journal article·2012-06

Study of corrosion performance of electrodeposited nanocrystalline Zn–Ni alloy coatings

S.H. Mosavat, M.H. Shariat, M.E. Bahrololoom

Corrosion Science· Volume 59
Publisher page

Abstract

Abstract The corrosion performance of nanocrystalline Zn–Ni alloy coatings electrodeposited from an alkaline bath using direct current has been investigated using EIS and polarization curves technique. Performance of these nanocrystalline alloy coatings with various Ni content was compared to that of microcrystalline Zn–Ni alloy. The corrosion product formed on the nanocrystalline Zn–Ni alloy coatings is stable and protective which proves to be better compared with microcrystalline. The nanocrystalline Zn–Ni alloy with 17.62 wt.% Ni and grain size 37 nm gives the best performance of the Zn–Ni alloy coatings tested. The corrosion resistance of nanocrystalline alloy coatings depends on the chemical compositions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Corrosion Behavior and Inhibition · Electrochemical Analysis and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Nanocrystalline materials10.1016/0079-6425(89)90001-7 ↗
2. Electroseposited nanocrystals, properties and industrial application10.1016/0965-9773(95)00114-X ↗
3. Electrodeposition of nanostructured coatings and their characterization – a review10.1088/1468-6996/9/4/043001 ↗
4. Electrodeposited nanocrystalline materials
5. Electrochemical corrosion behavior of nanocrystalline materials – a review10.1016/S1005-0302(10)60001-1 ↗
6. Effect of grain size on corrosion of nanocrystalline copper in NaOH solution10.1016/j.corsci.2010.06.029 ↗
7. Improving the corrosion and tribocorrosion resistance of Ni–Co nanocrystalline coatings in NaOH solution10.1016/j.corsci.2009.06.026 ↗
8. Effect of surface nanocrystallization on corrosion and corrosion inhibition of low carbon steel: synergistic effect of methionine and iodide ion10.1016/j.electacta.2007.05.023 ↗
9. Enhancement of the electrochemical behavior for Cu–70Zr alloy by grain refinement10.1016/j.surfcoat.2006.07.208 ↗
10. Improved corrosion behavior of nanocrystalline Cu–20Zr film in HCl solution10.1016/j.tsf.2006.01.009 ↗
11. Electrodeposited zinc–nickel alloy coatings – a review
12. Electrodeposited zinc alloy coatings10.1016/0010-938X(93)90345-H ↗
13. The corrosion resistance of electrodeposited zinc–nickel alloy coatings10.1016/0010-938X(93)90347-J ↗
14. The role of texture and morphology in optimizing the corrosion resistance of zinc-based electrogalvanized coatings10.1016/S0010-938X(97)00148-0 ↗
15. Zinc alloy plating for the automotive industry10.1016/0026-0576(96)82103-9 ↗
16. Alternatives to cadmium coating for electrical/electronic applications
17. Improved components for advanced alkaline water electrolysis10.1016/0360-3199(88)90014-6 ↗
18. Zinc alloy plating, metal finishing guidebook10.1016/0026-0576(95)93382-C ↗
19. Zinc–nickel electroplate as a replacement for cadmium on high-strength steels
20. Development of Zn–Ni alloy plated steel sheets10.2355/isijinternational1966.23.923 ↗
21. Electrodeposition of nickel–zinc alloys
22. Corrosion resistance of zinc–nickel alloy coatings in industrial production10.1016/0257-8972(95)02668-1 ↗
23. The microstructure of electrodeposited Zn–Ni coatings10.1016/0036-9748(89)90064-1 ↗
24. Hardness of electrodeposited microcrystalline and nanocrystalline γ-phase Zn–Ni alloys10.1016/S1359-6462(00)00680-1 ↗
25. Synthesis of nanocrystalline Zn–Ni alloy coatings10.1007/BF00240808 ↗
26. Investigation of nanocrystalline zinc–nickel alloy coatings in an alkaline zincate bath10.1016/j.surfcoat.2004.04.062 ↗
27. Electrodeposition of nanocrystalline Zn–Ni alloy from alkaline glycinate bath containing saccharin as additive10.1016/j.apsusc.2011.03.017 ↗
28. Kelly · 2003
29. Corrosion properties of pulse-plated zinc–nickel alloy coatings10.5006/1.3292081 ↗
30. Azaroff · 1968
31. Electrochemical deposition of zinc–nickel alloy coatings in a polyligand alkaline bath10.1016/j.surfcoat.2008.08.067 ↗
32. M.S. Chandrasekar, S. Srinivasan, M. Pushpavanam, Properties of zinc alloy electrodeposits produced from acid and alkaline electrolytes, J. Solid State Electrochem. 13 (2009) 781–789.10.1007/s10008-008-0607-2 ↗
33. Influence of structure factor on corrosion rate of functional Zn–Ni coatings10.1016/S1463-0184(02)00045-X ↗
34. The behavior of corrosion products on zinc in sodium chloride solution10.1016/0010-938X(85)90070-8 ↗
35. EIS behavior of anodized zinc in chloride environments10.1016/S0010-938X(99)00129-8 ↗
36. EIS study of the corrosion behaviour of zinc-based coatings on steel in quiescent 3% NaCl solution. Part 1: directly exposed coatings10.1016/j.corsci.2003.09.032 ↗
37. Barsoukov · 2005
38. The corrosion behaviour of nanocrystalline nickel10.1016/0956-716X(91)90171-V ↗
39. Effect of nanocrystalline grain size on the electrochemical and corrosion behavior of nickel10.1016/j.corsci.2004.04.007 ↗
40. Improved corrosion behavior of nanocrystalline zinc produced by pulse–current electrodeposition10.1016/S0010-938X(03)00142-2 ↗
41. Corrosion of nanocrystalline Ni–W alloys in alkaline and acidic 3.5wt.% NaCl solutions10.1016/j.corsci.2010.12.001 ↗