Abstract
High-temperature corrosion in the superheater of a large-scale waste-to-energy plant was investigated. A comparison of nickel-/iron-based alloys and austenitic stainless steel probes placed in the furnace demonstrated that temperature and particle deposition greatly influence corrosion. Nickel-based alloys performed better than the other metal alloys, though an aluminide coating further increased their corrosion resistance. Sacrificial baffles provided additional room for deposit accumulation, resulting in vigorous deposit-induced corrosion. Computational modelling (FLUENT code) was used to simulate flow characteristics and heat transfer. This study has shown that the use of aluminide coatings is a promising technique for minimising superheater corrosion in such facilities.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Thermochemical Biomass Conversion Processes · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Utilizing biomass and waste for power production – a decade of contributing to the understanding, interpretation and analysis of deposits and corrosion products10.1016/j.fuel.2004.08.026 ↗
2. High temperature corrosion in a 65 MW waste to energy plant10.1016/j.fuproc.2007.06.031 ↗
3. Analysis of failures in boiler tubes due to fireside corrosion in a waste heat recovery boiler10.1016/S1350-6307(02)00030-4 ↗
4. Streiff · 1987
5. High temperature corrosion in energy systems10.1016/0025-5416(81)90082-3 ↗
6. Hot corrosion of some superalloys and role of high-velocity oxy-fuel spray coatings – a review10.1016/j.surfcoat.2004.10.056 ↗
7. Stability of protective oxide films in waste incineration environment – solubility measurement of oxides in molten chlorides10.1016/S0010-938X(01)00059-2 ↗
8. Future integrated waste, energy and pollution management (WEP) systems exploit pyrotechnology10.1205/095758200530899 ↗
9. Influence of deposit formation on corrosion at a straw-fired boiler10.1016/S0378-3820(00)00063-1 ↗
10. Accelerated corrosion of pure Fe, Ni, Cr and several Fe-based alloys induced by ZnCl2–KCl at 450°C in oxidizing environment10.1016/S0921-5093(02)00386-6 ↗
11. A comparative study of the cyclic thermal oxidation of PVD nickel aluminide coatings10.1016/S0257-8972(02)00025-7 ↗
12. Synthesis and characterisation of pack cemented aluminide coatings on metals10.1016/j.apsusc.2004.04.026 ↗
13. The effect of NaCl deposit and thermal cycle on an aluminide layer coated on 310 stainless steel10.1016/j.matchemphys.2004.11.035 ↗
14. Thermal reaction modelling of a large municipal solid waste incinerator10.1080/00102200490504526 ↗
15. Converting moving-grate incineration from combustion to gasification – numerical simulation of the burning characteristics10.1016/j.wasman.2006.03.014 ↗
16. High temperature corrosion mechanisms and effect of alloying elements for materials used in waste incineration environment10.1016/S0010-938X(01)00058-0 ↗
17. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
18. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700°C10.1016/S0010-938X(99)00142-0 ↗
19. The corrosion of INCONEL alloy 740 in simulated environments for pulverized coal-fired boiler10.1016/j.matchemphys.2004.04.006 ↗
20. Callister · 2007
21. Schweitzer · 2007
22. Municipal solid waste combustion ash: state-of-the-knowledge10.1016/0304-3894(95)00120-4 ↗
23. Characterization of refuse-derived char from municipal solid waste: 2. Occurrence, abundance and source of trace elements10.1016/S0378-3820(99)00018-1 ↗
24. High temperature corrosion of coatings and boiler steels below chlorine-containing salt deposits10.1016/j.corsci.2003.09.026 ↗
25. P. Rademakers, W. Hesseling, J. van der Wetering, Review on Corrosion in Waste Incinerators, and Possible Effect of Bromine (2002) TNO Industrial Technology. Report No. I02/01333/RAD CEF-12.