The stress corrosion cracking behavior of austenitic stainless steels in boiling magnesium chloride solutions
Source abstract
Abstract
Abstract The change in the mechanism of stress corrosion cracking with test temperature for Type 304, 310 and 316 austenitic stainless steels was investigated in boiling saturated magnesium chloride solutions using a constant load method. Three parameters (time to failure; t f , steady-state elongation rate; l ss and transition time at which a linear increase in elongation starts to deviate; t ss ) obtained from the corrosion elongation curve showed clearly three regions; stress-dominated, stress corrosion cracking-dominated and corrosion-dominated regions. In the stress corrosion cracking-dominated region the fracture mode of type 304 and 316 steels was transgranular at higher temperatures of 416 and 428 K, respectively, but was intergranular at a lower temperature of 408 K. Type 310 steel showed no intergranular fracture but only transgranular fracture. The relationship between log l ss and log t f for three steels became good straight lines irrespective of applied stress. The slope depended upon fracture mode; −2 for transgranular mode and −1 for intergranular mode. On the basis of the results obtained, it was estimated that intergranular cracking was resulted from hydrogen embrittlement due to strain-induced formation of martensite along the grain boundaries, while transgranular cracking took place by propagating cracks nucleated at slip steps by dissolution.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Hoar · Proceeding of the Royal Society · 1962 · A268 · 30410.1098/rspa.1962.0142 ↗
2. Hoar · Journal of Electrochemistry · 1964 · 111 · 34810.1149/1.2426120 ↗
3. Nishimura · Corrosion Science · 2004 · 46 · 34310.1016/S0010-938X(03)00154-9 ↗
4. Nakayama · Corrosion · 1986 · 42 · 1010.5006/1.3584873 ↗
5. Whiteman · Corrosion · 1965 · 21 · 5310.5006/0010-9312-21.2.53 ↗
6. Holzworth · Corrosion · 1969 · 25 · 10710.5006/0010-9312-25.3.107 ↗
7. Rhodes · Corrosion · 1969 · 25 · 46210.5006/0010-9312-25.11.462 ↗
8. Hanninen · Metallurgical Transactions A · 1979 · 10A · 119610.1007/BF02811667 ↗
9. Narita · Metallurgical Transactions A · 1982 · 13A · 135510.1007/BF02642872 ↗
10. The role of hydrogen in stress corrosion cracking
11. Alyousif · Corrosion Science · 2006 · 48 · 428310.1016/j.corsci.2006.01.014 ↗
12. Nishimura · Corrosion · 1989 · 45 · 30810.5006/1.3577859 ↗
13. Nishimura · Corrosion Science · 1993 · 34 · 185910.1016/0010-938X(93)90023-A ↗
14. Briant · Metallurgical Transactions A · 1979 · 10A · 18110.1007/BF02817627 ↗
15. Sun · Acta Metallurgica · 1989 · 37 · 217110.1016/0001-6160(89)90142-9 ↗
16. Birley · Corrosion · 1971 · 27 · 6310.5006/0010-9312-27.2.63 ↗
17. Perng · Acta Metallurgica · 1986 · 34 · 177110.1016/0001-6160(86)90123-9 ↗
18. Hanninen · Corrosion · 1980 · 36 · 4710.5006/0010-9312-36.1.47 ↗
19. Nishimura · Corrosion · 1990 · 46 · 31110.5006/1.3585109 ↗
20. Diffusion and the dislocation sweeping mechanism
21. Reed-Hill · 1973
22. Nishimura · Corrosion Science · 2003 · 45 · 46510.1016/S0010-938X(02)00132-4 ↗
23. Nishimura · Corrosion Science · 1993 · 34 · 146310.1016/0010-938X(93)90241-8 ↗