low chloride concentration10.1016/j.corsci.2012.03.039 ↗
16. Corrosion behavior of rare earth cerium based conversion coating on aluminum alloy10.1016/S1002-0721(10)60338-9 ↗
17. Influence of oxidizing ability of the medium on the growth of lanthanide layers on galvanized steel10.1016/j.corsci.2010.01.011 ↗
18. Electrochemical study of inhibitor-containing organic–inorganic hybrid coatings on AA202410.1016/j.corsci.2009.02.018 ↗
19. Studies of formation of ceriumrich protective films using X-ray adsorption near-edge spectroscopy and rotating disk electrode methods10.1149/1.1836400 ↗
20. Inhibition of AA2024-T3 on a phase-by-phase basis using an environmentally benign inhibitor, cerium dibutyl phosphate10.1149/1.2073672 ↗
21. Cerium dibutylphosphate as a corrosion inhibitor for AA2024-T3 aluminum alloys10.1149/1.2217260 ↗
22. High-throughput channel arrays for inhibitor testing: proof of concept for AA2024-T310.1016/j.corsci.2009.06.038 ↗
23. TiOx self-assembled networks prepared by templating approach as nanostructured reservoirs for self-healing anticorrosion pre-treatments10.1016/j.elecom.2005.12.019 ↗
24. Two new layered complexes supported by helical {VO3}n−n chains: hydrothermal syntheses and crystal structures of [M(dpa)V2O6] (M=Zn(II) and Cu(II); dpa=2,20-dipyridylamine)10.1016/j.inoche.2008.01.016 ↗
25. Corrosion inhibition performance of polypyrrole Al flake composite coatings for Al alloys10.1016/j.corsci.2012.12.019 ↗
26. Quantum chemical studies on inhibition effect of amino acids and hydroxy carboxylic acids on pitting corrosion of aluminium alloy 7075 in NaCl solution10.1016/j.theochem.2005.01.048 ↗
27. The inhibition effect of amino acids and hydroxy carboxylic acids on pitting corrosion of aluminum alloy 707510.1016/S0010-938X(00)00135-9 ↗
28. The characterisation and performance of Ce(dbp)3-inhibited epoxy coatings10.1016/j.porgcoat.2010.10.009 ↗
29. Corrosion protection of AA2024-T3 using rare earth diphenyl phosphates10.1016/j.electacta.2006.11.028 ↗
30. Corrosion protection of aluminium alloy 2024-T3 in 0.05 M NaCl by cerium cinnamate10.1016/j.corsci.2011.03.012 ↗
31. Cerium cinnamate as an environmentally benign inhibitor pigment for epoxy coatings on AA 2024-T310.1016/j.porgcoat.2014.01.003 ↗
32. Wiberg · 2001
33. Statistical study of the corrosion behavior of Al2CuMg intermetallics in AA2024-T351 by SKPFM10.1149/1.2799089 ↗
34. Synthesis and characterization of cerium citric and tartaric complexes10.1016/j.jallcom.2007.01.005 ↗
35. Electrochemical features during pitting corrosion of LY12 aluminium alloy in different neutral solutions
36. Electrochemical study on carbon steel corrosion process in alkaline sour media10.1016/S0013-4686(02)00090-7 ↗
37. Determination of coating deterioration with EIS. 2. Development of a method for field testing of protective coatings10.5006/1.3316106 ↗
38. Simulating corrosion of Al2CuMg phase by measuring ionic currents, chloride concentration and pH10.1016/j.corsci.2014.07.021 ↗
39. Mechanism of corrosion inhibition of AA2024 by rare-earth compounds10.1021/jp0560664 ↗
40. The effect of post-treatment time and temperature on cerium-based conversion coatings on Al 2024-T310.1016/j.corsci.2009.09.023 ↗
41. Interaction of carboxylic acids with the oxyhydroxide surface of aluminium: poly(acrylic acid), acetic acid and propionic acid on pseudoboehmite10.1016/S0368-2048(01)00324-3 ↗
42. Unravelling the corrosion inhibition mechanisms of bi-functional inhibitors by EIS and SEM-EDS10.1016/j.corsci.2012.12.018 ↗